• Title/Summary/Keyword: 모르타르의 공학적 특성

Search Result 94, Processing Time 0.022 seconds

Effect of the Replacement Ratio and Sources of Blast Furnace Slag Powder on the Fundamental Properties of Recycled Fine Aggregates Based Mortar (고로슬래그 미분말의 산지 및 치환율 변화가 순환잔골재 사용 시멘트 모르타르의 특성에 미치는 영향)

  • Han, Cheon-Goo;Zhao, Yang
    • Journal of the Korea Institute of Building Construction
    • /
    • v.15 no.3
    • /
    • pp.257-263
    • /
    • 2015
  • In this study, the quality of blast furnace slag and the engineering properties of recycled aggregate based mortar with variable replacement of blast furnace slag have been focused. Blast furnace slag(BS) manufactured in various areas in Korea were prepared for this study. For the investigation results, 4 types(among the all of 9 types) of the experimental results were identified as below the standard level when using blast furnace slag chosen from different factories. Especially the particle size of the blast furnace slag was considered as the largest problem. When using BS in the recycled aggregates based mortar, the increase amount of blast furnace slag, increased the fluidity but delayed the setting time and decreased strength at early age. Based on the relationship of the amount of BS and the engineering properties of mortar, this study found that the amount of $SO_3$ and L.O.I affect the setting time, 3 days strength and 91 days strength to the certain standard level.

An Experimental Study on Engineering Properties of Self-healing Mortar according to PCC(Powder Compacted Capsule) Size and Mixing Ratio (PCC(Powder Compacted Capsule) 크기 및 혼입율에 따른 자기치유 모르타르의 공학적 특성에 관한 실험적 연구)

  • Jae-In, Lee;Chae-Young, Kim;Se-Jin, Choi
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.10 no.4
    • /
    • pp.514-522
    • /
    • 2022
  • In this study, as part of a study to improve the self-healing performance of concrete structures by applying self-healing capsules made of cementitious materials to cement composite materials, the engineering characteristics of mortars according to PCC(Powder Compacted Capsule) size and mixing ratio were compared and analyzed. For this, fluidity, compressive strength, reload test, carbonation, ultrasonic velocity, and water permeability characteristics were measured according to PCC size and mixing ratio of mortar. As a result of the measurement, the fluidity and compressive strength increased as the mixing ratio of PCC increased, and in the case of the load reload test, the healing ratio increased as the mixing ratio of PCC increased in the 03PC formulation. In the case of water permeability test, it was found that when PCC was used, the reduction ratio of water flow was up to 35 % higher than that of Plain, and when PCC with a size of 0.3 to 0.6 mm was mixed with 15 %, it was found to be effective in improving the crack healing ratio of the mortar.

An Experimental Study on the Engineering Characteristics of Ternary Lightweight aggregate Mortar Using Recycling Water (회수수를 사용한 3성분계 경량 골재 모르타르의 공학적 특성에 관한 실험적 연구)

  • Lee, Jae-In;Bae, Sung-Ho;Kim, Ji-Hwan;Choi, Se-Jin
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.10 no.1
    • /
    • pp.48-55
    • /
    • 2022
  • This study uses the recovered water as mixing water and artificial lightweight aggregate pre-wetting water as part of a study to increase the recycling rate and reduce greenhouse gas of the ready-mixed concrete recovered during the concrete transport process, and cement fine powder of blast furnace slag(BFS) and fly ash(FA). The engineering characteristics of the three-component lightweight aggregate mortar used as a substitute were reviewed. For this purpose, the flow, dry unit mass, compressive strength, drying shrinkage, neutralization depth, and chloride ion penetration resistance of the three-component lightweight aggregate mortar were measured. When used together with the formulation, when 15 % of BFS and 5 % of FA were used, it was found to be positive in improving the compressive strength and durability of the mortar.

Evaluation of Mechanical Properties and Alkali-Silica Reaction of High Strength Mortar Using Waste Glass Sand (폐유리 잔골재를 치환한 고강도 모르타르의 역학적 특성 및 알칼리-실리카 반응 평가)

  • Eu, Ha-Min;Kim, Gyu-Yong;Choe, Gyeong-Cheol;Son, Min-Jae;Nam, Jeong-Soo
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.8 no.4
    • /
    • pp.528-536
    • /
    • 2020
  • In this study, high strength mortar and normal strength mortar using waste glass sand were evaluated. The main parameters studied were mechanical properties, alkali-silica reaction(ASR) and residual mechanical properties after ASR. As a result of this experiment, it was found that the increase in strength of the mortar has a limitation in improving the slip of the waste glass sand(GS), and rather, it causes a larger ASR. However, the possibility of improving the slip of GS was confirmed by the temporary increase of initial residal compressive and flexural strength of the mortar containing GS after the ASR. Therefore, to improve the slip of GS, the additional research is required, such as modification of the surface of GS and the incorporation of a binder which can increase the strength and makes matrix compact.

Engineering Properties of the Non-Cement Mortar using the Fly ash from Combined Heat Power Plant and Recycled Fine Aggregate (열병합발전소 플라이애시와 순환잔골재를 사용한 무시멘트 모르타르의 공학적 특성)

  • Nam, Han-Kook;Lim, Jeong-Geun;Lee, Sang-Soo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.15 no.6
    • /
    • pp.553-559
    • /
    • 2015
  • In this study, to suggest the application method of recycled fine aggregate, the non-cement mortar was prepared and studied with the binders of blast furnace slag, fly ash, and fly ash from combined heat power plant. As a basic experiment, a series of tests was conducted to determine the potions of the binders and types of activator. When the binder was consisted with 20% of fly ash and 40% of fly ash from combined heat power plant, the highest strength of the mortar was obtained, and as an activator, the combination of sodium hydroxide 2.5%, and calcium hydroxide 7.5% showed the highest strength of the mortar. Therefore, this study focuses on engineering properties of mortar contains fly ash from combined heat power plant and recycled fine aggregate according to replacement ratio of recycled fine aggregate based on the optimum mix from the basic experiment. As a result, the best replacement ratio of recycled fine aggregate is 75%.

Effect of blast-furnace slag particle fineness changes on the engineering characteristics of mortar (고로슬래그 미분말의 분말도 변화가 모르타르의 공학적 특성에 미치는 영향)

  • Lee, Jae-Jin;Moon, Byeong-Ryong;Park, Yong-Jun;Joo, Eun-Hui;Han, Min-Cheol;Han, Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2016.10a
    • /
    • pp.102-103
    • /
    • 2016
  • Recently on construction sites, there is increased use of concrete with large quantities of blast-furnace slag(BS) admixture replacements, for purposes of reducing CO2 created from cement, one of the ingredients of concrete. But such high-BS fineness changes can have a huge effect on the quality of mortar and concrete. Therefore in this study an experiment was conducted in which liquidity and intensity of mortar depending on an artificially-applied change in fineness degree at degree 7. The results, though subtle, were that the larger the fineness degree, liquidity increased and air quantity decreased, and compression and flexural strength increased.

  • PDF

Effect of Phase Change Material on Hydration Heat of Mortar with Fly Ash and Blast Furnace Slag (상전이물질이 플라이애시 및 고로슬래그를 혼입한 모르타르의 수화발열에 미치는 영향)

  • Nam, Yi-Hyun;Jang, Seok-Joon;Kim, Sun-Woong;Park, Wan-Shin;Yun, Hyun-Do
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.23 no.1
    • /
    • pp.1-8
    • /
    • 2019
  • Phase change material(PCM) has the capacity to absorb or release energy in heat when the phase changes. This study conducted to investigate the effect of strontium-based PCM on the hydration heat and mechanical properties of mortar with fly ash and blast furnace slag. The amounts of PCM were 1%, 2%, 3%, 4%, and 5% by the cementitious materials weight. The tests about mortar flow, semi-adiabatic temperature rise, compressive and flexural strength tests were carried out for twelve types of mortar mixtures. The test results indicated that the use of PCM was effective to reduce hydration heat and retard hydration of mortar with industrial by-products. In particular, the heat generation rate of mortars with fly ash was lower than that of mortars with blast furnace slag. The compressive strength of mortar with fly ash and blast furnace slag were decreased with increasing PCM ratio.

Experimental Study on Evaluation of Material Properties in Cement Mortar with Pond Ash (매립회를 사용한 시멘트 모르타르의 재료 물성 평가에 대한 실험적 연구)

  • Jung, Sang Hwa;Kim, Joo Hyung;Kwon, Seung Jun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.17 no.3
    • /
    • pp.108-117
    • /
    • 2013
  • Among the byproducts from thermal power plant using coal combustion, fly ash as mineral admixture is widely utilized in concrete manufacturing for its engineering merits. However residuals including bottom ash are usually reclaimed. This study presents an evaluation of engineering properties in cement mortar with pond ash (PA). For this work, two types of pond ash (anthracite and bituminous coal) are selected from two reclamation sites. Cement mortar specimens considering two w/c (0.385 and 0.485) ratios and three replacement ratio of sand (0%, 30%, and 60%) are prepared and their workability, mechanical, and durability performance are evaluated. Anthracite pond ash has high absorption and smooth surface so that it shows reasonable workability, strength development, and durability performance since it has dense pore structure due to smooth surface and sufficient mixing water inside. Reuse of PA is expected to be feasible since PA cement mortar has reasonable engineering performance compared with normal cement mortar.

Prediction of the Rheological Properties of Cement Mortar Applying Multiscale Techniques (멀티스케일 기법을 적용한 시멘트 모르타르의 유변특성 예측)

  • Eun-Seok Choi;Jun-Woo Lee;Su-Tae Kang
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.28 no.2
    • /
    • pp.69-76
    • /
    • 2024
  • The rheological properties of fresh concrete significantly influence its manufacturing and performance. However, the diversification of newly developed mixtures and manufacturing techniques has made it challenging to accurately predict these properties using traditional empirical methods. This study introduces a multiscale rheological property prediction model designed to quantitatively anticipate the rheological characteristics from nano-scale interparticle interactions, such as those among cement particles, to micro-scale behaviors, such as those involving fine aggregates. The Yield Stress Model (YODEL), the Chateau-Ovarlez-Trung equation, and the Krieger-Dougherty equation were utilized to predict the yield stress for cement paste and mortar, as well as the plastic viscosity. Initially, predictions were made for the paste scale, using the water-cement ratio (W/C) of the cement paste. These predictions then served as a basis for further forecasting of the rheological properties at the mortar scale, incorporating the same W/C and adding the cement-sand volume ratio (C/S). Lastly, the practicality of the predictive model was assessed by comparing the forecasted outcomes to experimental results obtained from rotational rheometer.

Characteristics of Recycled Aggregate Powder Containing Mortar Depending on Grinding Efficiency (분쇄 효율에 따른 순환골재 분말 혼입 모르타르의 특성)

  • Bang, Jinwook;Jang, Youngil;Lee, Jongwon;Mun, Seokho;Chu, Hyunseung
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.23 no.2
    • /
    • pp.116-121
    • /
    • 2019
  • In order to evaluating applicability of RAP (recycled aggregate powder) in mortar, in this study, physical and mechanical tests was carried out. Material characteristics of recycled aggregate and RAP were evaluated and the mechanical properties of mortar replaced with RAP were analyzed. Test result of sieve analysis showed that as the milling time increased the fineness modulus was decreased and the distribution of 0.6 mm particle size was found to increase. The fluidity of mortar mixture substituted with RAP tended to increase than Plain mixture. It was result that the increasing fluidity was affected by unreacted surplus water in the mortar as the binder was replaced with RAP. From the compressive strength result of the mortar subjected to RAP, it was found that the RAP was able to replace up to about 10% of unit binder weight although the compressive strength of mortar was decreased as the RAP replacement increased. From the above study, it can be concluded that the physical properties of RAP satisfied the quality standard of aggregate for replacement with fine aggregate. Moreover, in case of the RAP was replaced up to 10% of unit cement weight, it was able to be possible to improve fluidity and compressive strength of mortar.