• Title/Summary/Keyword: 저온분무열분해

Search Result 7, Processing Time 0.022 seconds

Magnetic Properties of Sr-ferrite Powders via Modified Low Temperature Co-spray Roasting Process (저온 분무 열분해법으로 제조된 Sr-ferrite의 자기특성)

  • 김효준;조태식;남효덕;양충진
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.11 no.10
    • /
    • pp.931-939
    • /
    • 1998
  • Preparation of the hexagonal Sr-ferrite powsers with high performance by co-spraying precusor of the FeCl$_2$+SrCO$_3$ at a low temperature was proved as a cost =-effective method. The co-spray roasting was carried out in the temperature range of 300~$700^{\circ}C$ after SrCO$_3$ powders were mixed into 12FeCi$_2$.4$H_2O$ liquor. By this low temperature roasting method fine particles of multi-phased FeO$_2$+SrCO$_3$ were formulated. Powders calcined at 105$0^{\circ}C$ for 1 hour show the best magnetic property of M\ulcorner=69.96 emu/g, M\ulcorner=36.98 emu/g, and \ulcornerH\ulcorner=4.31 Oe. This calcining temperature is lower than that of the conventional dry method by 10$0^{\circ}C$.

  • PDF

An Experimental Study on Conversion of Reducing Agent from Aqueous Urea Solutions under Low Reaction Temperature (저온 반응장에서 요소 수용액의 환원제 전환에 관한 실험적 연구)

  • Ku, Kun Woo;Hong, Jung Goo
    • Journal of ILASS-Korea
    • /
    • v.20 no.1
    • /
    • pp.20-27
    • /
    • 2015
  • Urea-SCR which is one of the aftertreatment technologies for reducing the NOx emission is widely used. An experimental study was performed to investigate urea decomposition under various thermo-fluid conditions, with different temperatures and velocities of inflow gas, and urea solution quantities. 40 wt. % aqueous urea solutions were used in this study. The inflow gas conditions were similar to the exhaust conditions of a large marine engine. The spray performance of urea solution injector was identical under all experimental conditions. The conversion efficiency of $NH_3$ was larger than that of HNCO under all experimental conditions, unlike for the theoretical thermolysis reaction.

Synethisis of fine BSCCO precursor powder by spray pyrolysis (분무 열분해에 의한 미세 BSCCO 전구체 분말의 합성)

  • 김성환;유재무;고재웅;김영국;박성창
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 2003.10a
    • /
    • pp.99-102
    • /
    • 2003
  • Many researches on synthesis process for BSCCO precursor powders have been developed for high J$_{c}$ BSCCO-2223/Ag tape. Spray pyrolysis method for fabrication of precursor powder has many advantages, such as high purity, fine particle size of BSCCO precursor powder. Fine, spherical powders were prepared by ultrasonic spray pyrolysis from the aqueous solution of metal nitrates. BSCCO precursor powders were synthesized with 0.1 M concentration and heat treatment conditions. Average particle size for spray pyrolysis powders was 1.5 ~ 3 ${\mu}{\textrm}{m}$. BSCCO -2223/Ag tape was prepared by PIT method and followed by various sintering conditions. The critical current density of BSCCO-2223/Ag tape sintered in low oxygen partial pressure was ~ 23 kAcm$^{-2}$.

  • PDF

Preparation of Hexaaluminate Phosphor Particles with Spherical Shape by Gas Phase Reaction Process (기상 공정에 의한 구형 형상의 헥사알루미네이트계 형광체 제조)

  • Jung, Dae Soo;Hong, Seung Kwon;Koo, Hye Young;Ju, Seo Hee;Kang, Yun Chan
    • Korean Chemical Engineering Research
    • /
    • v.43 no.5
    • /
    • pp.616-620
    • /
    • 2005
  • The morphology and photoluminescence characteristics of green light emitting hexaaluminate phosphor particles prepared by high temperature spray pyrolysis from spray solution with and without ammonium dihydrogen phosphate flux were investigated. The particles prepared from spray solution without flux material had hollow morphology at preparation temperatures between $900^{\circ}C$ and $1,650^{\circ}C$. Ammonium dihydrogen phosphate flux added into spray solution enabled the formation of particles with spherical shape and filled morphology at preparation temperatures between $900^{\circ}C$ and $1,650^{\circ}C$. The hexaaluminate phosphor particles with magnetoplumbite structure were directly prepared by spray pyrolysis from spray solution with ammonium dihydrogen phosphate flux above $1,600^{\circ}C$. Ammonium dihydrogen phosphate flux was effective in improving the photoluminescence intensity of the phosphor particles at low preparation temperatures. The phosphor particles prepared from spray solution with and without flux material by spray pyrolysis under reducing atmosphere at $1,650^{\circ}C$ had comparable photoluminescence intensities with that of the phosphor particles optimized by post-treatment.

Synthesis of Carbon-Supported Pt-Ru Catalysts using a Flame Spray Pyrolysis Method for Fuel Electrode of Low Temperature Fuel Cell (화염분무열분해 공정을 이용한 저온 연료전지 연료전극용 탄소담지 Pt-Ru 촉매의 제조)

  • Lee, Hyun-Min;Lee, Dong-Geun
    • Particle and aerosol research
    • /
    • v.8 no.2
    • /
    • pp.69-74
    • /
    • 2012
  • This study describes how successfully a conventional flame aerosol synthesis was used to continuously synthesize Pt-Ru catalysts supported by carbon agglomerates. Nearly spherical catalysts produced in the flame were mainly composed of metallic Pt and Ru with the molar ratio of 1:1 and those sizes were controllable from ~1.5 nm to ~2.0 nm. Nevertheless, only Pt peaks were found from X-ray diffraction experiments, suggesting that amorphous-like Ru was well mixed in the crystalline Pt lattices. It was found from Cyclo-voltamograms and CO stripping experiments that the electrochemical properties of the catalysts are at least comparable to that of a conventional commercial sample.

Synthesis of $MgB_2$ powders by ultrasonic spray pyrolysis (초음파 분무열분해를 이용한 $MgB_2$ 분말 합성)

  • Park, S.C.;Lim, Y.J.;Kang, S.G.;Chung, J.K.;Kim, C.J.;Kim, C.J.
    • Progress in Superconductivity and Cryogenics
    • /
    • v.10 no.1
    • /
    • pp.19-23
    • /
    • 2008
  • Spherical $MgB_2$ powders was synthesized with the ultrasonic spray pyrolysis(USP) process using aqueous solutions of boron and magnesium ion. The properties of synthesized $MgB_2$ powder were characterized by XRD, SEM and EDS. A small amount of MgO was detected as the secondary phase out of the synthesized powder and the ratios of $MgB_2$ to MgO increased with increasing furnace temperature. The particle size and morphology of $MgB_2$ powder were investigated with varying molar concentration of the boron and magnesium solution and furnace temperature between $600^{\circ}C$ and $1000^{\circ}C$ in $Ar/H_2$. The average particle size of $MgB_2$ showed narrow distribution ranging from 300nm to 400nm. The morphology of particles exhibited mostly spherical shapes and uniform distribution.

The synthesis and formation mechanism of the fine $BaTiO_3$ powders by ultrasonic spray pyrolysis (초음파 분무 열분해법에 의한 $BaTiO_3$ 미분말의 합성 및 형성기구 규명)

  • Heo, H.B.;Shin, K.C.
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.4 no.2
    • /
    • pp.178-189
    • /
    • 1994
  • Fine $BaTiO_3$ powder was synthesized from the various starting solution with 0.05 M by ultrasonic spray pyrolysis method. The conditions of synthesis were fixed on flow rate was 0.5 cm/sec, low temperature furnace was $300^{\circ}C$, and high temperatures furnace was $700^{\circ}C$. The formation procedure was investigated directly by SEM with the collected particle from the each reaction step. Also, the trace of particle in reaction tube was researched theoretically. Fine $BaTiO_3$ was synthesized only in the case of nitrate aqueous solution. The synthesized $BaTiO_3$ powder was porous and spherical which was consist of primary particle at the size of 19.1 nm. The formation procedure was as follows : the particle size decreased in drying step and then increased in initial thermal decomposition step. Finally, particle size was decreased to $0.42 {mu}m$. The trace of particle in reaction tube was also theoretically simulated and discussed.

  • PDF