Development of Plasma Assisted ALD equipment and electrical characteristic of TaN thin film deposited PAALD method (Plasma Assisted ALD 장비 계발과 PAALD법으로 증착 된 TaN 박막의 전기적 특성)

  • Do Kwan-Woo;kim Kyoung-Min;Yang Chung-Mo;Park Seong-Guen;Na Kyoung-Il;Lee Jung-Hee;Lee Jong-Hyun
    • Proceedings of the Korean Society Of Semiconductor Equipment Technology
    • /
    • 2005.05a
    • /
    • pp.139-145
    • /
    • 2005
  • In the study, in order to deposit TaN thin film using diffusion barrier and bottom electrode we made the Plasma Assisted ALD equipment and confirmed the electrical characteristic of TaN thin films deposited PAALD method, PAALD equipment depositing TaN thin film using PEMAT(pentakis(ethylmethlyamlno) tantalum) Precursor and $NH_3$ reaction gas is aware that TaN thin film deposited of high density and amorphous phase with XRD measurement The degree of diffusion and react ion taking place in Cu/TaN(deposited using 150 W PAALD)/$SiO_2$/Si systems with increasing annealing temperature was estimated from MOS capacitor property and the $SiO_2(600\;\AA)$/Si system surface analysis by C-V measurement and secondary ion material spectrometer(SIMS) after Cu/TaN/$SiO_2(400\;\AA)$ system etching. TaN thin film deposited PAALD method diffusion barrier have a good diffusion barrier property up to $500^{\circ}C$.

  • PDF

Development of Plasma Assisted ALD equipment and Electrical Characteristic of TaN thin film deposited PAALD method (Plasma Assisted ALD 장비 계발과 PAALD법으로 증착 된 TaN 박막의 전기적 특성)

  • Do Kwan Woo;Kim Kyoung Min;Yang Chung Mo;Park Seong Guen;Na Kyoung Il;Lee Jung Hee;Lee Jong Hyun
    • Journal of the Semiconductor & Display Technology
    • /
    • v.4 no.2 s.11
    • /
    • pp.39-43
    • /
    • 2005
  • In the study, in order to deposit TaN thin film for diffusion barrier and bottom electrode we made the Plasma Assisted ALD equipment and confirmed the electrical characteristics of TaN thin films grown PAALD method. Plasma Assisted ALD equipment depositing TaN thin film using PEMAT(pentakis(ethylmethlyamino) tantalum) precursor and NH3 reaction gas is shown that TaN thin film deposited high density and amorphous phase with XRD measurement. The degree of diffusion and reaction taking place in Cu/TaN (deposited using 150W PAALD)/$SiO_{2}$/Si systems with increasing annealing temperature was estimated for MOS capacitor property and the $SiO_{2}$, (600${\AA}$)/Si system surface analysis by C-V measurement and secondary ion material spectrometer (SIMS) after Cu/TaN/$SiO_{2}$ (400 ${\AA}$) layer etching. TaN thin film deposited PAALD method diffusion barrier have a good diffusion barrier property up to 500$^{\circ}C$.

  • PDF

Improvement in Capacitor Characteristics of Titanium Dioxide Film with Surface Plasma Treatment (플라즈마 표면 처리를 이용한 TiO2 MOS 커패시터의 특성 개선)

  • Shin, Donghyuk;Cho, Hyelim;Park, Seran;Oh, Hoonjung;Ko, Dae-Hong
    • Journal of the Semiconductor & Display Technology
    • /
    • v.18 no.1
    • /
    • pp.32-37
    • /
    • 2019
  • Titanium dioxide ($TiO_2$) is a promising dielectric material in the semiconductor industry for its high dielectric constant. However, for utilization on Si substrate, $TiO_2$ film meets with a difficulty due to the large leakage currents caused by its small conduction band energy offset from Si substrate. In this study, we propose an in-situ plasma oxidation process in plasma-enhanced atomic layer deposition (PE-ALD) system to form an oxide barrier layer which can reduce the leakage currents from Si substrate to $TiO_2$ film. $TiO_2$ film depositions were followed by the plasma oxidation process using tetrakis(dimethylamino)titanium (TDMAT) as a Ti precursor. In our result, $SiO_2$ layer was successfully introduced by the plasma oxidation process and was used as a barrier layer between the Si substrate and $TiO_2$ film. Metal-oxide-semiconductor ($TiN/TiO_2/P-type$ Si substrate) capacitor with plasma oxidation barrier layer showed improved C-V and I-V characteristics compared to that without the plasma oxidation barrier layer.

Enhanced characteristics of TCO films with $(SiO_2)_3(ZnO)_7$ gas barrier layer on various plastic substrates (다양한 플라스틱 기판위에 $(SiO_2)_3(ZnO)_7$ 보호층을 갖는 투명 전도성 박막들의 특성 향상)

  • Kwon, Oh-Jeong;Kim, Dong-Yung;Ryu, Sung-Won;Sohn, Sun-Young;Hong, Woo-Pyo;Kim, Hwa-Min;Hong, Jae-Suk
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.11a
    • /
    • pp.283-284
    • /
    • 2008
  • Electrical and optical characteristics of indium tin oxide (ITO) and indium zinc oxide (IZO) films without and with $(SiO_2)_3(ZnO)_7$ at.% (SZO) film deposited on poly(ethylene naphthalate) (PEN) and poly(ethylene terephthalate (PET) substrates as a gas barrier layer for flexible display were studied. The ITO and IZO films with SZO gas barrier layer showed the improved properties which were both the high transmittance of average 80% in the visible light range and the decreased sheet resistance as compared to those of ITO and IZO films without SZO layer. Particularly, the PEN substrate with only SZO gas barrier layer had a low water vapor transmission rate (WVTR) of $\sim10^{-3}g/m^2$/day. Thus, we suggest that the SZO film with protection ability against the water vapor permeation can be applied to gas barrier layer for flexible display.

  • PDF

Barrier Property and Morphology of Biaxially Oriented PP/EVOH Blend Film (이축연신 PP/EVOH 블렌드 필름의 차단 성질 및 모폴로지)

  • 여종호;이종훈;박찬석;이기준;남재도
    • Polymer(Korea)
    • /
    • v.24 no.6
    • /
    • pp.820-828
    • /
    • 2000
  • In this study, biaxially oriented film process was used to improve barrier property of polypropylene (PP)/ethylene-vinyl alcohol copolymer (EVOH) blends by inducing a laminar morphology of the dispersed phase in the matrix phase. In order to examine the extent of deformation during melt extrusion process, the rheological properties of the resins were measured and the viscosity ratio of the dispersed phase to the continuous phase was determined. The effects of compatibilizer content, draw ratio, and draw temperature on the oxygen permeability and morphology of biaxially drawn blend films were studied. The laminar morphology of the EVOH phase with a larger area of thinner layer induced by biaxial orientation was found to result in a significant increase in oxygen barrier property of PP/EVOH (85/15) blends by about 10 times relative to the pure PP When both PP-g-MAH and ionomer were used as the compatibilizers, there existed an optimum level of compatibilizer content for obtaining improved barrier properties with a well developed laminar structure. In addition, higher draw ratio and draw temperature were found to be more favorable processing conditions in obtaining higher barrier blends.

  • PDF

Low Temperature PECVD for SiOx Thin Film Encapsulation

  • Ahn, Hyung June;Yong, Sang Heon;Kim, Sun Jung;Lee, Changmin;Chae, Heeyeop
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2016.02a
    • /
    • pp.198.1-198.1
    • /
    • 2016
  • Organic light-emitting diode (OLED) displays have promising potential to replace liquid crystal displays (LCDs) due to their advantages of low power consumption, fast response time, broad viewing angle and flexibility. Organic light emitting materials are vulnerable to moisture and oxygen, so inorganic thin films are required for barrier substrates and encapsulations.[1-2]. In this work, the silicon-based inorganic thin films are deposited on plastic substrates by plasma-enhanced chemical vapor deposition (PECVD) at low temperature. It is necessary to deposit thin film at low temperature. Because the heat gives damage to flexible plastic substrates. As one of the transparent diffusion barrier materials, silicon oxides have been investigated. $SiO_x$ have less toxic, so it is one of the more widely examined materials as a diffusion barrier in addition to the dielectric materials in solid-state electronics [3-4]. The $SiO_x$ thin films are deposited by a PECVD process in low temperature below $100^{\circ}C$. Water vapor transmission rate (WVTR) was determined by a calcium resistance test, and the rate less than $10.^{-2}g/m^2{\cdot}day$ was achieved. And then, flexibility of the film was also evaluated.

  • PDF

Comparison study of heatable window film using ITO and ATO

  • Park, Eun Mi;Lee, Dong Hoon;Suh, Moon Suhk
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2016.02a
    • /
    • pp.300.2-300.2
    • /
    • 2016
  • Increasing of the demand for energy savings for buildings, thermal barrier films have more attracted. In particular, as heat loss through the windows have been pointed out to major problems in the construction and automobile industries, the research is consistently conducted for improving the thermal blocking performance for windows. The main theory of the technology is reflect the infrared rays to help the cut off the inflow of the solar energy in summer and outflow of the heat from indoors in winter to save the energy on cooling and heating. Furthermore, this is well known for prevent glare, reduces fading caused by harmful ultraviolet radiation and easy to apply on constructed buildings if it made as a film. In addition to these advantages, apply the transparent electrode to eliminate condensation by heating. Generally ITO is used as a transparent electrode, but is has a low stability in environmental factors. In this study, ITO and its alternative, ATO, is deposited by sputtering system and then the characteristic is evaluated each material based thermal barrier thin film. The optical property was measured on wide range of wavelength (200 nm 2500 nm) to know the transparency in visible wavelength and reflectivity in IR wavelength range. The electrical property was judged by sheet resistivity. Finally the changes of the temperature and current of the deposited film was observed while applying a DC power.

  • PDF

Schottky barrier polycrystalline silicon thin film transistor by using platinum-silicided source and drain (플레티늄-실리사이드를 이용한 쇼트키 장벽 다결정 박막 트랜지스터트랜지스터)

  • Shin, Jin-Wook;Choi, Chel-Jong;Chung, Hong-Bay;Jung, Jong-Wan;Cho, Won-Ju
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.11a
    • /
    • pp.80-81
    • /
    • 2008
  • Schottky barrier thin film transistors (SB-TFT) on polycrystalline silicon(poly-Si) are fabricated by platinum silicided source/drain for p-type SB-TFT. High quality poly-Si film were obtained by crystallizing the amorphous Si film with excimer laser annealing (ELA) or solid phase crystallization (SPC) method. The fabricated poly-Si SB-TFTs showed low leakage current level and a large on/off current ratio larger than $10^5$. Significant improvement of electrical characteristics were obtained by the additional forming gas annealing in 2% $H_2/N_2$ ambient, which is attributed to the termination of dangling bond at the poly-Si grain boundaries as well as the reduction of interface trap states at gate oxide/poly-Si channel.

  • PDF

Characteristics of Ni/SiC Schottky Diodes Grown by ICP-CVD

  • Gil, Tae-Hyun;Kim, Han-Soo;Kim, Yong-Sang
    • KIEE International Transactions on Electrophysics and Applications
    • /
    • v.4C no.3
    • /
    • pp.111-116
    • /
    • 2004
  • The Ni/SiC Schottky diode was fabricated with the $\alpha$-SiC thin film grown by the ICP-CVD method on a (111) Si wafer. $\alpha$-SiC film has been grown on a carbonized Si layer in which the Si surface was chemically converted to a very thin SiC layer achieved using an ICP-CVD method at $700^{\circ}C$. To reduce defects between the Si and $\alpha$-SiC, the surface of the Si wafer was slightly carbonized. The film characteristics of $\alpha$-SiC were investigated by employing TEM (Transmission Electron Microscopy) and FT-IR (Fourier Transform Infrared Spectroscopy). Sputterd Ni thin film was used as the anode metal. The boundary status of the Ni/SiC contact was investigated by AES (Auger Electron Spectroscopy) as a function of the annealing temperature. It is shown that the ohmic contact could be acquired beyond a 100$0^{\circ}C$ annealing temperature. The forward voltage drop at 100A/cm was I.0V. The breakdown voltage of the Ni/$\alpha$-SiC Schottky diode was 545 V, which is five times larger than the ideal breakdown voltage of the silicon device. As well, the dependence of barrier height on temperature was observed. The barrier height from C- V characteristics was higher than those from I-V.