Fabrication of long length Bi-2223/Ag HTS tape (Bi-2223/Ag 고온초전도 장선재의 제조)

  • Kim, Sang-Cheol;Lee, Dong-Hoon;Ha, Dong-Woo;Oh, Sang-Soo
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2004.11a
    • /
    • pp.69-72
    • /
    • 2004
  • In order to use HTS tape on electric power applications, such as cable, motor, transformer, fault current limiter, a long length of HTS tape with a good uniformity of critical current is inevitable. The longer length of HTS tape, the wider in the range of application and the lower cost of HTS tape. In this study three long length Bi-2223/Ag tapes(268m, 253m and 187m) were fabricated. Critical current uniformity along the length was greatly improved through the optimization of cold deformation and thermo-mechanical process. Average critical current of the tapes was 63.2 A, 54.6 A and 64.2 A, respectively Critical tensile strength and critical bending radius (77 K, 5 % Ic degradation) was 135 MPa and 56 m, respectively.

  • PDF

The effects of moisture content in precursor powder for Bi-2223/Ag tape (Bi-2223/Ag 선재의 전구 분말에서 수분함량에 따른 효과)

  • 김성환;유재무;고재웅;김영국;김철진
    • Progress in Superconductivity
    • /
    • v.4 no.2
    • /
    • pp.162-167
    • /
    • 2003
  • The critical current value of Bi-2223/Ag tape can be influenced by various factors. In particular, it was known that properties of precursor powders could affect the formation of Bi -2223 and grain growth rate of the same. Since, moistures and organic matters can easily contaminate the precursor powders of Bi-2223 tapes and degrade properties of superconductors, the precursor powders should be kept in optimal conditions to minimize contamination. In this study, the effect of moisture and organic matters has been investigated. A Bi-2223/Ag tape contaminated with a large amount of moisture and organic matter has been characterized by low critical current values and bubbling. It has been found that as the quantity of moisture increases, the Bi-2223 phases are formed at lower temperature and the amount of non-superconducting phase increases.

  • PDF

The characterization of Bi-2223/Ag tape fabricated by using the rectangular dies (사각 다이스를 이용한 Bi-2223/Ag 선재의 특성평가)

  • 정재훈;유재무;고재웅;김영국;신평우
    • Progress in Superconductivity
    • /
    • v.4 no.2
    • /
    • pp.168-171
    • /
    • 2003
  • It was known that properties of superconducting tapes could be influenced by mechanical processing method. In this presentation, the effect of drawing method on the final properties of superconductor tape has been systematically studied. Firstly, BSCCO/Ag tapes have been fabricated via two-stage drawing method and conventional rolling process. The two-stage drawing process consists of circular dies drawing and rectangular dies drawing. Important parameters such as fill factor and critical current values of fully processed superconducting tapes have been evaluated to elucidate the effect of drawing method.

  • PDF

Development of km class Bi-2223/Ag HTS tapes (1km급 Bi-2223/Ag 고온초전도 선재 개발 연구)

  • 하동우;오상수;김상철;양주생;황선역;이동훈;최종규;하홍수;권영길
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 2003.10a
    • /
    • pp.63-66
    • /
    • 2003
  • 1 km length of Bi-2223/Ag superconducting wires were fabricated by stacking, drawing process with advanced heat-treatment schedules. Intermediate annealing was carried out to increase the homogeneity and uniformity of the superconducting filaments embedded in the silver matrix. Phase modification from tetragonal to orthorhombic Bi-2212 by pre heat treatment(PHT) was executed to improve the texture and phase transformation of Bi-2223. Drawing stress was measured to Predict the sausaging and stress limit, Rolling parameters such as thickness, width and winding tension were investigated to roll the tape with uniformity. Critical current of 1 km length of superconducting tapes was measured about 50 A continuously after final sintering.

  • PDF

Interlaboratory Comparison of Critical Current Measurements on Ag-sheathed Bi-2223 tapes (Bi-2223선재의 임계전류 측정기술 비교)

  • Lee, Kyu-Won;Han, Gi-Youl
    • Progress in Superconductivity
    • /
    • v.3 no.1
    • /
    • pp.99-103
    • /
    • 2001
  • We have conducted two runs of interlaboratory comparison on Ag-sheathed Bi-2223 tapes to evaluate the level of measurement techniques for the critical current measurement. Two classes of specimens were prepared for parallel and serial routings and sent to four participating laboratories. The critical currents of specimens were measured at 77 K in zero magnetic field. In the first comparison, we used twenty different Bi-2223 tapes as specimens for comparison and participating laboratories measured the specimens using their own instruments and procedures. As a result, the scattering of data on the first comparison showed -3.0% to +l2.2% for the parallel routing and -0.7% to +l5.1% for the serial routing. Major sources of these variations were attributed to different measurement techniques. Thus, the second comparison of measurement was done on the same specimens under specified measurement conditions, particularly in terms of cooling procedure and sweep rate of the test current. The variations for the second comparison were decreased -3.1% to +3.2% far the parallel routing and -1.8% to +7.7% fur the serial routing.

  • PDF

The effect of Ag addition and high-energy ball milling on Bi-2223 tapes (Ag 첨가 및 볼밀링에 의한 Bi-2223/Ag 초전도 선재의 특성변화)

  • 김영순;오상수;류강식;정대영;안중호
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 2000.02a
    • /
    • pp.101-103
    • /
    • 2000
  • In the present work, we have investigated the combined effect of high-energy milling and Agb addition on microstructure and superconducting properties for Bi-2223/Ag. tape. The addition of siver plays an important role in enhancing liquid phase formation, Resulting in densification and cracking during solidification. Further study is needed for the optimization of Ag content and heat-treatment which can reduce the cracking.

  • PDF

A study on Improvement of Critical Current for Bi-2223 HTS Tapes (Bi-2223 고온초전도 선재의 임계전류 향상에 관한 연구)

  • 하홍수;정종만;이남진;장현만;하동우;오상수;권영길;류강식
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 2000.02a
    • /
    • pp.3-5
    • /
    • 2000
  • Among the various processing techniques used in HTS wire fabrication, the PIP(Powder In Tube) method is currently one of the most promising for applications on an industrial scale. In this study, we have fabricated Bi-2223/Ag superconducting tapes using the modified PIT process, where several process factors were changed and improved, ie., powder packing, drawing, rolling and heat treatment. We obtained Bi-2223 tape that have high critical current, 46 a at 77.3 K, have high critical current, 46A at 77.3 K, self field although the tape was not pressed but only rolled. The critical current of 100m class long length tape was measured 21.6A at the same criterion. Besides, the critical current of Bi-2223/Ag tape was measured applying magnetic fields with different directions at various temperatures.