• 제목/요약/키워드: Cellulose Paper

검색결과 429건 처리시간 0.021초

알칼리 공용매 팽윤처리 시 알칼리 농도가 SwBKP 섬유 특성에 미치는 영향 (Effects of Alkali Concentration on Fiber Characteristics of SwBKP during Alkali Treatment in Cosolvent System)

  • 서지혜;최경화;조병욱
    • 펄프종이기술
    • /
    • 제48권3호
    • /
    • pp.37-43
    • /
    • 2016
  • Various mechanical and chemical pretreatment methods including alkali treatment, pre-beating, enzyme treatment and oxidation treatment have been used to reduce the production energy of the microfibrillated cellulose (MFC). Among them, alkali swelling can be helpful to reduce the energy consumption because the internal bonding between fibrils could be weakened. In this study, dimethyl sulfoxide (DMSO) was used as a cosolvent to improve alkali pretreatment efficiency and the effects of NaOH concentration during NaOH-DMSO swelling on changes in fiber characteristics of softwood bleached kraft pulp (SwBKP) were elucidated. For alkali treatment in H2O-DMSO solvents, fiber length were decreased with increasing NaOH concentration while fiber width, curl and WRV were increased. WRV began to increase at 8% NaOH solution. In addition, above 8% concentration of NaOH, crystalline structure of pulp fibers converted from cellulose II to cellulose III by DMSO cosolvent. Comparing the previous results with this study, it was shown that DMSO cosolvent could promote swelling of pulp fibers and thus reduce NaOH concentration for the maximum swelling of fibers.

초본류 3가지 암모니아수 침지 처리에서 바이오매스 성분(자이란과 리그닌) 용출 정도와 효소당화의 관계 (Relationship between biomass components dissolution (xylan and lignin) and enzymatic saccharification of several ammonium hydroxide soaked biomasses)

  • 신수정;한심희;조남석;박종문
    • 펄프종이기술
    • /
    • 제42권1호
    • /
    • pp.35-40
    • /
    • 2010
  • Corn stover, hemp woody core and tobacco stalk were treated by dilute ammonium hydroxide soaking for improving the enzymatic saccharification of cellulose and xylan to monosaccharides by commercial cellulase mixtures. As more lignin removal by dilute ammonium hydroxide impregnation led to more enzymatic saccaharification of cellulose and xylan to monosaccharides (corn stover vs tobacco stalk). There was no relationship between xylan removal by dilute ammonium hydroxide impregnation and enzymatic saccharification of polysaccharides in pretreated samples. Except corn stover, lower temperature and longer treatment ($50^{\circ}C$-6 day) was less lignin removal than higher temperature and shorter treatment ($90^{\circ}C$ 16 h). Corn stover showed the highest enzymatic saccharification of cellulose and xylan but tobacco stalk showed the lowest.

고지재생연구(제 7보)-지료조성이 효소활성에 미치는 영향- (Recycling of Wastepaper(Ⅶ)-The Effect of Stock Composition on Enzyme Activity-)

  • 여성국;류정용;신종호;송봉근;오세균
    • 펄프종이기술
    • /
    • 제31권3호
    • /
    • pp.1-9
    • /
    • 1999
  • Effect of furnish on enzyme activity was investigated by using the three components (cellulose, enzyme, and cationic polyelectrolyte) model papermaking system. Avicel was used as a cellulose model compound to observe the effect of adsorption and desorption of enzyme with other component and the resultant change of particle size. As an experimental result, the enzyme loses considerably its apparent activity due to the adsorption onto cellulose and cationic polyelectrolyte. Activities of enzyme applied to the actual papermaking stocks having controlled fiber length showed different behavior in terms of pulp species UKP and KOCC stocks. That is, the enzyme activity in UKP was increased as fines content increased, however, vice versa in KOCC stock . This result can be considered to be the existence of various contaminants included in the fines of KOCC . The effect of possible contaminants such as inorganic materials, calcium ion, surfactant, and conductivity on enzyme activity were also investigated.

  • PDF

오일 팜 수간 유래 CNF (cellulose nanofibrils)의 화장품 보습제 적용을 위한 보습력 평가 (Evaluation of water holding property for applying a cosmetic moisturizer from oil palm trunk CNF)

  • 송우용;신수정
    • 펄프종이기술
    • /
    • 제48권2호
    • /
    • pp.91-98
    • /
    • 2016
  • Cellulose nanofibrils (CNF) was made from oil palm trunk (OPT) with soda-anthraquinone pulping, chlorine dioxide bleaching, carboxymethylation, followed by mechanical grinding. Size of this CNF was 16-40 nm of width confirmed by TEM. To evaluate CNF from OPT as cosmetics raw materials for moisturizing component, water holding properties was compared with hyaluronic acid and collagen. CNF from OPT had better water holding property than collagen or hyaluronic acid whether phenoxyethanol was added as antiseptic or without additive.

전자빔으로 처리한 폐면의 버섯배지효과 (Utilization of Electron Beam-Radiated Cotton Waste for Agaric Mushroom Cultivation Bed)

  • 손효정;정선영;이종신;서영범
    • 펄프종이기술
    • /
    • 제41권3호
    • /
    • pp.71-75
    • /
    • 2009
  • Cotton waste is usually used for cultivating agaric mushroom after outdoor fermentation for a few months. Electron beam was used to break down the polymer chaims of cotton waste for increasing low molecular weight soluble sugars, which may enhance the agaric mushroom cultivation. By increasing electron beam radiation, alpha cellulose content of the cotton waste was decreased while beta cellulose content and hot water solubles were increased. Electron beam radiation over 240 kGy on cotton waste caused significant increase of mushroom yield without lowering mushroom quality.

각종 셀룰로오스 나노섬유의 첨가가 닥나무 인피섬유 시트의 특성에 미치는 영향 (Effect of The Addition of Various Cellulose Nanofibers on The Properties of Sheet of Paper Mulberry Bast Fiber)

  • 한송이;박찬우;김보연;이승환
    • Journal of the Korean Wood Science and Technology
    • /
    • 제43권6호
    • /
    • pp.730-739
    • /
    • 2015
  • 본 연구는 셀룰로오스 나노섬유를 닥나무 인피섬유 시트의 제조시 첨가하여, 닥나무 인피섬유 시트의 특성에 미치는 영향을 조사하였다. 형태학적 및 화학적 성질이 다른 5종류의 셀룰로오스 나노섬유, 즉 리그노셀룰로오스 나노섬유 (lignocellulose nanofiber, LCNF), 홀로셀룰로오스 나노섬유(holocellulose nanofiber, HCNF), 알칼리처리 홀로셀룰로오스 나노섬유(alkali-treated HCNF, AT-HCNF), TEMPO-산화 나노섬유(TEMPO-oxidated nanofiber, TEMPO-NF), 셀룰로오스 나노크리스탈(cellulose nanocrystal, CNC)을 제조하였으며, 각 나노섬유의 종류 및 첨가량이 닥나무 인피섬유시트 제조시의 여수시간 및 시트의 투기도, 평활도, 인장강도 특성에 미치는 영향을 조사하였다. 여수시간은 모든 나노섬유에 있어서 첨가량이 증가함으로서 길어졌으며, 5%의 첨가량에서 HCNF가 가장 여수시간이 길었다. 또한, 셀룰로오스 나노섬유 첨가량이 증가할수록 시트의 평활도, 인장강도 특성이 향상되었으며, 특히 0.1%의 극히 적은양의 나노섬유 첨가로도 비인장강도 및 탄성계수가 크게 향상되는 것을 알 수 있었다. 이러한 특성 향상은 닥나무 인피섬유 간에 교차적으로 적층되어 있는 셀룰로오스 나노섬유의 충전 효과에 기인하는 것을 전자현미경 사진을 통해 확인할 수 있었다.

REACTION OF PAPER PULP AND ALKYL KETENE DIMER BY AGING TREATMENT DURING PAPERMAKIN PROCESS

  • Shin, Young-Doo;Seo, Won-Sung;Cho, Nam-Seok
    • 한국펄프종이공학회:학술대회논문집
    • /
    • 한국펄프종이공학회 2000년도 추계학술발표논문집
    • /
    • pp.83-83
    • /
    • 2000
  • Alkylketene dimer was known as a cellulose reactive or alkaline size because it does not require to fix to the fiber as do the traditional rosin sizes. A proposed sizing mechanism of AKD was the formation of P -ketoester bond between AKD and cellulose which provides the permanent attachment and the orientation of the hydrophobic alkylchains outward. However, some questions about the reaction had arisen and thus, the sizing mechanism of AKD has been a subject of controversy for several decades. The major concern of the controversy is that AKD is really reactive with cellulose or not in the papermaking conditions. In this study, reaction between AKD and pulp fiber was investigated, in order to find out whether AKD forms P-ketoester with pulp fiber during aging under no catalyzed neutral condition with obvious spectroscopic evidence. In addition, effect of aging treatment on the sizing development was studied. It has been disclosed that, in absence of water, AKD reacted with cellulose to form P -ketoester linkage under no catalyzed neutral condition, while, in presence of water, most of AKD was hydrolyzed to a dialkyl ketone or P -ketoacid. In addition, during the aging treatment of AKD-sized paper, its typical IR spectra bands gradually were reduced, completely disappeared after 6hr aging, and formed new absorption bands at 1707cm-' and shoulder peak at 1700cm-' which refer to the typical dialkylketone absorption bands. Therefore, the formation of P -ketoester between AKD and pulp fiber is impossible in the practical papermaking process. It could be suggested that the sizing development of AKD-sized paper is obtained by next two mechanism: 1) formation of a thin-layer of AKD on the fiber surface through melting and spreading of AKD emulsion particles by heat and 2) the hydrolysis of AKD to dialkyl ketone which has higher melting point, during drying and storage of AKD sized papers.

  • PDF

셀롤로오즈 흡음재의 음향적 특성 평가 (Evaluations of the Acoustics Characteristics of Cellulose Absorbers)

  • 연준오;김경우;양관섭
    • 한국소음진동공학회:학술대회논문집
    • /
    • 한국소음진동공학회 2013년도 춘계학술대회 논문집
    • /
    • pp.760-765
    • /
    • 2013
  • Eco-friendly material applied to building would be one of the materials which is must developed for global environmental conservation and reduction of carbon dioxide. For development of eco-friendly material, a cellulose sound-absorbing material has been developed with waste paper through adjustment of various mix proportions. The developed cellulose sound-absorbing material has been tested for its acoustic properties such as acoustic absorptivity and dynamic elastic modulus. The absorptivity was evaluated by developing six samples and using impedance tube and reverberation chamber. As a result of the evaluation, 0.64(NRC) was secured in absorptivity and $4.7MN/m^3$ was indicated in dynamic elastic modulus. Also, for practical use of developed sound-absorbing material as inner heartwood in drywall, comparison test of sound reduction index was performed with existing glass wool sound-absorbing material and constructed drywall of gybsum board. The results have shown 55dB(Rw) of sound reduction index in glass-wool wall and 46dB(Rw) in cellulose.

  • PDF

셀룰로오즈 흡음재의 음향적 특성 평가 (Evaluations of the Acoustics Characteristics of Cellulose Absorbers)

  • 연준오;김경우;양관섭
    • 한국소음진동공학회논문집
    • /
    • 제23권5호
    • /
    • pp.456-462
    • /
    • 2013
  • Eco-friendly material applied to building would be one of the materials which is must developed for global environmental conservation and reduction of carbon dioxide. For development of eco-friendly material, a cellulose absorber has been developed with waste paper through adjustment of various mix proportions. The developed cellulose absorber has been tested for its acoustic properties such as absorption coefficient and dynamic stiffness. The absorption coefficient was evaluated by developing six samples and using impedance tube and reverberation chamber. As a result of the evaluation, 0.64(NRC) was secured in absorption coefficient and 4.7 $MN/m^3$ was indicated in dynamic stiffness. Also, for practical use of developed absorbers as inner heartwood in drywall, comparison test of sound reduction index was performed with existing glass wool absorbers and constructed drywall of gypsum board. The results have shown 55 dB(Rw) of sound reduction index in glass-wool wall and 46 dB(Rw) in cellulose.

Catalytic Conversion of Cellulose to Cellulose Acetate Propionate (CAP) Over SO42-/ZrO2 Solid Acid Catalyst

  • Leng, Yixin;Zhang, Yun;Huang, Chunxiang;Liu, Xiaocheng;Wu, Yuzhen
    • Bulletin of the Korean Chemical Society
    • /
    • 제34권4호
    • /
    • pp.1160-1164
    • /
    • 2013
  • The solid super acid catalyst $SO{_4}^{2-}$/$ZrO_2$ was prepared by impregnation method using $ZrO_2$ as the catalyst support. Catalyst forming was taken into consideration in order to separate catalyst from the mixture of cellulose acetate propionate (CAP). $Al_2O_3$ and sesbania gum powder were selected as binding agent and auxiliary agent respectively. The catalytic properties were evaluated through esterification of cellulose with acetic anhydride, propionic anhydride and characterized by XRD, FTIR and $NH_3$-TPD. In this paper, the effects of concentration of $H_2SO_4$ impregnated, calcination temperature, esterification temperature and esterification time on the yield, acyl content and viscosity of CAP were investigated. The results showed that $SO{_4}^{2-}/ZrO_2$ successfully catalyzed CAP synthesis over catalysts impregnated in 0.75 mol/L $H_2SO_4$ and calcined at $500^{\circ}C$. The yield, acetyl content and propionyl content of CAP reached the maximum value of 105.3%, 29.9% and 25.8% reacted at $50^{\circ}C$ for 8 h.