The purpose of this study was to investigate the cytotoxicity and mutagenicity of denture base resins. According to manufacturer's instructions, resin specimens were made. Group 1 : heat-polymerizing acrylic resin (Luciton $199^{(R)}$) Group 2 : heat-polymerizing acrylic resin containing polyhedraloligosilsesquioxane(POSS resin) Group 3 : auto-polymerizing acrylic resin (Repair $Acrylic^{(R)}$) Group 4 : direct relining auto-polymerizing acrylic resin (Tokuso $Rebase^{(R)}$). Fresh specimens 24 hrs. and 72 hrs. soaked specimens in distil)ed water were made. Responses with metabolic assay and mutagenesis assay to eluates from resin specimens were measured. Cultures with medium alone provided controls. Cytotoxicity was assessed with agar overlay test. The results were as follows; 1. Group 4 showed higher cytotoxicity than Group 1, Group 2 and Group 3 in fresh, 24-an4 72-hour immersion caries (p<.05). Group 3 showed higher cytotoxicity than Group 2 in fresh cases and showed higher cytotoxicity than Group 1 and Group 2 in 24-and 72-hour immersion cases (p<.05) . Group 1 and Group 2 showed no significant difference. 2. All acrylic denture base resins skewed significant increase of cell activity as immersion time increased (p<.05). 3. Auto-polymerizing acrylic denture base resins skewed higher cytotoxicity than heat-polymerizing acrylic denture base resins (p<.05). 4. All acrylic denture base resins showed lower mutagenicity than controls (p<.05).
Statement of problem: For a long time, many of denture base acrylic resins have been used for edentulous and partial edentulous patients because of easy manipulation and good mechanical properties, but its esthetic aspect has not been commented enough. Denture base acrylic resins also has caused esthetic problems due to discoloration or staining as in esthetic restoration. Many researches and reports have treated the problems and accomplished esthetic improvement. But these researches and reports dealt with general food colors or beverages, not with fermented foods. Purpose: This study is designed to assess what fermented foods, such as soy sauce, gochujang, and toenjang that many of Koreans have taken in, influence on the color and hardness variation of denture base acrylic resins. Materials and methods: For the procedure, twelve disks per 4 denture base acrylic resins were fabricated with a thickness of 2mm and 16mm in diameter. Each seven specimen were measured for discoloration with spectrophotometer, while the others, five specimen, for surface hardness change with Barcol hardness tester, over time. Each 12 specimen were immersed into the 4 beakers of fermented foods(soy sauces, gochujangs, toenjangs, deionized water), and $L^{*},a^{*}$, and $b^*$ values were measured for the color difference$({\Delta}E^*)$, on the 1st, 7th, and 28th day with spectrophotometer, with the measurement of surface hardness change. Each data observed was processed statistically. Results: The findings are as follows; Discoloration 1. All of denture base resins was not influenced by the kind of fermented foods, except for $QC20^{(R)}$ 2. Soy sauce and red pepper paste caused more change for denture base resins than deionized water and soy bean paste, except for Perform$^{(R)}$ 3. Most significant change was shown in Lucitone 199$^{(R)}$, whereas Perform$^{(R)}$ results in the least change for all immersed solution, with no statistical significance. Hardness change 1. Barcol hardness values in deposited specimens have been changed low degree, but with significant statistical change according to the kind of food and duration. 2. Lucitone$^{(R)}$ 199 as significantly lower Barcol hardness value than others do. Conclusion: Based on the above results, it suggests that the habitual intake of fermented foods is not helpful for the color stability of denture base acrylic resins because Soy sauce and red pepper paste mainly caused discoloration and surface hardness change. Particularly $Lucitone199^{(R)}$ shows specific discoloration and low surface hardness values. Therefore, it is recommended giving caution patients with denture of $Lucitone199^{(R)}$ especially against the habitual intake of fermented foods like soy sauce and red pepper paste.
Since heat curing acrylic resins undergo unavoidable dimensional changes following polymerization, adaptation can be altered. Until recently, although numerous studies on the dimensional changes of denture base were based on a microscopic technic that measures the relative displacement of a limited reference points on the denture base, but there have been few studies on the distortions of resins using holographic interferometry. Purpose of this study was to determine and compare the dimensional changes and fringe patterns of 4 heat curing acrylic resins, and observe the distortions of acrylic resin denture base by temperature change with the aid of the holographic interferometry. Holographic interferograms were taken on the resin specimens and acrylic resin denture base with the 10mW He-Ne laser and double exposure method. Comparison and analysis of fringe pattern on the recorded object surface was performed. The following results were obtained. 1. The dimensional changes for the high impact resin Lucitone 199 were statistically the greatest of all resins, and the rapid heat curing resin Premium super 20 were the least. 2. The most polymerization shrinkage of all materials occured in initial period of measurements, at this time the difference of polymerization shrinkage properties between resins was founded. 3. The stress distribution of specimens was seen by various type of fringe pattern which had directionality. 4. The polymerization shrinkage of resins was greatly influenced by temperature change. 5. The partial deformations of resin denture base were observed in 70 C and 90 C water.
PURPOSE. The aim of this study was to compare the color stability, water sorption and cytotoxicity of thermoplastic acrylic resin for the non-metal clasp dentures to those of thermoplastic polyamide and conventional heat-polymerized denture base resins. MATERIALS AND METHODS. Three types of denture base resin, which are conventional heat-polymerized acrylic resin (Paladent 20), thermoplastic polyamide resin (Bio Tone), thermoplastic acrylic resin (Acrytone) were used as materials for this study. One hundred five specimens were fabricated. For the color stability test, specimens were immersed in the coffee and green tee for 1 and 8 weeks. Color change was measured by spectrometer. Water sorption was tested after 1 and 8 weeks immersion in the water. For the test of cytotoxicity, cell viability assay was measured and cell attachment was analyzed by FE-SEM. RESULTS. All types of denture base resin showed color changes after 1 and 8 weeks immersion. However, there was no significant difference between denture base resins. All specimens showed significant color changes in the coffee than green tee. In water sorption test, thermoplastic acrylic resin showed lower values than conventional heat-polymerized acrylic resin and thermoplastic polyamide resin. Three types of denture base showed low cytotoxicity in cell viability assay. Thermoplastic acrylic resin showed the similar cell attachment but more stable attachment than conventional heat-polymerized acrylic resin. CONCLUSION. Thermoplastic acrylic resin for the non-metal clasp denture showed acceptable color stability, water sorption and cytotoxicity. To verify the long stability in the mouth, additional in vitro studies are needed.
PURPOSE. The purpose of this study was to compare mechanical and physical properties of injection-molded thermoplastic denture base resins. MATERIALS AND METHODS. In this study, six commercially available products (VA; Valplast, LC; Lucitone, ST; Smiltone, ES; Estheshot-Bright, AC; Acrytone, WE; Weldenz) were selected from four types of thermoplastic denture base materials (Polyamide, Polyester, Acrylic resin and Polypropylene). The flexural properties and shore D hardness have been investigated and water sorption and solubility, and color stability have evaluated. RESULTS. For the flexural modulus value, ES showed the highest value and WE showed significantly lower value than all other groups (P<.05). Most of experimental groups showed weak color stability beyond the clinically acceptable range. CONCLUSION. Within the limits of this study, thermoplastic denture base resin did not show sufficient modulus to function as a denture base. In addition, all resins showed discoloration with clinical significance, and especially polyamides showed the lowest color stability.
Purpose: The purpose of this study was to investigate the effect of addition of fiber glass on the physical properties of silanized fiber mesh and non silanized mesh of denture base resins. Methods: The denture base resins were used in this study heat curing acrylic resins(Vertex Rs, Lucitone 199, $20{\times}80mm$) and fiber glass(SES, Green B&D co., Ltd, $20{\times}80mm$) were used as reinforcement. The specimens were stored in distilled water at $37{\pm}2^{\circ}C$ for 72 hours before test. Bending strength and tensile strength were measured by an universal testing machine(Instron 4301, Instron Corp.). Penetration distribution on fiber was observed by scanning electron microscopy(JSM 840A, Jeol Ltd). Results: The bending strength and modulus were increased by 30% after adding fiber glass on denture base resins. Tensile strength showed significant increasing by adding fiber glass on denture base resins. Conclusion: In this study, Addition of silanized fiber in denture base resins were improved physical properties. we confirmed the fiber glass possibility of the replacement about conventional materials.
One of the primary advantage of acrylic resin teeth is their ability to bond chemically to the denture base resins. But, occasionally, failure have been observed in which acrylic resin teeth break lose from the denture, indicating that chemical bonding does not always occur. The most probable explanation for this type of failure was the presence of a trace of wax remaining as a residue on the surfaces of the teeth after the boiling-out procedure which adgered to the tooth surface and prevented bonding. The purpose of this stdy was preparing the specimens of denture base resin with acrylic resin teeth that four treatment method to ridge lap portion of the tooth and investigated bond between the teeth and denture base resin with tensile strength. Compared results of tensile strength on test specimens were as follows: 1. The mean of strength among the four test groups showed the difference was significant enough(P 0.01). The order of its strength mean was methylene chloride treatment group, detergent solution treatment group, kerosene-ether treatment grgoup, boiling water only group. 2. In compared results between the wax eliminating method groups, there were significant difference between the boiling water only group and other groups(P 0.01), no significant difference were found in the wax eliminating method groups except boiling water only group(P 0.05).
The purpose of this study was to investigate the color change of denture base resins by coffee. Denture base resins for this study were Triad VLG Denture Base (Dentsply, York Div. U.S.A.), Premium Super-20 (Lang Dental Mfg. Co., Inc., U.S.A.) for denture base, Toughron Rebase (Miki Chemical Prod., Kyoto, Japan), Jet Repair Acrylic (Lang Dental Mfg. Co., Inc., U.S.A.), Triad Reline (Dentsply, fork Div. U.S.A.) and Tokuso Rebase (Tokuyama Soda Co., Ltd., Japan) for denture rebase. Twenty specimens of each denture base resin were made and polished. The color of specimens was measured by colorimeter (Model Tc-6FX, Tokyo Denshoku Co. Japan), and they were stored in coffee for three weeks and then color changes were measured. The obtained results were as follows : 1. The L*, a*, b* and the E*ab values of all denture base resins were changed after three weeks. 2. The amount of color change on L*, a*, b* and the E*ab value of each specimens showed different patterns. 3. The b* values of Triad Reline materials were changed more than the other materials. 4. The E*ab values of Triad Denture Base materials were changed more than the other materials.
The purpose of this study was to evaluate the bond strength of rebase resin to denture base resin. The denture base resins in this study were Premium Super-20(Lang Dental Mfg. Co. Inc., Wheeling, USA) and Lucitone 199(Dentsply International Inc., York, USA). And the rebase resins were Repair Acrylic(Lang Dental Mfg. Co. Inc., Wheeling USA). Toughron Rebase(Miki Chemical Product Co. Ltd., Japan) , Tokuso Rebase(Tokuyama Soda. Co. Ltd., Japan) and Triad VLC Reline Material(Dentsply International Inc., York, USA). The obtained results were as follows : 1. The bond strength of Repair Acrylic to Premium Super-20, and that of Toughron Rebase to Lucitone 199 were the highest. 2. In Premium Super-20 and Lucitone 199, bond strength of all rebase resins had significant differences. 3. The bond strength of Triad VLC Reline Material was inclined to the lowset.
One of the primary advantages of acrylic resin teeth is their ability to bond chemically to the denture base resins. Fracture od acrylic resin teeth from a maxillary denture, however, is not uncommon. Bonding failures have been attributed to faulty boil-out procedures that fail to eliminate all traces of wax from the ridge lap surfaces of the teeth and to contamination of the ridge lap surface by careless application of tinfoil substitute. Attempts to increase the strength of the bond between acrylic resin teeth and heat-cured denture base resin include grinding the glossy ridge lap surface (in fluid system), painting the ridgelap surface of the teeth with monomer-polymer solution, and cutting retention grooves in the ridge lap surface of the teeth. This latter method has been tested by applying a tensile force in a labial direction to the incisal part of the lingual surface of the acrylic resin teeth. A progressive shear compressive load was applied at an angle to the lingual surface of acrylic resin teeth bonded to denture base acrylic resin. No statistically singificant advantage was derived by preparing retention grooves of different shapes in the ridgelap surface of the denture teeth.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.