• Title/Summary/Keyword: 단일구조 지르코니아

Search Result 46, Processing Time 0.034 seconds

Esthetic anterior restoration using 3M LavaTM Esthetic monolithic zirconia (3M LavaTM Esthetic monolithic zirconia를 이용한 전치부 심미 수복 증례)

  • Kim, Hyung Joon;Shin, Soo-Yeon
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.34 no.4
    • /
    • pp.306-316
    • /
    • 2018
  • Monolithic zirconia has been widely used in fixed partial dentures due to high strength and fracture toughness. Nevertheless, the usage of monolithic zirconia in anterior restoration was limited because of opacity. Recently, esthetic monolithic zirconia blocks are developed by improving translucency and using various shading systems. Manufacturer introduces 3M $Lava^{TM}$ Esthetic with increased cubic phase and fluorescent ingredients is more esthetic than previous monolithic zirconia. This case report describes favorable anterior restorations using translucent monolithic zirconia.

Effect of additional firing process after sintering of monolithic zirconia crown on marginal and internal fitness (단일구조 지르코니아 크라운의 소결 후 추가 소성 과정이 변연 및 내면 적합도에 미치는 영향)

  • Shin, Mi-Sun;Lee, Hyeonjong
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.57 no.4
    • /
    • pp.321-327
    • /
    • 2019
  • Purpose: To evaluate an effect of additional firing process after sintering of monolithic zirconia crown on marginal and internal fit through three-dimensional analysis. Materials and methods: Ten monolithic zirconia crowns were fabricated using titanium abutment model. Monolithic zirconia crowns were designed, milled, and sintered as a control group, and additional firing with coloring was performed as a test group. Three dimensional analysis were performed by using triple-scan protocol, and cross-section analysis on mesio-distal and disto-lingual section was evaluated to measure marginal and internal fitness. Then, three-dimensional surface difference on between two groups was evaluated (${\alpha}=.05$). Results: There was statistically significant difference between the control group ($32.0{\pm}24.3{\mu}m$) and the test group ($17.0{\pm}10.8{\mu}m$) in the mesial axial wall (P < .02) and the control group ($60.2{\pm}24.3{\mu}m$) and the test group ($71.8{\pm}21.5{\mu}m$) in the distal axial wall (P < .01). There was no statistically significant difference at the remaining point. Conclusion: There was no statistical significance on the deviation of inner surface of crown according to firing number, and the results of both group were considered clinically acceptable.

Full-mouth rehabilitation with implant-supported fixed dental prostheses for the edentulous maxilla and partially edentulous mandible: A case report (상악 완전 무치악 및 하악 부분 무치악 환자에서 임플란트 지지형 고정성 보철물을 이용한 전악 수복 증례 보고)

  • Kim, Tae-Hyung;Oh, Kyung-Chul;Moon, Hong-Seok
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.57 no.4
    • /
    • pp.374-381
    • /
    • 2019
  • A conventional approach for the treatment of long-span edentulous areas is the use of removable dentures. However, placing implants in these areas results in superior functional outcomes by increasing the stability, support, and resistance of the prostheses and improving the masticatory efficiency. Treatment modalities utilizing implants can be further classified into either removable or fixed-type prostheses. Several factors such as the amount of alveolar bone resorption, inter-arch relationship, patient preferences, and socioeconomic status should be considered when determining the appropriate treatment approach. Monolithic zirconia has been considered a suitable material for implant-supported fixed dental prosthesis, because of the drastic improvement in its mechanical properties. It exhibits fewer incidences of fracture and chipping of the prostheses, and has greater bulk of material than metal-ceramic crowns and zirconia-veneered ceramics. Moreover, highly translucent monolithic zirconia is also available in the market, and its application is gradually increasing for anterior tooth rehabilitation. The present report describes a patient who underwent full-mouth rehabilitation with fixed dental prostheses (eight upper and three lower implant placements). All teeth, except bilateral mandibular canines and left mandibular first and second premolars, were extracted after the diagnosis of generalized chronic moderate-to-advanced periodontitis of the remaining teeth. The patient reported satisfactory esthetic and functional outcomes during the one-year follow-up visit.

Full mouth rehabilitation using monolithic zirconia: a clinical report (Monolithic zirconia를 이용한 전악 보철 수복: a clinical report)

  • Oh, Won-Seok;Ryu, Jae-Jun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.31 no.4
    • /
    • pp.358-363
    • /
    • 2015
  • Previously, the usage of monolithic zirconia in anterior restoration was limited because of problems such as the monotony of tones and shades which would compromise the outcome of esthetic purpose. Zirconia was merely used as a coping with additional porcelain veneering whereas porcelain chipping cannot be evaded. Recently, with the improvement of monolithic zirconia, the various translucency and tones made it possible to use zirconia for anterior restoration. In this case, a male patient of 63 years old received a full mouth rehabilitation with monolithic zirconia. After a period of time usage, the outcome showed a favorable result functionally and esthetically.

Development of dental zirconia (치과용 지르코니아의 발전)

  • Kim Sung-Hun
    • Journal of the Korean Academy of Esthetic Dentistry
    • /
    • v.32 no.1
    • /
    • pp.4-7
    • /
    • 2023
  • Since the end of the 1990s, zirconia, which has been applied to dental prostheses, has been used in the form of coping or framework. The prostheses made in this way have been successfully used in the anterior teeth because they have no metal components as a structure. But in the posterior teeth, its use was limited due to the fracture or chipping of the veneering porcelain during the function. Later, as a solution to this shortcoming, a monolithic zirconia restoration was proposed in which a strong coping material was used in the form of a complete prosthesis. But, this resulted in some unesthetic results due to the characteristics of zirconia, which has excellent resistance to strong forces but is very white and opaque. However, now, due to technological advances in increasing the translucency of zirconia, it is possible to produce strong and esthetic zirconia restorations not only in the posterior region but also in the anterior region. In this article, the structural characteristics of various types of zirconia materials that have been developed so far, were discussed, and where the zirconia products actually in use belong to was explained.

Effect of coloring liquids on biaxial flexural strength of monolithic zirconia (착색 용액이 단일 구조 지르코니아의 이축 굴곡 강도에 미치는 영향)

  • Jung, Chaeyul;Kim, Min-Jeong;Kim, Jae-Hyun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.59 no.2
    • /
    • pp.190-200
    • /
    • 2021
  • Purpose. The aim of this study was to evaluate biaxial flexural strength and hardness of colored monolithic zirconia after dipping in different time intervals of coloring solution. Materials and Methods. Disk shaped specimens were prepared from monolithic zirconia (Eclipse V2.0, AMS, Gimpo, Korea). Four experimental groups were categorized (n = 12) due to coloring time (PU (0s); ST (8s); OV (1 min); PS (preshade)), to evaluate biaxial flexural strength and Vickers hardness. After fracture, X-ray diffraction analysis was performed using fractured specimens. Results were analyzed with one-way ANOVA test. Results. There was no significant difference between groups in the biaxial flexural strength test. However, in the Vickers hardness test, the group with standard dipping time (ST) showed significantly higher value than the group without dipping in coloring liquid (PU)(P=.038). Also, there was no significant difference in the rest of the groups (P>.05). As a result of X-ray diffraction analysis, specific peaks of tetragonal phase were shown and the volume of monoclinic phase fraction was lower than 25%. Conclusion. Although this study has several limitations, coloring liquids had no significant effect on biaxial flexural strength. Vickers hardness was significantly different between the group to which the coloring liquid was applied and the group to which the coloring solution was not applied, but there was no significant difference between the other groups. Also, the flexural strength of monolithic zirconia corresponds to Class 5 of the minimal flexural strength standard according to the use of dental ceramics.

Oral rehabilitation of a patient with severely worn dentition using monolithic zirconia (단일구조 지르코니아 보철물을 이용한 심한 마모 환자의 전악 수복 증례)

  • Park, Jun-Seo;Ryu, Jae-Jun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.54 no.3
    • /
    • pp.273-279
    • /
    • 2016
  • Severe tooth wear may lead to pathological changes of pulp, imbalance in occlusion as well as functional and esthetic problems. In this case, 34-year-old male came to the hospital because of generally worn dentition due to attrition and erosion. After evaluation, a full mouth restoration with elevation of the vertical dimension of occlusion was planned. After occlusion was stabilized by an occlusal stabilization appliance, centric relation position was recorded and subsequent provisional restorations were fabricated. After evaluation, a CAD-CAM (computer aided design-computer aided manufacturing) prosthetic restoration was carried out using monolithic zirconia. After 12 months of follow up observation, the patient was satisfied with function and esthetic appearance.

Full mouth rehabilitation of a patient using monolithic zirconia and dental CAD/CAM system: a case report (단일구조 수복용 지르코니아와 Dental CAD/CAM System을 이용한 전악 임플란트 고정성 보철 수복 증례)

  • Lee, Sang-Hoon;Yoon, Hyung-In;Yeo, In-Sung;Han, Jung-Suk;Kim, Sung-Hun
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.34 no.3
    • /
    • pp.196-207
    • /
    • 2018
  • An accurate implant placement with ideal location is significant for long-term success of the implant. An exact evaluation of nearby anatomic structures such as quality of residual bone, an inferior alveolar bone and a maxillary sinus is required. For a prosthetic-driven treatment, planned surgery, precise prosthesis and communication with the patient are significant requisites especially for full-mouth rehabilitation. In this case, the patient with severe alveolar bone resorption had a CT guided surgery supported by CT data and the data from scanning diagnostic wax-up. Afterward, edentulous area was restored by full mouth implant-supported prosthesis by using monolithic zirconia and CAD/CAM technique. This paper reports the outcome of the procedure which was remarkable both esthetically and functionally.

A case of full mouth rehabilitation with orthodontic treatment in patient with extensive tooth erosion and wear using monolithic zirconia prostheses (광범위한 치아부식 및 마모가 있는 환자에서 교정치료와 단일구조 지르코니아 보철물을 이용하여 완전 구강 회복술을 시행한 증례)

  • Yun, Byoung Soo;Kim, Jong Eun;Shim, Jun Sung;Kim, Jee Hwan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.56 no.4
    • /
    • pp.360-367
    • /
    • 2018
  • Extensive dental erosion and wear will cause serious loss of function and aesthetics in the mouth. In order to recover this condition, careful analysis of the patient's bite relationship is required. In particular, a treatment plan should be established considering the possibility of reproduction of the vertical dimension and centric relation, and appropriateness of the occlusal plane and anterior guidance. Also, the choice of prosthetic materials is an important consideration in patients with severe wear. In this case, patients with overall wear and erosion on tooth was established anterior guidance by orthodontic treatment and fully restored with monolithic zirconia, without increasing vertical dimension.

Fabrication of high purified zirconium dioxide (ZrO2) and stabilized zirconia (TZP: tetragonal zirconia polycrystal) powders (고순도 산화지르코늄(ZrO2) 및 안정화 지르코니아 (TZP: tetragonal zirconia polycrystal) 분말제조)

  • 최의석
    • Proceedings of the Korea Association of Crystal Growth Conference
    • /
    • 1996.06b
    • /
    • pp.55-85
    • /
    • 1996
  • 지르코니아 분말은 ZrO2 결정상이 온도변화에 따라 부피변화를 수반하는 상전이변태를 나타낸다. 단사정 ZrO2가 110$0^{\circ}C$에서는 정방정으로, 2$700^{\circ}C$ 내외에서는 입방정으로 결정구조가 가역적으로 변한다. 이 ZrO2에 금속산화물을 고용시키면 형석 (CaF2:Florite)형의 입방정 결정구조가 실온에서도 안정하게 존재하게 된다. 안정화제 산화물은 caO, MgO등 2가 산화물외에 3가 또는 4가의 금속산화물로서 Sc2O3, Y2O3, Sm2O3, Nd2O3, Gd2O3, Y2O3, CeO2 등이며 이들은 금속이온의 원자가가 변하기 쉬운 희토류 산화물이다. 안정화 지르코니아는 형석형 결정구조이며 결정화학적으로 보면 금속양이온이 산소이온에 대해서 정육면체형의 8배위를 하고 있다. 이때 이온반경비(양이온/음이온)에 따라 Zr+4자리와 O-2자리의 격자위치와 모양이 형성되므로 비틀어진 정육면체구조이건 이상적인 정육면체 형석구조를 이룬다. 이는 지르코니아의 결정상의 2상-3상인 부분안정화 지르코니아다결정체(PSZ : partially stabilized zirconia)이거나 단일상-2상인 정방정 지르코니아다결정체(TZP : tetragonal zirconia polycrystal)의 결정구조를 가지는데 기인한다. PSZ는 주로 MgO, CaO를 안정화제로 고용시켜 입방정 영역에서 소결하고 이를 다시 입방정과 정방정의 상 영역에서 열처리하여 입방정 입자내부에 정방정을 석출 형성시킨 것이며 TZP는 Y2O3 및 CeO2를 고용시켜 PSZ와 다르게 일반적인 상압소결한 정방정 결정상의 미립자이다. 산화지르코늄 분말은 지르콘사에서 열분해시킨 지르코늄소결.융해괴(caustic fusion clinker)를 산처리하여얻어진 지르코늄산용액(zirconyl acid solution : cloride, sulfide, nitride 등)으로부터 제조된다. 고순도 산화지르코늄은 용액 결정석출법에 의해 ZrOCl2.8H2O, 5ZrO2.3SO3.15H2O, ZrO(NO3)2.xH2O 등의 지르코늄 수화물만을 재결정화시킨 것으로부터 얻을 수 있으며 이 지르코늄염 수용액으로부터 입자미세구조를 효과적으로 제어하여 산화지르코늄 및 안정화 지르코니아 분말제조가 가능하다. 안정화 지르코니아 분말은 ZrO2와 안정화산화물의 고용을위하여 가열처리를 필요로 하며 일정온도에서 최적상태로 숙성하므로서 2가지 상(phase) 이상의 고용체를 가지게 된다. 안정화 지르코니아 분말은 고용처리온도를 낮추고 효과적으로 생성시키기 위해서는 지르코늄 및 안정화제염을 혼합하고 습식 직접합성하여 저온에서 고용체의 합해진상 영역을 생성시키는 것이다. 이는 지르코니아 원료분말의 미세구조를 제어하므로서 가능하며 이때 화학성분조성과 크기형태가 균일하게 분포된 입자분말을 얻을 수 있다.

  • PDF