• 제목/요약/키워드: CVD(chemical vapor deposition)

검색결과 722건 처리시간 0.027초

열선 CVD법에 의한 다결정 실리콘 박막증착 및 특성분석 (Poly-Si Thin Films by Hot-wire Chemical Vapor Deposition Method)

  • 정연식;이정철;김석기;윤경훈;송진수;박이준;권성원;임굉수
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 하계학술대회 논문집 Vol.4 No.2
    • /
    • pp.1030-1033
    • /
    • 2003
  • This paper presents the deposition characterization of polycrystalline silicon films by the HWCVD(Hot-wire Chemical Vapor Deposition) method at low substrate($300^{\circ}C$). The filament temperature, pressure and $SiH_4$ concentration were determined to be a critical parameter for the deposition of poly-Si films. Series A was deposited under the conditions of $1380^{\circ}C$(Tf), 100 mTorr and $2{\sim}10%\{SiH_4/(SiH_4+H_2)\}$ for 60 min. Series B was deposited under the conditions of $1400{\sim}1450^{\circ}C$ (Tf), 30 mTorr and $2{\sim}12%$ for 60 min. The physical characteristics were measured by Raman and FTIR spectroscopy, dark and photoconductivity measurements under AM1.5 illumination.

  • PDF

Multiple-inputs Dual-outputs Process Characterization and Optimization of HDP-CVD SiO2 Deposition

  • Hong, Sang-Jeen;Hwang, Jong-Ha;Chun, Sang-Hyun;Han, Seung-Soo
    • JSTS:Journal of Semiconductor Technology and Science
    • /
    • 제11권3호
    • /
    • pp.135-145
    • /
    • 2011
  • Accurate process characterization and optimization are the first step for a successful advanced process control (APC), and they should be followed by continuous monitoring and control in order to run manufacturing processes most efficiently. In this paper, process characterization and recipe optimization methods with multiple outputs are presented in high density plasma-chemical vapor deposition (HDP-CVD) silicon dioxide deposition process. Five controllable process variables of Top $SiH_4$, Bottom $SiH_4$, $O_2$, Top RF Power, and Bottom RF Power, and two responses of interest, such as deposition rate and uniformity, are simultaneously considered employing both statistical response surface methodology (RSM) and neural networks (NNs) based genetic algorithm (GA). Statistically, two phases of experimental design was performed, and the established statistical models were optimized using performance index (PI). Artificial intelligently, NN process model with two outputs were established, and recipe synthesis was performed employing GA. Statistical RSM offers minimum numbers of experiment to build regression models and response surface models, but the analysis of the data need to satisfy underlying assumption and statistical data analysis capability. NN based-GA does not require any underlying assumption for data modeling; however, the selection of the input data for the model establishment is important for accurate model construction. Both statistical and artificial intelligent methods suggest competitive characterization and optimization results in HDP-CVD $SiO_2$ deposition process, and the NN based-GA method showed 26% uniformity improvement with 36% less $SiH_4$ gas usage yielding 20.8 ${\AA}/sec$ deposition rate.

화학기상증착법을 이용하여 합성한 그래핀과 금속의 접촉저항 특성 연구 (A Study on Contact Resistance Properties of Metal/CVD Graphene)

  • 김동영;정하늘;이상현
    • 마이크로전자및패키징학회지
    • /
    • 제30권2호
    • /
    • pp.60-64
    • /
    • 2023
  • 본 연구에서는 그래핀 기반 소자의 성능에 영향을 미치는 그래핀과 금속 사이의 전기적 접촉저항 특성을 비교 분석하였다. 화학기상증착법을 이용하여 고품질의 그래핀을 합성하였으며, 전극 물질로 Al, Cu, Ni 및 Ti를 동일한 두께로 그래핀 표면 위에 증착하였다. TLM (transfer length method) 방법을 통해 SiO2/Si 기판에 전사된 그래핀과 금속의 접촉저항을 측정한 결과, Al, Cu, Ni, Ti의 평균 접촉저항은 각각 345 Ω, 553 Ω, 110 Ω, 174 Ω으로 측정되었다. 그래핀과 물리적 흡착 특성을 갖는 Al와 Cu에 비해 화학적 결합을 형성하는 Ni과 Ti의 경우, 상대적으로 더 낮은 접촉저항을 갖는 것을 확인하였다. 본 연구의 그래핀과 금속의 전기적 특성에 대한 연구 결과는 전극과의 낮은 접촉저항 형성을 통해 고성능 그래핀 기반 전자, 광전자소자 및 센서 등의 구현에 기여할 수 있을 것으로 기대한다.

CVD법에 의해 제작된 광촉매 TiO2 〈112〉 우선배향의 특성 (The Characteristics of 〈112〉-preferred Orientation for Photocatalytic TiO2 Fabricated by CVD)

  • 강경태;진정근;강필규;노대호;변동진
    • 한국재료학회지
    • /
    • 제13권7호
    • /
    • pp.436-441
    • /
    • 2003
  • The characteristics of <112> orientation were studied for the $TiO_2$thin films, which were prepared on the glass by CVD (chemical vapor deposition) at various substrate temperatures. It was confirmed that $TiO_2$ films exhibited <112>-preferred orientation in a specific temperature range. Although $TiO_2$polycrystalline film grown deposited at relatively low temperature showed the growth of random directions, the <112>-preferred orientation was gradually developed with increasing deposition temperature. According to exhibit higher degree of <112>-preferred orientation, $TiO_2$thin film showed porous surface morphology, well-developed columnar structure, and deeper voids resulted from non-aggregation of columns were observed. In addition, transmittance was enhanced. Therefore, the growth of $TiO_2$with <112>-preferred orientation is suitable for glass coating because of predominance of photocatalytic efficiency and transmittance.

Flowable oxide CVD Process for Shallow Trench Isolation in Silicon Semiconductor

  • Chung, Sung-Woong;Ahn, Sang-Tae;Sohn, Hyun-Chul;Lee, Sang-Don
    • JSTS:Journal of Semiconductor Technology and Science
    • /
    • 제4권1호
    • /
    • pp.45-51
    • /
    • 2004
  • We have proposed a new shallow trench isolation (STI) process using flowable oxide (F-oxide) chemical vapor deposition (CVD) for DRAM application and it was successfully developed. The combination of F-oxide CVD and HDP CVD is thought to be the superior STI gap-filling process for next generation DRAM fabrication because F-oxide not only improves STI gap-filling capability, but also the reduced local stress by F-oxide in narrow trenches leads to decrease in junction leakage and gate induced drain leakage (GIDL) current. Finally, this process increased data retention time of DRAM compared to HDP STI. However, a serious failure occurred by symphonizing its structural dependency of deposited thickness with poor resistance against HF chemicals. It could be suppressed by reducing the flow time during F-oxide deposition. It was investigated collectively in terms of device yield. In conclusion, the combination of F-oxide and HDP oxide is the very promising technology for STI gap filling process of sub-100nm DRAM technology.

유리 기판에 Catalytic CVD 저온공정으로 제조된 나노급 니켈실리사이드와 결정질 실리콘 (Nano-thick Nickel Silicide and Polycrystalline Silicon on Glass Substrate with Low Temperature Catalytic CVD)

  • 송오성;김건일;최용윤
    • 대한금속재료학회지
    • /
    • 제48권7호
    • /
    • pp.660-666
    • /
    • 2010
  • 30 nm thick Ni layers were deposited on a glass substrate by e-beam evaporation. Subsequently, 30 nm or 60 nm ${\alpha}-Si:H$ layers were grown at low temperatures ($<220^{\circ}C$) on the 30 nm Ni/Glass substrate by catalytic CVD (chemical vapor deposition). The sheet resistance, phase, microstructure, depth profile and surface roughness of the $\alpha-Si:H$ layers were examined using a four-point probe, HRXRD (high resolution Xray diffraction), Raman Spectroscopy, FE-SEM (field emission-scanning electron microscopy), TEM (transmission electron microscope) and AES depth profiler. The Ni layers reacted with Si to form NiSi layers with a low sheet resistance of $10{\Omega}/{\Box}$. The crystallinty of the $\alpha-Si:H$ layers on NiSi was up to 60% according to Raman spectroscopy. These results show that both nano-scale NiSi layers and crystalline Si layers can be formed simultaneously on a Ni deposited glass substrate using the proposed low temperature catalytic CVD process.

Atomic layer deposition of In-Sb-Te Thin Films for PRAM Application

  • Lee, Eui-Bok;Ju, Byeong-Kwon;Kim, Yong-Tae
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2011년도 제40회 동계학술대회 초록집
    • /
    • pp.132-132
    • /
    • 2011
  • For the programming volume of PRAM, Ge2Sb2Te5(GST) thin films have been dominantly used and prepared by physical vapor deposition (PVD), chemical vapor deposition (CVD), atomic layer deposition (ALD). Among these methods, ALD is particularly considered as the most promising technique for the integration of PRAM because the ALD offers a superior conformality to PVD and CVD methods and a digital thickness control precisely to the atomic level since the film is deposited one atomic layer at a time. Meanwhile, although the IST has been already known as an optical data storage material, recently, it is known that the IST benefits multistate switching behavior, meaning that the IST-PRAM can be used for mutli-level coding, which is quite different and unique performance compared with the GST-PRAM. Therefore, it is necessary to investigate a possibility of the IST materials for the application of PRAM. So far there are many attempts to deposit the IST with MOCVD and PVD. However, it has not been reported that the IST can be deposited with the ALD method since the ALD reaction mechanism of metal organic precursors and the deposition parameters related with the ALD window are rarely known. Therefore, the main aim of this work is to demonstrate the ALD process for IST films with various precursors and the conformal filling of a nano size programming volume structure with the ALD?IST film for the integration. InSbTe (IST) thin films were deposited by ALD method with different precursors and deposition parameters and demonstrated conformal filling of the nano size programmable volume of cell structure for the integration of phase change random access memory (PRAM). The deposition rate and incubation time are 1.98 A/cycle and 25 cycle, respectively. The complete filling of nano size volume will be useful to fabricate the bottom contact type PRAM.

  • PDF

B2O3-P2O5-SiO2 계 박막유리의 화학증착 및 물성에 관한 연구 (A Study on the Chemical Vapor Deposition of BPSG and its Thin Film Properties)

  • 김은산;양두영;김동원;김우식;최민성
    • 한국세라믹학회지
    • /
    • 제28권7호
    • /
    • pp.517-524
    • /
    • 1991
  • The CVD process of BPSG (BoroPhosphoSilicate Glass) and its thin film properties were studied. B2H6, PH3, SiH4 and O2 gases were reacted in a AP (Atmospheric Pressure) CVD system in the temperature range of 300℃ and 460℃. The interaction of B2H6 and PH3 was studied from the deposition rate and dopant incorporation change point of view. The dependency of BPSG step coverage on the temperature was changed with different O2/(B2H6+PH3+SiH4) ratio. Finally, the boundary which distinguishes the stable BPSG's from the ones that react with Di (Deionized) water or cleaning chemicals such as H2SO4, HCl, H2O2, NH4OH etc could be defined.

  • PDF

고주파플라즈마 CVD법에 의한 다이아몬드상 탄소박막의 합성 (Synthesis of Diamond-Like Carbon Films by R.F.Plasma CVD)

  • 박상현;이덕출
    • 대한전기학회논문지
    • /
    • 제39권10호
    • /
    • pp.1037-1043
    • /
    • 1990
  • Diamond thin films were synthesized from the mixed gases of methane and hydrogen on silicon substrates by RF plasma chemical vapor deposition and deposited films were investigated by SEM, X-ray diffractometry and Raman spectroscopy. It is found that high quality diamond-like carbon films were successfully synthesized by PECVD under the deposition condition of 1-10 vol% of methane concentration, 0.15-0.4torr of reactor pressure, 500W of RF power, and 5-20hr of reaction time. Especially, cubo-octahedral diamond-like carbon particles were synthesized by employing 1.0 vol % of methane concentration and 0.4torr of the reactor pressure.

  • PDF

HCl분위기에서 증기열처리된 BPSG 막의 평탄화효과에 관한 연구 (Planarization Effect of Steam Densified BPSG Film in HCl Atmosphere)

  • 김동현
    • 한국세라믹학회지
    • /
    • 제23권4호
    • /
    • pp.55-61
    • /
    • 1986
  • Phosphosilicate glass(PSG) films have been used as fusable deposited dielectrics in silicon gate MOS integrated circuits. But in this experiment BPSG(borophosphosilicate glass) will be optimized for more efficient utilization of the reactants. The BPSG films were deposited on silicon wafers by the oxidation of the hydrides at 430$^{\circ}$C in conventional atmospheric-pressure chemical-vapor-deposition (CVD) systems. Physical and chemical properties of CVD BPSG films have been characterized both for as-deposited and for fused films The. relationship between deposited BPSG film composition and infra-red absorption solution etch rate and fusion temperature is discussed and examples of BPSG composition that can be fused at 900~95$0^{\circ}C$ and 800~85$0^{\circ}C$ are given. In addition to having lower fusion temperature than PSG films BPSG films have lower as-deposited intrinsic tensile stress and low aqueous chemical etch rate they have been considered for applications where these characteristics are advantageous.

  • PDF