Kim, M.H.;Kim, T.Y.;Son, I.H.;Park, C.O.;Kim, J.H.;Kim, K.H.
Proceedings of the KIEE Conference
/
1997.11a
/
pp.294-295
/
1997
CO-Cr 수직자기기록 매체의 우수한 하지층을 개발하기 위하여, 스피넬 결점막$(Fe,M)_3O_4$ (M=Ni,Zn)이 스핀스프레이 페라이트 플레이팅 방법으로 유리 기판 위에 제작되었다. 반응액과 산화액은 기판이 회전하는 반응용기로 분사되었다. 반응은 기판의 회전소독, 반응온도, 반응액과 산화액의 유속 그리고 반응액과 산화액의 농도에 의해 영향받았다. 반응액과 산화액의 유속은 60(ml/min)으로 하고, 반응온도는 90[$^{\circ}C$] 그리고 기판의 회전속도는 150[rpm]의 조건하에서, 페라이트 플레이팅 반응에 미치는 반응액과 산화액 농도의 영향이 화학적 조성, 결정학적 및 자기적 특성의 관점에서 연구되었다. $Ni_{0.34}Zn_{0.66}Fe_2O_4$의 조성에서, 우리는 가장 안정한 결정학적 및 자기적 특성을 얻었다.
Baek, Jaewon;Choi, Jong-il;Park, Hyun;Lim, Sangyong;Park, Si Jae
Journal of Microbiology and Biotechnology
/
v.26
no.12
/
pp.2066-2075
/
2016
In this study, an enhanced lipid-producing mutant strain of the microalga Chlamydomonas reinhardtii was developed by gamma irradiation. To induce the mutation, C. reinhardtii was gamma irradiated at a dose of 400 Gy. After irradiation, the surviving cells were stained with Nile red. The mutant (Cr-4013) accumulating 20% more lipid than the wild type was selected. Thin-layer chromatography revealed the triglyceride and free fatty acid contents to be markedly increased in Cr-4013. The major fatty acids identified were palmitic acid, oleic acid, linoleic acid, and linolenic acid. Random amplified polymeric DNA analysis showed partial genetic modifications in Cr-4013. To ascertain the changes of protein expression in the mutant strain, two-dimensional electrophoresis was conducted. These results showed that gamma radiation could be used for the development of efficient microalgal strains for lipid production.
With increasing environmental demands in surface treatment of steel sheets, the passivation layers containing hexavalent chromium $(Cr^{+6})$ are being replaced by non-chromium or trivalent chromium compounds. After review on the various types of inorganic compounds, the zirconates was chosen as the candidate for alternative to sodium dichromate in the aspect of its barrier properties with excellent adhesion to organics. The ammonium zirconium carbonate (AZC) and sodium hexafluorozirconate (SFZ) could be reach $70-80\%$ level of CDC (cathodic dichromate) treatment by their single applications. But high porosity in the AZC layer and poor electrical conductivity of SFZ solution limit the single application of zirconate. Mixed composition of zirconates to compensate their inferiorities or incorporation of organic compounds to seal the porosity seems to be inevitable to match up the target level of Cr-free passivation of tinplate.
A modified surface layer by ion implantation is very thin (under 1 $\mu\textrm{m}$) but has superior mechanical characteristics. therefore ion implantation has been used successfully as a surface treatment technology to improve the wear, fatigue, and corrosion resistances of materials. MEVVA which is a kind of ion beam apparatus has merits of low cost and is usable to various metals, but occurs a droplet ranging from micron to tens of micron on the implanted surface at ion implantations. wear is a dynamic phenomenon on interacting surfaces with rotative motion. Since wear changes in condition of the surface, we should control to surface. In order to improve a wear resistance of Ti ion implanted 1C-3Cr steel(material for roller in the cold working process), it is essential to investigate the effect of the droplets on the wear characteristics. In this study, we investigate the effect of the droplets on the wear characteristics of 1C-3Cr steel using SEM Tribosystem as in-situ system. Results show that the droplet occurred at ion implantation becomes the cause of severe wear. Therefore, the ion-implanted surface should be removed the droplet to improve wear resistance.
Yoo, Dae Kyoung;Kong, Jung Hyun;Lee, Hea Joeng;Sung, Jang Hyun;Lee, Hae Woo
Korean Journal of Metals and Materials
/
v.46
no.11
/
pp.708-712
/
2008
The influence of high temperature gas nitriding (HTGN) in STS347 and STS310S steels was experimentally investigated. The HTGN was carried out at $1,050^{\circ}C{\sim}1,150^{\circ}C$ for 10 hrs in a gaseous atmosphere containing $1kg/mm^2$ of nitrogen. After HTGN, fine precipitates of $Cr_2N$ and NbN appeared in austenite on the surface of STS 347, while nitrogen pearlite, which was layeredof $Cr_2N$ and austenite alternatively, appeared in austenite on the surface of STS 310S. The surface hardness of HTGN-treated, STS 347 and STS 310S specimens was 250~360 Hv and 270~400 Hv, respectively, depending on the temperature of HTGN. The nitrogen content was analyzed 1.4 wt% and 1.6 wt% at the surface layer of STS 347 and STS 310S steels, respectively. In addition, an improvement in the corrosion resistance of HTGN treated specimens was observed.
The objective of this research was to characterize the fate and transport of Cr(VI) contaminated groundwater in the Daejeon industrial area. Five subsidiary monitoring wells were newly installed and two existing wells were utilized for the investigation and the reduction process of Cr(VI) contaminated groundwater of the Daejeon(Mun-pyeong) national groundwater monitoring station. The Cr(VI) concentrations at the shallow aquifer well of the station were in the range of 3.2-4.5 mg/L indicating continuous contamination. However, Cr was not detected at the deep bedrock well and the other monitoring wells except MPH-1 and 3. The Cr(VI) concentrations of MPH-1 and MPH-3 were below the drinking water guideline value (0.05 mg/L). Therefore, the plume of the Cr(VI) contaminated groundwater was predicted to be confined within the narrow boundary around the station. The soluble/exchangeable Cr(VI) concentrations were below the detection limit in all core and slime samples taken from the five newly installed wells. Although the exact source of contamination was not directly detected in the study area, the spatial Cr(VI) distribution in groundwater and characteristics of the core samples indicated that the source and the dispersion range were confined within the 100 m area from the monitoring station. The contamination might be induced from the unlined landfill of industrial wastes which was observed during the installation of an subsidiary monitoring well. For the evaluation of the natural attenuation of Cr(VI), available reduction capacities of Cr(VI) with an initial concentration of 5 mg/L were measured in soil and aquifer materials. Dark-gray clay layer samples have high capacities of Cr(VI) reduction ranging from 58 to 64%, which is obviously related to organic carbon contents of the samples. The analysis of reduction capacities implied that the soil and aquifer materials controlled the dispersion of Cr(VI) contamination in this area. However, some possibilities of dispersion by the preferential flow cannot be excluded due to the limited numbers of monitoring wells. We suggest the removal of Cr(VI) contaminated groundwater by periodical pumping, and the continuous groundwater quality monitoring for evaluation of the Cr(VI) dispersion should be followed in the study area.
The Thermal Barrier Coation(TBC) to improve the that barrier and wear resistant propenrty in high temperature ofthe aircraftength between the accumlation of the aircraft engine and the automobile engine has usually the two layer structure. One is a creamic top layer for heat insulation and the other is a metal bond layer to facilitate the bond strength between the top ceramic layer and the substrate. But, the coated layers should be peeled off because of the accumulation of the thermal stress by the differance of the thermal expantion coefficient between metal and ceramics in a hrat cyclic environment. In this study, the intermediate layer by plasm spray process was introduced to reduce the thermal stress. The powders of plasm spray coating were the Yttria Stabilized Zirconia (YSZ), the Magnesia Stabillized Zirconia(MSZ) and NiCrAlY. the intermediate layer was sprayed with the powders of the bond cast for the purpose of test were executed. The high temperature wear resistance tends to decreasnceee wear and thermal shock test were exeucuted. The high temperature were resistance of the YSZ TBC is better that of the MSZ TBC. The wearrsistance tends to decrease accoring to incresing the temperature between $400^{\circ}C$to $600^{\circ}C$. The thermal shock life of the 3 layer TBC with YSZ top casting was the most outstanding thermal shock rsisstasnce. This means that the intermediate layer should play an importnat roll to alleviate the diffrerence of the thermal expansion coef frcients between metallic layer and cermics layer.
The substrate patterned with the dry film has the cavity which has the $90^{\circ}$ wall angle. Electroplating Cu on this patterned substrate has the differrent shape history with the electrochemical parameters. By potential theory model, the reason of the variation of the shape change with the these parameters was investigated. The shape history could be explained by the current flow and the correlated area effects. By embedding the Ni layer between the Cu layers, shape history with the time was obtained experimentally and the results was compared with the numerical analysis by BEM. The adhesive Cr-Cu film in TAB application was etched with the various condition. The best condition for the etchant of the Cr-Cu film was found.
Proceedings of the Korean Society of Precision Engineering Conference
/
2004.10a
/
pp.921-924
/
2004
This paper is to investigate a crack for plasma sprayed MCrAlY coated material by acoustic emission method in 4-point bending test. The CoNiCrAlY is coated on Inconel-718 by vacuum plasma spray process. Micro-hardness measurement was conducted by means of Micro Vickers-hardness indentor. The porosity of coating layer was measured using a SEM and Image Analyzer. AE monitoring system is composed of PICO type sensor, a wide band preamplifier(40dB), a PC and AE DSP(16/32 PAC) board. The AE count, Hit and energy of coating specimens is measured according to coating thickness.
The molten carbonate fuel cell has conspicuous features and high potential in being used as an energy converter of various fuels to electricity and heat. However, the MCFC which use strongly corrosive molten carbonate at $650^{\circ}C$ have many problem. Systematic investigation on corrosion behavior of Fe/20Cr/Ti has been done in (62+38)mol % (Li+K) $CO_3$ melt at 923K by using. steady state polarization and electrochemical impedance spectroscopy method. It found that the corrosion current of these Febased alloys decreased with increasing Ti content, and this attribute to the formation of $LiCrO_2$ layer at the surface.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.