Laser bonding using liquid glass (유리액를 이용한 레이저 선택 접합)

  • Kim, Joo-Han;Lee, Jae-Hoon;Kim, Hyang-Tae
    • Laser Solutions
    • /
    • v.11 no.3
    • /
    • pp.1-4
    • /
    • 2008
  • A selective laser micro bonding process using liquid glass (methylsilsesquioxane) was developed and the results are analysed. The liquid glass can be solidified with Nd:YAG laser irradiation and it can be applied for joining two glass substrates. A bonding thickness of a few micrometers can be achieved. The appropriate laser power density (or this process is around 40-60 $kW/cm^2$ and its bonding force is 1000-1200 $gf/mm^2$. This process can be applied for bonding micro devices such as micro bio-sensors or display products. Its advantages and limitations are presented and discussed.

  • PDF

Melting induced diffusion bonding of Rene 80 superalloys using boron doping method (Ren380 超合金의 보론 塗布法을 이용한 液化誘導擴散接合法의 硏究)

  • 정재필;강춘식;이보영
    • Journal of Welding and Joining
    • /
    • v.9 no.3
    • /
    • pp.26-33
    • /
    • 1991
  • As it takes very long time for the Transient Liquid Phase(TLP) bonding, we tried to reduce the bonding time by changing insert material for the high diffusivity element. On this study boron powder was doped as a insert material on the bonding surface of Rene 80 superalloy, and diffusion treated at 1150.deg.C under vacuum. On this method differently from the TLP bonding the insert material was not melted during bonding but only the base metal reacted with the boron was inducedly melted. Therefore, as this bonding mechanism is different from the existing ones, it is suggested as a Melting Induced Diffusion Bonding. When this process was used for the diffusion bonding, the bonding time including homogenization decreased greatly compared to the conventional TLP bonding.

  • PDF

Thermo-ompression Process for High Power LEDs (High Power LED 열압착 공정 특성 연구)

  • Han, Jun-Mo;Seo, In-Jae;Ahn, Yoomin;Ko, Youn-Sung;Kim, Tae-Heon
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.23 no.4
    • /
    • pp.355-360
    • /
    • 2014
  • Recently, the use of LED is increasing. This paper presents the new package process of thermal compression bonding using metal layered LED chip for the high power LED device. Effective thermal dissipation, which is required in the high power LED device, is achieved by eutectic/flip chip bonding method using metal bond layer on a LED chip. In this study, the process condition for the LED eutectic die bonder system is proposed by using the analysis program, and some experimental results are compared with those obtained using a DST (Die Shear Tester) to illustrate the reliability of the proposed process condition. The cause of bonding failures in the proposed process is also investigated experimentally.

Collective laser-assisted bonding process for 3D TSV integration with NCP

  • Braganca, Wagno Alves Junior;Eom, Yong-Sung;Jang, Keon-Soo;Moon, Seok Hwan;Bae, Hyun-Cheol;Choi, Kwang-Seong
    • ETRI Journal
    • /
    • v.41 no.3
    • /
    • pp.396-407
    • /
    • 2019
  • Laser-assisted bonding (LAB) is an advanced technology in which a homogenized laser beam is selectively applied to a chip. Previous researches have demonstrated the feasibility of using a single-tier LAB process for 3D through-silicon via (TSV) integration with nonconductive paste (NCP), where each TSV die is bonded one at a time. A collective LAB process, where several TSV dies can be stacked simultaneously, is developed to improve the productivity while maintaining the reliability of the solder joints. A single-tier LAB process for 3D TSV integration with NCP is introduced for two different values of laser power, namely 100 W and 150 W. For the 100 W case, a maximum of three dies can be collectively stacked, whereas for the 150 W case, a total of six tiers can be simultaneously bonded. For the 100 W case, the intermetallic compound microstructure is a typical Cu-Sn phase system, whereas for the 150 W case, it is asymmetrical owing to a thermogradient across the solder joint. The collective LAB process can be realized through proper design of the bonding parameters such as laser power, time, and number of stacked dies.

Development of MEMS-based Micro Turbomachinery (MEMS-based 마이크로 터보기계의 개발)

  • Park, Kun-Joong;Min, Hong-Seok;Jeon, Byung-Sun;Song, Seung-Jin;Joo, Young-Chang;Min, Kyoung-Doug;You, Seung-Mun
    • Proceedings of the KSME Conference
    • /
    • 2001.06e
    • /
    • pp.169-174
    • /
    • 2001
  • This paper reports on the development of high aspect ratio structure and 3-D integrated process for MEMS-based micro gas turbines. To manufacture high aspect ratio structures, Deep Reactive Ion Etching (DRIE) process have been developed and optimized. Specially, in this study, structures with aspect ratios greater than 10 were fabricated. Also, wafer direct bonding and Infra-Red (IR) camera bonding inspection systems have been developed. Moreover, using glass/silicon wafer direct bonding, we optimized the 3-D integrated process.

  • PDF

Finite Element Analysis of Laser Class Bonding Process (레이저 유리 접합 공정의 유한요소해석)

  • Hong, Seok-Kwan;Kang, Jeong-Jin;Byun, Cheol-Woong
    • Laser Solutions
    • /
    • v.11 no.3
    • /
    • pp.10-15
    • /
    • 2008
  • This study is aimed to analyse the laser glass bonding process numerically. Due to the viscoelastic behaviour of glass, the extremely large deformation of the frit seal is resulted continuously over the transition temperature, so that the thermal boundary condition be changed in the entire calculation process. The commercial FEM algorithm is restrictively able to remesh the large geometrical boundary shape and to adapt the boundary conditions simultaneously. According to our manual adaptation of increasing the laser line intensity to 700 mW/mm, it is possible to estimate the thermal glass bonding process under the fracture stress in principle. But it should be studied further in the case of high laser line intensity.

  • PDF

Effect of Processing Conditions on the Morphological Structure and Strength Properties of Ultrasonically Laminated Nonwovens (초음파 라미네이트 부직포의 형태구조와 강도특성에 처리조건의 영향)

  • Kang, Jeon-Young;Jeon, Woo-Jin;Joo, Chang-Whan
    • Proceedings of the Korean Fiber Society Conference
    • /
    • 2003.04a
    • /
    • pp.146-149
    • /
    • 2003
  • There are three major bonding types such as chemical bonding, thermal bonding, mechanical bonding to produce nonwoven fabrics. The development of the past few years has shown that the share of thermally bonded webs is growing steadily. The viability of the thermal bonding process is rooted in the price advantage obtained by lower energy costs. However, the thermal bonding process also obtains the quality requirements of the market place. (omitted)

  • PDF

Study on the Bonding Property and Strength Evaluation in Bonding Interface Joints of Dissimilar Material using Response Surface Analysis (반응표면법을 이용한 이종재질의 접합 계면부 강도평가 및 접합특성에 관한 연구)

  • Lee, Seung-Hyun;Choi, Seong-Dae;Kim, Gi-Man;Lee, Jong-Hyung
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.8 no.2
    • /
    • pp.76-82
    • /
    • 2009
  • In this papers, Study on the Bonding property and Strength Evaluation in Bonding interface Joints of Dissimilar material using DOE. We found optimal condition that uses experimental design method (Response Surface Analysis, DOE) used temperature, pressure, time on experiment factor. And we could get bonding condition and strength that break and crack do not happen in mechanical processing about united dissimilar material. And progress 3 point bending tests and verified result.

  • PDF

Cold Roll Bonding of (Ag-10% Ni)/Cu Clad Metals ((Ag-10 % Ni)/Cu 접점재의 냉간압연접합)

  • 김종헌;김성일;박상용
    • Transactions of Materials Processing
    • /
    • v.6 no.2
    • /
    • pp.136-144
    • /
    • 1997
  • (Ag-10%Ni)/Cu clad metals for electric contact switch were fabricated by cold-roll bonding process. 2 or 3 passes of cold-rolling was carried out for each process to investigate the effect of the rolling passes on the bonding property. The effect of the annealing temperature of copper before the cold-roll bonding on the bond strength was also studied. The specimen bonded with copper annealed below 30$0^{\circ}C$ before roll bonding showed good bond strength. This is because high stored energy in copper promoted the short range diffusion and the grain refinement of copper by the static recrystallization increased the degree of the interfacial coherency. The maximum peel strength of clad metals bonded with Cu annealed below 30$0^{\circ}C$ was 120N.