Comparative evaluation of marginal and internal fit of metal copings fabricated by various CAD/CAM methods (다양한 CAD/CAM 방식으로 제작한 금속하부구조물 간의 변연 및 내면 적합도 비교 연구)

  • Jeong, Seung-Jin;Cho, Hye-Won;Jung, Ji-Hye;Kim, Jeong-Mi;Kim, Yu-Lee
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.57 no.3
    • /
    • pp.211-218
    • /
    • 2019
  • Purpose: The purpose of the present study was to compare the accuracy of four different metal copings fabricated by CAD/CAM technology and to evaluate clinical effectiveness. Materials and methods: Composite resin tooth of the maxillary central incisor was prepared for a metal ceramic crown and duplicated metal die was fabricated. Then scan the metal die for 12 times to obtain STL files using a confocal microscopy type oral scanner. Metal copings with a thickness of 0.5 mm and a cement space of $50{\mu}m$ were designed on a CAD program. The Co-Cr metal copings were fabricated by the following four methods: Wax pattern milling & Casting (WM), Resin pattern 3D Printing & casting (RP), Milling & Sintering (MS), Selective laser melting (SLM). Silicone replica technique was used to measure marginal and internal discrepancies. The data was statistically analyzed with One-way analysis of variance and appropriate post hoc test (Scheffe test) (${\alpha}=.05$). Results: Mean marginal discrepancy was significantly smaller in the Group WM ($27.66{\pm}9.85{\mu}m$) and Group MS ($28.88{\pm}10.13{\mu}m$) than in the Group RP ($38.09{\pm}11.14{\mu}m$). Mean cervical discrepancy was significantly smaller in the Group MS than in the Group RP. Mean axial discrepancy was significantly smaller in the Group WM and Group MS then in the Group RP and Group SLM. Mean incisal discrepancies was significantly smaller in the Group RP than in all other groups. Conclusion: The marginal and axial discrepancies of the Co-Cr coping fabricated by the Wax pattern milling and Milling/Sintering method were better than those of the other groups. The marginal, cervical and axial fit of Co-Cr copings in all groups are within a clinically acceptable range.

EFFECT OF TIME AND TEMPERATURE ON THE MARGINAL FIT OF PROVISIONAL RESIN CROWN DURING POLYMERIZATION (임시 수복물 중합시 시간과 중합온도가 변연 적합도에 미치는 효과)

  • Youn Seung-Hwan;Oh Nam-Sik;Kim Il-Kyu;Oh Sung-Seop;Choi Jin-Ho;Kim Wang-Sik;Rim Young-Il
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.39 no.5
    • /
    • pp.514-525
    • /
    • 2001
  • The purpose of this study was to compare the marginal fit of provisional restorations by differentiating the removal time and setting temperature during resin polymerization. After mixing autopolymerizing methyl methacrylate resin, the material was placed in a preformed resin shell crown. The crown was seated on a die with 1mm shoulder margin. Crowns were removed after 3, 4, 5, 6 minutes and polymerization was continued under the following conditions : $25^{\circ}C$ air, $30^{\circ}C,\;40^{\circ}C,\;50^{\circ}C,\;60^{\circ}C,\;70^{\circ}C$ water. After polymerization. the crown was sectioned. The marginal & occlusal discrepancies were measured. The mean marginal discrelpancies at 3 minutes, 4 minutes, 5 minutes and 6 minutes of removing time were $96.6{\mu}m.\;84.6{\mu}m,\;86.7{\mu}m$ and $105.6{\mu}m$. The mean occlusal discrepancies at 3 minutes, 4 minutes, 5 minutes and 6 minutes of removing time were $106.7{\mu}m,\;89.3{\mu}m,\;98.6{\mu}m$ and $127.7{\mu}m$. There was significant difference between 4 minutes group and 6 minutes group in occlusal discrepancies. The mean marginal & occlusal discrepancies for crowns polymerized in $25^{\circ}C$ air were $98.2{\mu}m$ and $124.1{\mu}m$. The crowns polymerized in $50^{\circ}C$ water demonstrated the smallest marginal & occlusal. discrepancies. The mean value of marginal & occlusal discrepancies in $50^{\circ}C$ water were $73.1{\mu}m$ and $77.5{\mu}m$. These values were smaller than that of $25^{\circ}C$ air. There were significant differences in the occlusal discrepancies between $25^{\circ}C$ air and water conditions of $50^{\circ}C$ water (${\alpha}=0.05$) but. no significant difference in marginal discrepancies. There was no significant difference in the interaction between time and temperature. 4 minutes waiting time & $50^{\circ}C$ water polymerizing condition produces the best fit at the margin of the provisional crown.

  • PDF

Comparison of fit accuracy and torque maintenance of zirconia and titanium abutments for internal tri-channel and external-hex implant connections

  • Siadat, Hakimeh;Beyabanaki, Elaheh;Mousavi, Niloufar;Alikhasi, Marzieh
    • The Journal of Advanced Prosthodontics
    • /
    • v.9 no.4
    • /
    • pp.271-277
    • /
    • 2017
  • PURPOSE. This in vitro study aimed to evaluate the effect of implant connection design (external vs. internal) on the fit discrepancy and torque loss of zirconia and titanium abutments. MATERIALS AND METHODS. Two regular platform dental implants, one with external connection ($Br{\aa}nemark$, Nobel Biocare AB) and the other with internal connection (Noble Replace, Nobel Biocare AB), were selected. Seven titanium and seven customized zirconia abutments were used for each connection design. Measurements of geometry, marginal discrepancy, and rotational freedom were done using video measuring machine. To measure the torque loss, each abutment was torqued to 35 Ncm and then opened by means of a digital torque wrench. Data were analyzed with two-way ANOVA and t-test at ${\alpha}=0.05$ of significance. RESULTS. There were significant differences in the geometrical measurements and rotational freedom between abutments of two connection groups (P<.001). Also, the results showed significant differences between titanium abutments of internal and external connection implants in terms of rotational freedom (P<.001). Not only customized internal abutments but also customized external abutments did not have the exact geometry of prefabricated abutments (P<.001). However, neither connection type (P=.15) nor abutment material (P=.38) affected torque loss. CONCLUSION. Abutments with internal connection showed less rotational freedom. However, better marginal fit was observed in externally connected abutments. Also, customized abutments with either connection could not duplicate the exact geometry of their corresponding prefabricated abutment. However, neither abutment connection nor material affected torque loss values.

THE EFFECTS OF SPURE AND INVENTS ON THE CASTING ACCURACY AND POROSITY OF TI-NI CASTINGS

  • Cho Lee-Ra;Yi Yang-Jin;Park Chan-Jin
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.41 no.3
    • /
    • pp.342-350
    • /
    • 2003
  • Statement of problem. Titanium-Nickel alloy might be used in various prosthetic restorations since it has a unique property such as super-elasticity and high fatigue resistance. However, little is known about the casting ability of this alloy. Purpose. This in vitro study compared the casting accuracy and the porosity made with different investments and various sprue designs to ascertain what casting condition would be better for the fabrication of Ti-Ni cast restorations. Material and methods. A total of 70 Ti-Ni alloy crowns were made and divided into 7 groups of 10 copings on a metal master die. For measuring the effect of the sprue numbers, two groups with one and two 8-gauge sprues were compared. Moreover, the results of the conventional sprue and the double thickness sprues were compared. Three investments were used; carbon free phosphate bonded investment, titanium investment and gypsum bonded investment. The cast restorations were evaluated at 48 points on the entire circumferential margin with a stereomicroscope measuring in micrometers. Each crown was radiographically examined for casting defects and porosity. Data on casting accuracy were analyzed using two-way and Post hoc Scheffe's comparison to determine whether significant differences existed at the 95% confidence level. Student-Newman-Keuls test were performed to identify significant differences in the number of voids. Results. The double sprueing group and double thickness group had significantly less marginal discrepancy than the single sprueing group (P<.05 and P<.01, respectively). The castings with phosphate bonded investment showed the least marginal discrepancy and the smoothest surface. The castings invested in the gypsum bonded investment had the greatest gaps in margin and the largest failure rate. The double sprueing group and phosphate bonded investment group had significantly smaller void numbers and smaller void size than the other groups. Conclusion. Within the limitations of this in vitro study, the casting accuracy of the groups using thicker, double sprue design and the phosphate bonded investment was significantly superior. Moreover, void number and size were less than other groups.

THE EFFECT OF SPRUE DESIGN ON THE MARGINAL REPRODUCIBILITY OF CAST TITANIUM CROWNS (주입선 형태가 티타늄 주조관의 변연재현성에 미치는 영향)

  • Park Jae-Kyoung;Jeong Chang-Mo;Jeon Young-Chan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.40 no.4
    • /
    • pp.352-364
    • /
    • 2002
  • There has been a great interest in the use of titanium for fixed and removable prostheses in recent because of its excellent biocompatibility. However the high melting temperature and chemical reactivity of titanium necessitates casting systems different from those used in conventional casting. The current titanium casting systems are based on an electric-arc design for melting the metal in an argon atmosphere and its exclusive investment. Despite the new developments in Ti casting systems, inadequate mold filling and internal porosity are frequently observed casting defects. Therefore, the study on the fabrication technique including sprue design to solve these casting defects is still necessary. In this study to evaluate the effect of sprue design on the castability of simulated cast titanium crowns, 10 cylindrical cast crowns for each group with four different sprue design(Single group. Double group, Runner bar group. Reservoir group) were fabricated. An impression of the entire casting margin was made and cut at $90^{\circ}$ intervals, and the sections were photographed in a microscope at $100{\times}$ magnification to record marginal discrepancy. The internal porosities of the cast crowns were disclosed by radiographs. Within the limits of this study. the following conclusions were drawn. 1. The overall mean marginal discrepancies for each group were as follows: Double group, $43.65{\mu}m$; Reservoir group, $50.27{\mu}m$; Single group, $54.17{\mu}m$; Runner bar group, $58.90{\mu}m$ (p<0.05). 2. The mean of marginal discrepancies for wax patterns was $10.65{\mu}m$. 3 The numbers of internal porosity showed the most in Runner bar group followed by Single group, Reservoir group, and Double group.

Effect of various casting alloys and abutment composition on the marginal accuracy of bar-type retainer (합금의 종류와 지대주 성분이 바형 유지 장치의 변연 적합도에 미치는 영향)

  • Lee, Yun-Hui;Song, Young-Gyun;Lee, Joon-Seok
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.50 no.2
    • /
    • pp.85-91
    • /
    • 2012
  • Purpose: The object of this study was to determine if the low-priced alloy and metal UCLA abutment could be available for manufacturing bar-retained framework of implant prosthesis. Materials and methods: Bar structure was classified into 4 groups, The specimen of group 1 and 2 were based on casting high noble metal alloys and noble metal alloys with gold UCLA abutment. The specimen of group 3 and 4 were based on casting noble metal alloys and base metal alloys with metal UCLA abutment. Cast bar structure was installed in an acrylic resin model and only the screw on the hexed abutment side was tightened to 20 Ncm. On the opposite side, vertical discrepancy was measured with stereo microscope from front, back, and lateral side of the implant-abutment interface. One-way ANOVA was performed to analyze the marginal fit discrepancy. Results: One-way ANOVA test showed significant differences among all groups ($P$<.05) except for Group 1 and 3. Among them, difference between Group 1 and 2 was noticeable. Measured vertical discrepancies were all below $70{\mu}m$ except to Group 2. Conclusion: Base metal alloy and metal UCLA abutment could be used as an alternative to high-priced gold alloy for implant bar-retained framework.

Fracture load and marginal fitness of zirconia ceramic coping by design and coloration (유색 및 백색 지르코니아 세라믹 코핑의 코핑 디자인에 따른 파절 하중과 변연 적합성)

  • Shin, Mee-Ran;Kim, Min-Jeong;Oh, Sang-Chun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.47 no.4
    • /
    • pp.406-415
    • /
    • 2009
  • Purpose: The purpose of this study was to compare the marginal fitness and fracture load of the zirconia copings according to the design with different thickness and coloration. Material and methods: The evaluation was based on 80 zirconia copings. Zirconia copings were fabricated in design with different thicknesses using CAD/CAM system (Everset, KAVO dental GmbH, Biberach, Germany). The designs of copings were divided into four groups. The first group consisted of copings with uniform thickness of 0.3 mm. The thickness in the second group was 0.3 mm on the buccal surface and 0.6 mm on the lingual surface. The third group consisted of coping with uniform thickness of 0.6 mm. The thickness in the fourth group was 0.6 mm on the buccal surface and 1mm on the lingual surface. Each group consisted of 10 colored and 10 uncolored copings. Half of the copings (40) processed with a milling system according to the specific design were sent to be given a color (A3) through saturation in special dye by a manufacturing company. Just after sintering, the marginal discrepancies of copings were measured on the buccal, lingual, mesial and distal surfaces of metal die, under a Video Microscope System (sv-35, Sometech, Seoul, Korea) at a magnification of $\times$ 100. It was remeasured after the adjusting of the inner surface. Next, all copings were luted to the metal dies using reinforced cement {GC FujiCEM (GC Corp. Tokyo, Japan)} and mounted on the testing jig in a Universal Testing Machine (Instron 4467, Norwood, MA, USA). The results were analyzed statistically using the one-way ANOVA test. Results: The obtained results were as follow: 1. The measured value of marginal discrepancy right after sintering was the greatest in the contraction of the buccal area in all groups, except for group I2. 2. There was no significant difference of marginal fitness among the groups in the colored zirconia group (P<.05). 3. When the marginal fitness among the groups in the uncolored zirconia group was considered, group II2 had the smallest marginal discrepancy. 4. When the colored and uncolored groups with the same design were compared, there was a significant difference between I1 and II1 groups. In group 2, 3, and 4, the uncolored zirconia had the greatest marginal fitness (P<.05). 5. After adjustment of inner surface, there was no significant difference in the marginal fitness in all groups when color and design of the zirconia coping were compared. 6. The fracture load of CAD/CAM zirconia copings showed significant difference in group 1, 2, 3, and 4. I4 and II4 had the strongest fracture load. 7. When groups with different color and same design were compared, all colored groups showed greater fracture load (P>.05), with no significance. Conclusion: There was difference in the marginal fitness according to the design and coloration of zirconia copings right after sintering, but it was decided that the copings may well be used clinically if the inner surface are adjusted. The copings should be thick enough for the reinforcement of fracture strength. But considering the esthetics of the visible surfaces (labial and buccal surface), the thickness of copings may be a little thin, without giving any significant effect on the fracture strength. This type of design may be considered when giving priority to preservation of tooth or esthetics.

The marginal fidelity of $Procera^{(R)}$ AllCeram alumina copings and crowns of patients ($Procera^{(R)}$ AllCeram 을 이용한 도재관의 임상적 변연적합도에 관한 연구)

  • Song, Young-Gyun;Cho, In-Ho;Lee, Jong-Hyuk
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.46 no.5
    • /
    • pp.470-478
    • /
    • 2008
  • Statement of problem: Use of all-ceramic prostheses fabricated with CAD/CAM systems is increasing in the dentistry. Marginal fidelity in production of all-ceramic restoration has important clinical implications and is a key consideration issue in CAD/CAM production as well. Purpose: The objective of this study was to analyse marginal fidelities of $Procera^{(R)}$ Allceram Crown. Material and methods: On 56 patients treated with $Procera^{(R)}$ system Allceram Crown at Dankook Dental Hospital, marginal discrepancies of 101 abutments were measured by stereomicroscope at coping and final restoration stages. Paired t-test and one-way analysis of variance on marginal discrepancy data were conducted to determine the presence of significant differences between measurement and measuring point stages. Results: Marginal discrepancies of final restoration ($45.82{\pm}30.84\;{\mu}m$) were lower than alumina coping ($53.84{\pm}38.83\;{\mu}m$). Furthermore, the differences were found to be statistically significant at 95% confidence level. Anterior marginal discrepancies were lower than posterior marginal discrepancies, but they were not statistically significant. Lingual marginal discrepancies were higher than other measurement sites, and the differences were found to be statistically significant at 95% confidence level. Conclusion: Within the conditions of this study, marginal fidelities of $Procera^{(R)}$ Allceram Crown were acceptable, and after porcelain build-up, marginal fitness improved over alumina coping. More careful scanning is needed for better results.

Revisiting the virial factor with the updated $M_{BH}-{\sigma}_*$ relation

  • Park, Dae-Seong;Woo, Jong-Hak
    • The Bulletin of The Korean Astronomical Society
    • /
    • v.37 no.1
    • /
    • pp.35.1-35.1
    • /
    • 2012
  • Determining the virial factor of the broad-line region (BLR) gas is crucial in calibrating AGN black hole mass estimators, since the measured line-of-sight velocity needs to be converted into the representative velocity of the BLR gas. The unknown virial factor has been empirically calibrated based on the $M_{BH}-{\sigma}_*$ relation of non-AGN galaxies, but the claimed values are different by a factor of 2 in recent studies. We investigate the origin of the difference by measuring the $M_{BH}-{\sigma}_*$ relation using the most updated nearby galaxy sample, and explore the dependence of the virial factor on the various fitting methods. We find that the discrepancy is mostly caused by the sample bias while the difference stemming from various regression methods is marginal. Based on the best-determined virial factor, we present the updated $M_{BH}-{\sigma}_*$ relation of local active galaxies.

  • PDF

A comparison of the fidelity of various zirconia-based all-ceramic crowns fabricated with CAD/CAM systems (수종의 CAD/CAM 시스템으로 제작한 지르코니아 기반 완전도재관의 적합도 비교)

  • Kim, Sung-Jun;Jo, Kwang-Hun;Lee, Kyu-Bok
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.47 no.2
    • /
    • pp.148-155
    • /
    • 2009
  • Statement of problem: The interest in all-ceramic restorations has increased as more techniques have become available. With the introduction of machinable dental ceramics and CAD/CAM systems there is a need to evaluate the quality levels of these new fabrication techniques. Purpose: This study is to evaluate the crown fidelity(absolute marginal discrepancy and internal gap) of various zirconia-based all-ceramic crowns fabricated with different CAD/CAM(computer-assisted design/computer-assisted manufacturing) systems and conventional cast metal-ceramic crowns. Material and methods: A resin tooth of lower right second premolar was prepared. After an impression was taken, one metal master die was made. Then 40 impressions of metal master dies were taken for working dies. 10 crowns per each system were fabricated using 40 working dies. Metal-ceramic crowns were cast by using the conventional method, and Procera, Lava, and Cerec inLab crowns were fabricated with their own CAD/CAM manufactruing procedures. The vertical marginal discrepancies and internal gaps of each crown groups were measured on a metal master die without a luting agent. The results were statistically analyzed using the one-way ANOVA and Tukey's HSD test. Results: 1. Vertical marginal discrepancies were $50.6{\pm}13.9{\mu}m$ for metal-ceramic crowns, $62.3{\pm}15.7{\mu}m$ for Procera crowns, $45.3{\pm}7.9{\mu}m$ for Lava crowns, and $71.2{\pm}2.0{\mu}m$ for Cerec inLab crowns. 2. The Internal gaps were $52.6{\pm}10.1{\mu}m$ for metal-ceramic crowns, $161.7{\pm}18.5{\mu}m$ for Procera crowns, $63.0{\pm}10.2{\mu}m$ for Lava crowns, and $73.7{\pm}10.7{\mu}m$ for Cerec inLab crowns. Conclusion: 1. The vertical marginal discrepancies of, 4 crown groups were all within the clinically acceptable range($120{\mu}m$). 2. The internal gaps of LAVA, Cerec inlab, and metal-ceramic crowns were within clinically acceptable range except Procera crown($140{\mu}m$).