Sn-Ag-Bi/Cu 솔더 조인트의 aging시 금속간화합물 성장 거동 (Growth Behavior of Intermetallic Compounds in Sn-Ag-Bi/Cu Solder Joints during Aging)

  • 한상욱;박창용;허주열
    • 한국마이크로전자및패키징학회:학술대회논문집
    • /
    • 한국마이크로전자및패키징학회 2003년도 기술심포지움 논문집
    • /
    • pp.133-137
    • /
    • 2003
  • The effect of Bi additions to the eutectic Sn-3.5Ag solder alloy on the growth kinetics of the intermetallic compound (IMC) layers during solid-state aging of Sn-Ag-Bi/Cu solder joints has been Investigated. The Bi additions enhanced the growth rate of the total IMC layer comprising of $Cu_6Sn_5$ and $Cu_3Sn$ sublayers. This enhanced IMC growth rate was primarily due to the rapid increase In the growth rate of $Cu_6Sn_5$ sublayer. The growth rate of $Cu_3Sn$ sublayers was little influenced and appeared to be retarded by the Bi additions. The observed growth behavior of $Cu_6Sn_5$ and $Cu_3Sn$ sublayers could be understood if the interfacial reaction barrier at the $Cu_6Sn_5/solder$ interface were reduced by the segregation of Bi at the interface.

  • PDF

LED용 리드프레임 상의 Sn-3.5Ag 솔더 도금의 젖음성 및 반사율 (Wetting Property and Reflectivity of Sn-3.5Ag Solder by Plating for LED Lead Frame)

  • 기세호;허증봉;김원중;정재필
    • 대한금속재료학회지
    • /
    • 제50권8호
    • /
    • pp.563-568
    • /
    • 2012
  • The wetting property and reflectivity of Sn-3.5Ag solder which was dip coated on a LED lead frame were investigated. The wettability of molten solder on Cu substrate was evaluated by the wetting balance tester, and surface tension was calculated from maximum withdrawal force and withdrawal time. Temperature of the molten solder in a bath was varied in the range of $250-290^{\circ}C$. With increasing temperature, the surface tension decreased a little. The reflectivity of Sn-3.5Ag coated on a substrate became a little lower than the highest current LED lead frame reflectivity.

Solder Paste로 접합된 비아볼의 Ball-off에 관한 연구 (A Study on the Ball-off of Via Balls Bonded by Solder Paste)

  • 김경수;김진영
    • 한국전기전자재료학회논문지
    • /
    • 제17권6호
    • /
    • pp.575-579
    • /
    • 2004
  • Package reliability test was conducted to investigate the effect of solder paste composition at BGA Package. It was found that the shape and size of the phase form are affected by the processing parameters. The material have used to fill in the via was Sn/36Pb/2Ag and Sn/0.75Cu type solder paste. Sn/36Pb/2Ag and Sn/0.75Cu paste were fabricated on Tape-BGA substrates by screen printing process, and via ball mount data were characterized with variations of dwell time of 85 seconds at reflow peak temperature at 22$0^{\circ}C$ or 24$0^{\circ}C$. The test condition was MRT 30 $^{\circ}C$/60 %RH/96 HR. Failures formed of a ball-off in solder paste process were observed by using a Optical Microscope and SEM(Scanning Electron Microscope). It was concluded that intermetallic layer growth played important roles in increasing solder fatigue strength for addition of Ag composition. The degradation of shear strength of solder composition is discussed.

Pb Free 솔더를 사용한 솔더 접합부의 접합 강도 향상에 관한 연구 (Study on Joining Strength Improvement of Solder Joint with Pb Free Solder)

  • 신영의;김영탁
    • Journal of Welding and Joining
    • /
    • 제15권2호
    • /
    • pp.36-42
    • /
    • 1997
  • In this paper, stability of initial strength at solder joint with lead free solders, such as Sn-In (52-48%) and Sn-Ag (96.5-3.5wt%) was studied. To obtain at solder joint with high quality, it is very important to control the temperature at the interface of solder joints. It is found that the thermal EMF (electro motive force) occurs betwee lead frame and copper pad on a substrate during reflow soldering process using heated tip. As a result of control the temperature at interface of solder joints, variation of initial strength at solder joint decreases from about $\pm40%$ to $\pm20%$, and it is realized Pb free soldering process using Sn/In and Sn-Ag solder paste.

  • PDF