• 제목/요약/키워드: Cr-Hydroxyapatite

검색결과 10건 처리시간 0.028초

Enhanced Hemolytic Biocompatibility of Hydroxyapatite by Chromium (Cr3+) Doping in Hydroxyapatite Nanoparticles Synthesized by Solution Combustion Method

  • Bandgar, Sneha S.;Yadav, Hemraj M.;Shirguppikar, Shailesh S.;Shinde, Mahesh A;Shejawal, Rajendra V.;Kolekar, Tanaji V.;Bamane, Sambhaji R.
    • 한국세라믹학회지
    • /
    • 제54권2호
    • /
    • pp.158-166
    • /
    • 2017
  • For the better success of biomedical implant surgery, we used a modified solution combustion method to synthesize Hydroxyapatite (HA) and Chromium ($Cr^{3+}$) modified Cr-HA with different concentrations of 0.5, 1.0, 1.5, 2.0 and 2.5. The Cr-HA nanopowder was characterized by TGA, XRD, SEM-EDS and TEM. The HA and Cr-HA powders were subjected to in vitro biological studies to determine their biocompatibility and hemocompatibility. The cytotoxicity of HA and Cr-HA were evaluated on Hela (Cervical cancer) cells and L929 (mouse fibroblast) cells by using MTT assay. Hemocompatibility studies demonstrated a noticeable haemolytic ratio below 5%, which confirms that these materials are compatible in nature with human blood. The results of the present work confirm that the synthesised HA and Cr-HA are biocompatible and can be extensively used in the biomedical field to improve overall material biological properties.

Apatite를 이용한 중금속 제거 (The Removal of Heavy Metals in Aqueous Solution by Hydroxyapatite)

  • 강전택;정기호
    • 한국환경과학회지
    • /
    • 제9권4호
    • /
    • pp.325-330
    • /
    • 2000
  • The hydroxyapatite (HAp) for the present study was prepared by precipitation method in semiconductor fabrication and the crystallized at ambient to 95$0^{\circ}C$ for 30min in electric furnace. The ion-exchange characteristics of HAp for various heavy metal ions such as $Cd^{2+}, Cu^{2+}, Mn^{2+}, Zn^{2+}, Fe^{2+}, Pb^{2+}, Al^{3+}, and Cr^{6+}$ in aqueous solution has been investigated. The removal ratio of various metal ions for HAp were investigated with regard to reaction time, concentration of standard solution, amount of HAp and pH of solution. The order of the ions exchanged amount was as follws: $Pb^{2+}, Fe^{3+}>Cu^{2+}>Zn^{2+}>Al^{3+}>Cd^{2+}>Mn^{2+}>Cr^{6+}. The Pb^{2+}$ ion was readily removed by the Hap, even in the strongly acidic region. The maximum amount of the ion-exchange equilibrium for $Pb^{2+}$ ion was about 45 mg/gram of HAp. The HAp would seem to be possible agent for the removal of heavy metal ions in waste water by recycling of waste sludge in semiconductor fabrication.

  • PDF

생물학적 축산분뇨처리시설에서 인 회수의 가능성 평가 (Feasibility of Phosphorus Recovery from Biological Livestock Wastewater Treatment Plant)

  • 안조환;김장호;민성재
    • 한국물환경학회지
    • /
    • 제32권4호
    • /
    • pp.343-348
    • /
    • 2016
  • A chemical sequencing batch reactor was operated to test the feasibility of nutrient recovery from a biological livestock wastewater treatment plant. Both phosphate and ammonia could be successfully recovered as magnesium ammonium phosphate (MAP) crystals. The contents of TP and TN in the recovered MAP crystals were 26.2% and 4.0%, respectively. Zn, Cr and Ti were identified in the crystals, but the contents remained below the Korean standard for an organic fertilizer. Chemical analyses confirmed that the MAP crystals could be useful phosphate fertilizers. On the other hand, the results of physical analyses using an X-ray diffractometer and an energy dispersive X-ray spectrometer strongly suggested that crystalline materials like magnesium potassium phosphate (KMP) and hydroxyapatite (HAP) were also formed during the MAP crystallization, depending on the availability of K+ and Ca2+.

물방울 레이저의 다양한 임상 적용 (Clinical applcation of water laser (Er,Cr:YSGG))

  • 박정현
    • 대한치과의사협회지
    • /
    • 제56권7호
    • /
    • pp.385-390
    • /
    • 2018
  • Laser means "Light amplification by stimulated emission of radiation". Laser have unique characteristics according to wavelength. Wavelenth of Waterlase is 2780nm and it can be absorbed to water and hydroxyapatite. When laser is applied to some material, its temperature goes up due to laser's energy. But in dental treatment high temperature is not good for teeth. High temperature can make dental pulp and bone necrosis. Waterlase can be absorbed to water droplet, so when it burst, it can cut soft and hard tissue without raising temperature. so it is so proper to dental treatment.

  • PDF

Variation in adhesion of Streptococcus mutans and Porphyromonas gingivalis in saliva-derived biofilms on raw materials of orthodontic brackets

  • Park, So-Hyun;Kim, Kyungsun;Cho, Soha;Chung, Dong-Hwa;Ahn, Sug-Joon
    • 대한치과교정학회지
    • /
    • 제52권4호
    • /
    • pp.278-286
    • /
    • 2022
  • Objective: To evaluate differences in the adhesion levels of the most common oral pathogens, Streptococcus mutans and Porphyromonas gingivalis, in human saliva-derived microcosm biofilms with respect to time and raw materials of orthodontic brackets. Methods: The samples were classified into three groups of bracket materials: 1) monocrystalline alumina ceramic (CR), 2) stainless steel metal (SS), and 3) polycarbonate plastic (PL), and a hydroxyapatite (HA) group was used to mimic the enamel surface. Saliva was collected from a healthy donor, and saliva-derived biofilms were grown on each sample. A real-time polymerase chain reaction was performed to quantitatively evaluate differences in the attachment levels of total bacteria, S. mutans and P. gingivalis at days 1 and 4. Results: Adhesion of S. mutans and P. gingivalis to CR and HA was higher than the other bracket materials (SS = PL < CR = HA). Total bacteria demonstrated higher adhesion to HA than to bracket materials, but no significant differences in adhesion were observed among the bracket materials (CR = SS = PL < HA). From days 1 to 4, the adhesion of P. gingivalis decreased, while that of S. mutans and total bacteria increased, regardless of material type. Conclusions: The higher adhesion of oral pathogens, such as S. mutans and P. gingivalis to CR suggests that the use of CR brackets possibly facilitates gingival inflammation and enamel decalcification during orthodontic treatment.

Assessment Corrosion and Bioactive Behavior of Bioglass Coating on Co-Cr-Mo Alloy By Electrophoretic Deposition For Biomedical Applications

  • Areege K. Abed;Ali. M. Mustafa;Ali M. Resen
    • Corrosion Science and Technology
    • /
    • 제23권3호
    • /
    • pp.179-194
    • /
    • 2024
  • A layer-by-layer coating was produced using electrophoretic deposition for a HA/Al2O3 coating layer and a bioglass coating layer on Co-Cr-Mo alloy with a roughness of 0.5 ㎛ (400 emery paper SiC). The corrosion behaviour was analyzed by assessing the coating layers' exceptional corrosion resistance, which outperformed the substrate. Cr ion release test using AAS was carried out, indicating that factional graded coating inhibited ion release from the uncoated substrate to coated sample. The porosity was expressed as a percentage, representing the extent of imperfections on the surface of all coatings. These imperfections fell within an acceptable range of 1% to 3%. The roughness of the coated surface was measured using atomic force microscopy, which revealed an excellent roughness value of 3.32 nm. Tape test technique for adhesion revealed that the removal area of the substrate coating layer varied by 11.92%. X-ray diffraction analysis confirmed the presence of all coating material peaks and verified phases of the deposited coating layers. These findings provided evidence that the coating composition remains unaffected by the electrophoretic deposition process. The bioactivity was assessed by immersion in a simulated bodily fluid, which revealed the formation of HCA during a period of 5 days.

매립지 복토재로의 활용을 위한 하수슬러지 내 중금속의 고형화/안정화 (Solidification/Stabilization of Heavy Metals in Sewage Sludge Prior to Use as a Landfill Cover Material)

  • 박연진;신원식;최상준;이훈하
    • 대한환경공학회지
    • /
    • 제32권7호
    • /
    • pp.665-675
    • /
    • 2010
  • 본 연구에서는 하수슬러지를 매립지 복토재로 재활용하기 위해 래들슬래그, 시멘트, 인회석, 소석회를 첨가하여 하수 슬러지 내 중금속(Cd, Cu, Ni, Pb, Zn)의 용출을 평가하였다. 하수슬러지의 용출 평가는 EDTA (ethylenediaminetetraacetic acid) 추출법과 TCLP (Toxicity Characteristic Leaching Procedure)를 통해 이루어졌으며, 중금속 결합 기작은 연속추출(sequential extraction)을 통해 평가하였다. EDTA 용출 결과 하수슬러지에 래들슬래그/시멘트/소석회의 투입량이 증가할수록 하수슬러지 내 중금속의 용출이 감소하였다. 그러나 인회석을 투입했을 때는 중금속 용출의 감소 효과가 거의 나타나지 않았으며, 이는 EDTA가 인회석에 의한 중금속 고정화를 방해하였기 때문이다. TCLP 용출 결과 하수슬러지 내 슬래그, 시멘트 또는 소석회의 투입량이 증가하여 용출액의 pH가 7 이상일 때는 Cu의 용출 농도가 원하수슬러지의 용출농도보다 증가하는 것으로 나타났다. 그러나 인회석은 투입량이 증가할수록 중금속의 용출 농도가 감소하는 것으로 나타났다. 혼합 고화제를 투입한 하수슬러지의 중금속 용출 결과, 하수슬러지의 중량비 100%를 기준으로 래들슬래그 20%와 소석회 10%를 투입한 혼합물이 최적의 고화 혼합 비율이며, 이 때 EDTA 추출법과 TCLP로 용출한 중금속의 농도가 가장 낮게 나타났다. 이러한 결과는 하수슬러지 내 중금속 결합이 약한 결합인 exchangeable fraction과 carbonate fraction에서 강한 결합인 organic fraction으로 이동하였음을 연속추출(SM&T, formaly BCR)을 통해 확인할 수 있었다. 하수슬러지와 고화제를 최적의 비율로 혼합한 혼합물을 폐기물공정시험법으로 중금속 용출을 평가한 결과 Cu가 기준농도 이상으로 검출되었다. 그러나 TCLP에 따른 하수슬러지의 용출시험 결과 Ba, Cd, Cr, Pb의 항목에서 미국 환경보호청의 용출 기준을 만족하였다.

BIOCOMPATIBISITY OF ION BEAM PROCESSED FILMS DEPOSITED ON SURGICAL TI-6AI-4V

  • Lee, I-S;Song and I-j Yu
    • 한국진공학회지
    • /
    • 제6권S1호
    • /
    • pp.16-22
    • /
    • 1997
  • ion beam processing of materials for medical application has gained increasing interest in the last decade and the implantation of nitrogen into TI-6AI-4V to improve corrosive-wear performance is currently used for processing of total hip and knee joints. Oxides and nitrides of Ti, Zr, Al, Cr were deposited on TI-6AI-4V substrates by DC magnetron sputtering dual ion beam sputtering and ion beam assisted deposition. The cytotoxicity of these films were investigated by MTT method and showed comparable to untreated TI-6AI-4V Plasm-sprayed hydroxyapatite(HAp) coatings showed excellent cytotoxicity regardless of heat treatment. intermediate layer coatings of nitrides and oxides increased the bond strength of HAp to substrate by intrdducing chemical bond at interface. Heat treatment of HAp coatings also improved the chemical bond at interfaces and increased the bond strength of untreated TI-6AI-4V to 16.4 kg/$\textrm{cm}^2$ but still lower than 33.1 kg./$\textrm{cm}^2$ of ir oxide as a imtermediate layer caoting.

  • PDF

Designing Materials for Hard Tissue Replacement

  • Nath, Shekhar;Basu, Bikramjit
    • 한국세라믹학회지
    • /
    • 제45권1호
    • /
    • pp.1-29
    • /
    • 2008
  • In last two decades, an impressive progress has been recorded in terms of developing new materials or refining existing material composition/microstructure in order to obtain better performance in biomedical applications. The success of such efforts clearly demands better understanding of various concepts, e.g. biocompatibility, host response, cell-biomaterial interaction. In this article, we review the fundamental understanding that is required with respect to biomaterials development, as well as various materials and their properties, which are relevant in applications, such as hard tissue replacement. A major emphasize has been placed to present various design aspects, in terms of materials processing, of ceramics and polymer based biocomposites, Among the bioceramic composites, the research results obtained with Hydroxyapatite (HAp)-based biomaterials with metallic (Ti) or ceramic (Mullite) reinforcements as well as $SiO_2-MgO-Al_2O_3-K_2O-B_2O_3-F$ glass ceramics and stabilized $ZrO_2$ based bioinert ceramics are summarized. The physical as well as tribological properties of Polyethylene (PE) based hybrid biocomposites are discussed to illustrate the concept on how can the physical/wear properties be enhanced along with biocompatibility due to combined addition of bioinert and bioactive ceramic to a bioinert polymeric matrix. The tribological and corrosion properties of some important orthopedic metallic alloys based on Ti or Co-Cr-Mo are also illustrated. At the close, the future perspective on orthopedic biomaterials development and some unresolved issues are presented.

HA 코팅된 스테인레스강과 뼈의 계면에서의 경조직 성장 및 결합력 향상 (Bone Ingrowth and Enhancement of Bone Bonding Strength at Interface between Bone and HA Coated Stainless Steel)

  • 김철생;김상윤;김동헌;강곤
    • 대한의용생체공학회:학술대회논문집
    • /
    • 대한의용생체공학회 1996년도 춘계학술대회
    • /
    • pp.133-136
    • /
    • 1996
  • We investigated how hydroxyapatite (HA) coating onto a porous super stainless steel (S.S.S, 22Cr-20Ni-6Mo-0.25N) affects bone ingrowth in a dog transcortical femoral model. Implants were histologically evaluated after 4 and 48 weeks of implantation, and the bone bonding strength at the bone/implant interface was examined by employing the pull-out test. The direct osseous tissue bonding onto the HA-coated S.S.S was observed, but the uncoated stainless steels had thin fibrous tissue layers. The mean interface strength of the HA-coated S.S.S was 1.5 and 2.5 times greater than those of the S.S.S and the 316L SS after one year of implantation, respectively. In preliminary studies, no toxic responce was observed from a cytotoxicity test of the S.S.S, having similar corrosion resistance to titanium. Our results suggest that early osteoconductive nature of HA coating may induce long term osteointegration for a bioinert substrate.

  • PDF