Ionic liquid coated magnetic core/shell CoFe2O4@SiO2 nanoparticles for the separation/analysis of trace gold in water sample

  • Zeng, Yanxia;Zhu, Xiashi;Xie, Jiliang;Chen, Li
    • Advances in nano research
    • /
    • 제10권3호
    • /
    • pp.295-312
    • /
    • 2021
  • A new ionic liquid functionalized magnetic silica nanoparticle was synthesized and characterized and tested as an adsorbent. The adsorbent was used for magnetic solid phase extraction on ICP-MS method. Simultaneous determination of precious metal Au has been addressed. The method is simple and fast and has been applied to standard water and surface water analysis. A new method for separation/analysis of trace precious metal Au by Magnetron Solid Phase Extraction (MSPE) combined with ICP-MS. The element to be tested is rapidly adsorbed on CoFe2O4@SiO2@[BMIM]PF6 composite nano-adsorbent and eluted with thiourea. The method has a preconcentration factor of 9.5-fold. This method has been successfully applied to the determination of gold in actual water samples. Hydrophobic Ionic Liquids (ILs) 1-butyl-3-methylimidazole hexafluorophosphate ([BMIM]PF6) coated CoFe2O4@SiO2 nanoparticles with core-shell structure to prepare magnetic solid phase extraction agent (CoFe2O4@SiO2@ILs) and establish a new method of MSPE coupled with inductively coupled plasma mass spectrometry for separation/analysis of trace gold. The results showed that trace gold was adsorbed rapidly by CoFe2O4@SiO2@[BMIM]PF6 and eluanted by thiourea. Under the optimal conditions, preconcentration factor of the proposed method was 9.5-fold. The linear range, detection limit, correlation coefficient (R) and relative standard deviation (RSD) were found to be 0.01~1000.00 ng·mL-1, 0.001 ng·mL-1, 0.9990 and 3.4% (n = 11, c = 4.5 ng·mL-1). The CoFe2O4@SiO2 nanoparticles could be used repeatedly for 8 times. This proposed method has been successfully applied to the determination of trace gold in water samples.

PET-CT 융합 영상에서 치과보철물의 금속 종류에 따른 표준섭취계수 값의 변화 (Changes in the Standardized Uptake Value According to the Type of Metal of Dental Prosthesis in PET-CT Fusion Image)

  • 한상현
    • 한국융합학회논문지
    • /
    • 제9권9호
    • /
    • pp.117-122
    • /
    • 2018
  • 본 연구는 PET-CT 검사를 시행할 때 치과보철물에 의해 발생되는 CT의 HU(Hounsfield Unit) 값을 금속의 종류에 따라 측정하고, PET 영상의 왜곡정도와 표준섭취계수(SUV)의 변화를 확인하여 영상 판독 시 오류의 감소방안을 제시하고자 하였다. 실험방법은 실제 치아와 메탈 크라운, 골드크라운, 티타늄, 지르코니아의 치과보철물을 이용하여 PET-CT 검사를 실시하였다. 일반 치아와 비교한 결과 HU 값이 증가함에 따라 SUV 값이 증가되는 것을 확인하였고, 메탈 크라운, 티타늄, 지르코니아의 SUV 값은 37% 정도 증가되었고, 골드 크라운에서는 45.4%로 가장 많이 증가했다. 그리고 일반치아, 메탈크라운, 티타늄, 지르코니아에서 영상 왜곡은 미미했지만, 골드 크라운에서는 선속경화현상이 심하게 발생하였고, 영상 왜곡이 나타났다. 따라서 치과보철물의 금속종류는 SUV 값에 영향을 미치기 때문에 치과 보철물 중에서 골드 재질을 사용한 환자를 진단할 때에는 영상 판독 시 보정된 PET 영상보다는 NAC(무보정) PET 영상을 확인한다면 판독에 도움을 줄 수 있을 것으로 생각된다.

백색금 합금용 모합금의 실리콘 함량에 따른 물성변화 (Properties of the Master Alloys for White Gold Products with Silicon Contents)

  • 송정호;노윤영;이현우;최민경;송오성
    • 한국재료학회지
    • /
    • 제25권2호
    • /
    • pp.90-94
    • /
    • 2015
  • We prepared 8 samples of non-silver and silver-added master alloys containing silicon to confirm the existence of nickel-silicides. We then prepared products made of 14K and 18K white gold by using the prepared master alloys containing 0.25, 0.35, and 0.50 wt% silicon to check for nickel release. We then employed the EN 1811 testing standard to investigate the nickel release of the white gold products, and we also confirmed the color of the white gold products with an UV-VIS-NIR-color meter. We observed $NiSi_x$ residue in all master alloys containing more than 0.50 wt% Si with EDS-nitric acid etching. For the white gold products, we could not confirm the existence of $NiSi_x$ through XRD after aqua-regia etching. In the EN 1811 test, only the white gold products with 0.25 wt% silicon master alloys successfully passed the nickel release regulations. Moreover, we confirmed that our white gold products showed excellent Lab indices as compared to those of commercial white gold ones, and the silver-added master alloys offered a larger L index. Our results indicate that employing 0.25 wt% silicon master alloys might be suitable for white gold products without nickel-silicide defects and nickel release problems.

Development of Array-based Technology for Detection of HAV Using Gold-DNA Probes

  • Wan, Zhixiang;Wang, Yefu;Li, Shawn Shun-Cheng;Duan, Lianlian;Zhai, Jianxin
    • BMB Reports
    • /
    • 제38권4호
    • /
    • pp.399-406
    • /
    • 2005
  • A sensitive method for detection of Hepatitis A virus (HAV) by utilizing gold-DNA probe on an array was developed. Amino- modified oligodeoxynucleotides at the 5' position were arrayed on an activated glass surface to function as capture probes. Sandwich hybridization occurred among capture probes, the HAV amplicon, and gold nanoparticle-supported oligonucleotide probes. After a silver enhancement step, signals were detected by a standard flatbed scanner or just by naked eyes. As little as 100 fM of HAV amplicon could be detected on the array. Therefore, the array technology is an alternative to be applied in detection of HAV due to its low-cost and high-sensitivity.

Fabrication of Chitosan-gold Nanocomposites Combined with Optical Fiber as SERS Substrates to Detect Dopamine Molecules

  • Lim, Jae-Wook;Kang, Ik-Joong
    • Bulletin of the Korean Chemical Society
    • /
    • 제35권1호
    • /
    • pp.25-29
    • /
    • 2014
  • This research was aimed to fabricate an optical fiber-based SERS substrate which can detect dopamine neurotransmitters. Chitosan nanoparticles (NPs) were firstly anchored on the surface of optical fiber, and then gold layer was subsequently deposited on the anchored chitosan NPs via electroless plating method. Finally, chitosan-gold nanocomposites combined with optical fiber reacted with dopamine molecules of 100-1500 mg/day which is a standard daily dose for Parkinson's disease patients. The amplified Raman signal at $1348cm^{-1}$ obtained from optical fiber-based SERS substrate was plotted versus dopamine concentrations (1-10 mM), demonstrating an approximate linearity of Y = 303.03X + 2385.8 ($R^2$ = 0.97) with narrow margin errors. The optical fiber-based Raman system can be potentially applicable to in-vitro (or in-vivo) detection of probe molecules.

Stabilization and solidification of tailings from a traditional gold mine using Portland cement

  • Rachman, Ranno Marlany;Bahri, Ayi Syaeful;Trihadiningrum, Yulinah
    • Environmental Engineering Research
    • /
    • 제23권2호
    • /
    • pp.189-194
    • /
    • 2018
  • The traditional gold mining in Kulon Progo district, Special Region of Yogyakarta Province produced tailings containing mercury (Hg) from the gold amalgamation process. Mercury accumulated in tailings has 164.19 mg/kg - 383.21 mg/kg in total concentration. Stabilization/solidification (S/S) is one of the remediation technologies to reduce waste pollution. Portland cement is one of the additive materials in S/S that effective encapsulates heavy metal waste. The aim of this research is to know the optimum composition of tailings mixture with Portland cement in S/S process. This research used variation of tailings composition. Variation of Portland cement composition with tailing are 100:0, 90:10, 80:20, 70:30, 60:40, 50:50, 40:60, 30:70, 20:80 and 10:90. The result of this study found that the optimum composition of Portland cement: tailings was 10:90, with compression test of $257ton/m^2$ and TCLP test was 0.0069 mg/L. The compression test results were in accordance to US EPA Standard quality of $35ton/m^2$. TCLP test results meet the standard of Indonesian Government Regulation No. 101 Year 2014 of 0.05 mg/L.

Single C-Reactive Protein Molecule Detection on a Gold-Nanopatterned Chip Based on Total Internal Reflection Fluorescence

  • Heo, Yunmi;Lee, Seungah;Lee, Sang-Won;Kang, Seong Ho
    • Bulletin of the Korean Chemical Society
    • /
    • 제34권9호
    • /
    • pp.2725-2730
    • /
    • 2013
  • Single C-reactive protein (CRP) molecules, which are non-specific acute phase markers and products of the innate immune system, were quantitatively detected on a gold-nanopatterned biochip using evanescent field-enhanced fluorescence imaging. The $4{\times}5$ gold-nanopatterned biochip (spot diameter of 500 nm) was fabricated by electron beam nanolithography. Unlabeled CRP molecules in human serum were identified with single-molecule sandwich immunoassay by detecting secondary fluorescence generated by total internal reflection fluorescence (TIRF) microscopy. With decreased standard CRP concentrations, relative fluorescence intensities reduced in the range of 33.3 zM-800 pM. To enhance fluorescence intensities in TIRF images, the distance between biochip surface and CRP molecules was optimally adjusted by considering the quenching effect of gold and the evanescent field intensity. As a result, TIRF only detected one single-CRP molecule on the biochip the first time.

처치치아에 있어서 치주 및 치근단변화에 대한 X-선학적연구 (RADIOLOGIC STUDY OF PERIODONTAL AND PERIAPICAL CHANGES FOR THE RESTORATED TEETH)

  • 안형규
    • 치과방사선
    • /
    • 제8권1호
    • /
    • pp.5-9
    • /
    • 1978
  • The purpose of this study is to investigate the effect of dental restorations on the periodontal and periapical tissues. The author examined 620 cases of amalgam, 390 cases of gold inlay, 422 cases of crown and 644 cases of bridge through the standard intraoral films being appended in the charts that had been kept at the Dept. of Oral Diagnosis in Seoul National University Hospital. This study obtained the following results; 1. The restorations of amalgam, gold inlay crown and bridge were found more frequently in female than in male. 2. The restorations of amalgam, gold inlay and crown were found more numerously in mandibular teeth than in maxillary teeth in both sexes. But in the case of crown, the fact is quite the reverse especially in anterior teeth. 3. On the contrary, in the case of bridge, the restorations of bridge were much more distributed in the maxillary teeth than in the mandibular teeth. 4. Roentgenographic changes of periodontal tissues whose teeth were treated with any type of four restorations were periodontal space widening, lamina dura discontinuity and periapical lesion in the order described in both sexes. 5. On the occasion of between amalgam and gold inlay or between crown and bridge, the differences of periodontal changes were of no consequence. On the other hand, the differences of periodontal changes were apparant between the group of amalgam & gold inlay and the group of crown & bridge.

  • PDF

미륵사지 석탑 출토 사리장엄 금제유물의 재료학적 특성 (Material Characteristics of Gold Artifacts of Sarira Reliquary inside Stone Pagoda of Mireuksa Temple Site)

  • 권혁남;유동완;이장존;한민수
    • 헤리티지:역사와 과학
    • /
    • 제47권4호
    • /
    • pp.210-223
    • /
    • 2014
  • 익산 미륵사지 석탑에서 출토된 사리장엄 중 금제유물은 사리내호, 봉영기 등 총 494점이다. 금제유물은 대부분 가공을 통해 제작하였으나 이 중 금정 22점과 금괴 4점은 형태를 가지고 있지 않은 금괴로 가공품을 만들기 전 단계의 것으로 판단된다. 일반적으로 금은 자연 상태에서 산화물이 아닌 금속의 형태로 존재하므로 용융, 가공 과정만을 통해서 형태를 제작할 수 있다. 그러나 자연금의 경우 은, 동 등 불순물이 포함되어 있으므로 연성을 가지기 위해서는 정제가 필요하다. 미륵사지 석탑 사리장엄에서 출토된 금제유물을 분석하여 그 특성을 알아보고자 하였다. 분석결과 순금제품과 은이 함유된 금제품, 자연금으로 추정되는 금괴류로 분류할 수 있었다. 순금으로 제작된 유물은 사리내호, 금제고리, 금제소형구슬이며, 1wt.% 내외의 동을 함유하고 있다. 이들 유물들은 두드려 형태를 만들기 위해 순금으로 제작한 것으로 보인다. 은이 함유된 유물은 봉영기, 족집게, 금제고리, 금정, 금괴 등이며, 강도가 필요한 형태를 제작하기 위해 은이 함유된 것으로 보인다. 특히, 금정, 금괴는 은, 동의 분포, 형태로 추정하였을 때 자연금으로 보이나 한국의 자료가 충분하지 않아 단정할 수는 없으며, 향후 다양한 지역의 괴 형태 금제유물에 대한 종합적인 조사가 이뤄져야 가능할 것으로 보인다. 금세공기술면에서는 미륵사지 석탑출토 사리장엄은 매우 정교한 기술을 보이고 있다. 또한 무게분포를 살펴보았을 때 한 냥의 명문이 있는 것의 무게가 14g 내외로 이를 기준으로 반 냥, 두 냥 등으로 무게가 분포하고 있다.