Synthesis of 6-Alkyl-3-Chromonealdehyde(2,2-dialkyl)hydrazone Derivatives for Green Light Emitting Materials (녹색발광 6-알킬-3-크로몬알데히드(2,2-디알킬)하이드라존 유도체의 합성)

  • Chung, Pyung-Jin;Chang, Hong-Joon
    • Applied Chemistry for Engineering
    • /
    • v.21 no.4
    • /
    • pp.424-429
    • /
    • 2010
  • 6-Alkyl-3-chromonealdehyde (2,2-dialkyl)hydrazone derivatives were synthesized by dehydration condensation. They are green-emitting materials for organic light emitting device (OLED) composed of electron acceptor of 6-alkyl-3-chromonealdehydes and electron donor of 2,2-dialkylhydrazones in a conjugated structure. The structural properties of reaction products were analyzed by FT-IR and $^1H$-NMR spectroscopy. The thermal stabilities and reactivities were measured by melting points and yields. The UV-visibles and PL properties were also determined by excitation spectra and emission spectra, respectively.

Synthesis and Luminescence of Lu3(Al,Si)5(O,N)12:Ce3+ Phosphors

  • Ahn, Wonsik;Kim, Young Jin
    • Journal of the Korean Ceramic Society
    • /
    • v.53 no.4
    • /
    • pp.463-467
    • /
    • 2016
  • $Si^{4+}-N^{3-}$ was incorporated into $Ce^{3+}-doped$ lutetium aluminum garnet ($Lu_{2.965}Ce_{0.035}Al_5O_{12}$, $LuAG:Ce^{3+}$) lattices, resulting in the formation of $Lu_{2.965}Ce_{0.035}Al_{5-x}Si_xO_{12-x}N_x$ [(Lu,Ce)AG:xSN]. For x = 0-0.25, the synthesized powders consisted of the LuAG single phase, and the lattice constant decreased owing to the smaller $Si^{4+}$ ions. However, for x > 0.25, a small amount of unknown impurity phases was observed, and the lattice constant increased. Under 450 nm excitation, the PL spectrum of $LuAG:Ce^{3+}$ exhibited the green band, peaking at 505 nm. The incorporation of $Si^{4+}-N^{3-}$ into the $Al^{3+}-O^{2-}$ sites of $LuAG:Ce^{3+}$ led to a red-shift of the emission peak wavelength from 505 to 570 nm with increasing x. Corresponding CIE chromaticity coordinates varied from the green to yellow regions. These behaviors were discussed based on the modification of the $5d^1$ split levels and crystal field surroundings of $Ce^{3+}$, which arose from the Ce-(O,N)8 bonds.

Evaluation of Acceptor Binding Energy of Nitrogen-Doped Zinc Oxide Thin Films Grown by Dielectric Barrier Discharge in Pulsed Laser Deposition

  • Lee, Deuk-Hee;Chun, Yoon-Soo;Lee, Sang-Yeol;Kim, Sang-Sig
    • Transactions on Electrical and Electronic Materials
    • /
    • v.12 no.5
    • /
    • pp.200-203
    • /
    • 2011
  • In this research, nitrogen (N)-doped zinc oxide (ZnO) thin films have been grown on a sapphire substrate by dielectric barrier discharge (DBD) in pulsed laser deposition (PLD). DBD has been used as an effective way for massive in-situ generation of N-plasma under conventional PLD process conditions. Low-temperature photoluminescence spectra of N-doped ZnO thin films provided near-band-edge emission after a thermal annealing process. The emission peak was resolved by Gaussian fitting and showed a dominant acceptor-bound excitation peak ($A^{\circ}X$) that indicated acceptor doping of ZnO with N. The acceptor binding energy of the N acceptor was estimated to be approximately 145 MeV based on the results of temperature-dependent photoluminescence (PL) measurements.

Preparation of dense $BaMgAl_{10}O_{17}:Eu^{2+}$ particles and their surface treatment

  • Lee, Dae-Won;Boo, Jin-Hyo;Jung, Ha-Kyun
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2005.07b
    • /
    • pp.1499-1502
    • /
    • 2005
  • Dense $BaMgAl_{10}O_{17}:Eu^{2+}$ phosphor particles with a spherical shape have been synthesized through spray pyrolysis method using basic aluminum nitrate precursor as a spray solution. This $BaMgAl_{10}O_{17}:Eu^{2+}$ particles prepared by the spray pyrolysis have shown the stronger emission intensity compared to the commercially-available $BaMgAl_{10}O_{17}:Eu^{2+}$. However, thermal stability of the BAM:Eu b lue phosphor is very poor due to changing from $Eu^{2+}$ to $Eu^{3+}$ at the thermal process, so brightness of the phosphor decreases. To improve the thermal stability of the dense BAM:Eu phosphor, the spherical BAM:Eu particles were coated with pure $BaMgAl_{10}O_{17}$ layer using the hydrolysis reaction in a solution system. The synthesized powders were characterized by XRD, SEM and PL. On the other hand, the emission properties of the BAM:Eu phosphors coated with $BaMgAl_{10}O_{17}$ layer before and after thermal treatment at $500^{\circ}C$ for 30 min were estimated under VUV excitation. The brightness of the coated phosphor was higher than that of the uncoated phosphor. Also, the coating thickness of BAM layer in the BAM:Eu particles was optimized.

  • PDF

Luminescence Properties of YTa7O19 doped with Tm3+ (Tm3+ 도핑에 따른 YTa7O19의 형광특성)

  • Ryu, Hojin;Park, Hee-Dong
    • Applied Chemistry for Engineering
    • /
    • v.8 no.4
    • /
    • pp.637-639
    • /
    • 1997
  • Samples of $YTa_7O_{19}$ doped with $Tm^{3+}$ were prepared using the solid state reaction method to investigate their photoluminescence characteristics. The samples were identified by XRD and SEM, and the optical measurement was also carried out. Under 359 nm excitation, $YTa_7O_{19}$ doped with $Tm^{3+}$ exhibited a narrow-band blue emission, at about 455 nm. The maximum emission intensity was obtained at $YTa_7O_{19}$ doped with 0.12 mole $Tm^{3+}$. This revealed the concentration quenching of emission intensity.

  • PDF

Synthesis and Photoluminescence Properties of ZrO2:Eu3+ Nanoparticles Using Salt-Assisted Ultrasonic Pyrolysis Process (염 보조 초음파 분무 열분해법을 이용한 ZrO2:Eu3+ 나노입자의 합성 및 발광 특성)

  • Hwangbo, Young;Lim, Hyo Ryoung;Lee, Young-In
    • Korean Journal of Materials Research
    • /
    • v.27 no.5
    • /
    • pp.270-275
    • /
    • 2017
  • Inorganic phosphors based on $ZrO_2:Eu^{3+}$ nanoparticles were synthesized by a salt-assisted ultrasonic spray pyrolysis process that is suitable for industrially-scalable production because of its continuous nature and because it does not require expensive precursors, long reaction time, physical templates or surfactant. This facile process results in the formation of tiny, highly crystalline spherical nanoparticles without hard agglomeration. The powder X-ray diffraction patterns of the $ZrO_2:Eu^{3+}$ (1-20 mol%) confirmed the body centered tetragonal phase. The average particle size, estimated from the Scherrer equation and from TEM images, was found to be approximately 11 nm. Photoluminescence (PL) emission was recorded under 266 nm excitation and shows an intense emission peak at 607 nm, along with other emission peaks at 580, 592 and 632 nm which are indicated in red.

Synthesis of 3-Chromonealdehyde(2,2-disubstituted)hydrazone Derivatives for Green Light Emitting Materials (녹색발광 3-크로몬알데히드(2,2-이치환)하이드라존 유도체의 합성)

  • Chung, Pyung Jin;Chang, Hong Joon
    • Applied Chemistry for Engineering
    • /
    • v.20 no.6
    • /
    • pp.670-674
    • /
    • 2009
  • 3-Chromonealdehyde(2,2-disubstituted)hydrazone derivatives were synthesized by dehydration condensation. They are green-emitting materials for organic light emitting device (OLED) composed of electron acceptor of 3-chromonealdehydes and electron donor of 2,2-disubstituted hydrazones by a conjugated structure. The structural properties of reaction products were analyzed FT-IR and $^1H-NMR$ spectroscopy. The thermal stabilities and reactivities were measured by melting points and yields. The UV-visibles and PL properties can be determined by excitation spectra and emission spectra, respectively.

Excitation Based Tunable Emissions from the Nanocrystalline $Ca_2Gd_8Si_6O_{26}$ : $Sm^{3+}/Tb^{3+}$ Phosphors for Novel Inorganic LEDs

  • Raju, G. Seeta Rama;Yu, Jae-Su
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2011.08a
    • /
    • pp.156-156
    • /
    • 2011
  • Nanocrystalline $Ca_2Gd_8Si_6O_{26}$ (CGS) : $Sm^{3+}$ and CGS : $Tb^{3+}/Sm^{3+}$ phosphors were prepared by solvothermal reaction method for light emitting diode (LED) and field emission display (FED) applications. The XRD patterns of these phosphors confirmed their oxyapatite structure in the hexagonal lattice. The visible luminescence properties of these phosphors were investigated by exciting with ultraviolet (UV) or near-UV light and low voltage electron beam. The photoluminescence (PL) properties of $Ca_2Gd_8Si_6O_{26}$ (CGS) : $Sm^{3+}$ and CGS : $Tb^{3+}/Sm^{3+}$ phosphors were investigated as a function of $Sm^{3+}$ concentration. Cathodoluminescence (CL) properties were examined by changing the acceleration voltage. The CGS : $Sm^{3+}$ showed the dominant orange emission due to the $^4G_{5/2}{\rightarrow}^6H_{7/2}$ transition. The CGS : $Tb^{3+}/Sm^{3+}$ phosphor showed the green, white and orange emissions when excited with 275, 378, and 405 nm wavelengths, respectively. The chromaticity coordinates of these phosphors were comparable to or better than those of standard phosphors for LED or FED devices.

  • PDF

Synthesis and Characterization Of Green- and Yellow-Emitting Zinc Silicate Thin Films Doped with Manganese

  • Cho, Yeon Ki;Kim, Joo Han
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.02a
    • /
    • pp.546-546
    • /
    • 2013
  • Zinc silicate ($Zn_2SiO_4$) has been identified as a suitable host material for a wide variety of luminescent activators, such as transition metal and rare earth elements. In particular, manganese-activated $Zn_2SiO_4$ exhibits highly efficient photoluminescenceand cathodoluminescence, which allows this material to be used in fluorescent lamps and display applications. In this study, we investigated the green and yellow luminescence from Mn-doped $Zn_2SiO_4$ thin films that were synthesized using radio frequency magnetron sputtering followed by annealing at $600{\sim}1,200^{\circ}C$ The refractive index of the $Zn_2SiO_4$: Mn films showed normal dispersion behavior. It was found that the $Zn_2SiO_4$: Mn films annealed at $800^{\circ}C$ ossessed a mixture of alpha and beta phases. The obtained photoluminescence spectrum consisted of two emission bands centered at 525 nm in the green range and 574 nm in the yellow range. The green luminescence originates from the divalent Mn ions in alpha phase of $Zn_2SiO_4$, while the yellow luminescence comes from the divalent Mn ions in beta phase. The films annealed at and above $900^{\circ}C$ xhibited only the alpha phase. The broad PL excitation band was observed ranging from 220 to 300 nm with a maximum at around 243 nm.

  • PDF

Preparation and Luminescene properties with invisible inoranic phosphors of nano size (나노크기의 비가시 무기형광체 제조와 발광특성)

  • Jeong, Jae-Hoon;Yun, Hyun;Jang, Gyu-Hwan;Shin, Sang-Sik
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.461-462
    • /
    • 2008
  • $BaMgAl_{10}O_{17}$:Mn, $Eu^{2+}$ green phosphors has been synthesized by the solid state reaction. Green phosphors of nano-size were manufactured in short time by shake method. which were easily manufactured respectively general method. Green phosphors of nano size were control additive, size of $ZrO_3$ ball, shake time and weight of ball in toluene. In result that green phosphors were obtained particle size of 140nm~150nm. The characteristics of fired samples were obtained by 365nm and 380nm excitation source under ultraviolet. In result that the highest PL intensity were observed in wavelength of 365nm.