• Title/Summary/Keyword: 기포단위중량

Search Result 26, Processing Time 0.027 seconds

Correlation between Compressive Strength and Unit Weight of Lightweight Foamed Controlled Low Strength Material (CLSM) Using Coal Ash (석탄회를 활용한 경량기포 CLSM의 압축강도와 단위중량의 상관관계)

  • Lee, Jong-Hwi;Lee, Hye-Jin;Chun, Byung-Sik
    • Journal of the Korean Geotechnical Society
    • /
    • v.29 no.1
    • /
    • pp.39-47
    • /
    • 2013
  • With the increase in the application of CLSM using coal ash, we performed a basic research on CLSM material, laying focus on the correlation between compressive strength and unit weight of lightweight foamed CLSM. The unconfined compression strength is a criterion for the judgment of the possibility of re-excavation and an important factor determining the economy, efficiency, and excavation character. However, to know the quantitative compression strength value takes a certain amount of time, because the applicability of unconfined compression strength of CLSM is judged by the standard of 28days. Therefore, in this study the relation between compressive strength and unit weight (foam slurry unit weight, apparent unit weight) is analyzed focusing on lightweight foamed CLSM. We also suggested a formula which can easily predict the 28-day compressive strength only using unit weight value without the need to cure the slurry for 28 days.

Effect of Mixing Time by Mix Truck on the Physical Properties of Lightweight Air-mixed Soil (믹스트럭 내 교반시간이 경량기포혼합토의 물성에 미치는 영향)

  • Kim, Taehyo;Kim, Nayoung;Im, Jongchul
    • Journal of the Korean GEO-environmental Society
    • /
    • v.16 no.2
    • /
    • pp.15-25
    • /
    • 2015
  • As the physical and mechanical properties of lightweight air-mixed soil change in the procedure of transportation of mix truck, it is necessary to assure whether the properties during construction satisfy those in design. In this study, variations of properties of mixed soil after transportation by mix truck are proved by field test. Lightweight air-mixed soil used field test the unit weight of $9.0{\pm}1.0kN/m^3$, the flow value of $190{\pm}20mm$ was produced. To analyze variations of properties of mixed soil the unit weight and flow value of the sample before and after transport was measured unconfined compressive strength tests were performed. Mixing time was 19~175 minutes diversified. As the test results, it is known that the density, the flow value and the unconfined compressive strength of lightweight air-mixed soil change by transportation, but these values satisfy the specifications of material of air-mixed soil. After transportation the average value of the unit weight and flow value change in the flow of the $(+)0.10kN/m^3$, 4.8 mm respectively, the average change in the unit weight and the flow value due to the mixing time was constant. And unconfined compressive strength of 28-day specimen increases from 20 to $150kN/m^2$. But, these values do not have some clear relationship with the transportation time within 175 minutes which is longest test time. Consequently, Within 175 minutes the changes of properties by transportation are too small to show some problems in the construction field.

Characteristics of Foam Concrete with Application of Mineral Admixture (무기혼화재 적용에 따른 기포콘크리트의 특성)

  • Kim, Sang-Chel;Kim, Yun-Tae
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.4 no.2
    • /
    • pp.97-106
    • /
    • 2009
  • self-loading, various problems related to construction can be solved as well as the save of construction cost. Thus, this study has an aim of applying foam concrete to structural purpose by adding bottom ash as a reinforcing material like fine aggregate, in contrast to conventional non-structural usage such as soundproofing or insulating materials. In addition, it was evaluated in terms of unit volume weight, flow value, air void, water absorption and dosage of foam agent wether replacement of cement by granulated blast furnace slag or fly-ash has an effect on the material characteristics of foam concrete. As results of experiments, it can be found that the increase of fine aggregate ratio, that is to say, the increase of bottom ash results in the increase of unit volume weight, while decreasing air void and flow value. But, appropriate addition of bottom ash to foam concrete makes it easy to control a homogeneous and uniform quality in foam concrete due to less sensitive to bubbles. As the replacement ratio of mineral admixtures such as granulated blast furnace slag and fly-ash increases, as unit volume weight tends to decrease. In the meanwhile, serious effects were shown on fluidity of foam concrete when more than limit of replacement ratio was applied.

  • PDF

Shear Strength and Deformation Characteristics of Lightweight Soils Mixed with Tire Powder (타이어 가루를 섞은 경량혼합토의 전단강도와 변형특성)

  • Yoon, Gil Lim;Yoon, Yeo Won;Ahn, Kwang Hyun
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.32 no.6C
    • /
    • pp.259-265
    • /
    • 2012
  • This paper investigates engineering characteristics of lightweight soils mixed with air foam and tire powder. Lightweight soils could be used as foundation materials, back-fills of reducing vibrating or abutment, and so on. Unconfined and triaxial compression tests were carried out to analyze strength and deformation characteristics of lightweight soils by changing target moist unit weight and cement contents. In comparison with strength characteristics of two different kinds of lightweight soils with same most unit weights ($13kN/m^3$), unconfined compression tests showed similar compressive strength, however, triaxial compression tests showed that compressive strength of lightweight soils mixed with waste tire powder was relatively larger strength than that of lightweight soils mixed with air foam because of elasticity of waste tire powder. Also, unconfined and triaxial compressive strengths of most of lightweight soils increase with increases of moist unit weight and cement contents. However, the strength of lightweight soils mixed with air foam under $11kN/m^3$, when moist unit weight exceeds a certain cement contents, decreases even though cement contents increase because of the effect in a void gap of air foam.

Mechanical Characteristics of Light-weighted Foam Soil Consisting of Dredged Soils (준설토를 이용한 경량기포혼합토의 역학적 특성 연구)

  • 김주철;이종규
    • Journal of the Korean Geotechnical Society
    • /
    • v.18 no.4
    • /
    • pp.309-317
    • /
    • 2002
  • The mechanical characteristics of Light-Weighted Foam Soil(LWFS) are investigated in this research. LWFS is composed of the dredged soil from offshore, cement and foam to reduce the unit-weight and increase compressive strength. For this purpose, the unconfined compression tests and triaxial compression tests are carried out on the prepared specimens of LWFS with various conditions such as initial water contents, cement contents, curing conditions and confining stresses. The test results of LWFS indicated that the stress-strain relationship and the compressive strength are strongly influenced by the cement contents rather than the intial water contents of the dredged soils. On the other hand, the stress-strain relationship from triaxial compression test has shown strain-softening behavior regardless of curing conditions. The stress-strain behavior for the various confining stress exhibited remarkable change at the boundary where the confining stress approached to the unconfined compression strength of LWFS. In order to obtain the ground improvement of the compressive strength above 200kPa, the required LWFS mixing ratio is found to be 100%~160% of the initial water contents of dredged soil and 6.6% of cement contents.

Flow and Strength Characteristics of the Lightweight Foamed CLSM(Controlled Low-Strength Materials) with Coal Ash (석탄회를 활용한 경량기포유동화재의 플로우 및 강도 특성)

  • Lee, Seungjun;Lee, Jonghwi;Chae, Hwiyoung;Chun, Byungsik
    • Journal of the Korean GEO-environmental Society
    • /
    • v.12 no.10
    • /
    • pp.73-82
    • /
    • 2011
  • Coal ash of industial by-products was not recycled about 30% in total emissions. Moreover, it caused environmental pollution as well as wasted unnecessary expenses and time. Currently, fly ash(FA) is recycled as construction material however ponded ash(PA) is mostly buried. Lightweight foamed Controlled Low-Strength Materials(CLSM) evaluated in this study reduces unit weight by mixing foam in the traditional Controlled Low-Strength Material and has lightweight and flowability to be available for backfill materials in construction. Flow test, unconfined compressive strength test, and foamed-slurry unit weight test were performed in this study and the applicability of lightweight foamed CLSM for construction materials was evaluated. The results indicate that the mixture ratio(PA:FA) ranging from 70:30 to 50:50, cement of 7%, foam of 2~3%, and water content of 26.5~29.5% were required to satisfy the following standards such as flow value(i.e., 20cm), unconfined compressive strength(i.e., 0.8~1.2MPa), and foamed-slurry unit weight(i.e., $12{\sim}15kN/m^3$).

Properties of the Concrete Foaming Agent According to Temperature and Concentration (기포제 온도 및 희석농도에 따른 콘크리트용 기포제의 특성)

  • Choi, Ji-Ho;Lee, Min-Jae;Jeong, Ji-Young;Hwang, Eui-Hwan;Kim, Jin-Man
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2011.11a
    • /
    • pp.247-249
    • /
    • 2011
  • Pre-foaming, one of the manufacturing way of foamed concrete, is influenced by foaming agent. When the foaming agent diluted with water, surface tension and viscosity are varied. Therefore, this study is reviewing the surface tension, viscosity and unit weight of foam by experimental factor such as foaming agent types(AES, AOS, VS FP) and foam agent dilution concentration (1, 3, 5%) and temperature of materials (5, 10, 20℃). As an expeimental result, the surface tension and viscosity slightly increased with increasing concentrations. Meanwhile, when increasing temperature, the viscosity has decreased. FP produce relatively stable foams only in case 3% or more, which produce unstable foams containing large amount of water content by decreasing only insignificant surface tension when diluted at concentration of 1%.

  • PDF

Engineering Characteristics of Light-weight Foamed CLSM using Coal Ash According to Final Mixing Time and Dilution Ratio (석탄회를 활용한 경량기포 저강도 고유동화재의 최종비빔시간과 희석비에 따른 공학적 특성)

  • Lee, Jong Hwi;Na, Jeong Hum;Lee, Chang Ki;Chun, Byung Sik
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.32 no.1C
    • /
    • pp.17-25
    • /
    • 2012
  • CLSM (Controlled Low Strength Material) using coal ash, which has the advantages of self-leveling, self-compacting, flowability, easy re-excavation, has been developed. In this study, CLSM additionally mixed with foaming agent for structural backfill material, aimed at lightness of materials, was developed called light-weight foamed CLSM. As the basic study of this material, to determine the optimum final mixing time and dilution ratio of existing light-weight foamed CLSM, flow, slurry unit weight and unconfined compressive strength test according to each impact factor were performed at the standard mix proportion. As the results of tests, CASE N (Final mixing time 4 min, dilution ratio 2%), CASE O (Final mixing time 3 min, foam agents ratio 3%, dilution ratio 2%) were satisfied with the standard of flow test (above 20cm), slurry unit weight test (12~15 $kN/m^3$) and unconfined compressive strength test (800 kPa~1200 kPa). These results will indicate the standard optimum final mixing time and dilution ratio of light-weight foamed CLSM for structural backfill.

Experimental Study on behavior of the Lightweight Air-foamed Soil Considering Freezing-thawing and Soaking Conditions (동결융해 및 수침조건을 고려한 경량기포혼합토의 거동 실험 연구)

  • Kang, Daekyu;Shin, Eunchul
    • Journal of the Korean GEO-environmental Society
    • /
    • v.17 no.5
    • /
    • pp.37-46
    • /
    • 2016
  • In order to determine the variability of environmental characteristics of lightweight air-foamed soil using marine clay according to freezing-thawing and soaking conditions, unconfined compressive strength of the lightweight air-foamed soil samples made by changing the amount of cement under curing conditions of outdoor low temperature, underground or indoor wetting were observed. Compressive strength was not increased under freezing-thawing (temperature range of $-9.1^{\circ}C{\sim}17.2^{\circ}C$) regardless of the amount of cement but the more cement using, it was increased rapidly by underground curing conditions within 30 cm beneath ground level. Therefore, it is necessary to install insulation layer cutting off exterior cold air after construction of lightweight air-foamed soil in condition of freezing-thawing. Bulk density was increased too small under the long-time soaking condition, it tended to decrease rapidly when samples were dried up and had below 6% of water contents. But variability of compressive strength and bulk density was very small for preventing drying and keeping its wet state. The lightweight air-foamed soil that installed beneath ground water level or covered by soil can be evaluated as a long-term reliable construction material.

Mechanical Properties of Lightweight Foamed Concrete Using Polymer Foam Agent (고분자 기포제를 이용한 경량 기포 콘크리트의 역학적 특성 (II))

  • 박상순;송하원;변근주
    • Magazine of the Korea Concrete Institute
    • /
    • v.9 no.1
    • /
    • pp.173-181
    • /
    • 1997
  • The objective of this study is to obtain the mechanical characteristics of prefoarmed lightweight foamed concrete using the polymer ham agent which has high lightness. flowability and strength. For this purpose, the prefoarmed lightweight foamed concrete which was developed to have flow value over 180mm. unit weight between 0.38t/$m^3$ and 0.64t/$m^3$, and compressive strength about 30kg/$cm^2$ was used. This paper presents extensive test data on Young's modulus. Poisson's ratio, stress-strain curve, the characteristics of strength of the foamed concrete and also presents the mechanical characteristics of the foamed concrete with different foam sizes. It is expected that this study provides an importance guide to design and manufacture lightweight foam concrete, so that it helps to expand its structural use.