• Title/Summary/Keyword: Ru-Ni based catalyst

Search Result 13, Processing Time 0.021 seconds

Ru-NiOx nanohybrids on TiO2 support prepared by impregnation-reduction method for efficient hydrogenation of lactose to lactitol

  • Mishra, Dinesh Kumar;Dabbawala, Aasif A.;Truong, Cong Chien;Alhassan, Saeed M.;Jegal, Jonggeon;Hwang, Jin Soo
    • Journal of Industrial and Engineering Chemistry
    • /
    • v.68
    • /
    • pp.325-334
    • /
    • 2018
  • Lactose is a reducing disaccharide consisting of two different monosaccharides such as galactose and glucose. The hydrogenation of lactose to lactitol is a formidable challenge because it is a complex process and several side products are formed. In this work, we synthesized Ru-Ni bimetallic nanohybrids as efficient catalysts for selective lactose hydrogenation to give selective lactitol. Ru-Ni bimetallic nanohybrids with $Ru-NiO_x$ (x = 1, 5, and 10 wt%) are prepared by impregnating Ru and Ni salts precursors with $TiO_2$ used as support material. Ru-Ni bimetallic nanohybrids (represented as $5Ru-5NiO/TiO_2$) catalyst is found to exhibit the remarkably high selectivity of lactitol (99.4%) and turnover frequency i.e. ($374h^{-1}$). In contrast, monometallic $Ru/TiO_2$ catalyst shows poor performance with ($TOF=251h^{-1}$). The detailed characterizations confirmed a strong interaction between Ru and NiO species, demonstrating a synergistic effect on the improvement on lactitol selectivity. The impregnation-reduction method for the preparation of bimetallic $Ru-NiO/TiO_2$ catalyst promoted Ru nanoparticles dispersed on NiO and intensified the interaction between Ru and NiO species. $Ru-NiO/TiO_2$ efficiently catalyzed the hydrogenation of lactose to lactitol with high yield/selectivity at almost complete conversion of lactose at $120^{\circ}C$ and 55 bar of hydrogen ($H_2$) pressure. Moreover, $Ru-NiO/TiO_2$ catalyst could also be easily recovered and reused up to four runs without notable change in original activity.

Steam reforming of biomass tar over Ni/Ru-x/Al2O3 catalysts (Ni/Ru-x/Al2O3 촉매를 이용한 바이오매스 타르 개질)

  • Yoon, Sang Jun;Oh, Kun Woong;Park, Seo Yoon;Kim, Yong Gu;Seo, Myung Won;Ra, Ho Won;Lee, Jae-Goo
    • 한국연소학회:학술대회논문집
    • /
    • 2014.11a
    • /
    • pp.355-356
    • /
    • 2014
  • Catalytic steam reforming of tar produced from biomass gasification was conducted using several Ni-based catalysts. K and Mn were used as a promoter over $Ni/Ru/Al_2O_3$ catalyst. The pellet and monolith type catalysts were prepared and applied to lab and bench-scale biomass gasification system. The $Ni/Ru-K/Al_2O_3$ catalyst shown higher performance than $Ni/Ru-Mn/Al_2O_3$ catalyst at low temperature range.

  • PDF

Tar Reforming for Biomass Gasification by Ru/$Al_2O_3$ catalyst (Ru/$Al_2O_3$ 촉매를 이용한 바이오매스 타르 개질 특성)

  • Park, Yeong-Su;Kim, Woo-Hyun;Keel, Sang-In;Yun, Jin-Han;Min, Tai-Jin;Roh, Seon-Ah
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2008.05a
    • /
    • pp.247-250
    • /
    • 2008
  • Biomass gasification is a promising technology for producing a fuel gas which is useful for power generation systems. In biomass gasification processes, tar formation often causes some problems such as pipeline plugging. Thus, proper tar treatment is necessary. So far, nickel (Ni)-based catalysts have been intensively studied for the catalytic tar removal. However, the deactivation of Ni-based catalysts takes place because of coke deposition and sintering of Ni metal particles. To overcome these problems, we have been using ruthenium (Ru)-based catalyst for tar removal. It is reported by Okada et al., that a Ru/$Al_2O_3$ catalyst is very effective for preventing the carbon deposition during the steam reforming of hydrocarbons. Also, this catalyst is more active than the Ni-based catalyst at a low steam to carbon ratio (S/C). Benzene was used for the tar model compound because it is the main constituent of biomass tar and also because it represents a stable aromatic structure apparent in tar formed in biomass gasification processes. The steam reforming process transforms hydrocarbons into gaseous mixtures constituted of carbon dioxide ($CO_2$), carbon monoxide (CO), methane ($CH_4$) and hydrogen ($H_2$).

  • PDF

Mid-Temperature Operation Characteristics of Commercial Reforming Catalysts: Comparison of Ru-Based and Ni-Based Catalyst (상용 개질촉매의 중온 영역 운전 특성: Ru 촉매와 Ni 촉매 비교)

  • KIM, YOUNGSANG;LEE, KANGHUN;LEE, DONGKEUN;LEE, YOUNGDUK;AHN, KOOKYOUNG
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.32 no.3
    • /
    • pp.149-155
    • /
    • 2021
  • Most of the reformer experiments have been conducted only in high-temperature operation conditions above 700℃. However, to design high efficiency solid oxide fuel cell, it is necessary to test actual reaction performance in mid-temperature (550℃) operation areas. In order to study the operation characteristics and performance of commercial reforming catalysts, a reforming performance experiment was conducted on mid-temperature. The catalysts used in this study are Ni-based FCR-4 and Ru-based RuA, RuAL. Experiments were conducted with a Steam-to-carbon ratio of 2.0 to 3.0 under gas hourly space velocity (GHSV) 2,000 to 5,000 hr-1. As a result, RuA and RuAL catalysts showed similar gas composition to the equilibrium regardless of the reforming temperature. However, the FCR-4 catalyst showed a lower hydrogen yield compared to the equilibrium under high GHSV conditions.

Steam Reforming of Tar Produced from Biomass Gasification Using Ni/Ru-X/Al2O3 (X=K or Mn) Catalyst (Ni/Ru-X/Al2O3 (X=K or Mn) 촉매를 이용한 바이오매스 가스화 타르의 수증기개질)

  • Oh, Gunung;Park, Seo Yoon;Lee, Jae-Goo;Kim, Yong Ku;Ra, Ho Won;Seo, Myung Won;Yoon, Sang Jun
    • Clean Technology
    • /
    • v.22 no.1
    • /
    • pp.53-61
    • /
    • 2016
  • Steam reforming of tar produced from biomass gasification was conducted using several Ni-based catalysts. In labscale, the catalytic steam reforming of toluene which is a major component of biomass tar was studied. A fixed bed reactor was used at various temperatures of 400-800 ℃. Ru (0.6 wt%) and Mn or K (1 wt%) were applied as a promoter in Ni based catalysts. Generally, Ni/Ru-K/Al2O3 catalyst shows higher performance on steam reforming of toluene than Ni/Ru-Mn/Al2O3 catalyst. Used catalysts were analyzed by XRD and TGA to detect sintering and carbon deposition. Base on the lab-scale studies, the monolith and pellet type catalysts were tested in 1 ton/day scale biomass gasification system. Ni/Ru-K/Al2O3 monolith catalyst shows high tar reforming performance at high temperature. In addition, Ni/Ru-Mn/Al2O3 monolith catalyst was showed deactivation with operation time. Reforming performance of Ni/Ru-K/Al2O3 pellet catalyst which showed 66.7% tar conversion at 587 ℃ was compared to regenerated one. Overall, Ni/Ru-K/Al2O3 pellet catalyst shows higher stability and performance than other used catalysts.

Effect of Promoter with Ru and Pd on Hydrogen Production over Ni/CeO2-ZrO2 Catalyst in Steam Reforming of Methane (메탄의 수증기 개질 반응에서 Ni/CeO2-ZrO2 촉매의 수소 생산에 대한 Ru 및 Pd의 조촉매 효과)

  • In Ho Seong;Kyung Tae Cho;Jong Dae Lee
    • Applied Chemistry for Engineering
    • /
    • v.35 no.2
    • /
    • pp.134-139
    • /
    • 2024
  • In the steam reforming of methane reactions, the effect of adding noble metals Ru and Pd to a Ni-based catalyst as promoters was analyzed in terms of catalytic activity and hydrogen production. The synthesized catalysts were coated on the surface of a honeycomb-structured metal monolith to perform steam methane reforming reactions. The catalysts were characterized by XRD, TPR, and SEM, and after the reforming reaction, the gas composition was analyzed by GC to measure methane conversion, hydrogen yield, and CO selectivity. The addition of 0.5 wt% Ru improved the reduction properties of the Ni catalyst and exhibited enhanced catalytic activity with a methane conversion of 99.91%. In addition, reaction characteristics were analyzed according to various process conditions. Methane conversion of over 90% and hydrogen yield of more than 3.3 were achieved at a reaction temperature of 800 ℃, a gas hourly space velocity (GHSV) of less than 10000 h-1, and a ratio of H2O to CH4 (S/C) higher than 3.

Activity test of post-reforming catalyst for removing the ethylene in diesel ATR reformate (디젤 자열개질 가스 내 포함된 $C_2H_4$ 제거를 위한 후개질기 촉매 활성 실험)

  • Yoon, Sang-Ho;Bae, Joong-Myeon;Lee, Sang-Ho
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2009.11a
    • /
    • pp.218-221
    • /
    • 2009
  • Solid oxide fuel cells (SOFCs), as high-temperature fuel cells, have various advantages. In some merits of SOFCs, high temperature operation can lead to the capability for internal reforming, providing fuel flexibility. SOFCs can directly use CH4 and CO as fuels with sufficient steam feeds. However, hydrocarbons heavier than CH4, such as ethylene, ethane, and propane, induce carbon deposition on the Ni-based anodes of SOFCs. In the case of the ethylene steam reforming reaction on a Ni-based catalyst, the rate of carbon deposition is faster than among other hydrocarbons, even aromatics. In the reformates of heavy hydrocarbons (diesel, gasoline, kerosene and JP-8), the concentration of ethylene is usually higher than other low hydrocarbons such as methane, propane and butane. It is importatnt that ethylene in the reformate is removed for stlable operation of SOFCs. A new methodology, termed post-reforming was introduced for removing low hydrocarbons from the reformate gas stream. In this work, activity tests of some post-reforming catalysts, such as CGO-Ru, CGO-Ni, and CGO-Pt, are investigated. CGO-Pt catalyst is not good for removing ethylene due to low conversion of ethylene and low selectivity of ethylene dehydrogenation. The other hand, CGO-Ru and CGO-Ni catalysts show good ethylene conversion, and CGO-Ni catalyst shows the best reaction selectivity of ethylene dehydrogenation.

  • PDF

Effect of Promoter on the Decomposition of Eco-Frendly Liquid Monopropellant on Cu/hexaaluminate Pellet Catalyst (Cu/hexaaluminate 펠렛 촉매를 이용한 친환경 액체 추진제 분해 반응에 미치는 조촉매의 영향)

  • Kim, Munjeong;Kim, Wooram;Jo, Young Min;Jeon, Jong Ki
    • Clean Technology
    • /
    • v.26 no.3
    • /
    • pp.196-203
    • /
    • 2020
  • In this study, a Cu/hexaaluminate catalyst was prepared by a co-precipitation method, and then a binder was added to form a pellet. A catalyst in which Ni and Ru promoters were added to a Cu/hexaaluminate pellet catalyst was prepared. This study focused on examining the effect of the addition of Ni and Ru promoters on the properties of Cu/hexaaluminate catalysts and the decomposition reaction of ADN-based liquid monopropellants. Cu/hexaaluminate catalysts had few micropores and well-developed mesopores. When Ru was added as a promoter to the Cu/hexaaluminate pellet catalyst, the pore volume and pore size increased significantly. In the thermal decomposition reaction of ADN-based liquid monopropellant, the decomposition onset temperature was 170.2 ℃. Meanwhile, the decomposition onset temperature was significantly reduced to 93.5 ℃ when the Cu/hexaaluminate pellet catalyst was employed. When 1% or 3% of Ru were added as a promoter, the decomposition onset temperatures of ADN-based liquid monopropellant were lowered to 91.0 ℃ and 83.3 ℃, respectively. This means that the Ru promoter is effective in lowering the decomposition onset temperature of the ADN-based liquid monopropellant because the Ru metal has excellent activity in the decomposition reaction of ADN-based liquid monopropellant, simultaneously contributing to the increase of the pore volume and pore size. After the thermal treatment at 1,200 ℃ and decomposition of ADN-based liquid monopropellant were repeatedly performed, it was confirmed that the addition of Ru could enhance the heat resistance of the Cu/hexaaluminate pellet catalyst.

A Study on Ammonia Formation with Nitrogen Impurity at a Natural Gas Steam Reforming Catalytic Process (소량의 질소를 포함한 천연가스 수증기 개질 반응에서 GHSV 변화에 따른 암모니아 생성 반응에 관한 연구)

  • KIM, CHUL-MIN;PARK, SANG-HYOUN;LEE, JUHAN;LEE, SANGYONG
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.30 no.6
    • /
    • pp.601-607
    • /
    • 2019
  • Ammonia would be formed in natural gas containing small amount of nitrogen reforming process in the process natural gas, which might damage the Pt catalyst and Prox catalyst. In the article, the effect of nitrogen contents on the formation of ammonia in the reforming process has been studied. In the experiments, Ru based and Ni based catalysts were used and the concentration of ammonia in the reformate gas at various gas hourly space velocity was measured. Experimental result shows that relatively higher ammonia concentration was measured with Ru based catalyst than with Ni based catalyst. It also shows that the concentration of ammonia increased rapidly after most of the methane converted into hydrogen. Based on the experimental results to reduce ammonia concentration it might be better to finish methane conversion at the exit position of the reforming reactor to minimize the contact time of catalyst and nitrogen with high concentration of hydrogen.

[ $CH_4$ ] steam reforming over Ni-Ru bimetallic catalysts (Ni-Ru 계열 촉매 상에서의 $CH_4$ 수증기 개질 반응)

  • Jeong Jin Hyeok;Lee Jung Won;Lee Duek Ki;Kim Dong Hyun;Seo Dong Joo;Seo Yutek;Yoon Wang Lei
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 2005.06a
    • /
    • pp.256-259
    • /
    • 2005
  • 본 연구에서는 기존 니켈 활성성분만의 알루미나담지 촉매에 비해 고온에서의 수소를 사용한 환원 전처리 과정을 거치지 않고도 높은 반응활성을 나타내며, 반응 중 탄소침적에 대한 촉매 저항성에서도 우수한 결과를 나타낸 루테늄-니켈 촉매에 대해보고 하고자 한다. 메탄 수증기 개질 반응을 통해, 루테늄을 최종적으로 담지한 알루미나 담지니켈계 촉매는 별도의 전처리과정 없이 $650^{\circ}C$에서부터 높은 반응성을 보였으며, 루테늄과 니켈을 동시에 담지한 경우보다 더 우수한 활성을 나타내었다. Ru의 담지량을 달리한 실험에서는$RU(0.5)/Ni(20)/Al_2O_3$ 촉매가 가장 높은 활성을 보였다. $H_2-TPR$ 분석 결과, $Ru(0.5)/Ni(20)/A1_2O_3$촉매의 경우 세 가지 환원 피크가 나타났으며, $Ni(20)/A1_2O_3$촉매와 비교해 볼 때, 저온(<$130^{\circ}C)$에서 환원가능한 $RUO_2$의 존재를 확인할 수 있었다. 담지된 RU은 분산도가 높아, XRD분석 결과에서 Ru이나 $RuO_2$의 특성 피크가 존재하지 않았다. 또한 $650^{\circ}C$에서 10시간 개질반응 후 얻어진 촉매에 대해 $O_2-TGA$를 분석한 결과, $Ni(20)/Al_2O_3$촉매는 $-7.2wt\%$ 정도의 큰 무게 감소를 보였으며, 이는 촉매 표면에 생성된 carbon tube에 의한 것임을 SEM 분석을 통해 알 수 있었다 이에 반해, $Ru(0.5)/Ni(20)/Al_2O_$ 촉매는 $O_2-TGA$$0.3wt\%$ 정도 무게 증가에 그쳤으며, SEM 분석상 carbon tube의 생성이 크게 억제되었음을 알 수 있었다.

  • PDF