• 제목/요약/키워드: Fine aggregate ratio

검색결과 407건 처리시간 0.021초

풍쇄슬래그 잔골재를 사용한 콘크리트의 공학적 특성에 관한 실험적 연구 (An Experimental Study on the Engineering Properties of Concrete using Fine Aggregate of PS ball Slag)

  • 이상수;송하영;김을용
    • 한국건축시공학회지
    • /
    • 제6권3호
    • /
    • pp.107-114
    • /
    • 2006
  • In this study, the experiment was carried out to investigate and analyze the engineering properties of concrete using fine aggregate of PS bal slagl. The main experimental variables were water/cement ratio 30, 40, 50(%), water content $170kg/m^3$, replacement ratio of slag fine aggregate 0, 25, 50, 75(%) in experiment I and water/cement ratio 30, 40, 50(%), water content 165, 170, 175($kg/m^3$), replacement ratio of fine aggregate of PS ball 0, 50 in experiment II. According to the test results, the principle conclusions are summarized as follows (1) The workability of slag fine aggregate-mixed concrete tends to improve, as the replacement rate increases. (2) The air content of slag fine aggregate-mixed concrete tends to decrease, as the replacement rate increases. (3) The unit volume weight of slag fine aggregate-mixed concrete tends to significantly increase, as the replacement rate increases. (4) The compressive strength of slag fine aggregate-mixed concrete tends to show more increasing propensity, in case the curing period is relatively long, as the replacement rate increases.

동제련 슬래그를 혼입한 포러스 콘크리트의 강도 및 투수성능에 관한 연구 (A Study on Strength and Permeability of Cooper Slag mixed Porous Concrete)

  • 심병주;김영수
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2011년도 춘계 학술논문 발표대회 1부
    • /
    • pp.69-72
    • /
    • 2011
  • The purpose of this study is to identify basic property of porous concrete using cooper slag as fine aggregate. The specimens were made with cooper slag with various mixing ratio(10, 20, 30, 50%), porous concrete and porous concrete containing river fine aggregate and crushed fine aggregate, which W/B ratio fixed 0.25. Compressive strength, Flexural strength, coefficient of permeability. From the test results, various fine aggregate mixing ratio improves compressive strength and flexural strength, but cooper slag fine aggregate mixing ratio over 20%, concrete indicates trend to decrease performance of permeability. Concrete containing fine aggregate is improved the performance of permeability and strength compared to other specimen, when age 28days, and cooper slag mixing ratio less than 20% concrete indicates better performance than cooper slag mixing ratio 20% over.

  • PDF

인공경량골재 혼합비율에 따른 경량 콘크리트의 물성 및 강도특성에 관한 연구 (The Study on the Physical and Strength Properties of Lightweight Concrete by Replacement Ratio of Artificial Lightweight Aggregate)

  • 최세진;김도빈;이경수;김영욱
    • 한국건축시공학회지
    • /
    • 제19권4호
    • /
    • pp.313-322
    • /
    • 2019
  • 본 연구는 최근 사용량이 증대하고 있는 저시멘트 배합을 대상으로 국내생산 인공경량 잔 굵은골재의 혼합비율에 따른 경량콘크리트의 물성 및 강도특성을 비교 검토한 것으로서 실험결과, 프리웨팅 시간이 24시간 증가할 경우 모르타르 플로우값이 약 3~5% 감소하는 것으로 나타났으며 경량잔골재 사용에 의해 모르타르 배합에서 약 10.4%의 기건단위질량 감소효과를 얻을 수 있는 것으로 나타났다. 또한 경량굵은골재의 혼합비율에 따른 경량콘크리트의 기건단위질량은 5~10mm 크기인 LWG10 경량굵은골재의 혼합비율이 높아질수록 선형적으로 기건단위질량이 증가하였으며 LWG10 경량굵은골재를 혼합할 경우 LWG10 혼합비율에 관계없이 재령 7일에 약 30~31MPa 수준의 유사한 압축강도를 발현하였다.

고강도 경량 자기충전콘크리트의 성능평가 (Properties of High Strength Lightweight Self-Compacting Concrete)

  • 최연왕;문대중;안성일;최욱;조선규
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2003년도 가을 학술발표회 논문집
    • /
    • pp.413-416
    • /
    • 2003
  • Experimental tests on the high strength self-compacting concrete with light-weight fine aggregate and light-weight coarse aggregate(LHSSC) were performed with slump-flow, reaching time to the slump-flow of 500mm, V-funnel dropping time and U-box difference level and compressive strength. LHSCC with light-weight fine aggregate of 75% and light-weight coarse aggregate of 100% was only satisfied with the property conditions of second self-compacting concrete(SCC), like as flowability, resistance to segregation and filling ability. The 28-day compressive strength of LHSCC indicated above 300kgf/$\textrm{cm}^2$ in all concrete mixtures, and it was increased to increase the replacement ratio of light-weight fine aggregate or to decrease the replacement ratio of light-weight coarse aggregate. Therefore, for satisfying the properties of fresh SCC and hardened concrete with above 350kgf/$\textrm{cm}^2$, it would expected that the replacement ratio of light-weight fine aggregate and light-weight coarse aggregate will be determined with 50~75% and 25~50%, respectively.

  • PDF

분체의 종류에 따른 고유동 콘크리트의 품질성능에 관한 연구 (A study on the quality performances of the high flowing concrete for binder types)

  • 권영호;이현호;하재담
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2002년도 가을 학술발표회 논문집
    • /
    • pp.567-572
    • /
    • 2002
  • This research investigates experimentally an effect on the quality performances of the high flowing concrete according to binder types. The purpose of this study is to determine the optimum mix proportion of the high flowing concrete having good flowability, viscosity and no-segregation. For this purpose, two types using belite cement+lime stone powder(LSP) and furnace slag cement+lime stone powder are selected and tested by design factors including water cement ratio, fine and coarse aggregate volume ratio. As test results of this study, the optimum mix proportion for binder types is as followings. 1) One type based belite cement ; water cement ratio $51^{\circ}C$, fine aggregate volume ratio $43^{\circ}C$ and coarse aggregate volume ratio $53^{\circ}C$, replacement ratio of LSP $42.7^{\circ}C$. 2) Another type based slag cement : water cement ratio $41^{\circ}C$, fine aggregate volume ratio $47^{\circ}C$ and coarse aggregate volume ratio $53^{\circ}C$, replacement ratio of LSP $13.5^{\circ}C$.

  • PDF

순환굵은골재와 순환잔골재 치환율에 따른 콘크리트의 물리적 특성에 관한 연구 (Concrete physical properties with substitution ratio of recycled Coarse aggregate and recycled fine aggregate)

  • 윤승조;서수연;이우진;김대영
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 춘계 학술발표회 논문집(II)
    • /
    • pp.161-164
    • /
    • 2006
  • The main objective of this study was to evaluated the physical properties of concrete with substitution ratio of recycled fine aggregate and recycled coarse aggregate made of waste concrete. The replacement ratios of recycled coarse and fine aggregate decided 0%, 30%, 40% and 50% respectively to get the deregulate of floor space Index. The test result showed that compression strength of cylinder mold decrease with the substitution ratio increase but its strength of replaced recycled fine aggregate higher than OPC.

  • PDF

초기 재령 콘크리트의 종파 속도와 강도의 상관관계 (Correlation between Longitudinal Wave Velocity and Strength of Early-aged Concrete)

  • 이휘근;이광명;김동수
    • 콘크리트학회논문집
    • /
    • 제12권6호
    • /
    • pp.67-74
    • /
    • 2000
  • The usage of nondestructive testing on early-aged concrete leads to enhacned safty and allows effective scheduling of construction, thus making it possible to maximize the time and cost efficiencies. In this study, a reliable nondestructive strength evaluation method for early-aged concrete using the longitudinal wave velocity is proposed. Compression tests were performed to examine factors influencing the velocity-strength relationship of concrete, such as water-cement (w/c) ratio, fine aggregate ratio, curing temperature, and curing condition. The test results show that a change in the w/c ratio and curing temperature has minor effect on the velocity-strength relationship/ However, curing condition significantly influences the velocity-strength relationship of early-aged concrete. Moreover, the longitudinal wave velocity increases with decreasing fine aggregate ratio. It is concluded from this study that the strength evaluation of early-age concrete can be achieved by a nonlinear equation which considers the effects of curing condition and fine aggregate ratio.

설계기준강도별 순환 잔골재 혼합비율에 따른 순환골재 콘크리트 특성에 관한 연구 (A Study on the Characteristics of Recycled Aggregate Concrete According to the Mixing Ratio of Recycled Fine Aggregate at Specific Concrete Strengths)

  • 윤상혁;이세현
    • 한국건설순환자원학회논문집
    • /
    • 제10권4호
    • /
    • pp.367-375
    • /
    • 2022
  • 순환 잔골재 혼합비율에 따른 압축강도는 설계기준강도별 보통콘크리트 대비 순환 잔골재 혼합비율에 따라 유사하거나 다소 낮은 강도 발현을 보였으며, 순환 잔골재 혼합비율이 증가할수록 압축강도는 감소하는 경향을 보였다. 재령일이 증가할수록 강도저하는 발생하지 않았으며, 설계기준강도 대비 강도 발현이 가능할 것으로 판단된다. 순환 잔골재 15 %, 20 %, 25 %로 혼합비율에 따른 순환골재 콘크리트의 길이변화 및 동결융해에 대한 내구특성은 보통콘크리트와 유사한 경향으로 나타났다. 콘크리트용 순환 잔골재의 비율은 총 골재량의 25 %(총잔골재의 50 %)까지 적용하면 슬럼프 및 공기량에 문제가 없을 것으로 판단되며, 설계기준강도에 따른 분체량과 단위수량 및 공기연행제량에 대한 관리가 필요할 것으로 판단된다.

순환잔골재를 활용한 콘크리트의 물리·역학적 특성에 관한 실험적 연구 (An Experimental Study on the Physical and Mechanical Properties of Concrete Using Recycled Sand)

  • 김정호;성종현;이승엽;권구혁;이세현
    • 한국건설순환자원학회논문집
    • /
    • 제5권4호
    • /
    • pp.359-365
    • /
    • 2017
  • 본 연구에서는 KS F 2573 콘크리트용 순환골재 기준에 적합한 순환잔골재의 치환율에 따른 콘크리트 특성을 검토하였다. 물리적 특성으로 슬럼프, 공기량, 경시변화, 압축강도에 대한 연구를 수행하였으며, 순환잔골재 재활용 활성화를 위한 기초자료를 제공하고자 한다. 슬럼프 경시변화 실험 결과 순환잔골재의 치환율 증가에 따라 슬럼프 경시변화 감소율은 커지는 것으로 나타났다. 공기량 측정 결과 순환잔골재의 치환율 증가에 따라 공기량 또한 증가하는 것으로 나타났으며, 경시변화의 경우 공기량 감소율은 낮아지는 것을 확인하였다. 반면 100% 치환 시 천연골재콘크리트보다 높은 공기량을 나타내 강도저하가 발생할 것으로 사료된다. 압축강도의 실험 결과 순환잔골재 치환율 증가에 따라 강도저감이 발생했으며, 24MPa 배합 결과 30% 치환 시 천연골재콘크리트와 동등한 강도발현을 나타냈다. 위의 결과를 토대로 순환잔골재 30%치환 시 천연골재콘크리트와 동등한 물리적 특성을 나타내 KS F 2573 콘크리트용 순환골재 기준에 적합한 순환잔골재 치환 시 목표강도 24MPa의 30%가 적합한 것으로 판단된다. 추후 순환골재의 사용 활성화를 위해 순환잔골재 개질을 통한 품질개선이 필요하며, 후속연구로서 개질된 순환잔골재를 이용한 순환잔골재콘크리트의 물리적 특성 평가가 수행되어야 할 것으로 판단된다.

굵은 골재 입형 개선이 고성능콘크리트의 충전특성에 미치는 영향 (Influence of the Improveal Grain Shape of Coarse Aggregates on Compactability of High Performance Concrete)

  • 이승한;김희중;정용욱
    • 콘크리트학회논문집
    • /
    • 제12권4호
    • /
    • pp.103-111
    • /
    • 2000
  • The influence of the improvement of grain shape of the coarse aggregate to the unit powder content of concrete and the fine aggregate ratio for the increase of the flowability and segregation resistance of high performance concrete was examined. According to the experimental results, flowability and compacting of concrete presents best states in the S/a which has the smallest 패야 ratio. The coarse aggregate after improvement of grain shape, that has changed from the 0.68 of spherical rate of disk shape to 0.73, led fine aggregate ratio to be down 6% (i.e from 47% to 41%). The improvement of grain shape of the coarse aggregate also led the lowest unit powder content to be down 60kg/㎥ (ie from 530kg/㎥ to 470kg/㎥). And approximate 10% of unit water content has been reduced as unit powder content was down. However, the compressive strength after the improvement of grain shape of the coarse aggregate decreased to 5% due to decrease of adhesiveness of the aggregate and cement paste.