Proposal of Matrix Spacing Factor for Analyzing Air Void System in Hardened Concrete (콘크리트 내부공극 분석을 위한 행렬간격계수 모델식의 제안)

  • Jeong Won-Kyong;Jun In-Koo;Kim Yong-Kon;Lee Bong-Hak
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2004.11a
    • /
    • pp.679-682
    • /
    • 2004
  • Air void systems in hardened concrete has an important influence on concrete durability such as freeze-thaw resistance, water permeability, surface scaling resistance. Linear traverse method and point count method described at ASTM is the routine analysis of the air void system that have been widely used to estimate the spacing factor in hardened concrete. Recently, many concretes often have a spacing factor higher than the generally accepted $200-250{\mu}m$ limit for the usual range of air contents. This study is proposed to estimate the matrix spacing factor by calculation of simplicity. The matrix spacing factor needs two parameters that are air content and numbers of air voids in the hardened concrete. Those are obtained from the standard air-void system analysis of the ASTM C 457. The equation is valid for all values of paste-to-air ratio because the estimation of paste content is unnecessary at the using ASTM C 457. The matrix spacing factor yields a similar estimate of the standard spacing factor.

  • PDF

Influence of Mix Factors and Mixing Ratio of Aggregate on the Strength and Water Permeability of Porous Concrete (포러스 콘크리트의 배합요인 및 골재 혼합비율이 강도 및 투수성능에 미치는 영향)

  • 김무한;김규용;백용관
    • Journal of the Korea Concrete Institute
    • /
    • v.12 no.6
    • /
    • pp.91-98
    • /
    • 2000
  • Porous concrete having continuous voids is gaining more interest as an ecological material. It has several useful functions such as water and air permeability, sound absorption, etc. Its strengths are considerably lower than those of conventional concrete due to the large and continuous voids in it. This study has been carried out to investigate the influence of mix factors and mixture proportion of aggregate on the strengths and water permeability of porous concrete. And it has been carried out to investigate the evaluation of void of porous concrete by the ultra-sonic pulse velocity. The results f this study are as follows: 1) The theoretical void ratio has greater influence than any other factor on the strengths and water permeability of porous concrete. And it is a little affected by the replacement proportion of silica-fume and mixture proportion of aggregate. 2) Because the coefficients of correlation between the void ratio and ultra-sonic pulse velocity were relatively high, it will be possible that the void ratio is predicted by the ultra-sonic pulse velocity.

Corrosion Properties of Reinforced Concrete with Types of Surface Cover and Covering Depth under the Combined Deterioration Environments (복합열화 환경하에서 표면피복종류 및 피복두께에 따른 철근콘크리트의 부식특성)

  • Kim, Moo-Han;Kwon, Young-Jin;Kim, Young-Ro;Kim, Jae-Hwan;Jang, Jong-Ho;Cho, Bong-Suk
    • Journal of the Korea Institute of Building Construction
    • /
    • v.4 no.1
    • /
    • pp.119-126
    • /
    • 2004
  • Generally, reinforced concrete is one of the most commonly used structural materials and it prevents corrosion of steel bar by high pH of interior, But, as time elapsed, reinforced concrete structure become deteriorated by many of combined deterioration factors and environmental conditions. And, there are large number of deteriorate mechanism of the reinforced concrete structure and it acts complexly. It is recognized that steel bar corrosion is the main distress behind the present concern regarding concrete durability. In this study, to institute combined deterioration environments, established acceleration condition and cycle for combined deterioration environments has a resemblance to environments which are real structures placed. After that to confirm corrosion properties of reinforced concrete due to permeability with covering depth and types of surface cover under combined deterioration environments, measured carbonation velocity coefficients, chloride ion diffusion coefficients, water absorption coefficients, air permeability coefficients and electric potential, corrosion area ratio, weight reduction, corrosion velocity of steel bar. The results showed that an increase in age also decrease carbonation velocity coefficients, increase Chloride ion diffusion coefficients and increases water absorption coefficients. As well, an increase in age also increases corrosion of steel bar. Data on the development of corrosion velocity of steel bar with types of surface cover made with none, organic B, organic A, inorganic B, and inorganic A is shown. As well, permeability and corrosion velocity of steel bar with covering depth is superior to 10mm than 20mm. And it is confirmed permeability and corrosion properties of steel bar are closely related.

A Study on the Air-Vent System of Complex Layer Applied Poly-Urethane Waterproofing Material and Air-Permeability Buffer Sheet (절연용 통기완충 시트와 폴리우레탄 도막 방수재를 복합 적층한 탈기 시스템에 관한 연구)

  • Oh, Sang-Keun;Park, Bong-Kyu;Ko, Jang-Ryeol;Park, Yoon-Chul;Kim, Su-Ryon
    • Journal of the Korea Institute of Building Construction
    • /
    • v.2 no.1
    • /
    • pp.139-146
    • /
    • 2002
  • This study deals with the characterizing and the application like as insulation materials in the joint part in concrete surface layer and waterproofing sheet especially for roof slabs. Using steel materials and butil-rubber tape to band waterproofing sheet and concrete surface together before this waterproofing system will be applied. It can be expected to both the curability and the watertightness by coating poly-urethane 2 or 3 times with sheet surface. Therefore this waterproofing system can be possible to protect water without the damage when vapor is going out from concrete and without air pockets because of the difference temperature inside and out. This system particularly consists of air bents and elastic waterproofing sheet considering the physical damage while water can cause purely physical damage. This system is one of the most efficient ways of waterproofing system without air pocket.

Development of Image Analysis Techniques for Measuring Air Void System in Hardened Concrete (콘크리트 내부 공극 분석을 위한 화상분석기법의 개발)

  • Jun In-Ku;Lee Bong-Hak;Yun Kyong-Ku;Jeong Won-Kyong
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2004.05a
    • /
    • pp.810-813
    • /
    • 2004
  • Air void systems in hardened concrete has an important influence on concrete durability such as freeze-thaw resistance, water permeability, surface scaling resistance, and etc. Linear traverse method and point count method described at ASTM have been widely used to estimate the air void system in hardened concrete. These methods, however, are rarely used at present, because they require many efforts, are time consuming works, depend on each person's decision, and are not repeatable. Thus, new image analysis method using microscope and computer processes has been approached for analyzing air void system in hardened concrete. However, it is just in initial step. The purposes of this study were to develope an effective and reliable image analysis technique for estimating air void system in hardened concrete. The developed technique was proved to be accurate, reasonable and repeatable.

  • PDF

An Experimental Study on NOx Degradation Efficiency and Physical Characteristics of Maximum Size 40 mm Porous Concrete (굵은골재 최대치수 40 mm 투수 콘크리트의 물리적 특성과 질소산화물 제거에 관한 연구)

  • Hong, Chong-Hyun;Kim, Moon-Hoon;Ryu, Seong-Pil;Choung, Kwang-Ok
    • Journal of Environmental Science International
    • /
    • v.15 no.5
    • /
    • pp.431-438
    • /
    • 2006
  • The strength, water permeability, and photo-degradation efficiency of NOx of porous concrete with a new concept were studied in this paper. The porous concrete was comprised of coarse aggregate of maximum size 40 mm, cement, silica fume, water and air-entraining(AE) water reducing agent. The strength of porous concrete was strongly related to its matrix proportion and compaction energy. An experimental test was carried out to study the parameters of cement proportions and silica fume content for pavement applications of porous concrete which were paving a footpath, a bikeway, a parking lot, and a driveway. The regressed equations of relation-ships between compressive strength and flexural strength, and coefficient permeability and void ratios were indicated as y=7.69x+71.74 and $y=0.42e^{0.28x}$. A method of making an air purification-functioning road, which was spraying a mixture of a photocatalyst, cement, and water onto the surface of the road, was suggested.

A Study on the Effects of Superplasticizers on the Engineering Preperties of Plain Concrete (I) (고성능유동화제가 콘크리트의 공학적 특성에 미치는 영향 (I))

  • 박승범;이보성
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.26 no.3
    • /
    • pp.68-80
    • /
    • 1984
  • This study was attempted in order to investigate the effects of superplasticizers on fresh and hardened concrete. The experimental program included tests on the slump and slump loss, bleeding, time of set, air content, the compacting, factor Vee Dee, compressive strength, tensile and flexural strength, permeability, shrinkage and freege-thaw durability. The major conclusions that can be drawn on the study are as follows. 1. Superplasticizers were observed to have an appreciable fluidifying action in fresh concrete so that tinder appropriate conditions, they either considerably improved its workability or permitted a water reduction of at least 8-12% to be made while maintaining normal workability. 2. The bleeding ratios of base and S,P. Concrete were much lower than those of the conventional concrete. Differences between the base and S.P. Concrete were insignifician. 3. The setting time was the longest for conventionla concrete, followed by S.P. concrete and base concrete in thatorder. And AE water reduction admixtures showed an appreciable influence on the setting and hardening characteristics of concrete and prolonged the stiffening times. 4. The high initial slump values of S.P. concrete generally decreased rapidly with increased standing time. CF values showed increasing tendencies with the increase of S.P. content, and excessive addition of S.P. caused the segregation of fresh concrete, resulting in its rejection. 5. Though there was a slight increase in strength, no significant differences are observed between base and S.P. concrete in terms of the compressive, tensile and flexural strength. 6. The permeability of S.P. concrete was significantly less than that of the conventional concrete, and the shrinkage of S.P. concrete was considerably smaller than that of the conventional concrete, but there were no significant differences between base and S.P. concrete. 7. Compared to base concrete, S.P. concrete without entrained air tended to slightly increase freeze-thaw durability, and S.P. concrete with an appropriate entrained air gave satisfactory resistance to freezing and thawing.

  • PDF

An Experimental Study on the Effect if Fiber Reinforced on CFRD Face Slab Concrere (CFRD 차수벽콘크리트에서의 섬유보강효과에 관한 실험적 연구)

  • 최세진;임정열;김완영;김무한
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2000.04a
    • /
    • pp.122-125
    • /
    • 2000
  • CFRD (Concrete Faced Rockfill Dam) face slab concrete has a much capability to occur crack due to drying shrinkage, hydration heat and bas compaction etc. Because of crack of concrete induce structural problem and decrease durability of concrete, it is need to reduce crack of concrete. This is an experimental study to analyze the effect of fiber reinforced on CFRD face slab concrete. for this purpose, it was investigated and analyzed the engineering properties of plain concrete and polypropylene fiber reinforced concrete (PFRC) according to test result ; the test include slump, air content, compressive strength, tensile strength, drying shrinkage and permeability etc. As the results, it was found permeability and drying shrinkage of PFRC less than that of plain concrete.

  • PDF

Estimation of Air Void System and Permeability of Latex-Modified Concretes by Image Analysis Method (화상분석법을 이용한 라텍스개질 콘크리트의 공극 구조와 투수성의 상관성 분석)

  • Jeong Won-Kyong;Yun Kyong-Ku;Hong Seung-Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.17 no.5 s.89
    • /
    • pp.695-702
    • /
    • 2005
  • It is known that latex-modified concretes were increased their durability and permeability by added latex. The purpose of this study was to analysis the air void systems in latex-modified concretes using a reasonable and objective image analysis method with main experimental variables such as water-cement ratios, latex contents(0%, 15%) and cement types(ordinary portland cement, high-early strength cement and very-early strength cement). The results are analyzed spacing factor, air volume after hardened, air distribution and structure. Also, air void systems and permeability of latex-modified concretes were compared with correlation. The results are as follows; The same w/c ratio LMC showed better air entraining effect than OPC with AE water reducer. The VES-LMC showed that the number of entrained air below $100{\mu}m$ increased more than four times. In the HES-LMC, micro entraining air having range from 50 to $500{\mu}m$ increased above 7 times without antifoamer. Though spacing factor was measured low, latex-modified concretes were showed that permeability was good. It is considered that air void system does not have an effect on the property of latex-modified concretes but latex film is more influenced in the their durability.

Sensitivity Analysis of Design Parameters of Air Tightness in Underground Lined Rock Cavern (LRC) for Compressed Air Energy Storage (CAES) (복공식 지하 압축공기에너지 저장공동 기밀시스템 설계변수의 민감도 해석)

  • Kim, Hyung-Mok;Rutqvist, Jonny;Ryu, Dong-Woo;Sun-Woo, Choon;Song, Won-Kyong
    • Tunnel and Underground Space
    • /
    • v.21 no.4
    • /
    • pp.287-296
    • /
    • 2011
  • We performed a numerical modeling study of thermodynamic and multiphase fluid flow processes associated with underground compressed air energy storage (CAES) in a lined rock cavern (LRC). We investigated air tightness performance by calculating air leakage rate of the underground storage cavern with concrete linings at a comparatively shallow depth of 100 m. Our air-mass balance analysis showed that the key parameter to assure the long-term air tightness of such a system was the permeability of both concrete linings and surrounding rock mass. It was noted that concrete linings with a permeability of less than $1.0{\times}10^{-18}\;m^2$ would result in an acceptable air leakage rate of less than 1% with the operational pressure range between 5 and 8 MPa. We also found that air leakage could be effectively prevented and the air tightness performance of underground lined rock cavern is enhanced if the concrete lining is kept at a higher moisture content.