  • The laser ablation/ionization time-of-flight mass spectrometry is applied to the isotopic analysis of solid samples using a home-made instrument. The technique is convenient for solid sample analysis due to the onestep process of vaporization and ionization of the samples. The analyzed samples were lead, cadmium, molybdenum, and ytterbium. To optimize the analytical conditions of the technique, several parameters, such as laser energy, laser wavelength, size of the laser beam on the samples surface, and high voltages applied on the ion source electrodes were varied. Low energy of laser light was necessary to obtain the optimal mass resolution of spectra. The 532 nm light generated mass spectra with the higher signal-to-noise ratio compared with the 355 nm light. The best mass resolution obtained in the present study is ~1,500 for the ytterbium.

레이저 보조선삭 중 주철환봉 내부의 온도분포 예측에 관한 연구 (A study for prediction of temperature distribution in laser-assisted turning for rod-shaped cast iron)

  • 김관우;조해용;이제훈;서정;신동식
    • 한국레이저가공학회지
    • /
    • 제13권2호
    • /
    • pp.10-16
    • /
    • 2010
  • Laser-assisted machining is dependent on absorbed energy density into workpiece. Generally, the absorptivity of laser beam is dependent on wave length of laser, materials, surface roughness, etc. Various shapes and energy densities for beam irradiation can be used to laser-assisted machining. In this thesis, efficient method of heat source modeling was developed and designed by using one fundamental experimental trials. And then, laser-assisted machining of rod-shaped cast iron was simulated by using commercial FEM code MARC. Simulations and experiments with various conditions were carried out to determine suitable condition of pre-heating for laser-assisted turning process. Temperature distribution of cutting zone could be predicted by simulation.

  • PDF

펄스 Nd:YAG 레이저에 의한 브라운관 부품의 용접시 빔의 출력특성과 광학변수 (Characteristics of Output Energy and Optical Parameters in Welding of Braun Tubes by Pulsed Nd:YAG Laser)

  • 김종도;하승협
    • 한국레이저가공학회지
    • /
    • 제8권1호
    • /
    • pp.27-37
    • /
    • 2005
  • During laser spot welding of the braun tube electron gun, phenomena such as serious spattering and oxidative reaction, etc. were occurred. The spatter occurred from weld pool affects the braun tube, namely it blocks up a very small hole on the shadow mask and causes short circuit between two poles of the electron gun. We guessed that high power density and oxidative reaction are main sources of these problems. So, we studied to prevent and to reduce spatter occurring in spot welding of the braun tube electron gun using pulsed Nd:YAG laser. The characteristics of laser output power was estimated, and the loss of laser energy by optical parameter and spatter was measured by powermeter. The effects of welding parameters, laser defocused distance and incident angle, were investigated on the shape and penetration depth of the laser welded bead in flare and flange joints. From these results, the laser peak power was a major factor to control penetration depth and to occur spatter. It was found that the losses of laser energy by optic parameter and sticked spatter affect seriously laser weldability of thin sheets.

  • PDF

Laser Welding Quality Monitoring with an Optical Fiber System

  • Kim, Jin-Tae;Kim, Do-Hyoung;Chung, Chin-Man;Baik, Sung-Hoon;Park, Seung-Kyu;Kim, Min-Suk
    • Journal of the Optical Society of Korea
    • /
    • 제7권3호
    • /
    • pp.193-196
    • /
    • 2003
  • We have developed a laser welding monitoring system to monitor laser welding process conditions such as sample feed rate, laser focal position, and laser power. A 2 ㎾ Nd:YAG CW laser beam has been applied to the welding of a stainless steel plate (SUS306) to investigate the welding monitoring. Theradiation signal from the weld pool was guided back through the focusing optics and the laser delivery fiber, and measured by a photo detector. By changing the focus of the laser beam along the z-direction, the penetration depth of the welding material has been measured. That shows the penetration depth depends on the frequency fluctuations of the plume signals which can be used in welding quality control.

레이저를 이용한 미세에칭에 관한 연구 (A Study on the Argon Laser Assisted Thermochemical Micro Etching)

  • 박준민;정해도
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.844-847
    • /
    • 2001
  • The application of laser direct etching has been discussed, and believed that the process is a very powerful method for micro machining. This study is focused on the micro patterning technology using laser direct etching process with no chemical damage of the material surface. A new introduced concept of energy synergy effect for surface micro machining is the combination of chemically ion reaction and laser thermal process. The etchant can't etch the material in room temperature, and used Ar laser has not power enough to machine. But, the machining is occurred in local area of the material by the combined energy. Using this process, the material is especially prevented from chemical damage for electric property. We have tested this new concept, and achieved a line with $1{mu}m$ width. The Ar laser with 488nm wavelength was used. The material was Si(100) wafer, and etchant is KOH solution. The application and flexibility of this process is in great hopes for MEMS structures and fabrication of the micro electric device parts.

  • PDF

The effect of laser energy on the preparation of iron oxide by a pulsed laser ablation in ethanol

  • Maneeratanasarn, P.;Khai, T.V.;Choi, B.G.;Shim, K.B.
    • 한국결정성장학회지
    • /
    • 제22권3호
    • /
    • pp.134-138
    • /
    • 2012
  • Recently the preparation magnetic nanoparticles by a pulsed laser ablation in liquid has gained much attention because it is easy to control experimental parameters. Iron oxide magnetic nanoparticles have been prepared by a pulsed laser ablation of ${\alpha}-Fe_2O_3$ target in ethanol at different magnitude of laser energy of 1, 20, 40 and 80 mJ/pulse. It revealed that particle size increases with increasing laser energy. It could be concluded that 40 mJ/pulse is an optimum laser energy for the preparation of iron oxide nanoparticles with uniform size distribution. The nanoparticles are homogeneously dispersed in ethanol and their stability maintained for several months.

High Power Lasers and Their New Applications

  • Izawa, Yasukazu;Miyanaga, Noriaki;Kawanaka, Junji;Yamakawa, Koichi
    • Journal of the Optical Society of Korea
    • /
    • 제12권3호
    • /
    • pp.178-185
    • /
    • 2008
  • Recent progress in high power lasers enables us to access a regime of high-energy-density and/or ultra-strong fields that was not accessible before, opening up a fundamentally new physical domain which includes laboratory astrophysics and laser nuclear physics. In this article, new applications of high-energy and ultra-intense laser will be reviewed.

Cu/Polyamide 혼합분말의 선택적 레이저 소결 (Selective Laser Sintering of Cu/Polyamide Mixed Powder)

  • 박흥일;이길근
    • 한국분말재료학회지
    • /
    • 제8권4호
    • /
    • pp.239-244
    • /
    • 2001
  • To investigate the effect of process parameters on selective laser sintering of Cu/polyamide mixed powder, Cu/polyamide mixed powder was sintered by selective laser with changing laser power and scanning speed. The properties of sintered body were evaluated by measuring the density and tensile strength, and analysis of XRD, FT-Raman and microstructure. With an increase in the laser power, the density and ultimate tensile strength of sintered Cu/polyamide body increase and then decrease. The maximum values of the density and ultimate tensile strength were decreased with increasing laser scanning speed. These changes were concerned with the difference of irradiation energy of laser into the powder layer. It was considered that the change of the mechanical property of the sintered body with irradiation energy of laser is due to the changes of amount of copper particle and property of polyamide.

  • PDF

High-resolution Spectroscopy of the Nickel-like Molybdenum X-ray Laser Toward the Generation of Circularly Polarized X-ray Laser

  • Hasegawa, Noboru;Sasaki, Akira;Yamatani, Hiroshi;Kishimoto, Maki;Tanaka, Momoko;Ochi, Yoshihiro;Nishikino, Masaharu;Kunieda, Yuichi;Kawachi, Tetsuya;Yoneda, Hitoki;Iwamae, Atsushi
    • Journal of the Optical Society of Korea
    • /
    • 제13권1호
    • /
    • pp.60-64
    • /
    • 2009
  • We attempted the first measurement of the spectral width of the nickel-like molybdenum x-ray laser (${\lambda}\;=\;18.895\;nm$) by use of a high-resolution spectrometer in order to determine the strength of the magnetic field required for the generation of a circularly polarized x-ray laser. The spectral width was measured to be ${\Delta}{\lambda}\;=\;18\;m{\AA}$ under the substantial lasing condition. The magnetic field required for the generation of a circularly polarized x-ray laser was 40 T. The splitting of the x-ray laser line was clearly obtained under 15 T external magnetic field. The strength of the magnetic field estimated from the splitting of the x-ray laser line was large compared with the external magnetic field. It implies that there might be an alternative mechanism for enhancement of the magnetic field in the gain medium plasma.

Performance Improvement of Flashlamp-Pumped Ti: sapphire Laser

  • Xia, Jinan;Lee, Min-Hee;Eur, Jeong-Pil
    • Journal of the Optical Society of Korea
    • /
    • 제6권2호
    • /
    • pp.48-54
    • /
    • 2002
  • Experimental study is performed on flashlamp-pumped Ti: sapphire lasers with single, double, and four-partial-ellipse-pump cavities aiming at improving the performance of the lasers. The output energy of 604 mJ per pulse with a width of 25 $\mu$s at a total laser efficiency of 0.13% is achieved in the laser pumped by a light pulse of 45$\mu$s without a fluorescent converter The laser output energy versus its Ti: sappy ire rod length, pumping-light pulse duration, and electrical input energy are discussed with or without using a fluorescent converter. The result shows that much more output energy is obtained il a longer Ti: sapphire-rod laser pumped by a shorter light pulse when its output coupler has an optimized transmittance. In addition, an enhancement of output energy by a factor of 7 is achieved. in the laser using a fluorescent converter LD490.