• 제목/요약/키워드: High rate dry etching

검색결과 63건 처리시간 0.029초

MEMS 적용을 위한 thermal CVD 방법에 의해 증착한 SiC막의 etching 특성 평가 (Reactive ion etching characterization of SiC film deposited by thermal CVD method for MEMS application)

  • 최기용;최덕균;박지연;김태송
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.2
    • /
    • pp.868-871
    • /
    • 2003
  • In recent years, silicon carbide has emerged as an important material for MEMS application. In order to fabricate an SiC film based MEMS structure by using chemical etching method, high operating temperature is required due to high chemical stability. Therefore, dry etching using plasma is the best solution. SiC film was deposited by thermal CVD at the temperature of $1000^{\circ}C$ and pressure of 10 torr. SiC was dry etched with a reactive ion etching (RIE) system, using $SF_6/O_2$ and $CF_4/O_2$ gas mixture. Etch rate have been investigated as a function of oxygen concentration in the gas mixture, RF power, and working pressure. Etch rate was measured by surface profiler and FE-SEM. $SF_6/O_2$ gas mixture has been shown high etch rate than $CF_4/O_2$ gas mixture. Maximum etch rate appeared at 450W of RF power. $O_2$ dilute mixtures resulted in an increasing of etch rate up to 40%, and the superior anisotropic cross section was observed.

  • PDF

MEMS 적용을 위한 Thermal CVD 방법에 의해 증착한 SiC막의 반응성 이온 Etching 특성 평가 (Reactive ion Etching Characterization of SiC Film Deposited by Thermal CVD Method for MEMS Application)

  • 최기용;최덕균;박지연;김태송
    • 한국전기전자재료학회논문지
    • /
    • 제17권3호
    • /
    • pp.299-304
    • /
    • 2004
  • In recent years, silicon carbide has emerged as an important material for MEMS application. In order to fabricate an SiC film based MEMS structure by using chemical etching method, high operating temperature is required due to high chemical stability Therefore, dry etching using plasma is the best solution. SiC film was deposited by thermal CVD at the temperature of 100$0^{\circ}C$ and pressure of 10 torr. SiC was dry etched with a reactive ion etching (RIE) system, using SF$_{6}$/O$_2$ and CF$_4$/O$_2$ gas mixture. Etch rate has been investigated as a function of oxygen concentration in the gas mixture, rf power, working pressure and gas flow rate. Etch rate was measured by surface profiler and FE-SEM. SF$_{6}$/O$_2$ gas mixture showed higher etch rate than CF$_4$/O$_2$ gas mixture. Maximum etch rate appeared at RF Power of 450W. $O_2$ dilute mixtures resulted in an increasing of etch rate up to 40%, and the superior anisotropic cross section was observe

HDP를 이용한 실리콘 단결정 Deep Dry Etching에 관한 특성 (Characterization of Deep Dry Etching of Silicon Single Crystal by HDP)

  • 박우정;김장현;김용탁;백형기;서수정;윤대호
    • 한국세라믹학회지
    • /
    • 제39권6호
    • /
    • pp.570-575
    • /
    • 2002
  • 현재 전기 . 전자 기술의 추세는 소형화를 비롯하여 집적화, 저전력화, 저가격화의 장점을 가진 MEMS(Micro Electro Mechanical Systems) device의 개발에 주력하고 있으며, 이를 위해서는 고종횡비와 높은 식각 속도를 가진 HDP(High Density Plasma) etching 기술 개발이 필수적이라 할 수 있다. 이를 위하여 우리는 Inductively Coupled Plasma(ICP) 장비를 이용하여 각 공정 변수에 의한 실리콘 deep trench식각 반응을 연구하였다. 실험 공정 변수인 platen power, etch/passivation cycle time에서 etching 단계 시간에 따른 변화와 SF$_{6}$:C$_4$F$_{8}$ 가스유량을 변화시켜 연구하였으며 또한 이들의 profile, scallops, 식각 속도, 균일도, 선택비도 관찰하였다.

High rate dry etching of Si in fluorine-based inductively coupled plasmas

  • Cho, Hyun;Pearton, S.J.
    • 한국결정성장학회지
    • /
    • 제14권5호
    • /
    • pp.220-225
    • /
    • 2004
  • Four different Fluorine-based gases ($SF_6/,NF_3, PF_5,\; and \; BF_3$) were examined for high rate Inductively Coupled Plasma etching of Si. Etch rates up to ~8$\mu\textrm{m}$/min were achieved with pure $SF_6$ discharges at high source power (1500 W) and pressure (35 mTorr). A direct comparison of the four feedstock gases under the same plasma conditions showed the Si etch rate to increase in the order $BF_3$ < $NF_3$< $PF_5$ < $SF_6$. This is in good correlation with the average bond energies of the gases, except for $NF_3$, which is the least strongly bound. Optical emission spectroscopy showed that the ICP source efficiently dissociated $NF_3$, but the etched Si surface morphologies were significantly worse with this gas than with the other 3 gases.

The Influence of He flow on the Si etching procedure using chlorine gas

  • Kim, J.W.;Park, J.H.;M.Y. Jung;Kim, D.W.;Park, S.S.
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 1999년도 제17회 학술발표회 논문개요집
    • /
    • pp.65-65
    • /
    • 1999
  • Dry etching technique provides more easy controllability on the etch profile such as anisotropic etching than wet etching process and the results of lots of researches on the characterization of various plasmas or ion beams for semiconductor etching have been reported. Chlorine-based plasmas or chlorine ion beam have been often used to etch several semiconductor materials, in particular Si-based materials. We have studied the effect of He flow rate on the Si and SiO2 dry etching using chlorine-based plasma. Experiments were performed using reactive ion etching system. RF power was 300W. Cl2 gas flow rate was fixed at 58.6 sccm, and the He flow rate was varied from 0 to 120 sccm. Fig. 1 presents the etch depth of si layer versus the etching time at various He flow rate. In case of low He flow rate, the etch rate was measured to be negligible for both Si and SiO2. As the He flow increases over 30% of the total inlet gas flow, the plasma state becomes stable and the etch rate starts to increase. In high Ge flow rate (over 60%), the relation between the etch depth and the time was observed to be nearly linear. Fig. 2 presents the variation of the etch rate depending on the He flow rate. The etch rate increases linearly with He flow rate. The results of this preliminary study show that Cl2/He mixture plasma is good candidate for the controllable si dry etching.

  • PDF

평판형 유도 결합 플라즈마틀 이용한 GaN 건식 식각 특성 (GaN Dry Etching Characteristics using a planar Inductively coupled plasma)

  • 김문영;김태현;장상훈;태흥식
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 1997년도 추계학술대회 논문집 학회본부
    • /
    • pp.276-278
    • /
    • 1997
  • The reliable etching process is one of the essential steps in fabricating GaN based-device. High etch rate is needed to obtain a deeply etched structure and perfect anisotropic etched facet is needed to obtain lasing profile. In the research, therefore, we had proposed a planar inductively coupled plasma etcher (Planar ICP Etcher) as a high density plasma source, and studied the etching mechanism using the $CH_4/H_2$/Ar gas mixture. Dry etching characteristics such as etch rate, anisotropic etching profile and so on, for the III-V nitride layers were investigated using Planar ICP Etcher, based on the plasma characteristic as a variation of plasma process parameters.

  • PDF

Dry Etching of Ru Electrodes using O2/Cl2 Inductively Coupled Plasmas

  • Kim, Hyoun Woo
    • Corrosion Science and Technology
    • /
    • 제2권5호
    • /
    • pp.238-242
    • /
    • 2003
  • The characteristics of Ru etching using $O_2/Cl_2$ plasmas were investigated by employing inductively coupled plasma (ICP) etcher. The changes of Ru etch rate, Ru to $SiO_2$ etch selectivity and Ru electrode etching slope with the gas flow ratio, bias power, total gas flow rate, and source power were scrutinized. A high etching slope (${\sim}86^{\circ}$) and a smooth surface after etching was attained using $O_2/Cl_2$ inductively coupled plasma.

Optimization of Etching Profile in Deep-Reactive-Ion Etching for MEMS Processes of Sensors

  • Yang, Chung Mo;Kim, Hee Yeoun;Park, Jae Hong
    • 센서학회지
    • /
    • 제24권1호
    • /
    • pp.10-14
    • /
    • 2015
  • This paper reports the results of a study on the optimization of the etching profile, which is an important factor in deep-reactive-ion etching (DRIE), i.e., dry etching. Dry etching is the key processing step necessary for the development of the Internet of Things (IoT) and various microelectromechanical sensors (MEMS). Large-area etching (open area > 20%) under a high-frequency (HF) condition with nonoptimized processing parameters results in damage to the etched sidewall. Therefore, in this study, optimization was performed under a low-frequency (LF) condition. The HF method, which is typically used for through-silicon via (TSV) technology, applies a high etch rate and cannot be easily adapted to processes sensitive to sidewall damage. The optimal etching profile was determined by controlling various parameters for the DRIE of a large Si wafer area (open area > 20%). The optimal processing condition was derived after establishing the correlations of etch rate, uniformity, and sidewall damage on a 6-in Si wafer to the parameters of coil power, run pressure, platen power for passivation etching, and $SF_6$ gas flow rate. The processing-parameter-dependent results of the experiments performed for optimization of the etching profile in terms of etch rate, uniformity, and sidewall damage in the case of large Si area etching can be summarized as follows. When LF is applied, the platen power, coil power, and $SF_6$ should be low, whereas the run pressure has little effect on the etching performance. Under the optimal LF condition of 380 Hz, the platen power, coil power, and $SF_6$ were set at 115W, 3500W, and 700 sccm, respectively. In addition, the aforementioned standard recipe was applied as follows: run pressure of 4 Pa, $C_4F_8$ content of 400 sccm, and a gas exchange interval of $SF_6/C_4F_8=2s/3s$.

Reactive Ion Etching of a-Si for high yield and low process cost

  • Hur, Chang-Wu
    • Journal of information and communication convergence engineering
    • /
    • 제5권3호
    • /
    • pp.215-218
    • /
    • 2007
  • In this paper, amorphous semiconductor and insulator thin film are etched using reactive ion etcher. At that time, we experiment in various RIE conditions (chamber pressure, gas flow rate, rf power, temperature) that have effects on quality of thin film. The using gases are $CF_4,\;CF_4+O_2,\;CCl_2F_2,\;CHF_3$ gases. The etching of a-Si:H thin film use $CF_4,\;CF_4+O_2$ gases and the etching of $a-SiO_2,\;a-SiN_x$ thin film use $CCl_2F_2,\;CHF_3$ gases. The $CCl_2F_2$ gas is particularly excellent because the selectivity of between a-Si:H thin film and $a-SiN_x$ thin film is 6:1. We made precise condition on dry etching with uniformity of 5%. If this dry etching condition is used, that process can acquire high yield and can cut down process cost.

2단계 건식식각에 의한 GaAs Via-Hole 형성 공정 (A Via-Hole Process for GaAs MMIC's using Two-Step Dry Etching)

  • 정문식;김흥락;이지은;김범만;강봉구
    • 전자공학회논문지A
    • /
    • 제30A권1호
    • /
    • pp.16-22
    • /
    • 1993
  • A via-hole process for reproducible and reliable GaAs MMIC fabrication is described. The via-hole etching process consists of two step dry etching. During the first etching step a BC $I_{3}$/C $I_{2}$/Ar gas mixure is used to achieve high etch rate and small lateral etching. In the second etching step. CC $L_{2}$ $F_{2}$ gas is used to achieve selective etching of the GaAs substrate with respect to the front side metal layer. Via holes are formed from the backside of a 100$\mu$m thick GaAs substrate that has been evaporated initially with 500.angs. thick chromium and subsequently a 2000.angs. thick gold layer. The fabricated via holes are electroplated with gold (~20$\mu$m thick) to form via connections. The results show that established via-hole process is satisfactory for GaAs MMIC fabrication.

  • PDF