• 제목/요약/키워드: Na-Ta mineralization

검색결과 7건 처리시간 0.02초

Electrochemical Advanced Oxidation of Lamotrigine at Ti/DSA (Ta2O5-Ir2O5) and Stainless Steel Anodes

  • Meena, Vinod Kumar;Ghatak, Himadri Roy
    • Journal of Electrochemical Science and Technology
    • /
    • 제13권2호
    • /
    • pp.292-307
    • /
    • 2022
  • The study presents kinetics of degradation and mineralization of an anti-epileptic drug Lamotrigine (LAM) in the aqueous matrix by electrochemical advanced oxidation process (EAOP) on Ti/DSA (Ta2O5-Ir2O5) and Stainless Steel (SS) anodes using sodium sulphate as supporting electrolyte. On both the anodes, kinetic behaviour was pseudo-first-order for degradation as well as mineralization of LAM. On Ti/DSA anode, maximum LAM degradation of 75.42% was observed at an associated specific charge of 3.1 (Ah/litre) at a current density of 1.38 mA/cm2 and 100 ppm Na2SO4 concentration. Maximum mineralization attained was 44.83% at an associated specific charge of 3.1 (Ah/litre) at a current density of 1.38 mA/cm2 and 50 ppm concentration of Na2SO4 with energy consumption of 2942.71 kWh/kgTOC. Under identical conditions on SS anode, a maximum of 98.92% LAM degradation was marked after a specific charge (Q) of 3.1 (Ah/litre) at a current density of 1.38 mA/cm2 and 100 ppm concentration of Na2SO4. Maximum LAM mineralization on SS anode was 98.53%, marked at a specific charge of 3.1 (Ah/litre) at a current density of 1.38 mA/cm2 and 75 ppm concentration of Na2SO4, with energy consumption of 1312.17 kWh/kgTOC. Higher Mineralization Current Efficiency (MCE) values were attained for EAOP on SS anode for both degradation and mineralization due to occurrence of combined electro-oxidation and electro-coagulation process in comparison to EAOP on Ti/DSA anode due to occurrence of lone electro-oxidation process.

무주 페그마타이트 내 Nb-Ta 광화대의 산출상태 (Occurrence of the Nb-Ta Ore Bodies in Pegmatites, Mujoo)

  • 강민우;김지현;최진범
    • 한국광물학회지
    • /
    • 제24권2호
    • /
    • pp.133-143
    • /
    • 2011
  • 무주군 적상면 사산리에는 선캠브리아기 화강암질 편마암 복합체가 분포하고 이를 쥬라기 편암질 화강암과 페그마타이트가 관입하고 있으며, 페그마타이브 내 Nb-Ta 광화대가 발달하고 있다. 페그마타이트의 구성광물은 거정질의 석영, 장석류, 및 백운모가 우세하며 장석류는 정장석과 알바이트의 탄종성분을 보여준다. Nb-Ta 광물로는 콜럼바이트가 우세하며 백운모는 후기 마그마 기원으로 콜럼바이트와 밀접히 수반되어 산출한다. 조립의 콜럼바이트는 석영, 장석과 함께 산출하는 반면, 미립의 콜럼바이트는 백운모와 함께 산출하는데 조립질에 비해 미립의 콜럼바이트는 상대적으로 낮은 Nb 함량을 보여준다. 조사지역에 발달한 페그마트이트 맥은 폭 4~15 m, 길이가 각각 120 및 250 m인데, 5개 공 총 600 m 시추 결과 맥의 지하 연장은 별로 좋지 못하며 콜럼바이트는 미량으로 산출하고 있다. 따라서 조사지역에서 희유금속에 대한 광산개발가능성은 적다고 판단된다.

계명산층 페그마타이트에 수반되는 우라늄·토륨 광상의 지구화학적 특성 (Geochemistry of Uranium and Thorium Deposits from the Kyemyeongsan Pegmatite)

  • 박맹언;김근수
    • 자원환경지질
    • /
    • 제31권5호
    • /
    • pp.365-374
    • /
    • 1998
  • Economic U- and Th-bearing pegmatite deposits occur in the Kyemyeongsan Formation, and are spatially closely associated with the Carboniferous alkali granite. The pegmatite is lithochemically alkaline and peralumious, and consists mainly of potassic feldspar and quartz with allanite and U- and Th-bearing minerals. Paragenetic stages of mineralization in the pegmatite are divided as follows: early silicate mineralization, main rare metal mineralization, and late silicate mineralization. Thorite, euxenite, fergusonite and uranpyrochlore are the predominant U- and Th-bearing minerals. Both the enrichments of Nb, Y, Th, U, and Ta and the depletions of Hf, Ba, and Rb in the pegmatite were resulted from magmatic differentiation. The increases of Na and Ca in uranpyrochlore, of Th and U in fergusonite, of Si, Th, U and Pb in thorite, and of Nb and Y in euxenite were possibly resulted from both later internal fractionation and hydrothermal alteration. The variation of chemical composition in a mineral species reflects the different pysico-chemical conditions during the crystallization.

  • PDF

봉화(奉化)-울진지역(蔚珍地域)의 석(錫), 중석광화작용(重石鑛化作用) (Tin, Tungsten Mineralization in Bonghwa-Uljin Area)

  • 박희인;이상만
    • 자원환경지질
    • /
    • 제17권1호
    • /
    • pp.1-15
    • /
    • 1984
  • The tin and tungsten deposits are embedded around the age unknown Buncheon granite gneiss which intruded the Precambrian schists, gneiss and amphibolites in Bonghwa-Uljin area. Pegmatite dike swarm developed intermittently about 4km along the southern border of Buncheon granite gneiss at Wangpiri area. Thickness of pegmatite dikes range from 0.5 to 15m. Pegmetite is consisted of quartz, microcline, albite, muscovite and frequently topaz, tourmaline, garnet, fluorite, fluorapatite and lepidolite. Pegmatite dikes are greisenized, albitized and microclinized along dike walls. Cassiterites are irregularly disseminated through the intensely greienized and albitized parts of the pegmatite. Cassiterite crystals are mainly black to dark brown and contain considerable Ta and Nb. Average Ta and Nb contents of the four cassiterite samples are 5300 and 3400 ppm. The Ssangjeon tungsten deposits is embedded within the pegmatite dike developed along the northern contact of Buncheon granite gneiss with amphibolite. This pegmatite developed 2km along the strike and thickness varies from 10 to 40m. Mineral constituents of the pegmatite are quartz, microcline, plagioclase, muscovite, biotite, tourmaline and garnet. Ore minerals are ferberite and scheelite with minor amount of molybdenite, arsenopyrite, pyrrhotite, pyrite, chalcopyrite, sphalerite, galena, pentlandite, bismuthinite, marcasite, and fluorite. Color and occurrence of quartz reveals that quartz formed at three different stages; quartz I, the earliest milky white quartz formed as a rock forming mineral of simple pegmatite; quartz II, gray to dark gray quartz which replace the minerals associated with quartz I; quartz III, the latest white translucent quartz which replace the quartz I and H. All of the ore minerals are precipitated during the quartz II stage. Fluid inclusion in quartz I and II are mainly gaseous inclusions and liquid inclusions are contained in quartz III and fluorite. Salinities of the inclusion in quartz I and II ranges from 4.5 to 9.5 wt. % and 5.1 to 6.0 wi. % equivalent NaCl respectively. Salinities of the inclusion in fluorite range from 3.5 to 8.3 wt. % equivalent NaCl. Homogenization temperatures of the inclusion in quartz I, II and III range from 415 to $465^{\circ}C$, from 397 to $441^{\circ}C$ and 278 to $357^{\circ}C$. Data gathered in this study reveals that tin and tungsten mineralization in this area are one of prolonged event after the pegmatite formation around Buncheon granite gneiss.

  • PDF

통가 TA25 해저산 칼데라 해저열수 분출구의 광석광물 산상 및 유체포유물 연구 (Mineralogical and Fluid Inclusion Study on Seafloor Hydrothermal Vents at TA25 Subsea Caldera in Tongan Waters)

  • 최선기;이경용;박상준;최상훈;이인경
    • 자원환경지질
    • /
    • 제48권4호
    • /
    • pp.273-285
    • /
    • 2015
  • 통가화산호의 TA25 해저산 서측에서는 열수광체가 처음 발견되었다. 이 지역에 분포하는 열수분출구들은 열수분출이 막 시작된 미성숙한 분출구로서 최저 $150^{\circ}C$에서 최대 $242^{\circ}C$ (평균: $203^{\circ}C$)의 열수온도를 보인다. 주요 황화광물로는 섬아연석, 황철석, 백철석, 방연석, 황동석, 코벨라이트, 비사면동석(tennantite), 황비동석(enargite)이 산출되며, 중정석, 석고/경석고 등의 황산염 광물들이 침니 외각에서 산출된다. 특히, 섬아연석이 높은 산출빈도를 보이는 아연 우세형 (Zn-rich) 광체로 분류된다. 광석광물 중 황비동석의 산출은 이 지역 열수분출구의 광화작용이 고유황형 환경에서 진행되었음을 시사한다. 섬아연석은 열수분출구의 외각부에서 내측부로 갈수록 산출빈도가 증가하며, 섬아연석 내 철함량 (mole% FeS)도 높아진다. 또한, 이들 섬아연석은 은 (~10 wt.%)을 함유하고 있는 특징을 보인다. 황동석은 침니에 비해 광체구에서 높은 산출빈도를 보여, 침니와 비교하여 광체구에서 다소 고온의 광화작용이 진행된 것으로 판단된다. 열수분출구 구성광물 중 광체구에서 산출되는 중정석을 대상으로 한 유체포유물 실험 결과, 균일화 온도 및 염농도는 $148^{\circ}C{\sim}341^{\circ}C$ (평균: $213^{\circ}C$) 및 0.4~3.1 equiv. wt.% NaCl를 보여 섬아연석 등 광석광물의 주된 광화작용이 약 ${\geq}200^{\circ}C$에서 진행된 것으로 확인되며, 동광화작용이 미약한 침니에서는 보다 낮은 온도에서 광화작용이 진행되었던 것으로 판단된다.

충주 어래산 일대에서 산출하는 희토류 광물의 광물학적 및 광물화학적 특성 (Mineralogy and Mineral-chemistry of REE Minerals Occurring at Mountain Eorae, Chungju)

  • 유병운;이길재;고상모
    • 자원환경지질
    • /
    • 제45권6호
    • /
    • pp.643-659
    • /
    • 2012
  • 충주 지역은 소위 옥천층군에 해당되는 계명산층이 분포하며, 계명산층내에는 변성화산암 모암과 페그마타이트 모암의 희토류 광체가 배태한다. 변성화산암 모암의 희토류 광체를 구성하는 희토류광물은 갈렴석, 저어콘, 인회석, 스핀이 산출하나 갈렴석이 가장 우세하게 산출한다. 페그마타이트 모암의 희토류 광체를 구성하는 희토류 광물은 퍼구소나이트, 카르나수르타이트, 저어콘, 토륨석이 산출하나 퍼구소나이트가 가장 우세하다. 변성화산암에서 산출하는 갈렴석의 화학식은 (Ca, Y, REE, Th)$_{2.095}$(Mg, Al, Ti, Mn, $Fe^{3+})_{2.770}(SiO_4)_{2.975}(OH)$로서 TREO 23.89-29.12 wt%, $La_2O_3$ 4.71-9.92 wt%, $Ce_2O_3$ 11.30-14.33 wt%, $Y_2O_3$ 0.11-0.29 wt%, $ThO_2$ 0.12-0.94 wt% 이다. A(2) 사이트 에서 $Ca^{2+}$$REE^{3+}$, M(2) 사이트에서 $Al^{3+}$$Fe^{2+}$의 치환이 일어나는데 이는 갈렴석의 화학조성에 밀접한 관련을 갖는 특징이고, Fe의 함량이 일반 갈렴석보다 높은 Ce 계열의 Ferriallanite에 해당된다. 이는 모암인 계명산층을 주로 구성하는 변성화산암(변성조면암)의 원암이 Fe이 풍부한 함철층이기 때문인 것으로 판단된다. 페그마타이트 모암에서 가장 우세하게 산출하는 퍼구소나이트의 화학조성은 A 사이트에서 Y-REE, Y-Th 치환이 우세하게 일어났으며, B 사이트에서는 Nb-Ta-Ti의 치환이 주로 초래되었으며, 계산된 화학식은 $YNbO_4$ 이다. 또한 $Y_2O_3$$Nb_2O_5$만의 비율로 상관도를 확인 한 결과 연구지역에서 산출되는 퍼구소나이트는 Y과 Nb의 이상적인 비율인 1:1 비율과 달리 1:1.5의 비율을 나타내고 있으며, Nb의 함량이 Y 함량보다 높으며, Y 사이트 즉, A 사이트에서 희토류 원소의 치환이 활발하게 초래되었다. 페그마타이트에서 산출하는 카르나수르타이트는 REE 및 Th를 치환하는 조성은 각각 $Ce_2O_3$ 9.16-22.88 wt%, $La_2O_3$ 2.15-9.16 wt%, $ThO_2$ 0.44-10.8 wt%, 화학조성으로 계산된 구조식은 (Y, REE, Th, K, Na, Ca)$_{1.478}$(Ti, Nb)$_{1.304}$(Mg, Al, Mn, $Fe^{+3})_{0.988}$(Si, P)$_{1.431}O_7(OH)_4{\cdot}3H_2O$이다. 870-860 Ma 인 초기 원생대에 로디니아 대륙의 분열기로서 한반도에서 A-1형 화산활동이 초래되어 철, 희토류원소 및 고장력원소(Nb, Zr, Y 등)가 풍부한 변성화산암으로 주로 구성되는 계명산층을 형성 시켰다면 갈렴석은 모암이 형성될 당시 알카리 화산암에서 정출되었거나 변성작용이 초래된 고생대 말(300-280 Ma, Cho et al., 2002) 광역변성작용에 의해 형성 되었을 가능성이 높다. 희토류를 함유하는 페그마타이트에서 산출하는 저어콘 연대가 190 Ma 인 것은 쥬라기에 충주지역에서 광범위하게 초래된 화강암 정치활동과 관련된 가능성이 크다. 따라서 충주지역 계명산층 내 배태된 희토류 광체는 인접한 지역에 배태되어 있지만 매우 차별적 희토류 광화작용이 초래 되어 희토류광물조성과 광체의 산상이 차별적으로 나타나는 것으로 해석된다.

대봉 금-은광상의 모암변질과 원소분산 특성 연구 (Element Dispersion and Wall-rock Alteration from Daebong Gold-silver Deposit, Republic of Korea)

  • 유봉철;지세정;이길재;이종길;이현구
    • 자원환경지질
    • /
    • 제40권6호
    • /
    • pp.713-726
    • /
    • 2007
  • 대봉광상은 선캠브리아기 경기육괴의 호상편마암 또는 화강편마암내에 발달된 단층($N10{\sim}20^{\circ}W,\;40{\sim}60^{\circ}SW$)을 따라 충진한 중열수 함금-은 괴상 석영맥광상이다. 이 광상의 광화작용은 여러번의 단열작용에 의해 형성된 괴상 백색 석영맥(광화I시기)과 투명 석영맥(광화II시기)으로 구성된다. 광화I시기의 열수작용에 의한 변질작용은 견운모화, 녹니석화, 탄산염화, 황철석화, 규화 및 점토화작용 등이 관찰되며, 견운모대는 석영맥과 접촉한 부분에서, 녹니석대는 석영맥으로부터 멀어짐에 따라 관찰된다. 견운모대의 모암변질광물은 대부분이 견운모 및 석영이며, 일부 일라이트, 탄산염광물, 녹염석으로 구성된다. 녹니석대의 모암변질광물은 주로 녹니석, 석영과 소량 견운모, 탄산염광물 및 녹염석으로 구성된다. 견운모의 Fe/(Fe+Mg) 값은 $0.36{\sim}0.59(0.51{\pm}0.10)$이며, 백운모-페차이트족에 해당되고 녹니석의 Fe/(Fe+Mg) 값은 $0.66{\sim}0.73(0.70{\pm}0.02)$이고 대부분 브룬스비자이트에 해당된다. 견운모와 녹니석에 대한 $Al_{IV}-Fe/(Fe+Mg)$의 다이어그램은 변질 시 같은 광종의 견운모와 녹니석의 형성온도를 나타내는 지시자로서 유용하다. 이것은 계산된 녹니석 단종의 활동도가 $a3(Fe_5Al_2Si_3O_{10}(OH){_6}:0.00964{\sim}0.0291,\;a2(Mg_5Al_2Si_3O_{10}(OH){_6}:9.99E-07{\sim}1.87E-05,\;a1(Mg_6Si_4O_{10}(OH){_6}:5.61E-07{\sim}1.79E-05$로서 대봉광상의 녹니석은 철이 풍부한 녹니석으로 비교적 고온($T>450^{\circ}C$)에서 모암과 평형상태에서 온도가 감소함에 따라 형성되었음을 알 수 있다. 모암변질시 $log\;{\alpha}K^+/{\alpha}H^+,\;log\;{\alpha}Na^+/{\alpha}H^+,\;log\;{\alpha}Ca^{2+}/{\alpha}^2H^+$ 값은 각각 $4.6(400^{\circ}C),\;4.1(350^{\circ}C),\;4.0(400^{\circ}C),\;4.2(350^{\circ}C),\;1.8(400^{\circ}C),\;4.5(350^{\circ}C)$이고 pH는 각각 $5.4{\sim}6.5(400^{\circ}C),\;5.1{\sim}5.5(350^{\circ}C)$로서 모암변질시 열수용액은 약산성이었음을 알 수 있다. 모암변질시 이득원소(부화원소)는 $K_2O,\;P_2O_5,\;Na2O$, Ba, Sr Cr, Sc, V, Pb, Zn, Be, Ag, As, Ta, Sb이며 특히 Sr, V, Pb, Zn, As, Sb등의 원소는 현저하게 증가하므로 중열수 및 천열수 금-은광상의 탐사에 지시원소로서 활용될 수 있을 것이다.