ONO 버퍼층을 이용한 Metal/Ferroelectrics/Insulator/Semiconductor 구조의 제작 및 특성 (Fabrication and Properties of Metal/Ferroelectrics/Insulator/Semiconductor Structures with ONO buffer layer)

  • 이남열;윤성민;유인규;류상욱;조성목;신웅철;최규정;유병곤;구진근
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2002년도 하계학술대회 논문집
    • /
    • pp.305-309
    • /
    • 2002
  • We have successfully fabricated a Metal-Ferroelectric-Insulator-Semiconductor (MFIS) structure using Bi$\sub$4-x/La$\sub$x/Ti$_3$O$\sub$12/ (BLT) ferroelectric thin film and SiO$_2$/Nitride/SiO$_2$ (ONO) stacked buffer layers for single transistor type ferroelectric nonvolatile memory applications. BLT films were deposited on 15 nm-thick ONO buffer layer by sol-gel spin-coating. The dielectric constant and the leakage current density of prepared ONO film were measured to be 5.6 and 1.0 x 10$\^$-8/ A/$\textrm{cm}^2$ at 2MV/cm, respectively, It was interesting to note that the crystallographic orientations of BLT thin films were strongly effected by pre-bake temperatures. X-ray diffraction patterns showed that (117) crystallites were mainly detected in the BLT film if pre-baked below 400$^{\circ}C$. Whereas, for the films pre-baked above 500$^{\circ}C$, the crystallites with preferred c-axis orientation were mainly detected. From the C-V measurement of the MFIS capacitor with c-axis oriented BLT films, the memory window of 0.6 V was obtained at a voltage sweep of ${\pm}$8 V, which evidently reflects the ferroelectric memory effect of a BLT/ONO/Si structure.

  • PDF

기판 조건에 따른 SBT 강유전체 커패시터의 특성 (Capacitor characteristics of SBT Ferroelectric Thin Films depending on substrate conditions)

  • 박상준;장건익
    • 한국전기전자재료학회논문지
    • /
    • 제13권2호
    • /
    • pp.143-150
    • /
    • 2000
  • Ferroelectric SrxBi2+yTa2O9+$\alpha$ thin films with various compositions(x=0.7, 0.8, 1, y=0.3, 0.4) were prepared by sol-gel method. The film with moled ratio of 0.8:2.3:2.0 in Sr/Bi/Ta, which was deposited on Pt/SiO2/Si (100), showed better ferroelectric properties than other films. To investigate substrate effects, the same compositions were spin coated on Pt/Ti/SiO2/Si (100) substrates. At an applied voltage of 5V, the dielectric constant($\varepsilon$r), remanent polarization (2Pr) and coercive field (Ec) of the Sr0.8Bi2.3Ta2O9+$\alpha$ thin film prepared on Pt/Ti/SiO2/Si (100) were about 296, 24$\mu$C/$\textrm{cm}^2$ and Ec of 49kV/cm respectively. Both SBT films firred at 80$0^{\circ}C$ revealed no fatigue up to 1010 cycles. Retention characteristics of these capacitors showed no degradation up to 104 sec.

  • PDF

엘라스토머 기판 상에 제작한 유기 강유전체 메모리 소자의 전기적 특성 (Electrical Characteristics of Organic Ferroelectric Memory Devices Fabricated on Elastomeric Substrate)

  • 정순원;류봉조;구경완
    • 전기학회논문지
    • /
    • 제67권6호
    • /
    • pp.799-803
    • /
    • 2018
  • We demonstrated memory thin-film transistors (MTFTs) with organic ferroelectric polymer poly(vinylidene fluoride-co-trifluoroethylene) and an amorphous oxide semiconducting indium gallium zinc oxide channel on the elastomeric substrate. The dielectric constant for the P(VDF-TrFE) thin film prepared on the elastomeric substrate was calculated to be 10 at a high frequency of 1 MHz. The voltage-dependent capacitance variations showed typical butterfly-shaped hysteresis behaviors owing to the polarization reversal in the film. The carrier mobility and memory on/off ratio of the MTFTs showed $15cm^2V^{-1}s^{-1}$ and $10^6$, respectively. This result indicates that the P(VDF-TrFE) film prepared on the elastomeric substrate exhibits ferroelectric natures. The fabricated MTFTs exhibited sufficiently encouraging device characteristics even on the elastomeric substrate to realize mechanically stretchable nonvolatile memory devices.

Random-Oriented (Bi,La)4Ti3O12 Thin Film Deposited by Pulsed-DC Sputtering Method on Ferroelectric Random Access Memory Device

  • Lee, Youn-Ki;Ryu, Sung-Lim;Kweon, Soon-Yong;Yeom, Seung-Jin;Kang, Hee-Bok
    • Transactions on Electrical and Electronic Materials
    • /
    • 제12권6호
    • /
    • pp.258-261
    • /
    • 2011
  • A ferroelectric $(Bi,La)_4Ti_3O_{12}$ (BLT) thin film fabricated by the pulsed-DC sputtering method was evaluated on a cell structure to check its compatibility to high density ferroelectric random access memory (FeRAM) devices. The BLT composition in the sputtering target was $Bi_{4.8}La_{1.0}Ti_{3.0}O_{12}$. Firstly, a BLT film was deposited on a buried Pt/$IrO_x$/Ir bottom electrode stack with W-plug connected to the transistor in a lower place. Then, the film was finally crystallized at $700^{\circ}C$ for 30 seconds in oxygen ambient. The annealed BLT layer was found to have randomly oriented and small ellipsoidal-shaped grains (long direction: ~100 nm, short direction: ~20 nm). The small and uniform-sized grains with random orientations were considered to be suitable for high density FeRAM devices.

화학적기계적연마 공정으로 제조한 PZT 캐패시터의 공정 조건에 따른 강유전 특성 연구 (Ferroelectric characteristics of PZT capacitors fabricated by using chemical mechanical polishing process with change of process parameters)

  • 전영길;정판검;고필주;김남훈;이우선
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2007년도 추계학술대회 논문집
    • /
    • pp.66-66
    • /
    • 2007
  • Lead zirconate titanate (PZT) is one of the most attractive perovskite-type materials for ferroelectric random access memory (FRAM) due to its higher remanant polarization and the ability to withstand higher coercive fields. We first applied the damascene process using chemical mechanical polishing (CMP) to fabricate the PZT thin film capacitor to solve the problems of plasma etching including low etching profile and ion charging. The $0.8{\times}0.8\;{\mu}m$ square patterns of silicon dioxide on Pt/Ti/$SiO_2$/Si substrate were coated by sol-gel method with the precursor solution of PZT. Damascene process by CMP was performed to pattern the PZT thin film with the vertical sidewall and no plasma damage. The polarization-voltage (P-V) characteristics of PZT capacitors and the current-voltage characteristics (I-V) were examined by change of process parameters. To examine the CMP induced damage to PZT capacitor, the domain structure of the polished PZT thin film was also investigated by piezoresponse force microscopy (PFM).

  • PDF

X-ray and Plasma Process Induced Damages to PLZT Capacitor Characteristics for DRAM Applications

  • Kim, Jiyoung
    • The Korean Journal of Ceramics
    • /
    • 제3권3호
    • /
    • pp.213-217
    • /
    • 1997
  • In this paper, the imparct of X-ray and plasma process-induced-damages to La doped Lead Zirconate Titanate (PLZT, (Pb1-xLa)(Zr0.5Ti0.5)O3) capacitor characteristics have been investigated from the viewpoint of gigabit scale dynamic random access memory (DRAM) applications. Plamsa damage causes asymmetric degradation on hysteresis characteristics of PLZT films. On the other hand, X-ray damage results in a symmetrical reduction of charge storage densities (Qc's) for both polarities. As La concentration increases in the films, the radiation hardness of PLZT films on X-ray and plasma exposures is improved. It is observed that the damaged devices are fully recovered by thermal annealing under oxygen ambient.

  • PDF

Dielectric, Ferroelectric, Energy Storage, and Pyroelectric Properties of Mn-Doped (Pb0.93La0.07)(Zr0.82Ti0.18)O3 Anti-Ferroelectric Ceramics

  • Kumar, Ajeet;Yoon, Jang Yuel;Thakre, Atul;Peddigari, Mahesh;Jeong, Dae-Yong;Kong, Young-Min;Ryu, Jungho
    • 한국세라믹학회지
    • /
    • 제56권4호
    • /
    • pp.412-420
    • /
    • 2019
  • In this study, the dielectric and polarization properties of manganese (Mn% = 0.0, 0.1, 0.2, 0.5) doped (Pb0.93La0.07)(Zr0.82Ti0.18)O3 (PLZT 7/82/18) anti-ferroelectric ceramics were studied for energy storage capacitor and pyroelectric applications. A systematic investigation demonstrated that the electric properties of PLZT 7/82/18 ceramics are affected significantly by the Mn-doping content. A maximum dielectric constant of ~ 2,128 at 1 kHz was found for 0.1% Mn-doped PLZT ceramics with a low dielectric loss of 0.018. The bipolar polarization versus electric field (P-E) hysteresis loops were traced for all compositions showing a typical anti-ferroelectric nature. The breakdown field was found to decrease with Mn-doping. The energy storage density and efficiency were found to be 460 J/㎤ and ~ 63%, respectively, for 0.2% Mn-doped PLZT ceramics. The pyroelectric coefficient of PLZT ceramics shows an increase based on the amount of Mn-doping.

Effects of Lanthanides-Substitution on the Ferroelectric Properties of Bismuth Titanate Thin Films Prepared by MOCVD Process

  • Kim, Byong-Ho;Kang, Dong-Kyun
    • 한국세라믹학회지
    • /
    • 제43권11호
    • /
    • pp.688-692
    • /
    • 2006
  • Ferroelectric lanthanides-substituted $Bi_4Ti_3O_{12}$ $(Bi_{4-x}Ln_xTi_3O_{12}, BLnT)$ thin films approximately 200 nm in thickness were deposited by metal organic chemical vapor deposition onto Pt(111)/Ti/SiO$_2$/Si(100) substrates. Many researchers reported that the lanthanides substitution for Bi in the pseudo-perovskite layer caused the distortion of TiO$_6$ octahedron in the a-b plane accompanied with a shift of the octahedron along the a-axis. In this study, the effect of lanthanides (Ln=Pr, Eu, Gd, Dy)-substitution and crystallization temperature on their ferroelectric properties of bismuth titanate $(Bi_4Ti_3O_{12}, BIT)$ thin films were investigated. As BLnT thin films were substituted to lanthanide elements (Pr, Eu, Gd, Dy) with a smaller ionic radius, the remnant polarization (2P$_r$) values had a tendency to increase and made an exception of the Eu-substituted case because $Bi_{4-x}Eu_xTi_3O_{12}$ (BET) thin films had the smaller grain sizes than the others. In this study, we confirmed that better ferroelectric properties can be expected for films composed of larger grains in bismuth layered peroskite materials. The crystallinity of the thin films was improved and the average grain size increased as the crystallization temperature,increased from 600 to 720$^{\circ}C$. Moreover, the BLnT thin film capacitor is characterized by well-saturated polarization-electric field (P-E) curves with an increase in annealing temperature. The BLnT thin films exhibited no significant degradation of switching charge for at least up to $1.0\times10^{11}$ switching cycles at a frequency of 1 MHz. From these results, we can suggest that the BLnT thin films are the suitable dielectric materials for ferroelectric random access memory applications.

열처리에 따른 $Pb[(Zr,Sn)Ti]NbO_3$ 박막의 강유전 특성 (Ferroelectric properties of $Pb[(Zr,Sn)Ti]NbO_3$ Thin Films by Annealing)

  • 최우창;최혁환;이명교;권태하
    • 대한전자공학회:학술대회논문집
    • /
    • 대한전자공학회 2000년도 하계종합학술대회 논문집(2)
    • /
    • pp.24-27
    • /
    • 2000
  • Ferroelectric P $b_{0.99}$〔(Z $r_{0.6}$S $n_{0.4}$)$_{0.9}$ $Ti_{0.1}$$_{0.98}$N $b_{0.02}$ $O_3$(PNZST) thin films were deposited by a RF magnetron sputtering on (L $a_{0.5}$S $r_{0.5}$)Co $O_3$(LSCO)/Pt/Ti/ $SiO_2$/Si substrate using a PNZST target with excess PbO of 10 mole%. The thin films deposited at the substrate temperature of 500 $^{\circ}C$ were crystallized to a perovskite phase after rapid thermal annealing(RTA) The thin films annealed at 650 $^{\circ}C$ for 10 seconds in air exhibited the good crystal structures and ferroelectric properties. The remanent polarization and coercive field of the PNZST capacitor were about 20 $\mu$C/$\textrm{cm}^2$ and 50 kV/cm, respectively. The reduction of the polarization after 2.2$\times$10$^{9}$ switching cycles was less than 10 %.0 %.%.0 %.0 %.

  • PDF

강유전체 $(Ba,\;Sr)TiO_3$ 박막을 이용한 분포 정수형 아날로그 위상 변위기 설계 및 제작 (Design and Fabrication of Distributed Analog Phase Shifter Using Ferroelectric $(Ba,\;Sr)TiO_3$ Thin Films)

  • 류한철;문승언;이수재;곽민환;이상석;김영태
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.2
    • /
    • pp.616-619
    • /
    • 2003
  • This work presents the design, fabrication and microwave performance of distributed analog phase shifter (DAPS) fabricated on $(Ba,\;Sr)TiO_3$ (BST) thin films for X-band applications. Ferroelectric BST thin films were deposited on MgO substrates by pulsed laser deposition. The DAPS consists of high impedance coplanar waveguide (CPW) and periodically loaded tunable BST interdigitated capacitors (IDC). In order to reduce the insertion loss of DAPS and to remove the alteration of unloaded CPW properties according to an applied dc bias voltage, BST layer under transmission lines were removed by photolithography and RF-ion milling. The measured results are in good agreement with the simulated results at the frequencies of interest. The measured differential phase shift based on BST thin films was $24^{\circ}$ and the insertion loss decreased from 1.1 dB to 0.7 dB with increasing the bias voltage from 0 to 40V at 10 GHz.