  • This study was performed with the questionnaire survey on mercury knowledge and mercury exposure avoidance behavior, which was conducted among 1076 dental personnel in September, 2004. As for the factors effecting the mercury knowledge, it seems that they are closely related with the personnel's educational backgrounds, and their understandings of causing environmental hazardousness in the dental offices. And also, the factors effecting the behavior of mercury exposure avoidance are strongly connected with the knowledge points on mercury, the knowledge of air states in the dental clinic offices, the use of pincettes and gloves in squeezing, and rubber dam and gloves in mulling, the experience of environmental education on mercury, etc. In the survey, the higher points in mercury knowledge is closely related with the higher points in the behavior of mercury exposure avoidance. Nevertheless, the very fact that the lower points in the behavior among personnel takes on the aspect of the relatively higher points in knowledge on mercury may be understood that the generally acquired knowledge on mercury cannot be the critical factor of the behavior of mercury exposure avoidance.

A study on the production techniques of ancient gilding-Focus on the mercury amalgam gilding (고대 도금 제작 기술에 관한 연구-수은 아말감 도금법을 중심으로)

  • Han, Min-Su;Hwang, Jin-Ju;Moon, Whan-Suk
    • 보존과학연구
    • /
    • s.23
    • /
    • pp.113-129
    • /
    • 2002
  • This study is to disclose the gilding technique and distinctive features of using surface improvement technique in ancient gilt. There are many kinds of the ancient gilding technique so this thesis mainly focused on mercury amalgam gilding. Gilding technique can be largely divided into two branches – the cladding and amalgam method - in ancient periods. The researches have been carried out on two parts; the first is to find the making progress of amalgam on all sort of the gilding materials and the second is to show features of the gilded layer among basic metals. As a result of this experiment, to achieve good quality of amalgam, suitable particle size of the gilding material should be needed and the heating, a primary factor, has an effect on amalgam to be formed. Aspecial features of amalgam gilding, according to changing the basicmetal, would be influenced by chemical attraction for the mercury, condition of the surface and some other factors. A platers abilities and the making progress of amalgam would be influenced by a uniform and good gilding layer. In conclusion, it should be profoundly studied and investigated on the ancient gilding techniques and gold-gilt relics.

  • PDF

COMPARISON OF MICROLEAKAGE OF GALLIUM ALLOY AND AMALGAM RESTORATION (갈륨과 아말감 수복물의 변연미세누출에 관한 비교 연구)

  • Lee, Min-Ho;Lee, Hee-Joo;Hur, Bock
    • Restorative Dentistry and Endodontics
    • /
    • v.23 no.1
    • /
    • pp.269-277
    • /
    • 1998
  • This in vitro study compared the microleakage of 4 lining conditions when used with Gallium alloy GF II and Valiant PhD. Class V cavity was prepared on both buccal and lingual surface of 80 extracted human premolar & molar teeth with one margin in enamel and another in dentin. Before restoration, prepared cavities were applied to no-liner, cavity varnish, Scotchbond multipurpose, and Superbond D-liner II plus according to manufacture's instructions. The restored teeth were stored in saline for 1 week, then thermocycled for 100 times, stained with 0.5% basic fuchsin dye for 1 day, sectioned, and observed using a light microscope. Following results were obtained. 1. The leakage value of Superbond-lined group showed significantly lower than that of nolined group on both margins of Valiant PhD(p<0.05). 2; There was no significant difference between the 4 lining conditions in Gallium alloy GF II (p>0.05). 3. When We make a comparison between Gallium alloy GF II and Valiant PhD under same lining conditions, the microleakage value of Gallium alloy GF II showed lower than that of Valiant PhD on occlusal & gingival margin(p<0.05) except for Superbond-lined group(p>0.05).

  • PDF

Conservation and Analysis of Gilding Silver Buddhas and Relics Discovered Inside Buddha of Joseon Period (조선시대 은제금도금불상과 그 복장품의 보존처리 및 재질연구)

  • Kwon, Yoonmi;Park, Seungwon;Yu, Heisun;Choi, Heeyoon;Yun, Eunyeong
    • Conservation Science in Museum
    • /
    • v.9
    • /
    • pp.31-49
    • /
    • 2008
  • We have investigated and conserved three small Buddha statues dating from Joseon period that were purchased by the National Museum of Korea. Chemical analysis and investigation of internal structures were enabled us to identify its compositions and hollow spaces which have various materials just like fabrics, silver ornaments, beads and wood fragments. The fabrics date from the early years of the Joseon dynasty to the middle one. The compositions of matrix of the Buddha statues vary 80-90 wt% Ag and 7-15 wt% Cu. And its surface layers were gilt with amalgam. Mechanical and chemical cleaning with EDTA-2Na were applied together during the cleaning process.

A STUDY ON THE MICROSTRUCTURE TRANSFORMATION IN SPHERICAL-DISPERSED TYPE AMALGAM (아말감충전물(充塡物)의 미세구조(微細構造) 변화(變化)에 관(關)한 연구(硏究))

  • Chang, Sang-Kohn;Min, Byeong-Sun;Park, Sang-Jin;Choi, Ho-Young
    • Restorative Dentistry and Endodontics
    • /
    • v.9 no.1
    • /
    • pp.81-87
    • /
    • 1983
  • The purpose of this study was to observe and identify the phases of amalgam and to know the transformation of microstructure in the set amalgam by lapse of time. In this study, shofu spherical-D alloy was used. After trituration of amalgam alloy and mercury (Wig-L-Bug), it was filled in the stone dies. This specimens being polished and etched by usual method was observed under optical microscope using metallurgical microscope. And then X-ray diffractometer was used to analyze the phases contents and transformation of microstructure at $2{\frac{1}{2}}$ hours, 15 hours, 28 hours and 2 years after being amalgamated. The following results were obtained: 1. Shofu spherical-D alloy powder was composed of ${\gamma}$ phase, ${\epsilon}$phase and Ag-Cu eutectic phases. 2. ${\gamma}_2$ phases were appeared at $2{\theta}$ values ($32.0^{\circ}$ and $43.8^{\circ}$) in the amalgam which was analyzed at $2{\frac{1}{2}}$ hours and 15 hours after trituration with mercury. 3. In the amalgam at 28 hours, ${\gamma}_2$ phase was found at $2{\theta}$ value ($43.8^{\circ}$) at 35 hour, $r_2$ phase was appeared at $2{\theta}$ value $32.0^{\circ}$. 4. No ${\gamma}_2$ phases were observed in the 2 years old amalgam. But ${\eta}$ ($Cu_6Sn_5$) phases were found at $2{\eta}$ values $29.4^{\circ}$ and $42.4^{\circ}$.

  • PDF

A Literature Review on Cracked Teeth (균열치 증후군에 대한 문헌고찰)

  • Cho, Woong-Rae;Kim, Dae-Gon;Park, Chan-Jin;Cho, Lee-Ra
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.27 no.3
    • /
    • pp.305-316
    • /
    • 2011
  • Cracked teeth are a common problem with incomplete fracture that typically shows pain on biting and temperature stimuli. The most common cause of crack is known to be the masticatory accident. Predisposing factors were aging, old restoration, and iatrogenic stress concentration, etc. Accurate diagnosis is needed for detecting the extent of crack and pulp vitality. There are many diagnostic tools like bite test, direct observation with transillumination, dye penetration, and radiographs. Immediate treatment for pain relief and occlusal adjustment would be needed. Composite resin and bonded amalgam showed favorable prognosis. Moreover, cusp protection is reliable permanent treatment for cracked teeth. The purpose of this article is to review the literature about the prevention, diagnosis, and treatment for cracked teeth.

A Study on Conservation and Manufacturing Technique of Saddle Ornament(Angyo) Excavated from South Tomb Hwangnamdaechong (황남대총 남분 출토 용문투조은판피안교의 보존과 제작기법 연구)

  • Kwon, Heehong;Jeon, Hyosoo;Yun, Eunyoung
    • Conservation Science in Museum
    • /
    • v.12
    • /
    • pp.59-69
    • /
    • 2011
  • The conservation treatment and production technique of Yongmuntujoeunpanpi-Angyo(Saddle Ornament) at Hwangnamdaechong were: The conservation treatment removed foreign material by using both chemical method and physical method to reinforce and to recover area by jointing that was destroyed and weakened. Not only Angyogeumgu but also Jwamokseongeumgu was made of 99wt% or more silver (Ag), and Wondujeong, Naeyeongeumgu and Bokryung were produced by amalgam gold plaiting. Not only Angyogeumgu but also Jwamokseongeumgu that was cast with silver plate was jointed by folding both and putting Naeyeongeumgu on it and then nailing gild ofwondujeong at specific interval. A tree that grew up in curve was used, and it was adhered by plain weave fabric of hemp cloth and wool.

A BIOLOGICAL EVALUATION OF HIGH COPPER AMALGAM AND GLASS IONOMER-SILVER CEMENT (고동아말감과 Glass ionomer-silver cement의 생물학적 평가에 관한 연구)

  • Oh, Boeng-Won;Choi, Ho-Young;Min, Byung-Soon;Park, Sang-Jin
    • Restorative Dentistry and Endodontics
    • /
    • v.15 no.2
    • /
    • pp.1-16
    • /
    • 1990
  • This study was to evaluate the cytotoxic effect in vitro and the tissue response within the rat peritoneal cavity to high copper amalgam and glass ionomer-silver cement, suggested for use as a retrograde endodontic filling material. In the cytotoxicity experiment, the radioactively ($^{51}Cr$) labeled L929 mouse fibroblasts were employed to determine the relative cytotoxicity of two experimental materials. Those materials were evaluated immediately after set and after one and seven days setting. In the tissue response experiment, two experimental materials were to evaluate mean peritoneal cellular count, differential cell count and the content of silver and copper in pooled packed cells and eluate samples taken by peritoneal lavage technique, and compared with surgical control after one day. two, four and six weeks of implantation. The results were as following: 1. High copper amalgam exhibited significant cytotoxicity immediately after set but showed no sign of toxicity after one day and seven days setting materials. 2. Glass ionomer-silver cement showed no sign of toxicity immediately after set and after one day and seven days setting. 3. High copper amalgam and glass ionomer-silver cement groups produce no significant difference in the mean peritoneal cell count when compared with the surgical control group after one day, two and four weeks of implantation. Surgical control group exhibited significantly a greater cell count when compared with the High copper amalgam group after six weeks. 4. High copper amalgam group increased significantly in the percentage macrophages after four and six weeks of implantation when compared with surgical control group. 5. The trace metal analysis involved an increased silver content in the elutes and an increased copper content in the packed cells of high copper amalgam group, and an increased silver content in the packed cells and elutes of glass ionomer-silver cement group.

  • PDF

THE EFFECT OF THE POLYSTYRENE LINER ON MICROLEAKAGE OF AMALGAM RESTORATION (Polystyrene 이장재가 아말감 변연부 미세누출에 미치는 영향)

  • Lee, Kyoung-Sun;Ro, Byeng-Duck;Youn, Tai-Cheol
    • Restorative Dentistry and Endodontics
    • /
    • v.23 no.2
    • /
    • pp.586-596
    • /
    • 1998
  • Amalgam is one of the most commonly used dental restoration material because of its convenience, economic and physical properties. But microleakage in the tooth and amalgam interface has been its major problem, and many efforts have been made to overcome this shortcoming. The purpose of this study is to compare the effect of various liners on microleakage of amalgam restoration. Cavities were prepared on the buccal or lingual surface of ninety sound, extracted human premolars and six different liners (Tubulitec$^{(R)}$, Superbond D-liner II Plus$^{(R)}$, Superbond D-liner II Plus$^{(R)}$ with polymer, Scotchbond Multipurpose Plus$^{(R)}$, Copalite$^{(R)}$, No liner) were unapplied according to manufacturer's instructions and amalgam had been condensed immediately. The specimens were thermocycled by dipping in methylene blue dye at $5^{\circ}C$ and $55^{\circ}C$ for 1500 cycles. The amalgam-tooth interface was examined under stereobinocular microscope and the dye penetration was scored. The results were as follows : 1. The Tubulitec$^{(R)}$ group showed less microleakage than no liner or Copalite$^{(R)}$ group (p<0.01). 2. The Tubulitec$^{(R)}$, Superbond D-liner II Plus$^{(R)}$, Superbond D-liner II Plus$^{(R)}$ with polymer and Scotch bond Multipurpose Plus$^{(R)}$ groups were not significantly different. 3. The Copalite$^{(R)}$ and Scotchbond Multipurpose Plus$^{(R)}$ groups were not significantly different. Using the polystyrene liner and resin liners under admixed type of high-copper amalgam restoration significantly reduced microleakage in the tooth-amalgam interface. Further clinical studies on polystyrene liner are recommended.

  • PDF

MICROLEAKAGE EVALUATION IN AMALGAM RESTORATIONS USED WITH BONDING AGENTS (수종의 접착제를 사용한 아말감 수복시의 미세 변연 누출에 관한 연구)

  • Choi, Sang-Cheol;Park, Joon-Il;Kwom, Hyuk-Choon
    • Restorative Dentistry and Endodontics
    • /
    • v.22 no.1
    • /
    • pp.447-463
    • /
    • 1997
  • The purpose of this study was to evaluate the effectiveness of copal varnish and five bonding agents(Scotchbond Multi-Purpose Plus Dental Adhesive System, Panavia 21, All Bond 2, Superbond D-Liner II plus, Fuji Duet) in reducing microleakage under amalgam restorations. Class V cavity were prepared on both buccal and lingual surface of sixty extracted human molars with cementum margin and were filled with different kinds of liners and amalgam. All teeth were stored at $37^{\circ}C$ in physiologic saline solution. After 1 week they were thermally stressed for 500 cycles between 5 and $55^{\circ}C$ in baths containing 0.5 % basic fuchsin dye. The dye penetrations were observed with a stereomicroscope. Scanning electron micrographs were taken of representative tooth sections from each group to assess the nature of the tooth/liner/amalgam interface. The statistical test were applied to the results using a one way analysis variance (ANOVA) and Duncan's multiple range test. The results were as follows ; 1. In all groups, the enamel margin showed significantly lower leakage value than the cementum margin (p<0.05). 2. At the dentin and enamel margins, the leakage value of Copalite-lined group showed significantly higher than that of no liner group (p<0.05), but showed significantly lower than that of bonding agent lined-groups (p<0.05). 3. There was no significant difference between the bonding agent lined-groups (p>0.05). 4. On the backscattered scanning electron microscopy observation, discontinuous gaps were observed between amalgam and dentin in the bonding agent-lined amalgam restorations and the bonding agents appeared to fill the gap space and were mixed with amalgam particles. At the amalgam/tooth interface, unsealed dentin and continuous gaps were found in both unlined and Copalite-lined restorations.