• Title/Summary/Keyword: Recombination lifetime

Search Result 72, Processing Time 0.023 seconds

Study on the Passivation of Si Surface by Incorporation of Nitrogen in Al2O3 Thin Films Grown by Atomic Layer Deposition (원자층 증착법으로 형성된 Al2O3 박막의 질소 도핑에 따른 실리콘 표면의 부동화 특성 연구)

  • Hong, Hee Kyeung;Heo, Jaeyeong
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.22 no.4
    • /
    • pp.111-115
    • /
    • 2015
  • To improve the efficiency of the Si solar cell, high minority carrier life time is required. Therefore, the passivation technology is important to eliminate point defects on the silicon surface, causing the loss of minority carrier recombination. PECVD or post-annealing of thermally-grown $SiO_2$ is commonly used to form the passivation layer, but a high-temperature process and low thermal stability is a critical factor of low minority carrier lifetime. In this study, atomic layer deposition was used to grow the $Al_2O_3$ passivation layer at low temperature process. $Al_2O_3$ was selected as a passivation layer which has a low surface recombination velocity because of the fixed charge density. For the high charge density, an improved minority carrier lifetime, and a low surface recombination, nitrogen was doped in the $Al_2O_3$ thin film and the improvement of passivation was studied.

Transport Properties of Conversion Materials for Digital Radiography

  • Kim, Jae-Hyung;Park, Chang-Hee;Nam, Sang-Hee
    • Transactions on Electrical and Electronic Materials
    • /
    • v.8 no.6
    • /
    • pp.250-254
    • /
    • 2007
  • Applying the moving photo-carrier grating(MPG) technique and time-of-flight(TOF) measurements, we studied the transport properties of stabilized amorphous selenium typical of the material used in direct conversion X-ray imaging devices. For MPG measurement, we obtained electron and hole mobility and the recombination lifetime of $\alpha-Se$ films with arsenic(As) additions. We found an apparent increase in hole drift mobility and recombination lifetime, especially when 0.3 % As was added into $\alpha-Se$ film, whereas electron mobility decreased with the addition of As due to the defect density. For TOF measurement, a laser beam with pulse duration of 5 ns and wavelength of 350 nm was illuminated on the surface of $\alpha-Se$ with a thickness of 400 ${\mu}m$. The measured hole and electron transit times were about 8.73 ${\mu}s$ and 229.17 ${\mu}s$, respectively.

Transport parameters in a-Se:As films for digital X-ray conversion material using the moving-photocarrier-grating technique

  • Park, Chang-Hee;Kim, Jeong-Bae;Kim, Jae-Hyung;Nam, Sang-Hee
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.11a
    • /
    • pp.305-306
    • /
    • 2005
  • The effects of As addition In amorphous selenium (a-Se) films for digital X-ray conversion material have been studied using the moving photocarrier grating (MPG) technique We have found an increase in hole drift mobility and recombination lifetime, especially when 0.3% As is added into a-Se film, whereas electron mobility decreases with As addition due to the defect density. The transport properties for As doped a-Se films obtained by using MPG technique have been compared with X-ray sensitivity for a-Se:As X-ray device. The fabricated a-Se (0.3%As) based X-ray detector exhibited the highest X-ray sensitivity of 5 samples.

  • PDF

Delayed auger recombination in silicon measured by time-resolved X-ray scattering

  • Jo, Wonhyuk;Landahl, Eric C.;Kim, Seongheun;Lee, Dong Ryeol;Lee, Sooheyong
    • Current Applied Physics
    • /
    • v.18 no.11
    • /
    • pp.1230-1234
    • /
    • 2018
  • We report a new method of measuring the non-radiative recombination rate in bulk Silicon. Synchrotron timeresolved x-ray scattering (TRXS) combines femtometer spatial sensitivity with nanosecond time resolution to record the temporal evolution of a crystal lattice following intense ultrafast laser excitation. Modeling this data requires an Auger recombination time that is considerably slower than previous measurements, which were made at lower laser intensities while probing only a relatively shallow surface depth. We attribute this difference to an enhanced Coulomb interaction that has been predicted to occur in bulk materials with high densities of photoexcited charge carriers.

Estimation of mechanical damage by minority carrier recombination lifetime and near surface micro defect in silicon wafer (실리콘 웨이퍼에서 소수 반송자 재결합 수명과 표면 부위 미세 결함에 의한 기계적 손상 평가)

  • 최치영;조상희
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.9 no.2
    • /
    • pp.157-161
    • /
    • 1999
  • We investigated the effect of mechanical back side damage in Czochralski silicon wafer. The intensity of mechanical damage was evaluated by minority carrier recombination lifetime by laser excitation/microwave reflection photoconductance decay ($\mu$-PCD) technique, wet oxidation/preferential etching methods, near surface micro defect (NSMD) analysis, and X-ray section topography. The data indicate that the higher the mechanical damage intensity, the lower the minority carrier lifetime, and NSMD density increased proportionally, also correlated to the oxidation induced stacking fault (OISF) density. Thus, NSMD technique can be used separately from conventional etching method in OISF measurement.

  • PDF

Evaluation of mechanical backside damage by minority carrier recombination lifetime and photo-acoustic displacement method in silicon wafer (실리콘 웨이퍼에서 광열 변위법과 소수 반송자 재결합 수명 측정에 의한 기계적 후면 손상 평가)

  • 최치영;조상희
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.8 no.1
    • /
    • pp.117-123
    • /
    • 1998
  • We investigated the effect of mechanical backside damage in Czochralski grown silicon wafer. The intensity of mechanical damage was evaluated by minority carrier recombination lifetime by laser excitation/microwave reflection photoconductivity decay method, photo-acoustic displacement method, X-ray section topography, and wet oxidation/preferential etching methods. The data indicate that the higher the mechanical damage intensity, the lower the minority carrier lifetime, and the photo-acoustic displacement values increased proportionally, and it was at Grade 1: Grade 2:Grade 3 = 1:19.6:41 that the normalized relative quantization ratio of excess photo-acoustic displacement in damaged wafer was calculated, which are normalized to the excess PAD from sample Grade 1.

  • PDF

Transport parameters in a-Se:As films for digital X-ray conversion material (디지털 X-선 변환물질 a-Se:As의 수송변수)

  • Park, Chang-Hee
    • Korean Journal of Digital Imaging in Medicine
    • /
    • v.8 no.1
    • /
    • pp.51-55
    • /
    • 2006
  • The effects of Asaddition in amorphous selenium(a-Se) films for digital X-ray conversion material have been studied using the moving photocarrier grating(MPG) technique. This method utilizes the moving interference pattern generated by the superposition of the two frequency shifted laser beams for the illumination of the sample. This moving intensity grating induces a short circuit current, j$_{sc}$ in a-Se:As film. The transport parameters of the sample are extracted from the grating-velocity dependent short circuit current induced in the sample along the modulation direction. The electron and hole mobility, and recombination lifetime of a-Se films with arsenic(As) additions have been obtained. We have found an Increase in hole drift mobility and recombination lifetime, especially when 0.3% As is added into a-Se film, whereas electron mobility decreases with As addition due to the defect density. The transport properties for As doped a-Se films obtained by using MPG technique have been compared with X-ray sensitivity for a-Se:As device. The fabricated a-Se(0.3% As) device film exhibited the highest X-ray sensitivity out of 5 samples.

  • PDF

Transport phenomena of a-Se:As thin film for digital X-ray Conversion Material (디지털 X-선 변환물질을 위한 비소(As) 첨가 비정질 셀레늄(a-Se) 박막의 수송현상)

  • Park, Chang-Hee;Kim, Jae-Hyung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.11a
    • /
    • pp.282-283
    • /
    • 2006
  • The transport phenomena of arsenic (As) doped amorphous selenium(a-Se:As) thin film for digital X-ray conversion material has been reported. The effect of As addition on the carrier mobility and recombination lifetime in a-Se:As sample has been measured using the moving photo-carrier grating (MPG) technique. An Increase in hole mobility and recombination was observed when 0.3% arsenic, was added into a-Se sample, whereas electron mobility decrease with arsenic addition due to the defect density. The fabricated a-Se:03% As device exhibited the highest X-ray sensitivity.

  • PDF

Controlled Charge Carrier Transport and Recombination for Efficient Electrophosphorescent OLED

  • Chin, Byung-Doo;Choi, Yu-Ri;Eo, Yong-Seok;Yu, Jai-Woong;Baek, Heume-Il;Lee, Chang-Hee
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2008.10a
    • /
    • pp.1418-1420
    • /
    • 2008
  • In this paper, the light emitting efficiency, spectrum, and the lifetime of the phosphorescent devices, whose emission characteristics are strongly dominated not only by the energy transfer but also by the charge carrier trapping induced by the emissive dopant, are explained by differences in the energy levels of the host, dopant, and nearby transport layers. On the basis of our finding on device performance and photocurrent measurement data by time-of-flight (TOF), we investigated the effect of the difference of carrier trapping dopant and properties of the host materials on the efficiency roll-off of phosphorescent organic light emitting diode (OLED), along with a physical interpretation and practical design scheme, such as a multiple host system, for improving the efficiency and lifetime of devices.

  • PDF

Influence of Metallic Contamination on Photovoltaic Characteristics of n-type Silicon Solar-cells (중금속 오염이 n형 실리콘 태양전지의 전기적 특성에 미치는 영향에 대한 연구)

  • Kim, Il-Hwan;Park, Jun-Seong;Park, Jea-Gun
    • Current Photovoltaic Research
    • /
    • v.6 no.1
    • /
    • pp.17-20
    • /
    • 2018
  • The dependency of the photovoltaic performance of p-/n-type silicon solar-cells on the metallic contaminant type (Fe, Cu, and Ni) and concentration was investigated. The minority-carrier recombination lifetime was degraded with increasing metallic contaminant concentration, however, the degradation sensitivity of recombination lifetime was lower at n-type than p-type silicon wafer, which means n-type silicon wafer have an immunity to the effect of metallic contamination. This is because heavy metal ions with positive charge have a much larger capture cross section of electron than hole, so that reaction with electrons occurs much more easily. The power conversion efficiency of n-type solar-cells was degraded by 9.73% when metallic impurities were introduced in the silicon bulk, which is lower degradation compared to p-type solar-cells (15.61% of efficiency degradation). Therefore, n-type silicon solar-cells have a potential to achieve high efficiency of the solar-cell in the future with a merit of immunity against metal contamination.