Properties of ${\beta}$-SIC TiB$_2$ Electroconductive Ceramic Composites Densified by Liquid-Phase Sintering(Ⅱ) (液狀 燒結에 의한 ${\beta}$-SIC TiB$_2$系 導電性 複合體의 特性(Ⅱ))

  • Shin, Yong-Deok;Yim Seung-Hyuk;Song Joon-Tae
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.50 no.6
    • /
    • pp.263-270
    • /
    • 2001
  • The mechanical and electrical properties of the hot-pressed and annealed ${\beta}-SiC-TiB_2$,/TEX> electroconductive ceramic composites were investigated as function as functions of the liquid forming additives of $Al_2O_3+Y_2O_3$. The result of phase analysis of composites by XRD revealed ${\alpha}$-SiC(6H), $TiB_2$,/TEX>, and YAG($Al_5Y_3O_{12}$) crystal phase. The relative density and the mechanical properties of composites were increased with increasing $Al_2O_3+Y_2O_3$ contents in pressureless annealing method because YAG of reaction between $Al_2O_3$ was increased. The flexural strength showed the highest value of 458.9 MPa for composites added with 4 wt% $Al_2O_3+Y_2O_3$ additives in pressed annealing method at room temperature. Owing to crack deflection, crack bridging, phase transition and YAG of fracture toughness mechanism, the fracture toughness showed 7.1 MPa ${\cdot}\;m^{1/2}$ for composites added with 12 wt% $Al_2O_3+Y_2O_3$ additives in pressureless annealing method at room temperature. The electrical resistivity and the resistance temperature coefficient showed the lowest value of $6.0{\times}10^{-4}\;{\Omega}\;{\cdot}\;cm(25\'^{\circ}C}$ and $3.0{\times}10^{-3}/^{\circ}C$ for composite added with 12 wt% $Al_2O_3+Y_2O_3$ additives in pressureless annealing method at room temperature, respectively. The electrical resistivity of the composites was all positive temperature coefficient resistance(PTCR) in the temperature ranges from 25 $^{\circ}C$ to 700 $^{\circ}C$.

  • PDF

Dependence of the Diode Characteristics of ZnO/b-ZnO/p-Si(111) on the Buffer Layer Thickness and Annealing Temperature (버퍼막 두께 및 버퍼막 열처리 온도에 따른 ZnO/b-ZnO/p-Si(111)의 전기적 특성 변화 및 이종접합 다이오드 특성 평가)

  • Heo, Joo-Hoe;Ryu, Hyuk-Hyun
    • Journal of the Korean Vacuum Society
    • /
    • v.20 no.1
    • /
    • pp.50-56
    • /
    • 2011
  • In this study, the effects of ZnO buffer layer thickness and annealing temperature on the heterojunction diode, ZnO/b-ZnO/p-Si(111), were reported. The effects of those on the structural and electrical properties of zinc oxide (ZnO) films on ZnO buffered p-Si (111) substrate were also studied. Structural properties of ZnO thin films were studied by X-ray diffraction and I-V characteristics were measured by a semiconductor parameter analyzer. ZnO thin films with 70 nm thick buffer layer and annealing temperature of $700^{\circ}C$ showed the best c-axis preferred orientation. The best electrical property was found at the condition of buffer layer annealing temperature of $700^{\circ}C$ and 50nm thick ZnO buffer layer (resistivity: $2.58{\times}10^{-4}[{\Omega}-cm]$, carrier concentration: $1.16{\times}1020[cm^{-3}]$). The I-V characteristics for ZnO/b-ZnO/p-Si(111) heterojunction diode were improved with increasing buffer layer thickness at buffer layer annealing temperature of $700^{\circ}C$.

Thermoelectric Properties of the 0.05wt% $SbI_3$-Doped n-Type $Bi_2({Te_{0.95}}{Se_{0.05}})_3$ Alloy with Variation of the Annealing Time (0.05wt% $SbI_3$를 첨가한 n형 $Bi_2({Te_{0.95}}{Se_{0.05}})_3$ 가압소결체의 열처리 시간에 따른 열전특성)

  • Lee, Sun-Kyong;Oh, Tae-Sung;Hyun, Dow-Bin
    • Korean Journal of Materials Research
    • /
    • v.10 no.4
    • /
    • pp.257-263
    • /
    • 2000
  • Thermoelectric properties of the 0.05wt% $SbI_3$-doped n-type $Bi_2(Te_{0.95}Se_{0.05})_3$ alloy, prepared by melting/grinding and hot pressing, were investigated with variation of the annealing time up to 36 hours. The electron concentration of the 0.05wt% SbI$_3$-doped n-type $Bi_2(Te_{0.95}Se_{0.05})_3$ alloy decreased with increasing the annealing time. The figure-of-merit of the 0.05wt% $SbI_3$-doped n-type $Bi_2(Te_{0.95}Se_{0.05})_3$ alloy was improved from $2.1{\times}10^{-3}/K$ to $2.35{\times}10^{-3}/K$ by annealing at $500^{\circ}C$ for 3 hours. When annealed longer than 12 hours, however, the figure-of-merit decreased substantially due to the increase of the electrical resistivity.

  • PDF

Formation of N Doped, p-type ZnO Films by Post-annealing in NH3 Ambient (NH3 분위기에서 후속 열처리에 의한 p형 ZnO 형성)

  • Jung, Eun-Soo;Kim, Hong-Seung;Cho, Hyung-Kun
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.19 no.7
    • /
    • pp.611-617
    • /
    • 2006
  • We report the preparation of N doped, p-type ZnO films by post-annealing in $NH_3$ ambient. The properties were examined by XRD, Hall-effect measurement, PL, and SIMS. ZnO films showed better crystallinity and electron concentration of $10^{15}-10^{17}/cm^3$ with post-annealing in $NH_3$ ambient. These films were converted to p-type ZnO by activation thermal annealing process at $800^{\circ}C$ under $N_2$ ambient. The electrical properties of the p-type ZnO showed a hole concentration of $1.06\times10^{16}/cm^3$, a mobility of $15.8cm^2/V{\cdot}s$, and a resistivity of $40.18\Omega{\cdot}cm$. The N doped ZnO films showed a strong photoluminescence peak at 3.306 eV at 13 K, which is closely related to neutral acceptor bound excitons of the p-type ZnO:N. In the SIMS spectra, the incorporation of nitrogen was confirmed.

Preparation of Sr2FeMoO6 Thin Films by RF Magnetron Sputtering and Their Electrical Conduction Properties (RF 스퍼터법을 이용한 Sr2FeMoO6 박막 제조 및 전기전도 특성)

  • Ryu, Hee-Uk;Sun, Ho-Jung
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.23 no.12
    • /
    • pp.966-972
    • /
    • 2010
  • Single-phase $Sr_2FeMoO_6$ thin films were produced by RF magnetron sputtering for use as electrodes in integrated sensors and found to be good conductors at room temperature. The films were deposited from a powder-type sputtering target under various conditions, and were crystallized by annealing. Elimination of $O_2$ gas during deposition, by the use of a solely Ar sputtering gas under a working pressure as low as possible, and vacuum annealing were important to promote the $Sr_2FeMoO_6$ phase. However, oxygen exclusion from sputtering and annealing was not enough to yield single-phase $Sr_2FeMoO_6$: hydrogen annealing was also required. Film production was optimized by varying the deposition parameters and hydrogen annealing conditions. The film had good electrical conduction, with a low resistivity of $1.6{\times}10^{-2}\Omega{\cdot}cm$ at room temperature.

Effect of the Sulfurization Temperature and Annealing Time of E-Beam Evaporated Sn Precursors on the Growth of SnSx Thin Films (E-빔 증착된 Sn 전구체의 황화 열처리 온도 및 시간에 따른 SnSx 박막 성장 효과)

  • Huang, Tingjian;Kim, Jeha
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.30 no.11
    • /
    • pp.734-739
    • /
    • 2017
  • We prepared $SnS_x$ thin films on both soda-lime glass (SLG) and molybdenum(Mo)/SLG substrates by a two-step process using a Sn precursor followed by sulfur reaction in rapid thermal annealing (RTA) at different sulfurization temperatures ($Ts=200^{\circ}C$, $230^{\circ}C$, $250^{\circ}C$, and $300^{\circ}C$) and annealing times ($t_s=10min$ and 30 min). The single SnS phase was dominant for $200^{\circ}C{\leq}T_s$<$250^{\circ}C$, while an additional phase of $SnS_2$ was appeared at $T_s{\geq}250^{\circ}C$ alongside SnS. The SnS grains in all the samples showed strong growth along the preferred [040] direction. The band-gap energy ($E_g$) of the films was estimated to be 1.24 eV.

The Microstructural Changes of Free-Annealed Nylon 6 Filament Yarns - Comparison of UDY, POY, and FDY - (무긴장 열처리 나일론 6 필라멘트사의 내부구조 변화 - 미연신사, 부분배향사 및 완전연신사의 비교 -)

  • Lee Jung Ju;Cho Gil Soo
    • Journal of the Korean Society of Clothing and Textiles
    • /
    • v.13 no.1 s.29
    • /
    • pp.43-47
    • /
    • 1989
  • The microstructural changes of nylon 6 UDY, POY and FDY were compared after free-annealing through crystallinity, birefringence, and melting behavior analyses. Free-annealing was done at various temperatures $(120^{\circ}C\;,140^{\circ}C,\;160^{\circ}C,\;180^{\circ}C,\;200^{\circ}C)$ and times (15 min., 30 min., 60 min.) using vaccum oven. Crystallinity was measured by the density gradient column technique and birefringence was measured using a Nikon polarizing microscope with a quartz wedge and Senarmont compensator. Melting behavior was investigated on the basis of DSC melting corves. Crystallinites of specimens increased as the treatment temperature and time increased. Birefringence of UDY increased after annealing and increased as the treatment temperature increased. On the other hand, those of POY and FDY decreased after annealing. Especially, the changes of crystallinity and birefringence of treated POY were particularly lower than those of treated UDY and FDY. Melting peaks of untreated UDY, POY and FDY were different in the position and the shape, but little change was seen in melting peaks in spite of increasing the annealing temperature and time. UDY and FDY showed single melting peaks in all the specimens. But POY showed double melting peaks, which means the coexistences of crystals with different thermal properties.

  • PDF

Effect of Rapid Thermal Annealing on the Ti doped In2O3 Films Grown by Linear Facing Target Sputtering

  • Seo, Ki-Won;Kim, Han-Ki
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2014.02a
    • /
    • pp.342.1-342.1
    • /
    • 2014
  • The electrical, optical and structural properties of Ti doped $In_2O_3$ (TIO) ohmic contacts to p-type GaN were investigated using linear facing target sputtering (LFTS) system. Sheet resistance and resistivity of TIO films are decreased with increasing rapid thermal annealing (RTA) temperature. Although the $400^{\circ}C$ and $500^{\circ}C$ annealed samples showed rectifying behavior, the $600^{\circ}C$ and $700^{\circ}C$ annealed samples showed linear I-V characteristics indicative of the formation of an ohmic contact between TIO and p-GaN. The annealing of the contact at $700^{\circ}C$ resulted in the lowest specific contact resistivity of $9.5{\times}10^{-4}{\Omega}cm^2$. Based on XPS depth profiling and synchrotron X-ray scattering analysis, we suggested a possible mechanism to explain the annealing dependence of the properties of TIO layer on rapid thermal annealing temperature.

  • PDF

Fabrication of Li2CO3-doped Thin Film Bulk Acoustic Resonator and Structural, Electrical Properties as a Function of Annealing Temperatures (Li2CO3:ZnO를 이용하여 제조한 FBAR의 제작 및 열처리에 따른 구조적, 전기적 특성)

  • Kim, Bong-Seok;Kim, Eung-Kwon;Lee, Tae-Yong;Oh, Su-Young;Song, Joon-Tae
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.20 no.2
    • /
    • pp.152-155
    • /
    • 2007
  • In this study, we fabricated FBAR(film bulk acoustic resonator) by using $Li_{2}CO_{3}:ZnO$ as a function of annealing temperature and concentrated on effect of frequency characteristic of FBAR. The results show that the annealing affects resistivity and crystallity. The optimum properties were observed for film annealed at $500^{\circ}C$. The resistivity was $1.5{\times}10^{11}\;{\Omega}{\cdot}cm$ and the roughness was 21.10 nm. And the return loss is improved from -24.9 at $300^{\circ}C$ to -29.8 at $500^{\circ}C$ without the resonant frequency change. We finally confirmed the improvement on the frequency characteristics of FBAR device by annealing process at the optimized condition.

PECVD Silicon Nitride Film Deposition and Annealing Optimization for Solar Cell Application (태양전지 응용을 위한 PECVD 실리콘 질화막 증착 및 열처리 최적화)

  • Yoo, Jin-Su;Dhungel Suresh Kumar;Yi, Jun-Sin
    • The Transactions of the Korean Institute of Electrical Engineers C
    • /
    • v.55 no.12
    • /
    • pp.565-569
    • /
    • 2006
  • Plasma enhanced chemical vapor deposition(PECVD) is a well established technique for the deposition of hydrogenated film of silicon nitride (SiNx:H), which is commonly used as an antireflection coating as well as passivating layer in crystalline silicon solar cell. PECVD-SiNx:H films were investigated by varying the deposition and annealing conditions to optimize for the application in silicon solar cells. By varying the gas ratio (ammonia to silane), the silicon nitride films of refractive indices 1.85 - 2.45 were obtained. The film deposited at $450^{\circ}C$ showed the best carrier lifetime through the film deposition rate was not encouraging. The film deposited with the gas ratio of 0.57 showed the best carrier lifetime after annealing at a temperature of $800^{\circ}C$. The single crystalline silicon solar cells fabricated in conventional industrial production line applying the optimized film deposition and annealing conditions on large area substrate of size $125mm{\times}125mm$ (pseudo square) was found to have the conversion efficiencies as high as 17.05 %. Low cost and high efficiency silicon solar cells fabrication sequence has also been explained in this paper.