• 제목/요약/키워드: Fe-Si nano powder

검색결과 43건 처리시간 0.03초

가스분무 Fe계 비정질 분말과 유체 내 전기선 폭발에 의한 나노 Cu 분말의 복합화와 방전플라즈마 소결 (Composite and Spark Plasma Sintering of the Atomized Fe Amorphous Powders and Wire-exploded Cu Nanopowder in Liquid)

  • 김진천;구왕회;유주식
    • 한국분말재료학회지
    • /
    • 제15권4호
    • /
    • pp.285-291
    • /
    • 2008
  • Fe based ($Fe_{68.2}C_{5.9}Si_{3.5}B_{6.7}P_{9.6}Cr_{2.1}Mo_{2.0}Al_{2.0}$) amorphous powder were produced by a gas atomization process, and then ductile Cu powder fabricated by the electric explosion of wire(EEW) were mixed in the liquid (methanol) consecutively. The Fe-based amorphous - nanometallic Cu composite powders were compacted by a spark plasma sintering (SPS) processes. The nano-sized Cu powders of ${\sim}\;nm$200 produced by EEW in the methanol were mixed and well coated with the atomized Fe amorphous powders through the simple drying process on the hot plate. The relative density of the compacts obtained by the SPS showed over 98% and its hardness was also found to reach over 1100 Hv.

두께 조절이 가능한 코어셸 형태의 SiO2 coated CoFe2O4 구조 (Thickness Control of Core Shell type Nano CoFe2O4@SiO2 Structure)

  • 유리;김유진;피재환;김경자
    • 한국분말재료학회지
    • /
    • 제17권3호
    • /
    • pp.230-234
    • /
    • 2010
  • Homogenous silica-coated $CoFe_2O_4$ samples with controlled silica thickness were synthesized by the reverse microemulsion method. First, 7 nm size cobalt ferrite nanoparticles were prepared by thermal decomposition methods. Hydrophobic cobalt ferrites were coated with controlled $SiO_2$ using polyoxyethylene(5)nonylphenylether (Igepal) as a surfactant, $NH_4OH$ and tetraethyl orthosilicate (TEOS). The well controlled thickness of the silica shell was found to depend on the reaction time and the amount of surfactant used during production. Thick shell was prepared by increasing reaction time and small amount of surfactant.

분무열분해 공정에 의한 폐액으로부터 니켈 페라이트 나노 분말 제조 (Manufacture of Nano-Sized Ni-ferrite Powder from Waste Solution by Spray Pyrolysis Process)

  • 유재근;서상기;강성구;김좌연;박시현;김용수;최재하;손진군
    • 자원리싸이클링
    • /
    • 제12권4호
    • /
    • pp.20-29
    • /
    • 2003
  • 본 연구에서는 새도우마스크 제조공정 중 발생되는 Fe-Ni 계 폐산용액을 효율적으로 재활용하기 위하여 폐산용액을 자체 제작한 분무열분해 system을 이용하여 분무열분해시킴에 의해 평균입도 100nm 이하의 니켈 페라이트($NiFe_2$$O_4$)나노 분발을 제조하였으며 반응온도, 용액의 농도 및 용액 유입속도의 반응인자들의 변화에 따른 생성된 분발의 특성변화를 파악하였다. 반응온도가 800∼$1100^{\circ}C$ 로 증가함에 따라 분무열분해 공정에 의해 생성된 분말의 평균입도가 현저히 증가하였고 점점 치밀한 조직을 나타내었으며 비표면적은 크게 감소하였다. 반응온도의 증가에 따라 니첼 페라이트 상의 생성비율 및 결정성이 증가하였다. 원료용액의 농도가 증가됨에 따라 분말의 평균입도는 점점 증가하고 비표면적은 감소하는 반면 입도분포는 더욱 불규칙하게 나타났다. 용액의 농도 증가에 따라 니켈 폐라이트 상의 생성비율 및 결정성은 현저히 증가하고 있었다. 용액의 유입속도 증가에 따라 분말들의 평균입도는 현저히 증가하고 비표면적은 감소하는 반면 입도분포는 불규칙하게 되며 조직의 치밀성도 감소하였다. 용액의 유입속도 감소에 따라 니켈 폐라이트 상의 결정성 및 생성비율이 현저히 증가하고 있었다.

철기(Fe Based) 나노결정질 합금 분말코어의 코팅제 및 입도가 연자기적 특성에 미치는 영향 (Influence of Coating Agent and Particle Size on the Soft Magnetic Properties of Fe Based Nano Crystalline Alloy Powder Core)

  • 장세종;최영진;김상욱;전병서;이태행;송창빈;남궁정
    • 한국자기학회지
    • /
    • 제25권3호
    • /
    • pp.67-73
    • /
    • 2015
  • 본 연구는 철기(Fe based) $Fe_{73.5}Si_{13.5}B_9Nb_3Cu_1$ 나노결정 합금의 분말코어(powder core)의 연자기적 특성 향상을 위한 기초연구로서, 절연 코팅제의 첨가량 및 분말입도에 따른 투자율, 코어손실 및 DC 바이어스 특성을 주로 조사하였다. 우선 합금조성을 PFC 장치를 이용하여 비정질 합금리본을 제조한 후, 열처리, 미분쇄 및 분급하여 얻어진 합금분말에 절연 코팅제(PEI)의 첨가량을 0.5, 1.0, 2.0, 2.5 wt%로 변화시켜 $16ton/cm^2$으로 압축성형 및 결정화 열처리하여 제조한 토로이달 나노결정 분말코어($OD12.7mm{\times}ID7.62mm{\times}H4.75mm$)는 절연 코팅제 함량이 증가할수록 투자율은 감소하였지만, 코어손실 및 DC 바이어스 특성은 향상됨을 확인하였다. 이러한 이유는 합금분말 절연 코팅제 첨가량이 증가할수록 비정질 합금분말 입자가 적어져 분말코어의 성형밀도가 낮아지기 때문으로 추정되었으며, 절연 코팅제의 함량은 1 wt%가 가장 적합한 것으로 판단되었다. 또한 절연 코팅제 함량을 1 wt%로 고정하고, 합금분말의 입도에 따라 제조한 분말코어의 경우, 실효투자율 및 코어손실은 입도가 클수록 우수하였지만, DC 바이어스 특성은 인가자장이 증가함에 따라 더욱 나빠짐을 확인하였다. 그 이유는 합금분말 표면의 코팅층 두께 차이에 의한 절연효과, 잔류기공 혹은 분말코어의 성형밀도 차이 등에 기인하는 것으로 추정되었다.

연자성 합금 분말의 입자크기에 따른 전자파 흡수 특성 비교 (Study of Electromagnetic Wave Absorption Properties with Particle Size in Soft Magnetic Alloy Powder)

  • 홍순호;손근용;박원욱;남정미;문병기;송용설
    • 한국분말재료학회지
    • /
    • 제14권4호
    • /
    • pp.261-264
    • /
    • 2007
  • The electromagnetic wave (EM) absorption properties of various particle size have been investigated in a sheet-type absorber using the $Fe_{73}Si_{16}B_{7}Nb_{3}Cu_{1}$ alloy powder. With decreasing the average particle size, the complex permeability (${\mu}_{r}$) and permittivity (${\varepsilon}_{r}$) increased and the matching frequency is shifted toward lower frequency. The fabricated EM wave absorbers showed permeability $2{\sim}6$, permittivity $17{\sim}23$ for a $-325{\sim}+400$ mesh sample, and the calculated power absorption was as high as 80% in the frequency range over 2 GHz.

AlN 첨가 SiC 세라믹스의 열전변환특성 (Thermoelectric Properties of AlN-doped SiC Ceramics)

  • 배철훈
    • 대한금속재료학회지
    • /
    • 제50권11호
    • /
    • pp.839-845
    • /
    • 2012
  • The effect of an AlN additive on the thermoelectric properties of SiC ceramics was studied. Porous SiC ceramics with 48-54% relative density were fabricated by sintering the pressed ${\alpha}-SiC$ powder compacts with AlN at $2100-2200^{\circ}C$ for 3 h in an Ar atmosphere. In the undoped specimens, the Seebeck coefficients were positive (p-type semiconducting) possibly due to a dominant effect of the acceptor impurities (Al, Fe) contained in the starting powder. With AlN addition, the reverse phase transformation of 6H-SiC to 4H-SiC was observed during the sintering process. The electrical conductivity of the AlN doped specimen was larger than that of the undoped specimen under the same conditions, which might be due to a reverse phase trans-formation. The Seebeck coefficient of the AlN doped specimen was also larger than that of the undoped specimen. The density of specimen and the amount of addition had significant effects on the thermoelectric properties.

Characteristics of Silicon Carbide Nanowires Synthesized on Porous Body by Carbothermal Reduction

  • Kim, Jung-Hun;Choi, Sung-Churl
    • 한국세라믹학회지
    • /
    • 제55권3호
    • /
    • pp.285-289
    • /
    • 2018
  • We synthesized silicon carbide (${\beta}-SiC$) nanowires with nano-scale diameter (30 - 400 nm) and micro-scale length ($50-200{\mu}m$) on a porous body using low-grade silica and carbon black powder by carbothermal reduction at $1300-1600^{\circ}C$. The SiC nanowires were formed by vapor-liquid-solid deposition with self-evaporated Fe catalysts in low-grade silica. We investigated the characteristics of the SiC nanowires, which were grown on a porous body with Ar flowing in a vacuum furnace. Their structural, optical, and electrical properties were analyzed with X-ray diffraction (XRD), transmission electron microscopy (TEM), and selective area electron diffraction (SAED). We obtained high-quality SiC single crystalline nanowire without stacking faults that may have uses in industrial applications.

Nano $TiN_x$와 그 복합체의 제조 및 소결 (Fabrication and sintering of nano $TiN_x$ and its composites)

  • 김동식;김성진;라노;박성범;박승식;이혜정;이상우;조경식;우흥식;안중호
    • 한국결정성장학회지
    • /
    • 제16권3호
    • /
    • pp.101-105
    • /
    • 2006
  • 본 연구에서는 planetary milling을 사용하여 Ti 분말과 $Si_3N_4$와의 반응이 일어나도록 하여 nano $TiN_x$을 제조하였다. 이렇게 얻어진 분말은 Ti 분말과 혼합하여 SPS 소결 장치를 이용하여 소결하였으며 이 소결체의 고온에서의 경도변화를 조사하기위해 $850^{\circ}C$에서 열처리하였다. 분말의 물성평가는 X선 회절분석을 통해 결정상의 변화를 분석하였으며, 그 결과 milling 시간이 10시간의 milling에서는 $TiN_{0.26}$과 TiN이 혼재되어 있으며 20시간의 milling에서는 주로 TiN이 생성되는 것으로 확인되었다. 제조된 분말의 표면관찰을 통해서는 milling 시간이 증가할 수로 입자표면에 새로 형성된 반응물 size 분포를 조사하였으며, milling 시간이 길수록 입자표면의 $TiN_x$ 입자의 사이즈가 $10{\sim}20nm$ 정도로 작아지는 것을 알 수 있었다. Ti와 $TiN_x$를 중량비로 50:50로 혼합하여 제조한 소결체의 경도는 마이크로비커스 경도 값으로 $1050kgf/mm^2$ 정도를 나타내었다.