• 제목/요약/키워드: Aluminium metal

검색결과 247건 처리시간 0.025초

삽입금속을 사용한 구상흑연주철과 2024 알미늄합금의 마찰압접에 관한 연구 (Friction Welding of Spheroidal Graphite Cast iron and 2024 Aluminium Alloys using Insert Metal)

  • 김창규;김치옥;심성보;김광일
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2002년도 추계학술대회 논문집
    • /
    • pp.283-288
    • /
    • 2002
  • This study accompanied with the friction welding of a spheroidal graphite cast iron bar and 2024 Aluminium alloy bar with A1050 insert metal and investigated between conditions of friction welding faces and welded joint strength. This principal results of the experimental investigation could be summarized as follows: If the optimum friction welding is selected, the aspect of the spheroidal graphite cast iron and 2024 Aluminium could be welded with a pure Aluminium insert metal.

  • PDF

용융금속 방호보호복소재의 성능수준 평가 (Performance Evaluation of Molten Metal Splash Protective Fabrics)

  • 박평규;김로;윤기종
    • 한국위험물학회지
    • /
    • 제6권2호
    • /
    • pp.55-61
    • /
    • 2018
  • In this study, the molten metal protective performance of various molten metal protective clothing materials such as herringbone twill laminated aluminium foils, oxydized-polyacrylonitrile laminated with aluminium deposited polyethylene terephthalate films, twill fabric laminated with aluminium deposited polyethylene terephthalate films and nonwoven laminated with aluminum deposited polyethylene terephthalate films, were evaluated according to modified EN ISO 9185. The results showed that the molten metal protective performance of tested samples improved with the increase in fabric structure density, weight and thickness. In addition the effect of the thickness of aluminum foil on the molten metal protective performance is not significant. It was found the fabric is more important in the molten metal splash protective clothing.

Sinfony 간접복합수지와 비귀금속합금간의 전단결합강도와 파절양상 (Shear Bond Strength and Failure Mode between Sinfony Indirect Composite Resin and Non Precious Metal)

  • 민병록;정인성
    • 대한치과기공학회지
    • /
    • 제30권2호
    • /
    • pp.79-86
    • /
    • 2008
  • The purpose of this study was to investigate the effect retention element formed by metal surface treatment method on the bond strength of indirect composite resin and metal. The metal specimens were cast from Ni-Cr alloy($Rexillium^{(R)}$ III). They were divided into 5 groups by applied retention element: $50{\mu}m$ aluminium oxide sandblasting group, $250{\mu}m$ aluminium oxide sandblasting group, 0.2mm retention crystal group, 10% $H_{2}SO_{4}$ solution etching group, $110{\mu}m$ $Rocatec^{TM}$ Plus system group. Total 50 metal specimens were veneered with Sinfony indirect composite resin system. Specimens were tested for shear bond strength on an Instron universal testing machine and fracture mode of fractured specimens were analyzed by SEM and EDS. 1. 0.2 mm retention crystals were most effective in improving the resin-metal shear bond strength (p<0.05). 2. Sandblasting by $250{\mu}m$ aluminium oxide were more effective than sandblasting by $50{\mu}m$ aluminium oxide in improving the resin-metal shear bond strength(p<0.05). 3. Fracture mode of resin-metal fractured surface were cohesive failure mode in 0.2mm retention crystal, mixed failure mode in sandblasted specimens, etched specimens and the specimens sandblasted with $110{\mu}m$ $Rocatec^{TM}$ Plus system.

  • PDF

Al 스크랩으로부터 금속회수에 관한 연구 (A Study of the Metal Recovery from the Aluminium Scrap)

  • 김준수;임병모;윤의박
    • 자원리싸이클링
    • /
    • 제4권1호
    • /
    • pp.25-30
    • /
    • 1995
  • 본 연구에서는 Al 스크랩으로부터 재생지금 제조시 시료의 예비처리, 용제첨가 및 용해분위기가 Al 회수율에 미치는 영향을 조사하였다. 실험결과에 따르면 Al 드로스는 용탕표면에서의 산화반응에 의해 발생하였다. 예비처리의 영향에 다르면 탈지하지 않고 압착한 칩 bale 시료의 경우에는 압착하지 않은 칩 시료에 비해 약 14%의 회수율이 증가하였으며, Al seed 용해공법을 채택하는 경우에는 탈지하지 않고 단지 세편과 압착만을 행하여도 97%의 높은 회수율을 얻을 수 있었다. Al 스크랩 용해시 7wt%까지 첨가된 염에 의해 회수율은 최대 95%까지 증대되었으며, 탄소 및 질소분위기에서도 역시 회수율은 증가하였으나, 염과 탄소의 혼합분 첨가시 과잉 첨가된 탄소는 오히려 회수율을 감소시켰다.

  • PDF

염산산성(鹽酸酸性) 용액(溶液)중에서 알루미늄에 의한 주석(朱錫)의 치환반응(置換反應) (Cementation of Tin by Aluminium from Hydrochloric acid Solution)

  • 안재우;소순섭
    • 자원리싸이클링
    • /
    • 제17권2호
    • /
    • pp.70-75
    • /
    • 2008
  • 폐전자스크랩, 함주석 폐액 등에서 주석 성분을 회수하기 위한 기초 연구로 주석이 함유된 염산용액에서 알루미늄 분말을 이용한 치환반응에 대한 연구를 실시하였다. 주석이온의 치환 반응에 미칠 수 있는 용액의 pH, 알루미늄 분말 첨가량, 반응온도, 반응시간, 염소이온($Cl^-$) 농도, 불순물 농도 둥에 대해 고찰하였다. 치환실험 결과 알루미늄 분말의 첨가량. 반응온도, pH 및 염소이온 농도가 증가함에 따라 주석이거 치환속도가 증가함을 알 수 있었다. 이들 결과로부터 알루미늄 금속분말을 이용한 금속 주석의 치환 및 회수에 관한 최적 조건을 제시하였다.

고강성 다층 메탈베어링의 접합 (High strength's union of mass layers metal bearing)

  • 전재억;황영모;김수광;계중읍;김준안;하만경
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2004년도 추계학술대회 논문집
    • /
    • pp.792-795
    • /
    • 2004
  • Despite is product that ship, vehicles, development equipment and Metal Bearing for plant equipment that is mass-produced by present domestic companies Cast White Metal Lining Bearing that is Bimetal Bearing standing 2 generation is accomplishing master and servant and this is foreseen to be used widely on industry whole in hereafter but Cast White Metal Bearing need minuteness processing, while price competitive power is depending on income from superior another thing area than itself manufacture already in advanced nation to lowdown that the technique is generalized widely, when take into account technology change aspect of industrial technology developing country, Go added value creation by deepening of price competition is judged to be difficult hereafter. Because domestic production and supply are wholly lacking almost in Metal Bearing Cladding that take advantage of these technology, Data-base about connection technology is weak with technique and Know-How for product. This research unites Back Steel and Aluminium Alloy different kind metal and make the Clad river studying technology about union of Gogangseong Dacheung metal bearing hereupon.

  • PDF

Studies on weldment performance of Ti/Al dissimilar sheet metal joints using laser beam welding

  • Kalaiselvan, K.;Elango, A.;Nagarajan, N.M.;Mathiazhagan, N.;Vignesh, Kannan
    • Coupled systems mechanics
    • /
    • 제7권5호
    • /
    • pp.627-634
    • /
    • 2018
  • Laser beam welding is more advantageous compared to conventional methods. Titanium/Aluminium dissimilar alloy thin sheet metals are difficult to weld due to large difference in melting point. The performance of the weldment depends upon interlayer formation and distribution of intermetallics. During welding, aluminium gets lost at the temperature below the melting point of titanium. Therefore, it is needed to improve a new metal joining techniques between these two alloys. The present work is carried for welding TI6AL4V and AA2024 alloy by using Nd:YAG Pulsed laser welding unit. The performance of the butt welded interlayer structures are discussed in detail using hardness test and SEM. Test results reveal that interlayer fracture is caused near aluminium side due to low strength at the weld joint.

An interface element for modelling the onset and growth of mixed-mode cracking in aluminium and fibre metal laminates

  • Hashagen, Frank;de Borst, Rene
    • Structural Engineering and Mechanics
    • /
    • 제5권6호
    • /
    • pp.817-837
    • /
    • 1997
  • In the present contribution an interface crack model is introduced which is capable of modelling crack initialisation and growth in aluminium as well as in Fibre Metal Laminates. Interface elements are inserted in a finite element mesh with a yield function which bounds all states of stress in the interface. Hardening occurs after a state of stress exceeds the yield stress of the material. The hardening branch is bounded by the ultimate stress of the material. Thereafter, the state of stress is reduced to zero while the inelastic deformations grow. The energy dissipated by the inelastic deformations in this process equals the fracture energy of the material. The model is applied to calculate the onset and growth of cracking in centre cracked plates made of aluminium and GLARE$^{(R)}$. The impact of the model parameters on the performance of the crack model is studied by comparisons of the numerical results with experimental data.

Cu-Zn 금속합금의 산화 환원반응과 Al-Silicate의 흡착반응을 이용한 폐수 중 중금속처리에 관한 연구 (A Study on the Treatment of Heavy Metal in Wastewater by Redox Reaction of Cu-Zn Metal Alloy and Adsorption reaction of Al-Silicate)

  • 이수정;김종화;송주영
    • 한국응용과학기술학회지
    • /
    • 제33권3호
    • /
    • pp.441-448
    • /
    • 2016
  • 본 연구는 구리 아연 금속합금의 산화 환원 반응과 합성 알루미늄 실리케이트의 흡착 반응을 이용한 폐수 중 중금속 처리에 관한 연구이다. 극세사 형태로 제조된 구리 아연 금속합금이 수용액 중에서 산화 환원반응에 의해 아연보다 이온화 경향이 작은 중금속은 환원 처리되고, 이온화 된 아연 및 미반응 중금속은 흡착 처리하여 제거하는 연구이다. 극세사 형태로 제조된 금속합금 물질은 표면적이 커서 1회 처리만으로도 반응 평형에 도달하게 하여 효율이 높은 것으로 나타났다. 크롬($Cr^{+3}$)은 redox 반응 1회 처리만으로도 100.0 % 제거 되었으며, 수은은 98.0 %, 주석 92.0 %, 구리는 91.4 % 정도 제거되었다. 카드뮴, 니켈, 납도 각각 40.0 %, 50.0 %, 58.0 %가 제거 되었다. 크롬($Cr^{+3}$)은 아연과 이온화 경향 차이가 거의 없지만 제거 효율이 높은 것으로 나타났는데 이는 3가 크롬은 이온 상태로 존재하면 redox 반응에서 발생한 $OH^-$ 이온과 결합하여 수산화물 침전을 형성하는 것으로 판단된다. Redox 반응 후 증가한 아연 및 미반응 중금속 농도를 알루미늄실리케이트를 1회 통과하여 거의 100.0 % 제거할 수 있었다. 이는 합성 알루미늄 실리케이트의 비표면적이 크고 금속 이온의 흡착능력이 우수한 것으로 나타났으며, 반응 후 알루미늄 이온은 증가하지 않는 것으로 보아 이온 교환이 아닌 흡착으로 아연 및 중금속 이온들을 제거할 수 있는 것으로 나타났다.

열교환기용 BAS111합금 고주파유도용접관에서 인발조건이 기계적 특성에 미치는 영향 (Effects of Drawing Parameters on Mechanical Properties in High Frequency Induction Welded Tubes of BAS111 Alloy for Heat-exchangers)

  • 국진선;김낙찬;송중근;전동태
    • Journal of Welding and Joining
    • /
    • 제22권4호
    • /
    • pp.65-72
    • /
    • 2004
  • The aim of this study is to investigate the optimum drawing parameter for BAS111 welded tubes. The BAS111 aluminium alloy tubes with 25.4mm in external diameter and 1.5mm in thickness for heat-exchangers were manufactured by high frequency induction welding with the V shaped convergence angle 6.8$^{\circ}$ and power input 50㎾. With increasing the reduction of area (1.6, 5.8, 11.5, 14.2, 18.5, 22.5%) by drawing, tensile strength was increased and elongation was decreased. With increasing the reduction of area by drawing, hardness in weld metal increased rapidly, while that of base metal increased slowly. In the specimen with the outer diameter smaller than 22mm, hardness of weld metal was higher than that of base metal. The optimum drawing parameter of area reduction was estimated about 15% because of the work hardening of welds.