  • Recycle methodology was researched on the HIPS(High Impact Poly Styrene) materials which are used in modern industry widely, For the various mixing ratio between virgin pellets of HIPS and recycled ones, tensile strength and shrinkage ratio were analyzed with injection molding experiments and numerical simulations. In addition, the deviations of dimensional accuracy were observed in accordance with various molding conditions. Molding conditions such as mold and melt temperature were changed by 3 steps. Mixing ratio between virgin pellets of HIPS and recycled ones were under controlled with 15%, 30% and 45%.

  • PDF

A Review of Kinetic Model for Production of Highgrade Steel : Part. 1. Simulation Model Based on Coupled Reaction (고급강 제조 반응 모델의 검토 : Part. 1. Coupled Reaction 기반 시뮬레이션 모델)

  • Kim, Jeong-In;Kim, Sun-Joong
    • Resources Recycling
    • /
    • v.30 no.1
    • /
    • pp.3-13
    • /
    • 2021
  • In the secondary refining process for the production of high-grade steel, the proper composition is maintained by alloying elements, and non-metallic inclusions are controlled for high cleanliness. Complex reactions occur simultaneously between the molten steel, slag, inclusions, refractories, and alloying elements during the secondary refining process. Previous works have reported simulation models based on kinetics to predict the compositional changes in molten steel, slag, and inclusions in actual processes. Analytical reviews are required for the models to predict the process accurately. In this study, we reviewed and analyzed simulation models based on the coupled reaction model for the secondary refining process.

Properties of Cement Mortar as Particle Size and Hydrothermal Synthesis Temperature Using Scheelite Tailing (중석 광미를 사용한 시멘트 모르타르의 입도 및 수열합성온도별 물리적 특성)

  • Chu, Yong Sik;Seo, Seong Gwan;Choi, Sung Bum;Kim, Gyoung man;Hong, Seok Hwan
    • Resources Recycling
    • /
    • v.28 no.6
    • /
    • pp.46-53
    • /
    • 2019
  • Cement mortar was hydrothermal-synthesized with particle size of tailings using scheelite tailings deposited without proper treatment, and its physical properties were investigated. The mixing ratios of water-cement and sand-cement were fixed at 75 % and 400 %, respectively, during preparing cemnt mortar, and the sand was replaced by the tailings at 0 ~ 50 %. The particle size of tailings was controlled at 9.3 ~ 53.0 ℃, and the hydrothermal temperature was kept at 60 ~ 180 ℃ for 6 hours after the temperature increased to pretermined temperature with 2 ℃ heating rate. The compressive strength increased with increasing hydrothermal temperature. The compressive strengths were 55.2 MPa and 54.5 MPa when the mortars were prepared with 30 % low arsenic and high arsenic tailings after 60 min grinding. The compresiive strenght was enhanced 300 % compared with reference sample.

Removal of Chlorine from Fly Ash in Municipal Solid Waste Incineration Ash by Water Washing (수세에 의한 생활폐기물 소각재 중 비산재로부터 염소성분의 제거)

  • 안지환;한기천;김형석
    • Resources Recycling
    • /
    • v.10 no.5
    • /
    • pp.36-43
    • /
    • 2001
  • The chlorine component in fly ash from municipal solid waste incineration ash was removed by water washing for the purpose of recycling fly ash as a raw material of ordinary portland cement. The samples were a different kind of 리y ashes using $Ca(OH)_2$and NaOH as media of wet scrubber for flue gas cleaning. The content of soluble salts of fly ash using $Ca(OH)_2$and NaOH was 32.8%, 50.1% and the content of chlorine component, 22.9% and 26.0% respectively, which was KCl, NaCl, CaC1OH mainly. When each fly ash was washed using water under conditions of a agitation speed of 300 rpm, a liquid to solid ratio of 10, most soluble salts in fly ash were dissolved within 30 minutes and the content of chlorine component in ash was diminished to the content of 4.4%, 2.O% at $20^{\circ}C$ and 1.7%, 0.8% at $50^{\circ}C$ respectively. And the main compound of residual chlorine component in ash after water washing was friedel`s salt ($3CaO.A1_2$$O_3$.$CaCl_2$.$10H2$O). From analysis results of water quality for wastewater by water washing, the components exceeding discharged wastewater standard were only Pb and Cd. But As pH was controlled to 10 with addition of $CO_2$(g) or $Na_2$$_CO3$in water, the concentration of heavy metals such as Pb and Cd was also under discharged wastewater standard.

  • PDF

Recycling of Sludgewater containing Set-retarder (지연제 첨가에 의한 회수수의 재이용)

  • Song, Young-Jin;Daiki, Atarashi
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2008.11a
    • /
    • pp.761-764
    • /
    • 2008
  • Most of ready-mixed concrete plants have the problem of construction waste sludge, which pollutes environment and causes economic loss due to the discard and increasing the cost of concrete. Thus, a recycling of the cement sludge has been strongly desired as one of their solution. This research is to the study on the recycling of the cement sludge, especially the study on the hydration control by the sodium gluconate as a set-retarder. The set-retarder can delay the hydration of the cement included in the sludge water, so that the sludge water can be substituted with some of new cement without the property of the cement. And it invests the effect of the sodium gluconate to the hydration of the cement in suspension. The degree of hydration of cement may be controlled by adding the sodium gliconate. The hydration delay time is observed that depends on the concentration of residual sodium gloconate, not how long the cement has been hydrated before the addition of the sodium gluconate.

  • PDF

Solubility and Yield Characteristics of KCl in Cement By-Pass Dust (시멘트 바이패스 더스트에 존재하는 염화칼륨의 용해 및 수득 특성)

  • Yun, Youngmin;Jeong, Jaehyun;Chu, Yongsik
    • Resources Recycling
    • /
    • v.25 no.3
    • /
    • pp.43-48
    • /
    • 2016
  • Cement manufacturing plant uses various kinds of industrial/municipal waste. The waste contains considerable amount of potassium, chlorine and small amount of heavy metal. Many researches were performed to fabricate valuable resources from the waste. In this study, various methods, which dissolves and crystallizes potassium/chlorine to extract potassium chloride, were experimented. Especially amount of water, slurry temperature, and stirring time were controlled. Then kind of heavy metal and content of potassium chloride were analyzed. The yield of potassium chloride increased, as the amount of water for slurry increased but it increased slightly, when the water content was over 200%. The yield tended to increase, when the temperature of slurry was over a certain point. The yield did not increase in case of over 10 minutes stirring time. The kind and content of heavy metal in potassium chloride were various according to stirring time. The main heavy metals were Pb, Cu, and $Cr^{6+}$.

Leaching Behavior of Nickel from Waste Multi-Layer Ceramic Capacitor (폐(廢) 적층형(積層形)세라믹콘덴서에 함유(含有)된 니켈의 침출거동(浸出擧動))

  • Kim, Eun-Young;Kim, Byung-Su;Kim, Min-Seuk;Jeong, Jin-Ki;Lee, Jae-Chun
    • Resources Recycling
    • /
    • v.14 no.5 s.67
    • /
    • pp.32-39
    • /
    • 2005
  • Leaching behavior of nickel contained in waste Multi-Layer Ceramic Capacitor (MLCC) was investigated using a batch reactor. The effects of acid type, acid concentration, leaching temperature, particle size, and reaction time on the extraction of nickel metal from waste MLCC were examined. As a result, 97% of nickel contained in waste MLCC was leached out in 30 min at the temperature of $90^{\circ}C$ under the condition of $HNO_3$ concentration 1N, solid/liquid ratio 5 g/L and particle size $-300/+180{\mu}m$. It was also found that a Jander equation was useful to fit well the leaching rate data. The rate of nickel leaching is controlled by pore diffusion in $BaTiO_3$ layer and has an activation energy of 37.6 kJ/mol (9.0 kcal/mol).

A Study on Synthesis of Potassium Sulfate used Sodium Sulfate and Potassium Chloride (황산나트륨과 염화칼륨을 사용한 황산칼륨 제조 연구)

  • Kim, Nam-Il;Kim, Tae-Yeon;Chu, Yong-Sik
    • Resources Recycling
    • /
    • v.30 no.1
    • /
    • pp.35-43
    • /
    • 2021
  • In this study, Na2SO4 and KCl reagents were used to synthesize K2SO4 as a basic study for recycling byproducts generated during the manufacture of steel and cement. The mole ratio of Na2SO4 to KCl, the saturation of the solution, and the stirring temperature were controlled to derive the optimal manufacturing conditions. The microstructure and crystallinity of the materials prepared were evaluated using scanning electron microscopy and X-ray diffraction analysis. Pure K2SO4 was obtained when the mole ratio of Na2SO4 to KCl was 1:6-18, the saturation of the solution was less than 160%, and the stirring temperature was 20℃, 50℃. The optimal manufacturing conditions to maximize the crystallinity and yield of K2SO4 while minimizing the energy consumption were 1:6 mole ratio of Na2SO4 to KCl, 140% saturation of the solution, and 20℃ stirring temperature.

Characterization of interfacial chemistry on the coal bottom ash (저회의 계면 화학적 특성 규명)

  • Lee, Ki-Gang
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.21 no.2
    • /
    • pp.92-97
    • /
    • 2011
  • Landfill is the main treatment method for bottom-ash because it has not only an irregular particle size and ingredients but also not proper recycling treatment. The aim of this study is to raise recycling rate of bottom-ash(nonplasticity pulverulent) and for the purpose of alternatives of clay to investigate the properties of Bottom-ash (B/A)-Hard Clay (H/C) bodies with controlled interfacial chemistry properties. After investigating the sedimentation height of suspensions with controlled pH, it was discovered that there was no hetero-polar aggregation for mixed slips because hard clay and bottom-ash had similar interfacial chemistry properties. Also, bulk density, water absorption, and microstructure properties of each pellet was observed that made by silp casting method and manufactured at $50^{\circ}C$ intervals between $1000{\sim}1250^{\circ}C$. As a result, dispersed slip of clay and bottom ash are possible for slip casting and plastic forming process because they exhibit Bingham plastic behavior. Products that made by slip with dispersed clay and bottom ash are not only suitable for KS L 4201 and KS L 1001 at $1250^{\circ}C$ but it is also possible to apply for ceramic and sanitary ware because specific gravity was about 15 % lighter than general ceramic materials.

Physical and Chemical Analysis of Organic Wastes for the Establishment of Total Management System (유기성 폐기물 종합관리기술구축을 위한 물리·화학적 성상 분석)

  • Kim, Young-Koo;Phae, Chae-Gun;Choi, Hoon-Keun;Kim, Sung-Mi;Hwang, Eui-young
    • Journal of the Korea Organic Resources Recycling Association
    • /
    • v.13 no.1
    • /
    • pp.100-114
    • /
    • 2005
  • Organic waste, which is defined as wastes derived from various biological organisms that contain more than 40% of organic materials, is generated about 100 million tons per year in Korea. These organic wastes are now controlled by several governmental entities, under different rules and regulations, leading to the improper management and inefficient treatment. Therefore, integrated management system is primarily needed for the efficient recycling of organic waste. In this study, six kinds of organic wastes, which are food waste, sludges(sewage, waste water, night soil), animal excreta, animals and plants residues, and three kinds of recycling by-products(compost, feed, anaerobic digestion by-products) made of organic wastes, were analyzed for their physical and chemical characteristics. On the basis of this result, a possibility for the efficient recycling of organic waste was investigated.

  • PDF