• Title/Summary/Keyword: Cr-Hydroxyapatite

Search Result 9, Processing Time 0.024 seconds

Enhanced Hemolytic Biocompatibility of Hydroxyapatite by Chromium (Cr3+) Doping in Hydroxyapatite Nanoparticles Synthesized by Solution Combustion Method

  • Bandgar, Sneha S.;Yadav, Hemraj M.;Shirguppikar, Shailesh S.;Shinde, Mahesh A;Shejawal, Rajendra V.;Kolekar, Tanaji V.;Bamane, Sambhaji R.
    • Journal of the Korean Ceramic Society
    • /
    • v.54 no.2
    • /
    • pp.158-166
    • /
    • 2017
  • For the better success of biomedical implant surgery, we used a modified solution combustion method to synthesize Hydroxyapatite (HA) and Chromium ($Cr^{3+}$) modified Cr-HA with different concentrations of 0.5, 1.0, 1.5, 2.0 and 2.5. The Cr-HA nanopowder was characterized by TGA, XRD, SEM-EDS and TEM. The HA and Cr-HA powders were subjected to in vitro biological studies to determine their biocompatibility and hemocompatibility. The cytotoxicity of HA and Cr-HA were evaluated on Hela (Cervical cancer) cells and L929 (mouse fibroblast) cells by using MTT assay. Hemocompatibility studies demonstrated a noticeable haemolytic ratio below 5%, which confirms that these materials are compatible in nature with human blood. The results of the present work confirm that the synthesised HA and Cr-HA are biocompatible and can be extensively used in the biomedical field to improve overall material biological properties.

The Removal of Heavy Metals in Aqueous Solution by Hydroxyapatite (Apatite를 이용한 중금속 제거)

  • 강전택;정기호
    • Journal of Environmental Science International
    • /
    • v.9 no.4
    • /
    • pp.325-330
    • /
    • 2000
  • The hydroxyapatite (HAp) for the present study was prepared by precipitation method in semiconductor fabrication and the crystallized at ambient to 95$0^{\circ}C$ for 30min in electric furnace. The ion-exchange characteristics of HAp for various heavy metal ions such as $Cd^{2+}, Cu^{2+}, Mn^{2+}, Zn^{2+}, Fe^{2+}, Pb^{2+}, Al^{3+}, and Cr^{6+}$ in aqueous solution has been investigated. The removal ratio of various metal ions for HAp were investigated with regard to reaction time, concentration of standard solution, amount of HAp and pH of solution. The order of the ions exchanged amount was as follws: $Pb^{2+}, Fe^{3+}>Cu^{2+}>Zn^{2+}>Al^{3+}>Cd^{2+}>Mn^{2+}>Cr^{6+}. The Pb^{2+}$ ion was readily removed by the Hap, even in the strongly acidic region. The maximum amount of the ion-exchange equilibrium for $Pb^{2+}$ ion was about 45 mg/gram of HAp. The HAp would seem to be possible agent for the removal of heavy metal ions in waste water by recycling of waste sludge in semiconductor fabrication.

  • PDF

Feasibility of Phosphorus Recovery from Biological Livestock Wastewater Treatment Plant (생물학적 축산분뇨처리시설에서 인 회수의 가능성 평가)

  • Ahn, Johwan;Kim, Jangho;Min, Sungjae
    • Journal of Korean Society on Water Environment
    • /
    • v.32 no.4
    • /
    • pp.343-348
    • /
    • 2016
  • A chemical sequencing batch reactor was operated to test the feasibility of nutrient recovery from a biological livestock wastewater treatment plant. Both phosphate and ammonia could be successfully recovered as magnesium ammonium phosphate (MAP) crystals. The contents of TP and TN in the recovered MAP crystals were 26.2% and 4.0%, respectively. Zn, Cr and Ti were identified in the crystals, but the contents remained below the Korean standard for an organic fertilizer. Chemical analyses confirmed that the MAP crystals could be useful phosphate fertilizers. On the other hand, the results of physical analyses using an X-ray diffractometer and an energy dispersive X-ray spectrometer strongly suggested that crystalline materials like magnesium potassium phosphate (KMP) and hydroxyapatite (HAP) were also formed during the MAP crystallization, depending on the availability of K+ and Ca2+.

Clinical applcation of water laser (Er,Cr:YSGG) (물방울 레이저의 다양한 임상 적용)

  • Park, Jung-Hyun
    • The Journal of the Korean dental association
    • /
    • v.56 no.7
    • /
    • pp.385-390
    • /
    • 2018
  • Laser means "Light amplification by stimulated emission of radiation". Laser have unique characteristics according to wavelength. Wavelenth of Waterlase is 2780nm and it can be absorbed to water and hydroxyapatite. When laser is applied to some material, its temperature goes up due to laser's energy. But in dental treatment high temperature is not good for teeth. High temperature can make dental pulp and bone necrosis. Waterlase can be absorbed to water droplet, so when it burst, it can cut soft and hard tissue without raising temperature. so it is so proper to dental treatment.

  • PDF

Variation in adhesion of Streptococcus mutans and Porphyromonas gingivalis in saliva-derived biofilms on raw materials of orthodontic brackets

  • Park, So-Hyun;Kim, Kyungsun;Cho, Soha;Chung, Dong-Hwa;Ahn, Sug-Joon
    • The korean journal of orthodontics
    • /
    • v.52 no.4
    • /
    • pp.278-286
    • /
    • 2022
  • Objective: To evaluate differences in the adhesion levels of the most common oral pathogens, Streptococcus mutans and Porphyromonas gingivalis, in human saliva-derived microcosm biofilms with respect to time and raw materials of orthodontic brackets. Methods: The samples were classified into three groups of bracket materials: 1) monocrystalline alumina ceramic (CR), 2) stainless steel metal (SS), and 3) polycarbonate plastic (PL), and a hydroxyapatite (HA) group was used to mimic the enamel surface. Saliva was collected from a healthy donor, and saliva-derived biofilms were grown on each sample. A real-time polymerase chain reaction was performed to quantitatively evaluate differences in the attachment levels of total bacteria, S. mutans and P. gingivalis at days 1 and 4. Results: Adhesion of S. mutans and P. gingivalis to CR and HA was higher than the other bracket materials (SS = PL < CR = HA). Total bacteria demonstrated higher adhesion to HA than to bracket materials, but no significant differences in adhesion were observed among the bracket materials (CR = SS = PL < HA). From days 1 to 4, the adhesion of P. gingivalis decreased, while that of S. mutans and total bacteria increased, regardless of material type. Conclusions: The higher adhesion of oral pathogens, such as S. mutans and P. gingivalis to CR suggests that the use of CR brackets possibly facilitates gingival inflammation and enamel decalcification during orthodontic treatment.

Solidification/Stabilization of Heavy Metals in Sewage Sludge Prior to Use as a Landfill Cover Material (매립지 복토재로의 활용을 위한 하수슬러지 내 중금속의 고형화/안정화)

  • Park, Youn-Jin;Shin, Won-Sik;Choi, Sang-June;Lee, Hoon-Ha
    • Journal of Korean Society of Environmental Engineers
    • /
    • v.32 no.7
    • /
    • pp.665-675
    • /
    • 2010
  • The effects of chemical binders (ladle slag, ordinary portland cement (OPC), hydroxyapatite and calcium hydroxide) on the solidification/stabilization of heavy metals (Cd, Cu, Ni, Pb, Zn) in sewage sludge were evaluated by chemical leaching tests such as EDTA extraction, TCLP and sequential extraction. The results of EDTA extraction showed that heavy metal concentrations in sewage sludge were highly reduced after solidification/stabilization with slag, cement or calcium hydroxide. However, EDTA interrupted solidification/stabilization of heavy metals by hydroxyapatite. The TCLP-extracted heavy metal concentrations in sewage sludge after solidification/stabilization with chemical amendments were highly reduced. However, Cu concentration in the sewage sludge solidified/stabilized with slag, cement or calcium hydroxide increased because the pH of TCLP solution was higher than 7. Mixtures of sludge 1 : slag 0.2 : calcium hydroxide 0.1 (wt ratio) showed the least leachability in batch TCLP and EDTA extraction. The results of sequential extraction (SM&T, formaly BCR) indicated that the distribution of heavy metals changed from exchangable and carbonate fractions to strongly bound organic fraction. It was found that maximum leachate concentrations of Ba, Cd, Cr and Pb from sewage sludge amended with slag and calcium hydroxide were far below US EPA TCLP regulations.

BIOCOMPATIBISITY OF ION BEAM PROCESSED FILMS DEPOSITED ON SURGICAL TI-6AI-4V

  • Lee, I-S;Song and I-j Yu
    • Journal of the Korean Vacuum Society
    • /
    • v.6 no.S1
    • /
    • pp.16-22
    • /
    • 1997
  • ion beam processing of materials for medical application has gained increasing interest in the last decade and the implantation of nitrogen into TI-6AI-4V to improve corrosive-wear performance is currently used for processing of total hip and knee joints. Oxides and nitrides of Ti, Zr, Al, Cr were deposited on TI-6AI-4V substrates by DC magnetron sputtering dual ion beam sputtering and ion beam assisted deposition. The cytotoxicity of these films were investigated by MTT method and showed comparable to untreated TI-6AI-4V Plasm-sprayed hydroxyapatite(HAp) coatings showed excellent cytotoxicity regardless of heat treatment. intermediate layer coatings of nitrides and oxides increased the bond strength of HAp to substrate by intrdducing chemical bond at interface. Heat treatment of HAp coatings also improved the chemical bond at interfaces and increased the bond strength of untreated TI-6AI-4V to 16.4 kg/$\textrm{cm}^2$ but still lower than 33.1 kg./$\textrm{cm}^2$ of ir oxide as a imtermediate layer caoting.

  • PDF

Designing Materials for Hard Tissue Replacement

  • Nath, Shekhar;Basu, Bikramjit
    • Journal of the Korean Ceramic Society
    • /
    • v.45 no.1
    • /
    • pp.1-29
    • /
    • 2008
  • In last two decades, an impressive progress has been recorded in terms of developing new materials or refining existing material composition/microstructure in order to obtain better performance in biomedical applications. The success of such efforts clearly demands better understanding of various concepts, e.g. biocompatibility, host response, cell-biomaterial interaction. In this article, we review the fundamental understanding that is required with respect to biomaterials development, as well as various materials and their properties, which are relevant in applications, such as hard tissue replacement. A major emphasize has been placed to present various design aspects, in terms of materials processing, of ceramics and polymer based biocomposites, Among the bioceramic composites, the research results obtained with Hydroxyapatite (HAp)-based biomaterials with metallic (Ti) or ceramic (Mullite) reinforcements as well as $SiO_2-MgO-Al_2O_3-K_2O-B_2O_3-F$ glass ceramics and stabilized $ZrO_2$ based bioinert ceramics are summarized. The physical as well as tribological properties of Polyethylene (PE) based hybrid biocomposites are discussed to illustrate the concept on how can the physical/wear properties be enhanced along with biocompatibility due to combined addition of bioinert and bioactive ceramic to a bioinert polymeric matrix. The tribological and corrosion properties of some important orthopedic metallic alloys based on Ti or Co-Cr-Mo are also illustrated. At the close, the future perspective on orthopedic biomaterials development and some unresolved issues are presented.

Bone Ingrowth and Enhancement of Bone Bonding Strength at Interface between Bone and HA Coated Stainless Steel (HA 코팅된 스테인레스강과 뼈의 계면에서의 경조직 성장 및 결합력 향상)

  • Kim, C.S.;Kim, S.Y.;Kim, D.H.;Khang, G.
    • Proceedings of the KOSOMBE Conference
    • /
    • v.1996 no.05
    • /
    • pp.133-136
    • /
    • 1996
  • We investigated how hydroxyapatite (HA) coating onto a porous super stainless steel (S.S.S, 22Cr-20Ni-6Mo-0.25N) affects bone ingrowth in a dog transcortical femoral model. Implants were histologically evaluated after 4 and 48 weeks of implantation, and the bone bonding strength at the bone/implant interface was examined by employing the pull-out test. The direct osseous tissue bonding onto the HA-coated S.S.S was observed, but the uncoated stainless steels had thin fibrous tissue layers. The mean interface strength of the HA-coated S.S.S was 1.5 and 2.5 times greater than those of the S.S.S and the 316L SS after one year of implantation, respectively. In preliminary studies, no toxic responce was observed from a cytotoxicity test of the S.S.S, having similar corrosion resistance to titanium. Our results suggest that early osteoconductive nature of HA coating may induce long term osteointegration for a bioinert substrate.

  • PDF