In this paper, sol-gel-spin coated $Pb(ZrTi)O_3$ thin film with $ZrO_2$ buffer-layer and $PbTiO_3$ seed-layer was investigated for vibration MEMS energy harvester to scavenge power from ambient vibration via d33 piezoelectric mode. Piezoelectric thin film deposition techniques on insulating layer is the important key for $d_{33}$ mode of piezoelectric vibration energy harvester. $ZrO_2$ buff-layer was utilized as an insulating layer. $PbTIO_3$ seed-layer was applied as an inter-layer between PZT and $ZrO_2$ layer to improve the crystalline of PZT thin film. The fabricated PZT thin film had a remanent polarization of 5.3uC/$cm^2$ and the coercive field of 60kV/cm. The fabricated energy harvester using PZT thin film with PTO seed-layer generated 1.1uW of electrical power to $2.2M{\Omega}$ of load with $4.4V_{pvp}$ from vibration of 0.39g at 528Hz.
The structures of two VBS (viral binding site) RNAs, SL1 and SL2, of Yeast Saccharomyces cerevisiae vims have been studied by 2D and 3D NMR experiments. VBSs play a crucial role in viral particle binding to the plus strand and packaging of the RNA. The secondary structures of the two VBS RNAs share a common feature of the stem-internal loop-stem-hairpin loop structure although the size of the internal loops of SL1 and SL2 differs. 2D experiments were sufficient for fill assignments of SL1. However, isotope labeling of the sample and multidimensional experiments were required for 28-nucleotide-long SL2 due to the spectral overlap. Several 3D HCCH experiments have accomplished full assignment of SL2 RNA.
In this study, after measuring polarization characteristics of 97.3 wt% Ag, Au-Coated 97.3 wt% Ag (ACA) and 100 wt% Au wires in 1 wt% H2SO4 and 1 wt% HCl electrolytes at 25 ℃, corrosion rate and corrosion characteristics were comparatively analyzed. Comparing corrosion potential (ECORR) values in sulfuric acid solution, ACA wire had more than six times higher ECORR value than Au wire. Thus, it seems possible to use a broad applied voltage range of bonding wire for semiconductor packaging which ACA wire could be substituted for the Au wire. However, since the ECORR value of ACA wire was three times lower than that of the Au wire in a hydrochloric acid solution, it was judged that the use range of the applied voltage and current of the bonding wire should be considered. In hydrochloric acid solution, 97.3 wt% Ag wire showed the highest corrosion rate, while ACA and Au showed similar corrosion rates. Additionally, in the case of sulfuric acid solution, all three types showed lower corrosion rates than those under the hydrochloric acid solution environment. The corrosion rate was higher in the order of 97.3 wt% Ag > ACA > 100 wt% Au wires.
본 연구에서는 솔더 분말 크기에 따른 솔더페이스트의 젖음성 및 레올로지 특성을 평가하였다. 솔더페이스트는 T4 (20~28 ㎛), T5 (15~25 ㎛), T6 (5~15 ㎛) 3종류의 Sn-Ag-Cu 합금 분말을 사용하였고, 플럭스와 진공에서 혼합하여 솔더페이스트를 제조하였다. 스파이럴 점도계로 10 rpm의 속도로 측정했을 때 T4, T5, T6 솔더페이스트의 점도는 각각 155, 263, 418 Pa·s의 점도를 보이며, 분말크기가 감소함에 따라 점도는 증가되는 것이 관찰되었다. 또한, 솔더페이스트의 경시변화에 따른 점도변화를 관찰하였으며, 7일 후 T4 솔더페이스트의 경우 점도가 2.6% 증가하여 거의 변화가 없었으나, T5는 20.6%의 증가를 보였으며, T6의 경우 점도 증가가 매우 높아 스파이럴 점도계로는 측정이 불가하였다. 분말 크기에 따른 솔더페이스트 점도 특성은 솔더의 인쇄성에 큰 영향을 주었다. T4 솔더페이스트의 경우 인쇄특성 및 슬럼프와 브릿징 특성이 우수하였지만, 분말 크기가 작은 T5의 경우 인쇄성이 다소 떨어졌으며, T6의 경우 점도가 높아 솔더페이스트가 마스크 개구홀의 벽에 붙고, 따라서 인쇄성이 매우 떨어지는 모습을 보였다. 솔더링을 진행할 경우, T6 솔더페이스트는 디웨팅(dewetting)이 발생하여 젖음성도 T4, T5에 비해 낮은 것이 관찰되었다.
The effects of organic acids mix (0.4%) and modified atmosphere packaging (MAP) on the storage quality of sliced bacon were investigated. Pork bellies were treated with or without organic acids at the curing stage. The organic acids mix comprised 35% sodium acetate, 25% salt, 15% calcium lactate, 11% trisodium citrate, 7% ascorbate, and 7% citric acid. The cured pork bellies were smoked and packaged with 50% $CO_2$ + 50% $N_2$ (50% $CO_2$-MAP) and 100% $N_2$ (100% $N_2$-MAP), and stored at $5^{\circ}C$ for 14 d. The 50% $CO_2$-MAP showed a higher pH value (p<0.05) up to 10 d, a lower protein deterioration (p<0.05) as measured by volatile basic nitrogen (VBN) from 6 to 14 d, and a higher color value of lightness (CIE $L^*$) compared to 100% $N_2$-MAP. The development of lipid oxidation measured by thiobarbituric acid reactive substance (TBARS) values seemed to be effectively controlled throughout the storage period in both 50% $CO_2$-MAP and 100% $N_2$-MAP regardless of the application of organic acids. The 50% $CO_2$-MAP inhibited the growth of aerobic and anaerobic bacteria (p<0.05) both in non-added and bacon added with organic acids mix. The 50% $CO_2$-MAP alone seemed to be effective in delaying the growth of bacteria since the use of organic acids mix gave no additional effects. The addition of organic acids mix lowered the pH value (p<0.05), effectively retarded the protein deterioration (p<0.05), and showed a higher color value of lightness (CIE $L^*$) value (p<0.05) and lower color value of redness (CIE $a^*$) value (p<0.05). In conclusion, 50% $CO^2$-MAP showed better quality and self-life of sliced bacon during storage. However, the beneficial effect of organic acids mix was not noticed in the concentration used in this experiment.
Powdered infant formula is susceptible to oxidation in the presence of oxygen. Even though the product is usually packaged in nitrogen atmosphere, the oxygen ingress through the package layer may occur in case of flexible pouches and affects the oxidation of the product. $O_2$ barrier of the package is thus important variable to protect the product from oxidative deterioration. $O_2$ barrier property was investigated for aluminum-laminated small pillow packs of $3.5{\times}17.5cm$. Storage temperature and combination of primary and secondary packages were evaluated as variables affecting the barrier for conditions of empty pouch flushed with nitrogen. Apparent oxygen transmission rate of the primary package exposed to air was $2.32{\times}10^{-3}mL\;(STP)\;atm^{-1}\;d^{-1}$ at $30^{\circ}C$ and its temperature dependence could be explained by activation energy of $28.5kJ\;mol^{-1}$ in Arrhenius relationship. The additional secondary package of nylon/PE film containing 20 primary packages was ineffective in modulating package $O_2$ transmission and was only marginally helpful when combined with oxygen scavenger. The same was true in suppressing the product oxidation when the primary package was filled with 14 g of the formula.
Tn this paper, PCB (Printed Circuit Board) embedded $BaTiO_3$ MIM capacitors were designed, fabricated, and characterized for low cost organic SOP applications by using 3-D EM simulator and low temperature processes. Size of electrodes and thickness of high dielectric films are optimized for improving the performance characteristics of the proposed embedded MIM capacitors at high frequency regime. The selected thicknesses of the $BaTiO_3$ film are $12{\mu}m$, $16{\mu}m$, and $20{\mu}m$. The fabricated MIM capacitor with dielectric constant of 30 and thickness of $12{\mu}m$ has capacitance density of $21.5p\;F/mm^2$ at 100MHz, maximum quality factor of 37.4 at 300 MHz, a quality factor of 30.9 at 1GHz, self resonant frequency of 5.4 GHz, respectively. The measured capacitances and quality factors are well matched with 3-D EM simulated ones. These embedded capacitors are promising for SOP based advanced electronic systems with various functionality, low cost, small size and volume.
MCM-D 기판에 수동소자를 내장시키는 공정을 개발하였다. MCM-D 기판은 Cu/감광성 BCB를 각각 금속배선 및 절연막 재료로 사용하였고, 금속배선은 Ti/cu를 각각 1000$\AA$/3000$\AA$으로 스퍼터한 후 fountain 방식으로 전기 도금하여 3 um Cu를 형성하였으며, BCB 층에 신뢰성있는 비아형성을 위하여 BCB의 공정특성과 $C_2F_6$를 사용한 플라즈마 cleaning영향을 AES로 분석하였다. 이 실험에서 제작한 MCM-D 기판은 절연막과 금속배선 층이 각각 5개, 4개 층으로 구성되는데 저항은 2번째 절연막 위에 thermal evaporator 방식으로 NiCr을 600$\AA$증착하여 시트저항이 21 $\Omega$/sq가 되게 형성하였고. 인덕터는 coplanar 구조로 3, 4번째 금속배선층에 형성하였으며, 커패시터는 절연막으로 PECVD $Si_3N_4$를 900$\AA$증착한 후 1, 2번째 금속배선층에 형성하여 88nF/$\textrm {cm}^2$의 커패시턴스를 얻었다. 이 공정은 PECVD $Si_3N_4$와 thermal evaporation NiCr 공정을 이용함으로써 기존의 반도체 공정을 이용하여 MCM-D 기판에 수동소자를 안정적으로 내장시킬 수 있었다.
TSV기술은 실리콘 칩에 관통 홀(through silicon via)을 형성하고, 비아 내부에 전도성 금속으로 채워 수직으로 쌓아 올려 칩의 집적도를 향상시키는 3차원 패키징 기술로서, 와이어 본딩(wire bonding)방식으로 접속하는 기존의 방식에 비해 배선의 거리를 크게 단축시킬 수 있다. 이를 통해 빠른 처리 속도, 낮은 소비전력, 높은 소자밀도를 얻을 수 있다. 본 연구에서는 웨이퍼 레벨에서의 TSV 충전 경향을 조사하기 위하여, 실리콘의 칩 레벨에서부터 4" 웨이퍼까지 전해 도금법을 이용하여 Cu를 충전하였다. Cu 충전을 위한 도금액은 CuSO4 5H2O, H2SO4 와 소량의 첨가제로 구성하였다. 양극은 Pt를 사용하였으며, 음극은 $0.5{\times}0.5 cm^2{\sim}5{\times}5cm^2$ 실리콘 칩과 4" 실리콘 wafer를 사용하였다. 실험 결과, $0.5{\times}0.5cm^2$ 실리콘 칩을 이용하여 양극과 음극과의 거리에 따라 충전률을 비교하여 전극간 거리가 4 cm일 때 충전률이 가장 양호하였다. $5{\times}5cm^2$ 실리콘 칩의 경우, 전류 공급위치로부터 0~0.5 cm 거리에 위치한 TSV의 경우 100%의 Cu충전률을 보였고, 4.5~5 cm 거리에 위치한 TSV의 경우 충전률이 약 95%로 비아의 입구 부분이 완전히 충전되지 않는 경향을 보였다. 전극에서 멀리 떨어져있는 TSV에서 Cu 충전률이 감소하였으며, 안정된 충전을 위하여 전류를 인가하는 시간을 2 hrs에서 2.5 hrs로 증가시켜 4" 웨이퍼에서 양호한 TSV 충전을 할 수 있었다.
ENIG 층의 결함구조를 이해하고자 immersion gold 층의 결함을 TEM 분석을 이용하여 분석하였다. 세가지 다른 종류의 금도금액을 통하여 immersion gold 층을 얻은 후 습식적으로 TEM 시편을 만들어 이를 비교하였다 이를 통해 immersion gold 도금액의 종류에 의하여 도금막의 결함구조는 크게 영향을 받음을 확인할 수 있었다. 즉, 시안형 치환형 금도금 액을 이용하여 얻은 immersion 금도금 층인 경우에는 결정계면을 따라서 결함들이 집중적으로 존재함을 관찰할 수 있었다. 반면 유기환원제를 도금액에 첨가한 시안형 부분환원형 금도금 액을 이용하여 얻은 immersion금도금 층인 경우에는 grain boundary를 따라 존재하는 공극은 사라졌지만 $5\sim20nm$ 크기의 구형의 공극이 결정계면, 결정내를 상관하지 않고 존재하고 있음을 확인할수 있었다. 이에 비하여 아황산형 치환형 금도금 액을사용하여 얻어진 금도금 층에서는 이러한 결함들이 거의 사라지는 것을 관찰할 수 있었다.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.