A Study of Reduced and Carburized Reactions in Dry-milled $WO_3+Co_3O_4+C$ Mixed Powders with Different Carbon Content

  • Im, Hoo-Soon;Lee, Wan-Jae
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.648-649
    • /
    • 2006
  • The dry-milling technique was used for mixing and crushing oxides and graphite powders. The ratio of ball-to-powder was 30:1 and argon gas was filled in jar. The excess carbon was $10{\sim}20wt%$ of the stoichiometric amount. The dry-milling was carried for 20 hours. The mixed powders were reduced and carburized at $900{\sim}980^{\circ}C$ for 3 hours flowing Ar gas in tube furnace. The dry-milled powders showed the wide diffraction patterns of X-ray. The reactions of reduction and carburization were completed in 3 hours at $980^{\circ}C$. After the reactions, the mean size of WC particles was about 200 nm. The content of free carbon in WC/Co mixed powders was less as the reaction temperature increased.

  • PDF

Production of the ultra fine-composite powders of WC-Co and WC-Ni (초미립의 탄화 텅스텐-코발트와 탄화 텅스텐-니켈 복합분말의 제조)

  • 김병재;윤병하
    • Journal of the Korean institute of surface engineering
    • /
    • v.26 no.2
    • /
    • pp.87-107
    • /
    • 1993
  • The grain size of the final products of WC-Co and WC-Ni composite powders is dependent on the size of the starting material and the conditions employed for the reduction and carburization. APT-Co and -Ni com-plex salts were prepared by the substitution reaction between ammonium ions in APT and the metal ions in Co(NO3)2 and Ni(NO3)2 solutions of different concentrations(0.1 to 0.7M) at $50^{\circ}C$ and the grain sizes of the com-plex salts was $0.54~0.76\mu\textrm{m}$. The complex which calcined the complex salts at $700^{\circ}$~80$0^{\circ}C$ for 60min. were 0.2~0.5$\mu\textrm{m}$. W-Co($5.92^{\circ}C$) and -Ni(6.95%) powders which reduced the complex oxides with H2d atmo-sphere(flow rate;600cc/min.) at $700^{\circ}$~$800^{\circ}C$ for 60min. were $0.5~0.6\mu\textrm{m}$. The mean grain sizes of WC-Co and WC-Ni composite powders which carburized both complex metals of W-Co and W-Ni at $800^{\circ}C$ for 60min. were $0.5~0.6\mu\textrm{m}$, and take place the coarsening of the grain above $800^{\circ}C$ and the optmium ratio of C3H8 and H2 was 0.2 for the control of the free carbon. The effect of Co contents on the particle sizes decreased from 0.4 to $0.25\mu\textrm{m}$ with increasing the content from 2.0 to 7.6w%. The activation energies on the reductions of oxides and the formations of carbides were as follows ; W-Co : Q = 8.7 kcal/mole, W-Ni : Q = 8.1 kcal/mole, WC-Co pow-der : Q = 17.8 kcal/mole, WC-Ni powder : Q = 16.6 kcal/mole.

  • PDF

Mechanical Properties and Fabrication of Nanostructured Ti3Al-Al2O3 Composite from Mechanically Synthesized Powders by Pulsed Current Activated Sintering (기계적 합성된 분말로부터 펄스전류활성 소결에 의한 나노구조 Ti3Al-Al2O3 복합재료 제조 및 기계적 특성)

  • Shon, In-Jin;Wang, Hee-Ji;Suh, Chang-Yul;Cho, Sung-Wook;Kim, Wonbaek
    • Korean Journal of Metals and Materials
    • /
    • v.49 no.5
    • /
    • pp.374-379
    • /
    • 2011
  • Nano-powders of $Ti_3Al$ and $2Al_2O_3$ were synthesized from $3TiO_2$ and 5Al powders by high energy ball milling. A nanocrystalline $Al_2O_3$ reinforced composite was consolidated by pulsed current activated sintering within 2 minutes from mechanochemically synthesized powders of $Al_2O_3$ and $Ti_3Al$. Nanocrystalline materials, have received much attention as advanced engineering materials due to their improved physical and mechanical properties. The relative density of the composite was 99.5%. The average obtained hardness and fracture toughness values were 1510 kg/$mm^2$ and $9\;MPa{\cdot}m^{1/2}$, respectively.

Ballistic Properties of Zr-based Amorphous Alloy Surface Composites Fabricated by High-Energy Electron-Beam Irradiation (고에너지 전자빔 투사방법으로 제조된 Zr계 비정질 합금 표면복합재료의 탄도충격 성능)

  • Do, Jeonghyeon;Jeon, Changwoo;Nam, Duk-Hyun;Kim, Choongnyun Paul;Song, Young Buem;Lee, Sunghak
    • Korean Journal of Metals and Materials
    • /
    • v.48 no.12
    • /
    • pp.1047-1055
    • /
    • 2010
  • The objective of this study is to investigate the ballistic properties of Zr-based amorphous alloy surface composites fabricated by high-energy electron-beam irradiation. The mixture of Zr-based amorphous powders and $LiF+MgF_2$ flux powders was deposited on a pure Ti substrate, and then an electron beam irradiated this powder mixture to fabricate a one-layer surface composite. A four-layer surface composite, in which the composite layer thickness was larger than 3 mm, was also fabricated by irradiating the deposited powder mixture by an electron beam three times on the one-layer surface composite. The microstructural analysis results indicated that a small amount of fine crystalline particles were homogeneously distributed in the amorphous matrix of the surface composite layer. According to the ballistic impact test results, the surface composite layers effectively blocked a fast traveling projectile, while many cracks were formed at the composite layers, and thus the surface composite plates were not perforated. The surface composite layer containing ductile ${\beta}$ dendritic phases showed a better ballistic performance than the one without dendrites because dendritic phases hindered the propagation of shear bands or cracks.

Chemical Homogeneity and Dispersoid Formation in Mechanically Alloyed Al-Ti Composite Metal Powders (기계적 합금화한 Al-Ti 복합금속분말의 화학적 균질성과 분산상 형성)

  • Lee, Kwang-Min;Moon, In-Hyung
    • Analytical Science and Technology
    • /
    • v.5 no.1
    • /
    • pp.103-110
    • /
    • 1992
  • Chemical homogeneity and dispersoid formation in mechanically alloyed Al-Ti composite metal powders were investigated in order to fabricate the high temperature Al-Ti alloys. The homogeneity of composite particles was able to be obtained by MA milling time more than 10 hours with the milling velocity of 400 rpm. The amounts of titanium, carbon and oxygen elements in MA Al-Ti alloys by chemical analysis were 8.2, 1.135 and 0.233 wt.%, respectively. The amount of carbon analyzed corresponds to 90 pet. of carbon contained the PCA of stearic acid. TEM analysis has revealed the presence of the rounded $Al_3Ti$ dispersoids with the size of 250nm and the $Al_4C_3$ dispersoids of cylindrical shape with a size of 50nm in thickness and 150nm in length. Also, the some rounded $Al_2O_3$ dispersoids with a size of about 20nm were found in grain boundaries as well as in matrix.

  • PDF

Comparison of Experimental Values and Theoretical Predictions of the Dielectric Constant of Epoxy/BaTiO$_3$ Composite Embedded Capacitor Films (에폭시/BaTiO$_3$ 복합 내장형 커패시터 필름의 유전상수에 관한 실험값과 이론적 예측값과의 비교)

  • 조성동;이상용;현진걸;백경욱
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.11 no.1
    • /
    • pp.87-96
    • /
    • 2004
  • Polymer/ceramic composites are the most promising embedded capacitor material for organic substrates application. Predicting the effective dielectric constant of polymer/ceramic composites is very important for design of composite materials. In this paper, we measured the dielectric constant of epoxy/$BaTiO_3$ composite embedded capacitor films with various $BaTiO_3$ particles loading for 5 different sizes $BaTiO_3$ powders. Experimental data were fitted to several theoretical equations to find the equation useful for the prediction of the effective dielectric constant of polymer/ceramic composites and also to estimate the dielectric constant of $BaTiO_3$ powders. The Lichtenecker equation and the Jayasundere-Smith equation were useful for the prediction of the effective dielectric constant of epoxy/$BaTiO_3$ composites. And calculated dielectric constants of the $BaTiO_3$ powders were in the range of 100 to 600, which were lower than those of $BaTiO_3$ bulk ceramics.

  • PDF

Preparation of β-TCP/TiO2 Composite by Hot-Pressing (가압소결에 의한 β-TCP/TiO2복합체의 제조)

  • 정항철;이종국
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.3
    • /
    • pp.202-209
    • /
    • 2004
  • Hydroxyapatite(HA)/TiO$_2$ composite powders were prepared by mixing of spherical TiO$_2$ (10-15 nm, 500 nm) and needle-shaped HA (50-70 nm, 120-250 nm) powders which had been synthesized through precipitation, sol-gel and hydrothermal methods. From the three types of starting composite powders (HA/TiO$_2$ wt% of 75/25, 50/50, and 25/75), dense $\beta$-TCP/TiO$_2$ composites were prepared by hot-pressing at 800-100$0^{\circ}C$ for 30 min under the pressure of 30 ㎫ in Af atmosphere. The $\beta$-TCP/TiO$_2$ composites showed different microstructures and sintering densities depending on their powder morphology, composition and sintering temperature. With increasing the sintering temperature and the content of TiO$_2$, sintered density was increased and microstructure became more homogeneous.

Synthesis and Optical Properties of TiO2/TiOF2 Composite Powder with Controlled Phase Fractions via an Ultrasonic Spray Pyrolysis Process (초음파 분무 열분해 공정을 이용한 TiO2와 TiOF2 복합체 분말의 합성과 상 분율에 따른 광학적 성질)

  • Hwangbo, Young;Park, Woo-Young;Lee, Young-In
    • Korean Journal of Materials Research
    • /
    • v.27 no.6
    • /
    • pp.325-330
    • /
    • 2017
  • Photoelectron-hole separation efficiency plays an important role in the enhancement of the photocatalytic activity of photocatalysts towards the degradation of organic molecules. In this study, $TiO_2/TiOF_2$ heterostructured composite powders with suitable band structures, which structures are able to separate photoelectron-hole pairs, have been synthesized using a simple and versatile ultrasonic spray pyrolysis process. In addition, their phase volume fractions have been controlled by varying the pyrolysis temperature from $400^{\circ}C$ to $800^{\circ}C$. The structural and optical properties of the synthesized powders have been characterized by X-ray diffraction, scanning electronic microscopy and UV-vis spectroscopy. The powder with a phase volume ratio close to 1, compared with single $TiOF_2$ and other composite powders with different phase volume fractions, was found to have superior photocatalytic activity for the degradation of rhodamine B. This result shows that the $TiO_2/TiOF_2$ heterostructure promotes the separation of the photoinduced electrons and holes and that this powder can be applicable to environmental cleaning applications.

Microstructural Evolution of Aluminum Nitride - Yttrium Aluminum Garnet Composite Coatings by Plasma Spraying from Different Feedstock Powders (Aluminum Nitride - Yttrium Aluminum Garnet 분말 특성과 플라즈마 용사 코팅층의 미세조직)

  • So, Woong-Sub;Baik, Kyeong-Ho
    • Korean Journal of Materials Research
    • /
    • v.21 no.2
    • /
    • pp.106-110
    • /
    • 2011
  • A high thermal conductive AlN composite coating is attractive in thermal management applications. In this study, AlN-YAG composite coatings were manufactured by atmospheric plasma spraying from two different powders: spray-dried and plasma-treated. The mixture of both AlN and YAG was first mechanically alloyed and then spray-dried to obtain an agglomerated powder. The spray-dried powder was primarily spherical in shape and composed of an agglomerate of primary particles. The decomposition of AlN was pronounced at elevated temperatures due to the porous nature of the spray-dried powder, and was completely eliminated in nitrogen environment. A highly spherical, dense AlN-YAG composite powder was synthesized by plasma alloying and spheroidization (PAS) in an inert gas environment. The AlN-YAG coatings consisted of irregular-shaped, crystalline AlN particles embedded in amorphous YAG phase, indicating solid deposition of AlN and liquid deposition of YAG. The PAS-processed powder produced a lower-porosity and higher-hardness AlN-YAG coating due to a greater degree of melting in the plasma jet, compared to that of the spray-dried powder. The amorphization of the YAG matrix was evidence of melting degree of feedstock powder in flight because a fully molten YAG droplet formed an amorphous phase during splat quenching.