The heat transfer characteristics of solar tower receivers are experimentally investigated with receiver shapes. Generally, these become different according to the shapes and materials of the volumetric air receiver. In order to study these effects, the apparatus adopting laminated mesh and honeycombs as the volumetric air receiver is proposed. The receiver consists of laminated mesh (diameter; 100 mm, thickness; 1 mm), honeycombs (diameter; 100 mm, thickness; 30 mm) inserted into ceramic tube (inside diameter; 100 mm, outside diameter; 120 mm, length: 1000 mm). To apply heat to the receiver, an electric heater is used. To find out the heat transfer characteristics of the laminated mesh, the air temperatures are obtained by installing 3 thermocouples on each layer, dividing ceramic tube into 4 layers. Also, a radiative shield is installed to measure the only air temperature. The data for laminated mesh and honeycomb thickness of 30, 60, 90 mm are obtained. The results show that the temperature of layer 3 is higher than those of layer 2 and layer 1.
With aids of square wave voltammetry (SWV) the redox behavior for various combination of polyvalent ions (Sb+Fe, Sb+Zn, Sb+Ce+Ti+Zn) was investigated in alkali-alkaline earth-silica CRT (Cathode Ray Tube) glass melts. The current-potential curve so called voltammogram was produced at temperature range of 1400 to $1000^{\circ}C$ under the scanned potential between 0 and -800 mV at 100 Hz. In the case of the Sb+Fe and Sb+Zn doped melts, peak for $Sb^{3+}/Sb^0$ shown voltammogram was shifted to negative direction comparing to the only Sb doped melts. However, according to voltammogram of Sb+Ce+Ti+Zn doped melt, Ti and Ce except Zn had hardly any influence on the redox reaction of Sb. Based on the temperature dependence of the peak potential, standard enthalpy (${\Delta}H^0$) and standard entropy (${\Delta}S^0$) for the reduction of $Fe^{3+}$ to $Fe^{2+}$, $Sb^{3+}$ to $Sb^0$, $Zn^{2+}$ to $Zn^0$ and $Ti^{2+}$ to $Ti^0$ in each polyvalent ion combination of CRT glass melts were calculated.
Kim, Daejong;Lee, Jongmin;Park, Ji Yeon;Kim, Weon-Ju
Journal of the Korean Ceramic Society
/
v.50
no.6
/
pp.359-363
/
2013
Silicon carbide and its composites are being considered as a nuclear fuel cladding material for LWR nuclear reactors because they have a low neutron absorption cross section, low hydrogen production under accident conditions, and high strength at high temperatures. The SiC composite cladding tube considered in this study consists of three layers, monolith CVD SiC - $SiC_f$/SiC composite -monolith CVD SiC. The volume fraction of SiC fiber and surface roughness of the composite layer affect mechanical and corrosion properties of the cladding tube. In this study, various types of SiC fiber preforms with tubular shapes were fabricated by a filament winding method using two types of Tyranno SA3 grade SiC fibers with 800 filaments/yarn and 1600 filaments/yarn. After chemical vapor infiltration of the SiC matrix, the surface roughness and fiber volume fraction were measured. As filament counts were changed from 800 to 1600, the surface roughness increased but the fiber volume fraction decreased. The $SiC_f$/SiC composite with a bamboo-like winding pattern has a smaller surface roughness and a higher fiber volume fraction than that with a zigzag winding pattern.
The purpose of this research is to expand the realm of a button for a decorative purpose through embossing the effect and gravity of a button in fashion by designing the new ceramic buttons which are mainly used for decorative function in costume. In order to acquire a motif for the design, I analyzed several works of Gustav Klimt. As the result, those feature can be classified into the use of decorative lines, mosaic forms, and harmony of golden yellow and black, and it can be applied to buttons and clothes design. The sort of clay used in manufacturing the ceramic buttons was white clay to have high density and to diffuse light well, and press shaping techniques using plaster mold were employed. The baking was performed in an electronic kiln at $800^{\circ}C$ for the first time and at $1250^{\circ}C$ for the second time. Based on wearable designs in 2002/2003 F/W Trend of Interfashion Planning, I made three pieces of dress which could express the button's capability of decoration with effect. This is expressing a simplified form which shows up in details of and yellow and red pink were used to harmonize with golden yellow clothes. As an application of shapes of foliage in I transformed its size and form to be consistent with a jacket and a tube top. To accord with golden beige costume, I made a curve, showing up in Klimt's paintings, with golden color on a circle shape which was also a main motif in his paintings.
Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
/
v.21
no.2
/
pp.46-53
/
2007
Extension of the mobile communication and the rapidly developing services connected with wireless multimedia(W-CDMA, DMB, Wibro, and so on) need great many base station transceiver systems, antennas, and many signal transmission line to embody these services. The min communication appliances system is exposed always in danger of transient overvoltage by direct stroke or induced lightning surge flowing in through antenna because the antenna of base station transceiver system or relay equipment is combined with expensive communication network equipments through signal transmission line. Now, gas discharge tube(GDT) or narrow band stub arrestor which is used by the surge protector for communication use is exposing limitations as for lightning surge protective means of the communication facility with high speed and wide frequency band. Therefore, for improving performance of surge arrestor, we applied ceramic filter which can reduce lightning surge invading from antenna effectively, and proved that ceramic filter is effective in residual voltage reduction through the experimental research.
Journal of the Korean Institute of Illuminating and Electrical Installation Engineers
/
v.16
no.6
/
pp.130-136
/
2002
A novel ozonizer has been developed using a high frequency surface discharge and a high purity Ti-Si-Al ceramic catalyst as its dielectric component. A cylindrical thin compound ceramic catalyst in reactor is adhered to inside of the film-like outside electrode. And, when experiment condition are oxygen gas temperature of 20 [$^{\circ}C$], inner reactor pressure of 1.6 atm 600[Hz] and flow late of 2[l/min]. the ozonizer can easily produce ozone concentration(50~60[g/㎥]for oxygen) and power efficiency(180[g/kWh]for oxygen) without using a special enrichment means. At 2[l/min], 20[$^{\circ}C$], 1.6[atm], 600[Hz]and 40[W], the result of simulation to gas temperature of reactor using general code Phoenics, the maximum temperature of reactor was 132[$^{\circ}C$]in reactor. Ant the result electric field simulation of Ti-Si-Al type reactor using general code Flux 2D, maximum electric field was 0.131E.08[V/m].
Statement of problem : Although zirconium oxide ceramics are more and more commonly used in restorative dentistry, for many clinical applications only limited data can be found in the literature. However it is quite clear that hydrofluoric acid etching is impossible with zirconia ceramics. Therefore, other bonding techniques are required in order to lute these materials adhesively. Purpose : The purpose or this study was to evaluate the effects of surface treatments on shear bond strengths between two resin cements and a zirconia ceramic. Materials and methods : Experimental industrially manufactured yttrium-oxide-partially-stabilized zirconia ceramic discs (Adens, Korea) were used for this study. The ceramic specimens divided into five experimental groups and a control group (as received). Five surface treatments were studied 1) sandblasting with 110$\mu$m $Al_2O_3$ at 3 bars pressure 13 seconds at a distance of 10 mm, 2) flame-treated with the Silano-Pen for 5 $s/cm^3$, 3) grinding with a diamond bur. 4) sandblasting + Silano-Pen treatment, 5) diamond bur preparation + Silano-Pen treatment. Acrylic plastic tube (5 mm in height and 3 mm in diameter) were filled with composite to fabricate composite cylinders The composite cylinders were bonded to the ceramic specimens with either Superbond C&B or Panavia F resin luting agents. All cemented specimens were tested under shear loading until fracture on universal testing machine at a crosshead speed 1mm/min; the maximum load at fracture was recorded. Sheat bond strength data were analyzed with oneway analysis of variance and Tukey HSD tests (P<.05). Treated ceramic surfaces and fracture surfaces after shear testing were examined morphologically using scanning electron microscope. Results: Ceramic surface treatment with Silano-Pen after sandblasting improved the bond strength of Superbond C&B resin cement. Supevbond C& B resin cement at Silano-Pen aiker sandblasting($27.4{\pm}3.8MPa$) showed statistically higher shear bond strength than the others. Conclusion: Within the limitation of this study, Superbond C& &B resin cement are suitable for cementation of zirconia ceramics and flame-treated with the Silano-Pen after sandblasting is required to enhance the bond strength.
Kim, Kyoung-Bum;Jang, Yong-Ho;Kim, Chang-Il;Jeong, Young-Hun;Lee, Young-Jin;Jo, Jeong-Ho;Paik, Jong-Hoo;Nahm, Sahn
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.24
no.10
/
pp.839-843
/
2011
ZnO nanostructures were developed on a Si (100) substrate from powder mixture of ZnO and 5 mol% Pd (ZP-5) as reactants by ${\times}$ sccm oxygen pressures(x= 0, 10, 20, 40). DTA (differential thermal analysis) result shows the Pd(5 mol%)+ZnO mixtured powder(PZ-5) is easily evaporated than pure ZnO powder. The PZ-5 mixtured powder was characterized by DTA to determine the thermal decomposition which was found to be at $800^{\circ}C$, $1,100^{\circ}C$. Weight loss(%) and ICP (inductively coupled plasma) analysis reveal that Zn vaporization is decreased by increased oxygen pressures from the PZ-5 at $1,100^{\circ}C$ for 30 mins. Needle-like ZnO nanostructures array developed from 10 sccm oxygen pressure, was well aligned vertically on the Si substrate at $1,100^{\circ}C$ for 30 mins. The lengths of the Needle-like ZnO nanostructures is about 2 ${\mu}m$ with diameters of about 65 nm. The developed ZnO nanostructures exhibited growth direction along [001] with defect-free high crystallinity. It is considered that Zn vaporization is responsible for the growth of Needle-like ZnO nanostructures by controlling the oxygen pressures. The photoluminescence spectra of ZnO nanostructures exhibited stronger 376.7 nm NBE (near band-edge emission) peak and 529.3 nm DLE (deep level energy) peak.
As a material for SFCL(Superconducting Fault Current Limiter), BSCCO tube with metal stabilizer is a promising candidate, assuring the stability and large power capacity, For the application, the proper soldering technique, which overcome the difficulties of the joining between BSCCO and metal stabilizer, is required. In this study, after soldering In-Bi solder and In-Sn solder with BSCCO superconductor, welding properties between BSCCO and solders were investigated. Because ceramic materials is difficult to weld, Ag electro-plating on BSCCO 2212 is used for intermetallic layer. To find out the best welding condition for superconductor, soldering is tested in the maximum temperature from $155^{\circ}C\;to\;165^{\circ}C$ in the reflow oven. By investigating the composition and thickness of IMC (lntermetallic Compound) created in the reaction of Ag with solder, we analyzed the welding properties of High-Tc superconductor from a micro point of view.
Proceedings of the Korea Society for Energy Engineering kosee Conference
/
2004.05a
/
pp.171-176
/
2004
Heat regenerator attached in small-scale regenerative radiant tube burner was designed using the theoretical computation code and was confirmed the performance of waste heat recovery ratio. From the computation, when ceramic ball of 4-5kg was used, temperature efficiency and available waste heat recovery ratio were predicted 80% and 70%, respectively. Similar efficiencies were obtained from the experiments using LPG. However, since exhaust gas temperature entered into regenerator was below 85$0^{\circ}C$ which was much lower than that we expected, preheat air temperature was lowered below 80$0^{\circ}C$.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.