  • There has been a rapid progress for flexible polymer-based MEMS(Microelectromechanical Systems) technology. Polycarbonate (PC) and Poly Methyl Methacrylate (PMMA), so-called acrylic, have many advantages for optical, non-toxic and micro-device application. We studied dry etching of PC and PMMA as a function of % gas ratio in the $O_2/SF_6/CH_4$ temary plasma. A photoresist pattern was defined on the polymer samples with a mask using a conventional lithography. Plasma etching was done at 100 W RIE chuck power and 10 sccm total gas flow rate. The etch rates of PMMA were typically 2 times higher than those of PC in the whole experimental range. The result would be related to higher melting point of PC compared to that of PMMA. The highest etch rates of PMMA and PC were found in the $O_2/SF_6$ discharges among $O_2/SF_6$, $O_2/CH_4$ and $SF_6/CH_4$ and $O_2/SF_6/CH_4$ plasma composition (PC: ${\sim}350\;nm/min$ at 5 sccm $O_2/5$ sccm $SF_6$, PMMA: ${\sim}570\;nm/min$ at 2.5 sccm $O_2/7.5$ sccm $SF_6$). PC has smoother surface morphology than PMMA after etching in the $O_2/SF_6/CH_4$ discharges. The surface roughness of PC was in the range of 1.9$\sim$3.88 nm. However, that of PMMA was 17.3$\sim$26.1 nm.

Sheathless electrospray ionization with integrated metal emitter on microfluidic device (전기 분무 이온화를 이용한 단백질 질량분석용 마이크로 유체 소자의 제작 및 실험)

  • Kim, Min-Su;Joo, Hwang-Soo;Lee, Kook-Nyung;Kim, Byung-Gee;Kim, Yong-Kweon
    • Proceedings of the KIEE Conference
    • /
    • 2004.07c
    • /
    • pp.2102-2104
    • /
    • 2004
  • In this study, sheathless electrospray from PDMS/glass microchips with conducting metal emitter tip is described. A chip-based capillary electrophoresis/mass spectrometry (CE/MS) system has advantages of the CE separation and on-line electrospray detection of peptide solution. We have fabricated a new electrospray ionization(ESI) device composed of the metal emitter tip and CE separation channel monolithically in a glass microchip. The separation channel and metal emitter tip are fabricated using a glass wet etching and gold electro plating process, respectively. The fabricated micro electrospray chip was tested by spraying peptide sample for mass spectrometric analysis. Singlely-charged peak and doublely-charged peak of peptide were detected and further MS/MS fragmentation was performed in each peak. Direct comparisons with conventional glass or fused silica emitters showed very similar performance with respect to signal strength and stability.

  • PDF

Pentacene Thin Film Transistors Fabricated by High-aspect Ratio Metal Shadow Mask

  • Jin, Sung-Hun;Jung, Keum-Dong;Shin, Hyung-Chul;Park, Byung-Gook;Lee, Jong-Duk;Yi, Sang-Min;Chu, Chong-Nam
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 2004.08a
    • /
    • pp.881-884
    • /
    • 2004
  • The robust and large-area applicable metal shadow masks with a high aspect ratio more than 20 are fabricated by a combination of micro-electro-discharge machining (${\mu}$-EDM) and electro chemical etching (ECE). After defining S/D contacts using a 100 ${\mu}m$ thick stainless steel shadow mask, the top-contact pentacene TFTs with channel length of 5 ${\mu}m$ showed routinely the results of mobility of 0.498 ${\pm}$ 0.05 $cm^2$/Vsec, current on/off ratio of 1.6 ${times}$ $10^5$, and threshold voltage of 0 V. The straightly defined atomic force microscopy (AFM) images of channel area demonstrated that shadow effects caused by the S/D electrode deposition were negligible. The fabricated pentacene TFTs have an average channel length of 5 ${\pm}$ 0.25 ${\mu}m$.

  • PDF

Sol-gel Mechanism of Self-patternable PZT Film Starting from Alkoxides Precursors

  • Hwang, Jae-Seob;Kim, Woo-Sik;Park, Hyung-Ho;Kim, Tae-Song
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.4
    • /
    • pp.385-392
    • /
    • 2003
  • Sol-gel preparation technique using a chemical reaction of metal alkoxides has been widely used for the fabrication of various materials including ceramics. However, its mechanism has been studied till now because a number of chemical ways are possible from various alkoxides and additives. In this study, the mechanism of hydrolysis, condensation, and polymerization of alkoxides were investigated from the fabrication of lead-zirconate-titanate (PbZr$\_$x/Ti$\_$l-x/O$_3$; PZT) thin film that is used as various micro-actuator, transducer, and sensor because of its high electro-mechanical coupling factors and thermal stability. Furthermore, the fabrication process and characteristics of self-patternable PZT film using photosensitive stabilizer were studied in order to resolve the problem of physical damage and properties degradation during dry etching for device fabrication. Using an optimum condition to prepare the self-patternable PZT film, more than 5000 ${\AA}$ thick self-patternable PZT film could be fabricated by three times coating. The PZT film showed 28.4 ${\mu}$c/cm$^2$ of remnant polarization (Pr) and 37.0 kV/cm of coercive field (E$\_$c/).

Design and fabrication of microgripper using thermal actuator and SU-8 (열 구동 엑츄에이터와 SU-8을 이용한 마이크로 그리퍼 설계 및 제조)

  • Jung, Seoung-Ho;Park, Joon-Shik;Lee, Min-Ho;Park, Sang-Il;Lee, In-Kyu
    • Proceedings of the KSME Conference
    • /
    • 2007.05a
    • /
    • pp.1613-1616
    • /
    • 2007
  • A microgripper using thermal actuator and SU-8 polymer was designed and fabricated to manipulate cells and microparts. A chip size of a microgripper was 3 mm ${\times}$ 5 mm. The thermally actuated microgripper consisted of two couples of hot and cold arm actuators. The high thermal expansion coefficient, 52 $ppm/^{\circ}C$, of SU-8 compared to silicon and metals, allows the actuation of the microgripper. Thickness and width of SU-8 as an end-effector were 26 ${\mu}m$ and 80 ${\mu}m$, respectively. Initial gap between left jaw and right jaw was 120 ${\mu}m$. The ANSYS program as FEM tool was introduced to analyze the thermal distribution and displacement induced by thermal actuators. $XeF_2$ gas was used for isotropic silicon dry etching process to release SU-8 end-effector. Mechanical displacements of the fabricated microgripper were measured by optical microscopy in the range of input voltage from 0 V to 2.5 V. The maximum displacement between two jaws of a microgripper Type OG 1_1 was 22.4 ${\mu}m$ at 2.5 V.

  • PDF

Ion beam induced surface modifications of sapphire and gold film deposition: studies on the adhesion enhancement and mechanisms (Ion Beam을 이용한 사파이어($Al_2O_3$) 표면개질 및 금(Au) 박막증착: 접합성 향상 및 접학기구에 대한 연구)

  • 박재원;이광원;이재형;최병호
    • Journal of the Korean Vacuum Society
    • /
    • v.8 no.4B
    • /
    • pp.514-518
    • /
    • 1999
  • Gold (Au) is not supposed to react with sapphire(single crystalline ) under thermodynamic equillibrium, therefore, a strong adhesion between these two dissimilar materials is not expected. However, pull test showed that the gold film sputter-deposited onto annealed and pre-sputtered sapphire exhibited very strong adhesion even without post-deposition annealing. Strongly and weakly adhered samples as a result of the pull testing were selected to investigate the adhesion mechanisms with Auger electron spectroscopy. The Au/ interfaces were analyzed using a new technique that probes the interface on the film using Auger electron escape depth. It revealed that one or two monolayers of Au-Al-O compound formed at the Au/Sapphire interface when AES in the UHV chamber. It showed that metallic aluminum was detected on the surface of sapphire substrates after irradiating for 3 min. with 7keV Ar+ -ions. These results agree with TRIM calculations that yield preferential ion-beam etching. It is concluded that the formation of Au-Al-O compound, which is responsible for the strong metal-ceramic bonding, is due to ion-induced cleaning and reduction of the sapphire surface, and the kinetic energy of depositing gold atoms, molecules, and micro-particles as a driving force for the inter-facial reaction.

  • PDF

Development of having double-chamber in micro-bubble pump (두 개의 챔버를 갖는 마이크로 버블펌프의 개발)

  • 최종필;박대섭;반준호;김병희;장인배;김헌영
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2003.06a
    • /
    • pp.1186-1190
    • /
    • 2003
  • In this paper, a valveless bubble-actuated fluid micropump was has been developed and its performance was tested. The valveless micropump consists of the lower plate, the middle plate, the upper plate and a resistive heater. The lower plate includes the nozzle-diffuser elements and the double-chamber. Nozzle-diffuser elements and a double-chamber are fabricated on the silicon wafer by the DRIE(Deep Reactive Ion Etching) process. The lower plate also has inlet/outlet channels for fluid flow. The middle plate is made of glass and plays the role of the diaphragm. The chamber in the upper plate is filled with deionized water, and which contacts with the resistive heater. The resistive heater is patterned on a silicon substrate by Ti/Pt sputtering. Three plates and the resister heater are laminated by the aligner and bonded in the anodic bonder. Since the bubble is evaporated and condensed periodically in the chamber, the fluid flows from inlet to outlet with respect to the diffusion effect. In order to avoid backflow, the double chamber system is introduced. Analytical and experimental results show the validity of the developed double-chamber micropump.

  • PDF

A Study on the Fabrication Method of Mold for 2 inch LCD-BLU by 50μm Microlens : Effect of Different Aspect Ratio (50μm급 마이크로렌즈 적용 2인치 휴대폰 LCD-BLU 금형 개발 : 광학패턴의 세장비 영향)

  • Kim, J.S.;Ko, Y.B.;Min, I.K.;Yu, J.W.;Heo, Y.M.;Yoon, K.H.;Hwang, C.J.
    • Transactions of Materials Processing
    • /
    • v.16 no.1 s.91
    • /
    • pp.48-53
    • /
    • 2007
  • LCD-BLU(Liquid Crystal Display - Back Light Unit) consists of several optical sheets: LGP(Light Guiding Plate), light source and mold frame. The LGP of LCD-BLU is usually manufactured by etching process and forming numerous dots with $50{\mu}m$ in diameter on the surface. But the surface roughness of LGP with etched dots is very high, so there is much loss of light. In order to overcome the limit of current etched dot patterned LGP, optical pattern design with microlens of $50{\mu}m$ diameter was applied in the present study. The microlens pattern fabricated by modified LiGA with thermal reflow process was applied to the optical design of LGP and optical simulation was carried out to know tendency of microlens patterned LGP simultaneously. The attention was paid to the effects of different aspect ratio(i.e. $0.2\sim0.5$) of optical pattern conditions to the brightness distribution of BLU with microlens patterned LGP. Finally, high aspect ratio microlens patterned LGP showed superior results to the one made by low aspect ratio in average luminance.

비정질 탄소막 (a-C:H) 내에 존재하는 수소에 관한 연구

  • 박노길;박형국;손영호;정재인
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 1999.07a
    • /
    • pp.133-133
    • /
    • 1999
  • 비정질 탄소막 제조에 있어서 수소가 포함된 반응성 가스를 사용할 경우 제작된 탄소막 내부에는 수소가 포함되게 되며, 이러한 수소원자들은 막의 특성에 중요한 영향을 주는 것으로 알려져 있다. 따라서, 본 연구에서는 비정질 탄소막(a-C:H) 내부에 존재하는 수소가 탄소막의 특성에 미치는 영향을 알아보고, 막 내부에 포함된 수소의 함량과 공정조건 사이의 함수계를 조사함으로써 수소의 함량을 인위적으로 통제할 수 있는 가능성을 제시하고자 한다. 수소가 포함된 비정질 탄소막은 2.45 GHz의 전자기파를 사용하는 electron cyclotron resonance plasma enhanced chemical vapor deposition (ECR-PECVD) 방법과 DC magnetron sputtering 법을 사용하여 제작하였다. 기판으로는 Si(001) wafer를 사용하였으며, 아세톤과 에탄올을 사용하여 표면의 유기성분을 제거하고, 진공챔버속에서 Ar 플라즈마를 발생시켜 sputter etching 방법으로 표면을 세척하였다. ECR-PECVD 방법에서는 반응가스로 메탄(CH4)과 수소(H2)의 혼합가스를 사용하였으며, 혼합가스의 비는 5~50% 범위내에서 변화를 주었다. 수소가스의 유량은 100SCCM으로 고정하였으며, 마이크로웨이브의 power는 360~900W였고, 기판에 가해준 negative DC bias 전압은 0~-500V이었다. DC magnetron sputtering 방법에서는 반응가스로 아세틸린(C2H2) 가스를 사용하였으며, 플라즈마 발생을 용이하게 하기 위해서 Ar 가스와 혼합하여 사용하였다. Ar 가스의 유량은 10SCCM으로 고정하였으며, 아세틸렌 가스의 유량은 5~20SCCM 범위내에서 주입하였다. 이때, 기판에 가해준 negative DC bias 전압은 0~-100V이었다. 제작된 탄소막의 수소 함량을 조사하기 위하여 Fourier Transform Infrared (FTIR) 분광법과 Elastic Recoil Detection Analysis (EFDA) 법을 사용하였으며, 증착율은 SEM 단면촬영과 a-step을 이용하여 측정하였고, 막의 경도는 Micro-Hardness Testing 법을 사용하여 측정하였다.

  • PDF

Characteristics of Spray from Pressure-Swirl Nozzle with Different Liquid Properties and Nozzle Geometries (액체의 물성치와 노즐의 형상 변화에 따른 압력스월 노즐의 분무 특성)

  • Choe, Yun-Cheol;Jeong, Ji-Won;Kim, Deok-Jul
    • Transactions of the Korean Society of Mechanical Engineers B
    • /
    • v.25 no.12
    • /
    • pp.1813-1820
    • /
    • 2001
  • The purpose of this study was to investigate the significant characteristics in atomization process of industrial etching spray fur the design or Precise pressure-swirl nozzles. The experiment was carried out with different viscosities and densities of the liquid. The macro characteristics of liquid spray, such as the spray angle and breakup process were captured by PMAS and the micro characteristics of liquid spray. such as droplet size and velocity measurements were obtained by PDA. The droplet axial and radial velocity and SMD were measured along axial and radial direction. The RMS of two velocities was measured along radial direction. It was found that the fluid with higher kinematic viscosity resulted in the larger SMD and the lower mean droplet velocity. And we could divide breakup processes into three regions that is atomization, non-dilution and dilution one in spray of pressure-swirl nozzle. The radial as well as axial velocity of droplet played an important role in the atomization process of higher kinematic viscosity fluid.