Monitoring the Degradation Process of Inconel 600 and its Aluminide Coatings under Molten Sulfate Film with Thermal Cycles by Electrochemical Measurements

  • Take, S.;Yoshinaga, S.;Yanagita, M.;Itoi, Y.
    • Corrosion Science and Technology
    • /
    • 제15권6호
    • /
    • pp.259-264
    • /
    • 2016
  • With a specially designed electrochemical cell, the changes in impedance behavior for Inconel 600 and aluminide diffusion coatings under molten sulfate film with thermal cycles (from $800^{\circ}C$ to $350^{\circ}C$) were monitored with electrochemical impedance measurements. It was found that corrosion resistance for both materials increased with lower temperatures. At the same time, the state of molten salt was also monitored successfully by measuring the changes in impedance at high frequency, which generally represents the resistance of molten salt itself. After two thermal cycles, both Inconel 600 and aluminide diffusion coatings showed excellent corrosion resistance. The results from SEM observation and EDS analysis correlated well with the results obtained by electrochemical impedance measurements. It is concluded that electrochemical impedance is very useful for monitoring the corrosion resistance of materials under molten salt film conditions even with thermal cycles.

가스흡수식 냉온수기 열교환기용 세관의 부식특성에 관한 연구 (The Study on Corrosion Characteristics of Heat Exchanger Tube for Gas Absorption Refrigeration & Hot Water System)

  • 정기철
    • 한국가스학회지
    • /
    • 제6권1호
    • /
    • pp.92-97
    • /
    • 2002
  • 가스흡수식 냉온수기의 작동매체로 사용되고 있는 LiBr 수용액 중에서 열교환기 세관용 재료인 동 세관 및 동합금재인 큐프로니켈 세관의 부식특성에 관한 연두를 하기 위하여 $62\%$ LiBr 수용액 중에서 각 재료에 대한 전기화학적 분극실험을 실시하여 부식특성을 고찰한 결과 다음과 같은 결론을 얻었다 1) 열교환기 세관재의 분극저항은 $30\%$ 큐프로니켈 세관 > $10\%$ 큐프로니켈 세관 > 동 세관의 순으로 높게 나타난다 2) 큐프로니켈 세관의 개로전위는 동 세관보다 귀전위화되면서 부식전류밑도는 더 억제된다 3) $30\%$ 큐프로니켈 세관의 부동태 영역은 $10\%$ 큐프로니켈 세관보다 전위구간이 더 크게. 나타나면서 부동태유지 전류밀도는 더 낮아진다.

  • PDF

Effect of Annealed Oxides on the Formation of Inhibition Layer During Hot-Dip Galvanizing of 590Mpa Trip Steel

  • Kim, Seong-Hwan;Huh, Joo-Youl;Lee, Suk-Kyu;Park, Rho-Bum;Kim, Jong-Sang
    • Corrosion Science and Technology
    • /
    • 제10권1호
    • /
    • pp.6-12
    • /
    • 2011
  • The selective surface oxidation of a transformation-induced-plasticity (TRIP) steel containing 1.6 wt.% Mn and 1.5 wt.% Si during annealing at $800^{\circ}C$ was investigated for its influence on the formation of an inhibition layer during hot-dip galvanizing. The selective oxidation of the alloying elements and the oxide morphology were significantly influenced by the annealing atmosphere. The pure $N_{2}$ atmosphere with a dew point $-40^{\circ}C$ promoted the selective oxidation of Mn as a crystalline $Mn_{2}SiO_{4}$ phase, whereas the $N_{2}$ + 10% $H_{2}$ atmosphere with the same dew point $-40^{\circ}C$ promoted the selective oxidation of Si as an amorphous Si-rich oxide phase. During hot-dip galvanizing, the $Mn_{2}SiO_{4}$ phase was reduced more readily by Al in the Zn bath than the Si-rich oxide phase. Consequently, the pure $N_{2}$ atmosphere resulted in a higher formation rate of $Fe_{2}Al_{5}$ particles at the Zn/steel interface and better galvanizability than the $N_{2}$ + 10% $H_{2}$ atmosphere.

Effect of Cr, Mo and W on the Microstructure of Al Hot Dipped Carbon Steels

  • Trung, Trinh Van;Kim, Min Jung;Park, Soon Yong;Yadav, Poonam;Abro, Muhammad Ali;Lee, Dong Bok
    • Corrosion Science and Technology
    • /
    • 제13권1호
    • /
    • pp.1-5
    • /
    • 2014
  • A low carbon steel, Fe-2.25%Cr steel (ASTM T22), and Fe-2.25%Cr-1.6%W steel (ASTM T23) were aluminized by hot dipping into molten Al baths. After hot-dipping, a thin Al-rich topcoat and a thick alloy layer formed on the surface. The topcoat consisted primarily of a thin Al layer that contained a small amount of Fe, whereas the alloy layer consisted of Al-Fe intermetallics such as $Al_5Fe_2$ and AlFe. Cr, Mo, and W in T22 and T23 steels reduced the thickness of the topcoat and the alloy layer, and flattened the reaction front of the aluminized layer, when compared to the low carbon steel.

In-Situ SEM Observation and DIC Strain Analysis for Deformation and Cracking of Hot-Dip ZnMgAl Alloy Coating

  • Naoki Takata;Hiroki Yokoi;Dasom Kim;Asuka Suzuki;Makoto Kobashi
    • Corrosion Science and Technology
    • /
    • 제23권2호
    • /
    • pp.113-120
    • /
    • 2024
  • An attempt was made to apply digital image correlation (DIC) strain analysis to in-situ scanning electron microscopy (SEM) observations of bending deformation to quantify local strain distribution inside a ZnMgAl-alloy coating in deformation. Interstitial-free steel sheets were hot-dipped in a Zn-3Mg-6Al (mass%) alloy melt at 400 ℃ for 2 s. The specimens were deformed using a miniature-sized 4-point bending test machine inside the SEM chamber. The observed in situ SEM images were used for DIC strain analysis. The hot-dip ZnMgAl-alloy coating exhibited a solidification microstructure composed of a three-phase eutectic of fine Al (fcc), Zn (hcp), and Zn2Mg phases surrounding the primary solidified Al phases. The relatively coarsened Zn2Mg phases were locally observed inside the ZnMgAl-alloy coating. The DIC strain analysis revealed that the strain was localized in the primary solidified Al phases and fine eutectic microstructure around the Zn2Mg phase. The results indicated high deformability of the multi-phase microstructure of the ZnMgAl-alloy coating.

The Characteristics of Cr-Free Coating Hot Dip Galvanized Sheet Steel

  • Kim, Jong-Gi;Moon, Man-Been;Yun, Jeong-Mo
    • Corrosion Science and Technology
    • /
    • 제10권1호
    • /
    • pp.24-29
    • /
    • 2011
  • The greatest purpose of chromate treatment is to improve anti-corrosion by stabilizing a metal surface. Because metal surface forms a compound by absorbing oxygen or water in the air by being generally unstable, it is necessary to improve anti-corrosion of the metal by forming the metal surface with a stable film. When considering the economical efficiency and requirements together because the film of the metal surface treated with chromate has good anti-corrosion and the stability also in the air by being compact and strong, Chromate treatment has been used most up to the electronics industry from the auto industry. However, these days, because hexavalent chromium is both a toxic agent to be able to cause cancers and deadly poisonous environmental pollutant, the strong legal controls on its use is being imposed all over the world. Because of this reason, a new anti-corrosion method is being required. Also, by users' various demands, the passivations that have recently been developed require various characteristics such as conductivity, chemical resistance, alkali cleaning resistance as well as anti-corrosion. We could confirm the results such as excellent anti-corrosion compared to chromate, conductivity, chemical resistance and detergent resistance as the result of analysis of various characteristics of the galvannealed sheet steels coated with Cr-Free solution developed in this research.

Accelerated and Outdoor Exposure Tests of Aluminum Coated Steel Sheets

  • Kim, Jongmin;Lee, Jaemin;Lim, Sangkyu;Jung, Choonho
    • Corrosion Science and Technology
    • /
    • 제10권6호
    • /
    • pp.199-204
    • /
    • 2011
  • Hot dip metallic coated steels like as galvanized (GI), zinc-aluminium (GL) and aluminium coated steels are mostly used where corrosion resistance is needed. There are two kinds (type 1 and type 2) of aluminium coated steel being commercially used among them. Type 1 aluminium coated steel is coated with an Al-5~11 wt%Si alloy and Type 2 aluminium coated steel consists of commercially pure aluminium. Type 1 Al coated steel is generally used in automotive components and electrical appliances while type 2 aluminium coated steel is mainly used in construction applications such as building cladding panels, air conditioning and ventilation system. In this study, Type 1 aluminium coated steels have tested by accelerated conditions (salt spray or corrosive gas) and outdoor exposure condition in order to understand their corrosion behaviour. Due to the distinct corrosion mechanism of Al which exposes to the severe chloric condition, Salt Spray Test cannot predict the ordinary atmospheric corrosion of Al based coated materials. In addition, the test results and their corrosion feature of Al coated steel sheets will be discussed comparing with other metallic coated steel sheets of GI and GL.

Al-Si확산코팅에 따른 Ni기 초합금의 미세조직과 부식특성 (Microstructure and Corrosion Characteristics of Al-Si Diffusion Coated Ni Base Super alloy)

  • 안종천;김택수;윤동주;이경구
    • 한국표면공학회지
    • /
    • 제32권2호
    • /
    • pp.100-108
    • /
    • 1999
  • The microstructure and corrosion properties of Al-Si diffusion coated PWA1426 alloy have been investigated. Experimental variables are included temperatures of heat-treatment and coating thickness. The microstructure of coated layer and corrosion properties were analysed by SEM, EDS and hot corrosion test. Two major processes have been found to contribute to microstructural changes in the coating. These are, firstly, the transformation of the NiAl to other $Ni_2Al_3$-based phase and secondly, the precipitation of Cr containing phases. Specimens heat treated at $1080^{\circ}C$ showed superior corrosion resistance to heat treated at $880^{\circ}C$. These increase in life was attributed to the transformation of NiAl and increased coating thickness of PWA1426 alloy.

  • PDF