• Title/Summary/Keyword: High-Mn steels

검색결과 103건 처리시간 0.024초

Fe-34.4Cr-14.5Ni-2.5Mo-0.4W-0.4Mn-0.5Si 합금의 고온 산화에 미치는 S의 영향 (Effect of Sulfur on the High-temperature Oxidation of Fe-34.4Cr-14.5Ni-2.5Mo-0.4W-0.4Mn-0.5Si Alloys)

  • 이동복;이경환;배근수;조규철;정재옥;김민정
    • 한국표면공학회지
    • /
    • 제50권5호
    • /
    • pp.386-391
    • /
    • 2017
  • Two kinds of steels whose compositions were Fe-34.4Cr-14.5Ni-2.5Mo-0.4W-0.4Mn-0.5Si-(0.009 or 0.35)S (wt.%) were centrifugally cast, and oxidized at $900^{\circ}C$ for 50-350 h in order to find the effect of sulfur on the high-temperature oxidation of Fe-34.4Cr-14.5Ni-2.5Mo-0.4W-0.4Mn-0.5Si-(0.009 or 0.35)S (wt.%) alloys. These alloys formed oxide scales that consisted primarily of $Cr_2O_3$ as the major oxide and $Cr_2MnO_4$ as the minor one through preferential oxidation of Cr and Mn. They additionally formed $SiO_2$ particles around the scale/alloy interface as well as inside the matrices. The high affinity of Mn with S led to the formation of scattered MnS inclusions particularly in the 0.35S-containing cast alloy. Sulfur was harmful to the oxidation resistance, because it deteriorated the scale/alloy adherence so as to accerelate the adherence and compactness of the formed scales.

이중복합 주조체의 제조에 미치는 구성 재질과 주조 조건의 영향 (Influences of Casting Conditions and Constituent Materials on the Production of Duo-castings)

  • 정재영
    • 한국주조공학회지
    • /
    • 제38권1호
    • /
    • pp.16-26
    • /
    • 2018
  • In this study, the effects of the pouring temperature, preheating temperature, surface condition and fraction of the wear resistant part on the production of duo-castings were investigated using a high Cr white cast iron with excellent abrasion resistance and a low Cr alloy steel with good toughness. The constituent materials of the duo-castings were designed to have high hardness, fracture toughness and abrasive wear resistance for the replacement of high Mn alloy steels with low abrasive wear resistance. In particular, the amount of abrasive wear of 17% Cr white cast iron was about 1/20 of that of high Mn alloy steel. There was an intermediate area of about 3mm due to local melting at the bonding interface of the duo-castings. These intermediate regions were different from those of the constituent materials in chemical composition and microstructure. This region led to fracture within the wear resistant part rather than at the bonding interface in the bending strength test. The bending fracture strengths were 516-824 MPa, which were equivalent to the bending proof strength of high Mn steel. The effects of various casting conditions on the duo-cast behavior were studied by simple pouring of low Cr alloy steel melt, but the results proved practically impossible to manufacture duo-castings with a sound bonding interface. However, the external heating method was suitable for the production of duo-castings with a sound bonding interface.

Surface Oxidation of High Strength Automotive Steels during Continuous Annealing, and the Influence of Trace Elements of P,B, and Sb

  • Sohn, Il-Ryoung;Park, Joong-Chul;Kim, Jong-Sang
    • Corrosion Science and Technology
    • /
    • 제9권6호
    • /
    • pp.259-264
    • /
    • 2010
  • In continuous hot dip galvanizing process, oxide formation on steel surface has an influence on Zn wetting. High strength automotive steel contains high amount of Si and Mn, where Si-Mn composite oxides such as $Mn_2SiO_4$ or $MnSiO_3$ covers the surface after annealing. Zn wetting depends on how the aluminothermia reaction can reduce the Mn-Si composite oxides and then form inhibition layer such as $Fe_2Al_5$ on the steel surface. The outward diffusion of metallic ions such as $Mn^{2+}$, $Si^{2+}$ in the steel matrix is very important factor for the formation of the surface oxides on the steel surface. The surface state and grain boundaries provide an important role for the diffusion and the surface oxide reactions. Some elements such as P, Sb, and B have a strong affinity for the interface precipitation, and it influence the diffusivity of metallic ions on grain boundaries. B oxide forms very rapildly on the steel surface during the annealing, and this promote complex oxides with $SiO_2$ or MnO. P has inter-reacted with other elements on the grain boundaries and influence the diffusion through on them. Small addition of Sb could suppress the decarburization from steel surface and retards the formation of internal and external selective oxides on the steel surface. Interface control by the trace elements such as Sb could be available to improve the Zn wettability during the hot dip galvanizing.

Ti-Nb-P 첨가 극저탄소 고강도 강판의 기계적 성질과 연성-취 천이거동 (Mechanical Property and Ductile-Brittle Transition Behavior of Ti-Nb-P Added Extra Low Carbon High Strength Steel Sheets)

  • 박종재;이오연;박영구;한상호;진광근
    • 한국재료학회지
    • /
    • 제14권12호
    • /
    • pp.863-869
    • /
    • 2004
  • The purpose of this research is to investigate the mechanical property and ductile-brittle transition temperature of Ti-Nb-P added extra low carbon interstitial free steel having a tensile strength of 440 MPa. The mechanical property and transition temperature of hot rolled steel sheets were more influenced by the coiling temperature rather than by the small amount of alloying element. Further, at the same composition, the property of the specimen coiled at low temperature was superior to that obtained at higher coiling temperature. The fracture surface of 0.005C-0.2Si-1.43Mn steel coiled at $630^{\circ}C$ showed a ductile fracture mode at $-100^{\circ}C$, but coiling at $670^{\circ}C$ showed a transgranular brittle fracture mode at $-90^{\circ}C$. The galvannealed 0.006C-0.07Si-1.33Mn steel sheet annealed at $810^{\circ}C$ has tensile strength and elongation of 442.8 MPa and $36.6\%$, respectively. The transition temperature of galvannealed 0.006C-0.07Si-1.33Mn steel sheet was increased with a drawing ratio, and the transition temperature of the galvannealed 0.006C-0.07Si-1.33Mn steel was $-60^{\circ}C$ at a drawing ratio of 1.8

2단열처리를 이용한 고연신율 고장력 강판의 개발 (Development of the high elonagation and high strength steel sheets utilizing two step heat treatment)

  • 김용현;김영훈;김한군
    • 열처리공학회지
    • /
    • 제10권1호
    • /
    • pp.1-9
    • /
    • 1997
  • The variation of the mechanical properties and the formation of retained austenite with heat treatment conditions in austempered Si bearing carbon steels has been investigated. In the case of a steel containing 0.35C-1.48Si-0.95Mn, it has been found that a feather shape bainite structure of lath are obtained under a isothermal treated condition at just below the Ms temperature, and the martensite, bainitic ferrite and retained austenite of second phase particles on the ferrite matrix for a isothermal treated steels after intercritical annealing are precipitated in a linked shape. The retained austenite with $2{\mu}m$ size induced as TRIP is found to increase with increasing the formation rate of retained austenite for the intercritical annealing and high Si containing steels. The tensile strength is increased as austempering temperature increases in all isothermal treatment temperature, whereas the elongation is shown to roughly decrease as the tensile strength increases. The values of tensile strength-elongation balance have showed a marked dependence upon the elongation rather than the tensile stregth, and their values are increased for high Si containing steels and intercritical annealing condition. The most optimum result has been shown to be the tensile stregth-elongation balance of $2882.4kgf/mm^2.%$ and the elongation of 33.3% for a "B" steel in the heat treating temperature range of $780{\sim}370^{\circ}C$.

  • PDF

차세대 원전 대형 압력용기용 고강도 SA508 Gr.4N Ni-Cr-Mo계 저합금강 개발 (High Strength SA508 Gr.4N Ni-Cr-Mo Low Alloy Steels for Larger Pressure Vessels of the Advanced Nuclear Power Plant)

  • 김민철;박상규;이기형;이봉상
    • 한국압력기기공학회 논문집
    • /
    • 제10권1호
    • /
    • pp.100-106
    • /
    • 2014
  • There is a growing need to introduce advanced pressure vessel steels with higher strength and toughness for the optimizatiooCn of the design and construction of longer life and larger capacity nuclear power plants. SA508 Gr.4N Ni-Cr-Mo low alloy steels have superior strength and fracture toughness, compared to SA508 Gr.3 Mn-Mo-Ni low alloy steel. Therefore, the application of SA508 Gr.4N low alloy steel could be considered to satisfy the strength and toughness required in advanced nuclear power plants. The purpose of this study is to characterize the microstructure and mechanical properties of SA508 Gr.4N low alloy steels. 1 ton ingot of SA508 Gr.4N model alloy was fabricated by vacuum induction melting followed by forging, quenching, and tempering. The predominant microstructure of the SA508 Gr.4N model alloy is tempered martensite having small packet and fine Cr-rich carbides. The yield strength at room temperature was 540MPa, and it was decreased with an increase of test temperature while DSA phenomenon occurred at around $288^{\circ}C$. Overall transition property of SA508 Gr.4N model alloy was much better than SA508 Gr.3 low alloy steel. The index temperature, $T_{41J}$, of SA508 Gr.4N model alloy was $-132^{\circ}C$ in Charpy impact tests, and reference nil-ductility transition temperature, $RT_{NDT}$ of $-105^{\circ}C$ was obtained from drop weight tests. From the fracture toughness tests performed in accordance with the ASTM standard E1921 Master curve method, the reference temperature, $T_0$ was $-147^{\circ}C$, which was improved more than $60^{\circ}C$ compared to SA508 Gr.3 low alloy steels.

변형률 속도에 따른 Fe-24.5Mn-4Cr-0.45C 합금의 인장 특성과 동적 변형시효 (Influence of Strain Rate on Tensile Properties and Dynamic Strain Aging of an Fe-24.5Mn-4Cr-0.45C Alloy)

  • 이승용;황병철
    • 한국재료학회지
    • /
    • 제26권5호
    • /
    • pp.281-286
    • /
    • 2016
  • In the present study, the tensile properties and dynamic strain aging of an Fe-24.5Mn-4Cr-0.45C alloy were investigated in terms of strain rate. During tensile testing at room temperature, all the stress-strain curves exhibited serrated plastic flows related to dynamic strain aging, regardless of the strain rate. Serration appeared right after yield stress at lower strain rates, while it was hardly observed at high strain rates. On the other hand, strain-rate sensitivity, indicating a general relationship between flow stress and strain rate at constant strain and temperature, changed from positive to negative as the strain increased. The negative strain-rate sensitivity can be explained by the Portevin Le Chatelier effect, which is associated with dynamic strain aging and is dependent on the strain rate because it is very likely that the dynamic strain aging phenomenon in high-manganese steels is involved in the interaction between moving dislocations and point-defect complexes.

B첨가 고탄소강의 흑연화에 미치는 냉간압연의 영향 (The Effects of Cold Rolling on the Graphitization in Boron Addition High Carbon Steel)

  • 우기도;박영구;류재화;이창희;나종필
    • 열처리공학회지
    • /
    • 제12권2호
    • /
    • pp.99-107
    • /
    • 1999
  • The graphitization is affected by the addition of small amount of the elements(such as Si, Al, Ni, B, Cr and Mn etc.) and the pre-treatment(such as cold rolling). Boron is well known element to accelerate the graphitization of cementite in high carbon steels. Also, cold rolling is known to accelerate the graphitization. But the graphitization nucleation mechanism by cold rolling is few reported. Therefore the effect of cold rolling in Fe-0.5%C-1.0%Si-0.47%Mn-0.005%B steel on the graphitization is investigated quantitatively using hardness test, optical microscope and scanning electron microscope, neutron induced microscopic radiography. The nucleation of graphite in cold-rolled Fe-0.5%C-1.0%Si-0.47%Mn-0.005%B steel is formed at void which is formed at pearlite/pearlite boundary by cold rolling. But the effect of cold rolling on graphitization in boron addition steel is more effective than that of no boron addition steel due to segregation of BN at void in boron addition steel.

  • PDF

0.27% C-1.0% Si-1.5% Mn 강의 미세조직과 기계적성질에 미치는 Cr의 영향 (Effect of Cr on Mechanical Properties and Microstructure in 0.27% C-1.0% Si-1.5% Mn Steel)

  • 정우창
    • 열처리공학회지
    • /
    • 제29권4호
    • /
    • pp.181-189
    • /
    • 2016
  • The variation in microstructure and mechanical properties during heat treatment was examined in a series of 0.27% C-1.0% Si-1.5% Mn steels with chromium contents in the range of 0 to 1.0 wt%. It was found that chromium decreased the martensite packet size through the austenite grain refinement and increased tensile strength in the as-quenched steel, about 70 MPa per 1.0 wt%. The 0.27% C-1.0% Si-1.5% Mn-1.0% Cr steel showed tensile strength of 1700 MPa in the as-quenched steel. The 0.27% C-1.0% Si-1.5% Mn-1.0% Cr steel revealed a full martensitic structure after air cooling from $900^{\circ}C$ to room temperature, showing air hardening characteristics. Tempering at $150^{\circ}C$ slightly decreased the tensile strength and increased elongation, which is in a good agreement with impact toughness result.

고망간강 플랜지의 열간 단조 후 냉각방법에 따른 미세조직 및 기계적 특성 평가 (Evaluation of Microstructure and Mechanical Properties according to Cooling Method after Hot Forging of High Manganese Steel Flange)

  • 박민하;이강호;김병준;김병구
    • 한국재료학회지
    • /
    • 제34권1호
    • /
    • pp.44-54
    • /
    • 2024
  • High-Manganese (Mn) austenitic steel, with over 24 wt% Mn content, offers outstanding mechanical properties in cryogenic settings, making it a potential replacement for existing cryogenic materials. This high manganese steel exhibits high strength, ductility, and wear resistance, making it promising for applications like LNG tanks, flanges, and valves. To operate in cryogenic environments, hot forging and heat treatment processes are vital, especially in flange production. The cooling rate during high-temperature cooling after hot forging plays a critical role in influencing the microstructure and mechanical properties of high manganese steel. The rate at which cooling occurs during this process influences the size of the grains and the distribution of manganese and consequently has an impact on mechanical properties. This study assessed the microstructure and mechanical properties based on different cooling rates during the hot forging of High-Mn steel flanges. Comparing air and water cooling after hot forging, followed by heat treatment, revealed notable differences in grain size. These differences directly impacted mechanical properties such as tensile strength, hardness, and Charpy impact property. Understanding these effects is crucial for optimizing the performance and reliability of High-Mn steel in cryogenic applications.