The Resistance of Penetrability and Diffusion of Chloride Ion in Blended Low Heat Type Cement Concrete (저발열형 시멘트 콘크리트의 염소이온 침투$\cdot$확산에 대한 저항성)

  • 문한영;신화철
    • Journal of the Korea Concrete Institute
    • /
    • v.11 no.4
    • /
    • pp.31-41
    • /
    • 1999
  • Blended Low Heat type cement is ground granulated blast furnace slag and fly ash mixed ternary with ordinary portland cement. From the viewpoint of X-ray patterns of domestic LHC, the main components of cement such as $C_2$S, $C_3$A, $C_3$S are considerably reduced. Therefore the heat evolution of LHC paste is 42cal/g lower than of OPC paste. At early age, the compressive strength development of LHC concrete is delayed, but the slump loss ratio of fresh concrete is reduced more than 20% with elapsed time. The penetrability of LHC is lower than that of OPC by 1/7.8 with the penetrability of chloride ion into the concrete until the age of 120 days. And the PD Index value of LHC is 0.44$\times$10-6 $\textrm{cm}^2$/s, which indicates only 39.3% of OPC. From the Mercury Intrusion Porosimetry test of cement past, we know that the pore size of LHC is more dense than that of OPC by production of C-S-H.

A Comparison Study Between Evaluation Methods on the Rheological Properties of Cement Paste (시멘트 페이스트의 유동 특성에 관한 평가방법 비교연구)

  • Han Cheon-Goo;Lee Gun-Cheol;Heo Young-Sun
    • Journal of the Korea Institute of Building Construction
    • /
    • v.6 no.3 s.21
    • /
    • pp.75-82
    • /
    • 2006
  • This study investigates the influence of various blending factors on cement paste fluidity and find out the most effective evaluation method of cement paste flow, comparing flow test apparatuses such as ring flow(R-F), flow cone(F-C) and mini slump(M-S). A viscometer also measures the rheology coefficients to secure faithful numerical data. Firstly, series I examines cement paste, affected by several cement products and mineral admixture types in the range of W/B 40%, ordinary fluidity, and W/B 30%, high fluidity. In this series, the three types of cement product depended on companies, are randomly used and the mineral admixture, such as fly ash, blast furnace slag and silica fume, are incorporated in the cement paste, in response to the ratio of 10, 20, to 30%, respectively. In addition, series II studies various chemical admixture types, affecting the cement paste. This series is carried out with manufacturing companies and component types in the range of W/C 30%, high fluidity. For the manufacturing companies, randomly four products are used and for the component types, polycaboxylate, melamine, naphthalene and lignosulfonate type are chosen. Test results showed that in the fluidity test of cement paste considering various types of blending factors, R-F exhibited similar tendency with F-C and M-S. In the analysis of consistency curves measured by viscometer, the fluidity evaluation method using flow test apparatuses was significantly effective, except for the some of the low fluidity specimens. In conclusion of this study, R-F was the most convenient, faithful and effective fluidity evaluation method of cement paste.

A Study on Physical Properties of Concrete using Admixtures for High Strength Concrete (고강도콘크리트용 혼화재를 사용한 콘크리트의 물성에 관한 연구)

  • 이승한
    • Magazine of the Korea Concrete Institute
    • /
    • v.7 no.2
    • /
    • pp.155-164
    • /
    • 1995
  • This study was performed to get high strength of the precase concrete adopting a steam curing by using a gypsum-admixture for the high strength concrete. The superplasticizer was used to compensate low slump of base concrete keeping its slump up about $6{\pm}1cm$. To examine the property for strength revelation of concrete using admixtures for a high strength concrete, steam and standard curing were compared each other. Test results were shown that admixtures for high strength concrete were more effective in steam curing than standard curing. On the condition that the unit cement content is about $530{\sim}600kg/m^3$, the compressive strength of concrete replacing by 10% of the admixture was obtained over $65Okgf/cm^2$, which was increased as 1.3 times as that for the nonreplacement. When the admixture was replaced to 15-30%, the compressive strengh was obtained over $700kgf/cm^2$ which was increased as 1.4 - 1.5 times. Therefore, the admixture for high strength concrete, being effective in steam curing, was more efficient to get a high strength concrete using only steam curing instead of an autoclave curing for the secondary products of cement.

A study on properties of ultra high strength concrete of above 100MPa - fluidity and rheology properties (100MPa급 이상의 초고강도 콘크리트의 특성에 관한 연구 - 유동성 및 rheology 특성)

  • Seo, Il;Lee, Jin-Woo;Park, Hee-Gon;Bae, Yeon-Ki;Cho, Sung-Hyun;Lee, Han-Seung
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.11a
    • /
    • pp.317-320
    • /
    • 2008
  • In recent year, the ultra high strength concrete has highly increased and been used in many parts of the world. However, the viscosity of the ultra high strength concrete is high because of a low water to binder ratio (w/b). So that in this pater, the shear stress and the shear strain rate are directly measured by the viscometer in order to estimate the rheological properties of the ultra high strength concrete and a linear regression analysis was carried out to determine the plastic viscosity and the yield stress as slope. According to the test results, the yield stress and plastic viscosity are correlated to slump-flow, V-funnel flow time, O-lot flow time

  • PDF

A Fundamental Study on the Superplasticized Concrete (유동화(流動化)콘크리트에 관한 기초연구(基礎研究))

  • Moon, Han Young
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.2 no.2
    • /
    • pp.47-59
    • /
    • 1982
  • It is well practised in the field of concrete engineering that the effort of improving the low slumped concrete and uplifting the quality of the soft concrete by adopting the superplasticizer. In this paper, an attempt is made to find out the optimum mix design of the superplasticized concrete with an unit weight of cement 400 kg and the range of $19{\pm}1cm$ of slump by variatlng the sand percentage, unit water content and the dosage of superplasticizer. As a result, the author obtained the basic idea on the optimum mix design and strength of superplasticized concrete. On the other hand, it is also considered during the research the method of preventing the slump loss of the superplasticized concrete due to the delayed time after concrete mixing.

  • PDF

Shear behavior of foam-conditioned gravelly sands: Insights from pressurized vane shear tests

  • Shuying Wang;Jiazheng Zhong;Qiujing Pan;Tongming Qu;Fanlin Ling
    • Geomechanics and Engineering
    • /
    • v.34 no.6
    • /
    • pp.637-648
    • /
    • 2023
  • When an earth pressure balance (EPB) shield machine bores a tunnel in gravelly sand stratum, the excavated natural soil is normally transformed using foam and water to reduce cutter wear and the risk of direct muck squeezing out of the screw conveyor (i.e., muck spewing). Understanding the undrained shear behavior of conditioned soils under pressure is a potential perspective for optimizing the earth pressure balance shield tunnelling strategies. Owing to the unconventional properties of conditioned soil, a pressurized vane shear apparatus was utilized to investigate the undrained shear behavior of foam-conditioned gravelly sands under normal pressure. The results showed that the shear stress-displacement curves exhibited strain-softening behavior only when the initial void ratio (e0) of the foam-conditioned sand was less than the maximum void ratio (emax) of the unconditioned sand. The peak and residual strength increased with an increase in normal pressure and a decrease in foam injection ratio. A unique relation between the void ratio and the shear strength in the residual stage was observed in the e-ln(τ) space. When e0 was greater than emax, the fluid-like specimens had quite low strengths. Besides, the stick-slip behavior, characterized by the variation coefficient of measured shear stress in the residual stage, was more evident under lower pressure but it appeared to be independent of the foam injection. A comparison between the results of pressurized vane shear tests and those of slump tests indicated that the slump test has its limitations to characterize the chamber muck fluidity and build the optimal conditioning parameters.

Carbonation Properties of Recycled Aggregate Concrete by Specified Concrete Strength (설계기준 강도별 순환골재 콘크리트의 탄산화 특성)

  • Lee, Jun;Lee, Bong-Chun;Cho, Young-Keun;Park, Kwang-Min;Jung, Sang-Hwa
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.1
    • /
    • pp.85-93
    • /
    • 2017
  • This paper presents mechanical properties and carbonation behavior of the recycled aggregate concretes(RAC) in which natural aggregate was replaced by recycled coarse aggregate and fine aggregate by specified concrete strength levels(21, 35, 50MPa). A total of 18 RAC were produced and classified into six series, each of which included three mixes designed with three specified concrete strength levels of 21MPa, 35MPa and 50MPa and three recycled aggregate replacement ratios of 0, 50 and 100%. Physical and mechanical properties of RAC were tested for slump test, compressive strength, and carbonation depth. The test results indicated that the slump of RAC could be improved or same by recycled coarse aggregate replacement ratios, when compared with natural aggregate. But slump of RAC was decreased as the recycled fine aggregate replacement ratios increase. Also, the test results showed that the compressive strength was decreased as the recycled aggregate replacement ratios increased and it had a conspicuous tendency to decrease when the content of the recycled aggregate exceeded 50%. Furthermore, the result indicated that the measured carbonation depth increases by 40% with the increase of the recycled aggregate replacement. In the case of the concrete having low level compressive strength, the increase of carbonation depth tends to be higher when using the RCA. However, the trend of carbonation resistivity in high level compressive strength concrete is similar to that obtained in natural aggregate concrete. Therefore, an advance on the admixture application and mix ratio control are required to improve the carbonation resistivity when using the recycled aggregate in large scale.

Compressive Strength Evaluation of Concrete with Mixed Plastic Waste Aggregates Filled with Blast Furnace Slag Fine Powder (무기충진재를 혼입한 복합 폐플라스틱 골재를 활용한 콘크리트 압축강도 특성)

  • Lee, Jun;Kim, Kyung-Min;Cho, Young-Keun;Kim, Ho-Kyu;Kim, Young-Wook
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.9 no.3
    • /
    • pp.253-259
    • /
    • 2021
  • Plastic wastes generated from household waste are separated by mixed discharge with foreign substances, and recycling is relatively low. In this study, the effect of the ratio and content of mixed plastic waste coarse aggregate(MPWCA)s and mixed plastic waste fine aggregate(MPWFA)s filled with blast furnace slag fine powder on the slump and compressive strength of concrete was evaluated experimentally. The MPWCAs were found to have a similar fineness modulus, but have a single particle size distribution with a smaller particle size compared to coarse aggregates. However, the MPWFAs were found to have a single particle size distribution with a larger fineness modulus and particle size compared to fine aggregates. Meanwhile, the effect of improving the density and filling pores by the blast furnace slag fine power was found to be greater in the MPWFA compared to the MPWCA. As the amount of the mixed plastic waste aggregate(MPWA)s increased, the slump and compressive strength of concrete decreased. In particular, the lower the slump and compressive strength of concrete was found to decrease the greater the amount of MPWFA than MPWCA when the amount of MPWA was the same. This is because of the entrapped air and voids formed under the angular- and ROD-shaped aggregates among the MPWFAs. On the other hand, the addition of the admixture and the increase in the unit amount of cement were found to be effective in improving the compressive strength of the concrete with MPWAs.

Performance Evaluation of Concrete using Performance Improving-type Polycarboxylic acid-based Admixture (성능개선형 폴리카르본산계 혼화제를 사용한 콘크리트의 성능평가에 관한 실험적 연구)

  • Seo, Tae-Seok;Choi, Hoon-Jae;Gong, Min-Ho
    • Journal of the Korea Institute of Building Construction
    • /
    • v.17 no.5
    • /
    • pp.445-451
    • /
    • 2017
  • Because of the supply-demand problem of aggregate, recently, the construction sites using 100% crushed sand are increasing and the use of low quality aggregate such as farmland sand is increasing too. When the low quality aggregate is used, the various quality defect of concrete such as the strength reduction, the increase of shrinkage and bleeding can be occurred. Therefore, in this study, the performance improvement PC admixture was developed to minimize the quality defect of plain concrete of basement parking area, when the low quality aggregate was used at the plain concrete of basement parking area. The slump loss to elapsed time test, the compressive strength test, the bleeding test and the drying shrinkage test were carried out.

Study on Hydration Heat Analysis of Pier Foundation-Column Using Low Heat Concrete (저발열 콘크리트를 사용한 교각 기초-기둥의 수화열 해석에 관한 연구)

  • Jeon, Joong-Kyu;Kim, Sun-Gil;Jeon, Chan-Ki;Kim, Ki-Hyung
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.2 no.3
    • /
    • pp.217-224
    • /
    • 2014
  • This study carried out to evaluate the hydration heat analysis and fundamental characteristics such as air content, slump and compressive strength for field application of low heat concrete with premixed cement. The results of experiment show that low heat concrete with premixed cement have sufficient performances on the workability and compressive strength. In addition, hydration heat analysis shows that low heat concrete with premixed cement make sure of target thermal cracking index. Therefore, it is desirable to apply the low heat concrete with premixed cement on pier foundation-column.