  • For the development of high-fluidity concrete using low-binder, The effect of the use of the developed acrylic viscosity agent on the physical properties of concrete evaluated. The amount acrylic viscosity agent used was 1.5%, 1.7%, and 2.0% based on the binder amount of 400kg/m3, and slump flow test, slump flow 500mm arrival time measurement, air volume measurement, and U-Box passing test were conducted to determine the effect of the physical properties of concrete. it was judged that 1.5% of the acrylic viscosity agent used in high-fluidity concrete using low-binder was most suitable.

  • PDF

재생 골재 콘크리트의 슬럼프 손실 개선을 위한 분말형 감수제의 활용 (Application of Powdered Superplasticizer to Improve of Slump Loss Rate in Recycled Aggregate Concrete)

  • 양근혁;심재일;이재삼;정헌수
    • 콘크리트학회논문집
    • /
    • 제18권5호
    • /
    • pp.649-656
    • /
    • 2006
  • 본 연구에서는 재생 골재 콘크리트의 현장적용성을 높이기 위해 보통 콘크리트에 비해 큰 슬럼프 손실을 개선할 수 있는 분말형 감수제(PSP제)를 개발하였다. 이 PSP제가 혼입된 콘크리트의 유동성 및 역학적 성질들을 평가하기 위하여 재생 굵은골재와 재생 잔골재 혼입조건에 24배합이 실험되었다. 액상형 고성능 감수제를 투입한 콘크리트의 슬럼프는 시간경과와 함께 급격히 감소하며 120분 후에는 초기 슬럼프의 50% 이하로 떨어졌다. 하지만 PSP 제를 혼입한 콘크리트의 슬럼프는 배합 후 30분 까지는 거의 변화가 없으며 1시간 경과 후에도 초기 슬럼프의 85% 이상을 유지하였다. 뿐만 아니라 PSP제는 콘크리트의 압축강도, 할렬인장강도, 휨강도 및 탄성계수들도 향상시켰으며 건조수축 변형률을 감소시켰다. 콘크리트의 성능향상을 고려하였을 때 PSP제의 최적 혼입률은 시멘트 양 대비 5%이었다.

굵은 골재 최대치수 변경에 따른 슬럼프 플로 타입 콘크리트의 배합조정방법별 유동특성변화에 대한 실험적 연구 (An Experimental Research on Changes of Properties in Flow by Slump Flow Type Concrete Mix Design Adjustment of the Way according to the Various Gmax Size)

  • 권해원;서일;이진우;박희곤;이재삼;이종서
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2010년도 춘계 학술논문 발표대회 2부
    • /
    • pp.67-68
    • /
    • 2010
  • Recently, there were not enough studies regarding the mix adjustment and changes of normal physical properties of slump flow type concrete in domestically. Therefore in this paper, it is aimed securing the fundamental data about flow its mix design method by experimental research. The experiment includes the adjustment of the way for slump flow type concrete by the variation of size of coarse aggregate. In the result, it is advisable raising the ratio of fine aggregate and unit water amount by considering the specific surface when increasing the Gmax size.

  • PDF

신경망을 이용한 콘크리트의 압축강도 및 슬럼프값 추정 (The Prediction of Compressive Strength and Slump Value of Concrete Using Neural Networks)

  • 최영화;김종인;김인수
    • 한국산업융합학회 논문집
    • /
    • 제5권2호
    • /
    • pp.103-110
    • /
    • 2002
  • An artificial neural network is applied to the prediction of compressive strength, slump value of concrete. Standard mixed tables arc trained and estimated, and the results are compared with those of experiments. To consider the varieties of material properties, the standard mixed tables of two companies of Ready Mixed Concrete are used. And they are trained with the neural network. In this paper, standard back propagation network is used. For the arrangement on the approval of prediction of compressive strength and slump value, the standard compressive strength of 210, $240kgf/cm^2$ and target slump value of 12, 15cm are used because the amount of production of that range arc the most at ordinary companies. In results, in the prediction of compressive strength and slump value, the predicted values are converged well to those of standard mixed tables at the target error of 0.10, 0.05, 0.001 regardless of two companies.

  • PDF

고로슬래그와 폴리카르본산계 유기 혼화제를 첨가한 Belite-rich Cement 모르타르 유동특성 (Rheology Properties of Belite-rich Cement Mortar Added Blastfurnace Slag and Polycarbonate-based Superplasticizer)

  • 송종택;송종택;조현태;황인수;박춘근
    • 한국세라믹학회지
    • /
    • 제37권2호
    • /
    • pp.145-151
    • /
    • 2000
  • In order to investigate the rheological properties of belite-rich cement(BRC) added polycarbonate-based superplasticizer and blastfurnace slags which have different blaines at 4500, 6000 and 8000$\textrm{cm}^2$/g, the change of minislumps and mortar slumps are measured with time. The rheological properties improve as specific surface area of added slag decreases or amount of polycarbonate-based superplasticizer increases. The slump loss can be controlled effectively by the steric hinderance effect of polycarbonate-based superplasticizer. According to the results, when mix proportion of the mortar is 1.5% mass content of superplasticizer and 30% mass addition of blastfurnace slag which blaine is 4500$\textrm{cm}^2$/g, the best mortar slump can be achieved without any significant segregation of materials.

  • PDF

셀룰로스계 증점제의 첨가량이 고유동 저분체 콘크리트의 물리적 특성에 미치는 영향에 관한 실험적 연구 (Experimental Study on the Effect of the Amount of Cellulose type Viscosity Agent on the Physical Properties of High-Fluidity Concrete Using Low-Binder)

  • 고혜빈;조인성;이한승
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2021년도 가을 학술논문 발표대회
    • /
    • pp.129-130
    • /
    • 2021
  • For the development of high-fluidity concrete using low-binder, The effect of the use of the developed acrylic viscosity agent on the physical properties of concrete evaluated. The amount acrylic viscosity agent used was 0.28%, 0.29% and 0.30% based on the binder amount of 350kg/m3, and slump flow test, air volume measurement, U-Box passing test and strength compressive were conducted to determine the effect of the physical properties of concrete. it was judged that 0.29% of the cellulose type viscosity agent used in high-fluidity concrete using low-binder was most suitable.

  • PDF

고유동 시멘트를 사용한 고성능 콘크리트특성에 관한 연구 (A Study on the Properties of High Performance Concrete using High Flowable Cement)

  • 최광일;현석훈;박춘근;강민호
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 1996년도 가을 학술발표회 논문집
    • /
    • pp.290-294
    • /
    • 1996
  • High-Belite cement had a better slump flow characteristics than type I cement and slag cement, and its varation of slump flow with time was also excellent. As the amount binder added was increased, the strength increased while material separation decreased. This phenomena was obvious when the amount of cement was abobe 500kg/$\textrm{m}^3$ . When the amount of cement and S/a were 516kg/$\textrm{m}^3$ and 52% respectively, the application strength of 600kg/$\textrm{m}^3$ was satisfied. Since, however, the aggreate size of 25mm was somewhat unsatisfactory, the characteristics of high performance concrete could be obtained by the addition of the viscosity-enhancing agent.

  • PDF

유지제 혼입율 변화에 따른 콘크리트의 유동성 및 역학적 특성 (Liquidity and Mechanical Properties of Concrete by Fluidity Retention Agent Mix Rate Change)

  • 박병관;최성용;배장춘;노동현;한민철;한천구
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2008년도 추계 학술논문 발표대회
    • /
    • pp.89-92
    • /
    • 2008
  • This research analyzed the basic characteristics of unhardened concrete and the compression strength characteristics of hardened concrete according to liquidity retention agent mix rate change to improve the liquidity fluidity retention performance of high performance concrete, and produced the following results. The moment fluidity retention agent is added according to fluidity retention agent mix rate change, which increased fluidity retention agent mix rate, slump flow decreased, and in the case of slump flow according to the progress time change by the fluidity retention agent mix rates, the more fluidity retention agent mix rate increased, the lower slump flow change rate became. The moment fluidity retention agent is added according to fluidity retention agent mix rate change, fluidity retention agent mix rate increased compared to non-mixture of fluidity retention agent, and the air amount by progress time change by the fluidity retention agent mix rates slightly increased, however target range is still met and unit volume mass is inversely proportional to air amount. Compression strength according to age progress by the fluidity retention agent mix rates was shown to increase slightly with increase in fluidity retention agent mix rate, and yet the difference was not significant.

  • PDF

Fly Ash를 사용한 수중불분리 콘크리트의 유동성에 관한 연구 (A Study on the Fluidity of Antiwashout Underwater Concrete Containing Fly Ash)

  • 권중현;배기성
    • 한국해양공학회지
    • /
    • 제12권1호
    • /
    • pp.153-161
    • /
    • 1998
  • This paper is to investigate the Fluidity of Antiwashout Underwater Concrete containing Fly Ash. The results of study are concluded as follows: the increase in Slump Flow value did not happen in the plain concrete which was replaced cement by Fly Ash; however, the maximum value could reach in the replacement of 30% of Fly Ash by weight of cement in the Fly Ash replaced concrete. On the condition of Fly Ash-Antiwashout Underwater Concrete in expecting 50 cm of the Slump Flow, it was necessary that the usage amount of Superplasticizer be around 1% of unit Binder, and 1.5% in 60 cm of the Slump Flow, respoectively.

  • PDF

온도조건 및 시간경과에 따른 고강도 콘크리트의 시공성에 관한 실험 연구 (An Experimental Study on the Workability of High Strength Concrete according to Temperature and Elapsed time)

  • 박준호;윤명덕;임병호;김태곤;박정민;김화중
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 봄 학술발표회 논문집
    • /
    • pp.25-30
    • /
    • 2001
  • The purpose of this study is to present a basic data about the workability of high strength concrete to apply to a field of construction work. The main parameters are as follows; environmental temperature, elapsed time and the use of mineral admixture or not under the same mixing proportions. From the result, Adding amounts of superplasticizer to get a target slump were different in the respective temperature condition. Slump loss according to elapsed time was influenced by environmental temperature. the amount of superplasticizer and the slump loss were decreased by using mineral admixture(garnet powder) and by making concrete under lower temperature.

  • PDF