  • ZnO was doped up to 0.3 wt% for improving the electrical properties of lead-free $[Li_{0.04}(Na_{0.44}Ko_{0.52})-(Nb_{0.86}\;Ta_{0.10}\;Sb_{0.04})]O_3$ piezoelectric ceramics. The ceramics were fabricated with the conventional sintering processes. Crystal structure of the samples was tetragonal phase regardless of ZnO amount. However, the piezoelectric properties were varied with the ZnO amount. The electro-mechanical coupling factor $(k_p)$ was with the ZnO amount up to 0.2 wt% but decreased with the further addition. the maximum value of $k_p$ was 0.475. Density, piezoelectric charge constant and relative dielectric constant was also showed maximum value at 0.2 wt%. The maximum values are $4.75g/cm^3$, 275 pC/N, 1403, respectively. In contrast, the mechanical quality factor $(Q_m)$ was not varied with increasing the ZnO addition up to 0.2 wt% but rapidly increased at 0.3 wt%.

정적연소기에서의 메탄-공기 혼합기의 연소특성(1) : 균질급기 (Combustion Characteristics of Methane-Air Mixture in a Constant Volume Combustion Chamber(1): Homogeneous Charge)

  • 최승환;전충환;장연준
    • 한국자동차공학회논문집
    • /
    • 제11권3호
    • /
    • pp.48-57
    • /
    • 2003
  • A cylindrical constant volume combustion chamber was used to investigate the flow characteristics at spark plug and the combustion characteristics of homogeneous charge methane-air mixture under various initial pressure, excess air ratio and ignition times in quiescent mixture. The flow characteristics such as mean velocity and turbulence intensity was analyzed by hot wire anemometer. Combustion pressure development measured by piezoelectric pressure transducer and flame propagation acquired by ICCD camera were used to investigate the effect of initial pressure, excess air ratio and ignition times on pressure, combustion duration, flame speed and burning velocity. Mean velocity and turbulence intensity had the maximum value at 200 or 300ms and then decreased to near 0 value gradually after 3 seconds. Combustion duration, flame speed and burning velocity were observed to be promoted with excess air ratio of 1.1, lower initial pressure and ignition time of 300ms.

두께를 증가시킨 셀룰로오스 Electro-Active Paper 의 제조와 특성평가 (Fabrication and Characterization of Cellulose Electro-Active Paper with Increased Thickness)

  • 김기백;정혜전;김재환
    • 한국정밀공학회지
    • /
    • 제30권2호
    • /
    • pp.241-246
    • /
    • 2013
  • This paper reports fabrication and characterization of cellulose Electro-Active Paper (EAPap) with increased thickness. Usual thickness of cellulose EAPap was $15{\mu}m$. This thickness needs to be increased to enhance the mechanical force output of EAPap. To fabricate thick cellulose EAPap, the fabrication process parameters including casting and drying processes should be investigated. In this paper, the casting thickness is increased from $800{\mu}m$ to $1500{\mu}m$, and heating times on a hot plate before and after curing process are introduced at 40 and $60^{\circ}C$ for 30 and 60 minutes, respectively. Thickness measurement, Thermal Gravitational Analysis (TGA), UV-transmittance, Young's modulus, and piezoelectric charge constant are measured. Heated EAPaps with increased thickness have similar TGA result, higher transmittance, higher Young's modulus and lower piezoelectric charge constant.

$La_2O_3$ 첨가에 따른 (Ka,K)$NbO_3$ 세라믹스의 미세구조 및 압전 특성

  • 서병호;성금현;노정래;이상호;류주현;김인성;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2010년도 춘계학술회의 초록집
    • /
    • pp.12-12
    • /
    • 2010
  • The piezoelecric properties of $(K_{0.5}Na_{0.5})(Nb_{0.96}Sb_{0.04})O_3$+$1.2mol%K_4CuNb_8O_{23}$+$xmol%La_2O_3$ lead-free piezoelecric ceramics were investigated as a function x. These ceramics were fabricated by conventional ceramics processing. Piezoelectric constant ($d_{33}$) and piezoelectric charge coefficient ($g_{33}$) of x=0.2 mol% composition exhibited good properties of 160.3pC/N and 37.4($10^{-3}Vm/N$), respectively.

  • PDF

캔틸레버 구조해석을 통한 압전소자의 최대 전력량 산출 (Cantilever Structural Analysis for Optimal Piezoelectric Power Harvesting)

  • 임근수;조성식;김수현;박우태
    • 마이크로전자및패키징학회지
    • /
    • 제20권4호
    • /
    • pp.31-34
    • /
    • 2013
  • 외팔보의 형상적인 해석과 압전효과에 의거하여, 최대 전력량 산출을 위한 에너지 수확기를 설계하였다. 두가지의 외팔보 형상으로 에너지 수확기의 구조가 설계되었다. 에너지 수확기의 성능을 좌우하는 주요 변수는 외팔보 형상과 끝단에 부착된 질량이다. 수확되는 전하량은 압전재료의 압전상수와 외팔보의 기계적인 변형량에 비례한다.

PMS-PZT 세라믹스의 압전특성에 미치는 ZnO의 영향 (Effects of ZnO on the Piezoelectric Properties of PMS-PZT Ceramics)

  • 손영진;황동연;김재창;조경원;김영민;어순철;김일호
    • 한국재료학회지
    • /
    • 제14권11호
    • /
    • pp.764-768
    • /
    • 2004
  • Perovskite Pb(Mn_{1/3}Sbu_{2/3})O_2-Pb(Zr,Ti)O_3\;(PMS-PZT) was prepared and ZnO doping effects on its piezoelectric properties were investigated. Pyrochlore phase was not identified in the PMS-PZT ceramics with $0\sim5\;mol\%$ ZnO sintered at $1100^{\circ}C$ for 2 hrs, and maximum sintered density of $7.92 g/cm^3$ was obtained. Piezoelectric charge constant and voltage constant increased to $359{\times}10^{-12}\;C/N\;and\;22.5{\times}10^{-13}\;Vm/N$, respectively, with increasing ZnO content. Mechanical quality factor reduced considerably with increasing ZnO content. When the ZnO content was 3 $mol\%$, electromechanical coupling factor and relative dielectric constant showed maximum values of $56\%$ and 1727, respectively. This should be evaluated by complicated variations of sintered density, tetragonality of lattice, grain size, and A-site vacancy generated by ZnO addition and $Zn^{2+}$ substitution.

Unified solutions for piezoelectric bilayer cantilevers and solution modifications

  • Wang, Xianfeng;Shi, Zhifei
    • Smart Structures and Systems
    • /
    • 제16권5호
    • /
    • pp.759-780
    • /
    • 2015
  • Based on the theory of piezoelasticity, the static performance of a piezoelectric bilayer cantilever fully covered with electrodes on the upper and lower surfaces is studied. Three models are considered, i.e., the sensor model, the driving displacement model and the blocking force model. By establishing suitable boundary conditions and proposing an appropriate Airy stress function, the exact solutions for piezoelectric bilayer cantilevers are obtained, and the effect of ambient thermal excitation is taken into account. Since the layer thicknesses and material parameters are distinguished in different layers, this paper gives unified solutions for composite piezoelectric bilayer cantilevers including piezoelectric bimorph and piezoelectric heterogeneous bimorph, etc. For some special cases, the simplifications of the present results are compared with other solutions given by other researches based on one-dimensional constitutive equations, and some amendments have been found. The present investigation shows: (1) for a PZT-4 piezoelectric bimorph, the amendments of tip deflections induced by an end shear force, an end moment or an external voltage are about 19.59%, 23.72% and 7.21%, respectively; (2) for a PZT-4-Al piezoelectric heterogeneous bimorph with constant layer thicknesses, the amendments of tip deflections induced by an end shear force, an end moment or an external voltage are 9.85%, 11.78% and 4.07%, respectively, and the amendments of the electrode charges induced by an end shear force or an end moment are both 1.04%; (3) for a PZT-4-Al piezoelectric heterogeneous bimorph with different layer thicknesses, the maximum amendment of tip deflection approaches 23.72%, and the maximum amendment of electrode charge approaches 31.09%. The present solutions can be used to optimize bilayer devices, and the Airy stress function can be used to study other piezoelectric cantilevers including multi-layered piezoelectric cantilevers under corresponding loads.

Effect of Mn on Dielectric and Piezoelectric Properties of 71PMN-29PT [71Pb(Mg1/3Nb2/3)O3-29PbTiO3] Single Crystals and Polycrystalline Ceramics

  • Oh, Hyun-Taek;Joo, Hyun-Jae;Kim, Moon-Chan;Lee, Ho-Yong
    • 한국세라믹학회지
    • /
    • 제55권2호
    • /
    • pp.166-173
    • /
    • 2018
  • In order to investigate the effect of Mn on the dielectric and piezoelectric properties of PMN-PT [$Pb(Mg_{1/3}Nb_{2/3})O_3-PbTiO_3$], four different types of 71PMN-29PT samples were prepared using the solid-state single crystal growth (SSCG) method: (1) Undoped single crystals, (2) undoped polycrystalline ceramics, (3) Mn-doped single crystals, and (4) Mn-doped polycrystalline ceramics. In the case of single crystals, the addition of 0.5 mol% Mn to PMN-PT decreased the dielectric constant ($K_3{^T}$), piezoelectric charge constant ($d_{33}$), and dielectric loss (tan ${\delta}$) by about 50%, but increased the coercive electric field ($E_C$) by 50% and the electromechanical quality factor ($Q_m$) by 500%, respectively. The addition of Mn to PMN-PT induced an internal bias electric field ($E_I$) and thus specimens changed from piezoelectrically soft-type to piezoelectrically hard-type. This Mn effect was more significant in single crystals than in ceramics. These results demonstrate that Mn-doped 71PMN-29PT single crystals, because they are piezoelectrically hard and simultaneously have high piezoelectric and electromechanical properties, have great potential for application in fields of SONAR transducers, high intensity focused ultrasound (HIFU), and ultrasonic motors.

COMBUSTION CHARACTERISTICS OF HOMOGENEOUS CHARGED METHANE-AIR MIXTURE IN A CONSTANT VOLUME COMBUSTION CHAMBER

  • CHOI S. H.;CHO S. W.;JEONG D. S.;JEON C. H.;CHANG Y. J.
    • International Journal of Automotive Technology
    • /
    • 제6권4호
    • /
    • pp.323-332
    • /
    • 2005
  • A cylindrical constant volume combustion chamber was used to investigate the flow characteristics at the spark electrode gap and the combustion characteristics of a homogeneous charged methane-air mixture under various overall charge pressures, excess air ratios and ignition times. The flow characteristics, including the mean velocity and turbulence intensity, were analyzed with a hot wire anemometer. Combustion pressure development measured by piezoelectric pressure transducer, a flame propagation image acquired by ICCD camera and exhaust emissions measured by 2-valve gas chromatography were used to investigate effects of initial pressures, excess air ratios and ignition times on the combustion characteristics. It was found that the mean velocity and turbulence intensity had the maximum value around 200-300 ms and then decreased gradually to a near-zero value after 3000 ms and that the combustion duration was shorten and the flame speed and laminar burning velocity had the highest value under the condition of an excess air ratio of 1.1, an overall charge pressure of 0.15 MPa and an ignition time of 300 ms in the present study. The $CO_2$ concentration was proportional to the ignition time and overall charge pressure, the $CO_2$ concentration was proportional to the excess air ratio, and the UHC concentration was inversely proportional to the ignition time and overall charge pressure.

Pb(Sb1/2Sn1/2)O3-PbTiO3-PbZrO3 세라믹스의 유전 및 압전 특성에 관한 연구 (A Study on the Dielectric and Piezoelectric properties of the Pb(SbS11/2TSnS11/2T)OS13T-PbTiOS13T-PbZrOS13T Ceramics)

  • 정장호;류기원;이성갑;이영희
    • 대한전기학회논문지
    • /
    • 제41권5호
    • /
    • pp.517-524
    • /
    • 1992
  • In this study, 0.10Pb(SbS11/2TSnS11/2T)OS13T-(0.90-x)PbZrOS13T (0.25 x 0.40) ceramics were fabricated by the atmospheric method. The sintering temperature and time were 1250[$^{\circ}C$] and 2[2hr], respectively. The structureal, dielectric and piezoelectric properties with composition of PbTiOS13T were studied. As the results of XRD ans SEM, the crystal structure of a specimen was rhombohedral, lattice constant and average grain size were decreased with increasing the contents of PbTiOS13T. Relative dielectric constant and Curie temperature were increased with increasing the contents of PbTiOS13T, 0.10PSS-0.40PT-0.50PZ specimen had the highest values of 904 and 265[$^{\circ}C$], respectively. In increasing of PbTiOS13T contents form 25[mol%] to 40[mol%], piezoelectric charge constant and electromechanical coupling factors were increased form 114[pC/N] to 142[pC/N], 17[%] to 24[%] and mechanical quality factor were decreased with increasing the contents of PbTiOS13T. In the 0.10PSS-0.40PT-0.50PZ specimens, those values were 14.2[kV/cm] and 9.43[x10S0-6TC/cmS02T], resectively.