• Title/Summary/Keyword: Mg-Ti-Ni

Search Result 181, Processing Time 0.027 seconds

Effect of NiO on Microstructure and Properties of PMN-PT-BT Ceramics Prepared by Mixed Oxide Method

  • Han, Kyoung-Ran;Jung, Jung-Woong;Kim, Chang-Sam
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.12 s.271
    • /
    • pp.884-888
    • /
    • 2004
  • Effects of NiO were studied in aspects of dielectric properties and microstructure of $0.96(0.91Pb(Mg_{1/3}Nb_{2/3})O_3-0.09PbTiO_3)­0.04BaTiO_3$ (PMN-PT-BT, PBT). The PBT was prepared by a conventional mixed oxide method using $(MgCO_3)_4{\cdot}Mg(OH)_2$ instead of MgO through Lewis acid-base interaction. NiO was added in the range of 0.5 to $3.0\;wt\%$ as thermally decomposable $2NiCO_3{\cdot}3Ni(OH)_2$ and it seemed to enhance densification to a large extent below $1000^{\circ}C$. But all the systems gave rise to ceramics with almost same relative sintered density of 96% by sintering at $1000^{\circ}C$ for 2 h. But it turned out that the addition of NiO was detrimental to dielectric constant but beneficial to the loss of dielectric constant.

Dielectric and Piezoelectric Characteristics of Ceramics in the $Pb(Mg_{1/2}W_{1/2})O_3-Pb(Ni_{1/3}Nb_{2/3})O_3-PbTiO_3-PbZrO_3$ system ($Pb(Mg_{1/2}W_{1/2})O_3-Pb(Ni_{1/3}Nb_{2/3})O_3-PbTiO_3-PbZrO_3$계 세라믹스의 유전 및 압전 특성)

  • Kim, Woo-Hyun;Yoon, Kwang-Hee;Yoon, Hyun-Sang;Park, Yong-Wook;Park, Chang-Yeop
    • Proceedings of the KIEE Conference
    • /
    • 1994.11a
    • /
    • pp.193-195
    • /
    • 1994
  • In this study, the structural, dielectric and piezoelectrical properties of $xPb(Mg_{1/2}W_{1/2})O_3-(1-x)[0.41Pb(Ni_{1/3}Nb_{2/3})O_3-0.36PbTiO_3-0.23P Zr)_3]$ (x=0, 0.01, 0.02, 0.03, 0.04, 0.05) system ceramics were investigated. The dielectric constant ${\varepsilon_{33}}^{\tau}$ at loon temperature increased up to 3mol% PMW and decreased with further PMW content. The specimen with 1mol% $Pb(Mg_{1/2}W_{1/2})O_3$, which has the ${\varepsilon_{33}}^{\tau}=5509$, kp=59[%] and $d_{33}=758{\times}10^{-12}[C/N]$, exhibits good characteristics.

  • PDF

Fabrication of Bulk Metallic Glass Alloys by Warm Processing of Amorphous Powders (비정질 분말의 열간 성형법에 의한 벌크 비정질합금의 제조)

  • 이민하;김도향
    • Journal of Powder Materials
    • /
    • v.11 no.3
    • /
    • pp.193-201
    • /
    • 2004
  • 1960년 Au-Si계 합금에서 처음으로 비정질상이 급속 응고법에 의해 보고된 이래/sup 1)/ 지난 40년 간 많은 합금계에서 비정질상이 보고되어졌다. 대표적으로 Fe-, Ni-, Co기 합금 등 많은 합금계에서 비정질상이 보고되었으나, 비정질상의 형성을 위해서는 약 105 K/s이상의 높은 냉각속도를 필요로 하였다. 1980년대 수백 K/s의 낮은 냉각속도 하에서도 비정질상이 형성될 수 있는 다원계 합금(multi-component alloy)이 Mg-Ln-(Ni, Cu, Zn), Ln-Al-TM 합금에서 보고되어 졌으나 많은 관심을 받지 못하다가 1993년 Zr-Ti-Ni-Cu-Be 합금에서 수 ㎝ 크기의 비정질합금 제조가 보고되면서 전 세계적으로 많은 관심을 받게 되었다. Zr-Ti-Ni-Cu-Be계 벌크 비정질 합금이 보고된 후 Zr-(Nb,Pd)-Al-TM, Pd-Cu-Ni-P, Fe-Co-Zr-Mo-W-B, Ti-Zr-Ni-Cu-Sn등 여러 합금계에서 벌크 비정질 합금이 보고되었다. (중략)

Synthesis and Properties of Amorphous Matrix Composites using Cu-based/Ni-based Amorphous Powders (Cu계 및 Ni계 비정질 합금 분말을 이용한 비정질기지 복합재의 제조 및 특성)

  • Kim Taek-Soo;Lee Jin-Kyu;Kim Hwi-Jun;Bae Jung-Chan
    • Journal of Powder Materials
    • /
    • v.12 no.6 s.53
    • /
    • pp.406-412
    • /
    • 2005
  • This work is to present a new synthesis of metallic glass (MG)/metallic glass (MG) composites using gas atomization and spark plasma sintering (SPS) processes. The MG powders of $Cu_{54}Ni_6Zr_{22}Ti_{18}$ (CuA) and $Ni_{59}Zr_{15}Ti_{13}Nb_7Si_3Sn_2Al_1$(NiA) as atomized consist of fully amorphous phases and present a different thermal behavior; $T_g$ (glass transition temperature) and $T_x$ (crystallization temperature) are 716K and 765K for the Cu base powder, but 836K and 890K for the Ni base ones, respectively. SPS process was used to consolidate the mixture of each amorphous powder, being $CuA/10\%NiA\;and\;NiA/10\%CuA$ in weight. The resultant phases were Cu crystalline dispersed NiA matrix composites as well as NiA phase dispersed CuA matrix composites, depending on the SPS temperatures. Effect of the second phases embedded in the MG matrix was discussed on the micro-structure and mechanical properties.

A Study on the Dielectric Properties of the Pb($Mg_{1/3}Nb_{2/3}$)$O_3$-$PbTiO_3$-Pb($Ni_\frac{1}{2}W_\frac{1}{2}$)$O_3$ Ceramics (Pb($Mg_{1/3}Nb_{2/3}$)$O_3$-$PbTiO_3$-Pb($Ni_\frac{1}{2}W_\frac{1}{2}$)$O_3$세라믹의 유전특성에 관한 연구)

  • 유남산;류기원;이성갑;이영희
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1990.10a
    • /
    • pp.65-67
    • /
    • 1990
  • In this study, (0.80-x)Pb($Mg_{1/3}Nb_{2/3}$)$O_3$-$PbTiO_3$-Pb($Ni_\frac{1}{2}W_\frac{1}{2}$)$O_3$ 0.05$\leq$x$\leq$0.20) ceramics were fabricated by the mixed oxide method, the sintering temperature and time were 950∼1200[$^{\circ}C$], 2[hr], respectively. The dielectric and structural properties with composition and sintering temperature were investigated for the application as multilayer ceramic capacitors. Dielectric constant of 0.70PMN-0.2PT-0.10PNW composition with repeated calcination was increased rapidly. Increasing the Pb($Mg_{1/3}Nb_{2/3}$)$O_3$-$PbTiO_3$-Pb($Ni_\frac{1}{2}W_\frac{1}{2}$)$O_3$ contents from 0.05 to 0.20 [mol], phase transition temperature was shifted from 68 to 2[$^{\circ}C$] and dielectric constant was decreased while sintered density was increased. In the specimens containing 0.10, 0.15[mol] of PNW, dielectri constants at room temperature were exhibited the highest values 11199, 10114, respectively. Resistivity of specimens were $10^{10}$$10^{12}$($\Omega$.m) and there was no dependence on sintering temperature and composition.

Effects of Catalyst Dispersion for Reaction Energy Control on Eco-AZ91 MgH2 (Eco-AZ91 MgH2의 반응열 제어에 미치는 촉매 분산 효과)

  • SOOSUN LEE;SONG SEOK;TAE-WHAN HONG
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.34 no.6
    • /
    • pp.631-640
    • /
    • 2023
  • This study selected Eco-AZ91 MgH2, which shows high enthalpy as a material for this purpose, as the basic material, and analyzed the change in characteristics by synthesizing TiNi as a catalyst to control the thermodynamic behavior of MgH2. In addition, the catalyst dispersion technology using graphene oxide (GO) was studied to improve the high-temperature aggregation phenomenon of Ni catalyst and to secure a source technology that can properly disperse the catalyst. XRD, SEM, and BET analysis were conducted to analyze the metallurgical properties of the material, and TGA and DSC analysis were conducted to analyze the dehydrogenation temperature and calorific value, and the correlation between MgH2, TiNi catalyst, and GO reforming catalyst was analyzed. As a result, the MgH2-5 wt% TiNi at GO composite could lower the dehydrogenation temperature to 478-492 K due to the reduction of the catalyst aggregation phenomenon and the increase in the reaction specific surface area, and an experimental result for the catalyst dispersion technology by GO could be ensured.

Effects of ${Er_2}{O_3}$ Addition on the Dielectric Properties of Non-reducible $BaTiO_3$-based X7R Dielectrics (${Er_2}{O_3}$첨가가 $BaTiO_3$계 내환원성 X7R 재질의 유전특성에 미치는 효과)

  • Park, Jae-Seong;Hwang, Jin-Hyeon;Han, Yeong-Ho
    • Korean Journal of Materials Research
    • /
    • v.11 no.1
    • /
    • pp.44-47
    • /
    • 2001
  • Effects of $Er_2O_3$ addition on the dielectric properties of non-reducible $BaTi_3$-based X7R dielectrics with Ni electrode have been studied in reducing atmosphere. X7R with moderate temperature-dependence was developed after addition of $Er_2O_3$ with $MnO_2-MgO$; room-temperature dielectric constant and dissipation factor were >2900 and < 1.0%, respectively. The addition of $Er_2O_3$ greater than 3.0 mol% improved the temperature dependence of dielectric properties, but a significant decrease of the dielectric constant at room-temperature was observed. The TCC curves rebated clockwise with increasing MnO$_2$ content at a given additive system, 1.5 mol% $Er_2O_3$ and 2.0 mol% MgO.

  • PDF

Electrochemical Properties of Ti/IrO2/SnO2-Sb-Ni Electrode for Water Treatment (수처리용 Ti/IrO2/SnO2-Sb-Ni 전극의 전기화학적 특성평가)

  • Yang, So Young
    • Journal of Environmental Science International
    • /
    • v.29 no.10
    • /
    • pp.943-949
    • /
    • 2020
  • In this work, we prepared a heterojunction anode with a surface layer of SnO2-Sb-Ni (SSN) on a Ti/IrO2 electrode by thermal decomposition to improve the electrochemical activity of the Ti/IrO2 electrode. The Ti/IrO2-SSN electrode showed significantly improved electrochemical activity compared with Ti/IrO2. For the 0.1 M NaCl and 0.1 M Na2SO4 electrolytes, the onset potential of the Ti/IrO2-SSN electrode shifted in the positive direction by 0.1 VSCE and 0.4 VSCE, respectively. In 2.0-2.5 V voltages, the concentration in Ti/IrO2-SSN was 2.59-214.6 mg/L Cl2, and Ti/IrO2 was 0.55-49.21 mg/L Cl2. Moreover, the generation of the reactive chlorine species and degradation of Eosin-Y increased by 3.79-7.60 times and 1.06-2.15 times compared with that of Ti/IrO2. Among these voltages, the generation of the reactive chlorine species and degradation of Eosin-Y were the most improved at 2.25 V. Accordingly, in the Ti/IrO2-SSN electrode, it can be assumed that the competitive reaction between chlorine ion oxidation and water oxidation is minimized at an applied voltage of 2.25V.

Influences of the Addition of Hydride-Forming Elements and Oxide and Hydriding-Dehydriding Cycling on the Hydriding and Dehydriding Characteristics of Mg

  • Song, Myoung Youp;Kwak, Young Jun;Park, Hye Ryoung
    • Korean Journal of Metals and Materials
    • /
    • v.50 no.5
    • /
    • pp.375-381
    • /
    • 2012
  • Magnesium prepared by mechanical grinding under $H_2$ (reactive mechanical grinding) with transition elements or oxides showed relatively high hydriding and dehydriding rates when the content of additives was about 20 wt%. Ni was chosen as a transition element to be added. $Fe_2O_3$ was selected as an oxide to be added. Ti was also selected since it was considered to increase the hydriding and dehydriding rates by forming Ti hydride. A sample $Mg-14Ni-3Fe_2O_3-3Ti$ was prepared by reactive mechanical grinding, and its hydrogen storage properties were examined. This sample absorbs 4.02 wt% H for 5 min, and 4.15 wt% H for 10 min, and 4.42 wt% H for 60 min at n = 2. It desorbs 2.46 wt% H for 10 min, 3.98 wt% H for 30 min, and 4.20 wt% H for 60 min at n = 2. The effects of the Ni, $3Fe_2O_3$, and Ti addition, and hydriding-dehydriding cycling were discussed.