Variation of Nanoindentation Curve due to Wear of Indenter Apex and Its Correction Method (압입자 첨단마모에 따른 나노압입곡선의 변화 및 이의 보정기법)

  • Lee, Yun-Hee;Kim, Yong-Il;Park, Jong Seo;Kim, Kwang Ho
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.33 no.2
    • /
    • pp.129-137
    • /
    • 2013
  • A force calibration of a nanoindenter and a 3D morphology observation of indenters were carried out in this study. A microbalance calibrated with standard weights was used for measuring the loads generated by a nanoindenter. The indentation load could be calibrated from the ratio of measured and generated loads and the first contact load also could be detected from the microbalance data. By analyzing atomic force microscopy images of two indenters, curvature radii of apexes were determined by $19.71{\pm}3.03$ and $1043.94{\pm}50.91$ nm, respectively, for the nearly new indenter A and the severly worn indenter B. Corresponding bluntness depths were estimated by 1.22 and 64.56 nm for the both indenters by overlapping their profiles on the perfect pyramidal shape. In addition, nanoindentation curves obtained from a fused silica reference material with the both indenters showed a depth difference corresponding to the bluntness depth difference along the indentation depth axis. By shifting amounts of the bluntness depths along the horizontal axis, whole nanoindentation curves overlapped on themselves and resulted in nanohardness values consistent within 1.11 % without considering the complex indenter area function of each indenter.

Flexibility Study of Silicon Thin Film Transferred on Flexible Substrate (폴리머 기판 위에 전사된 실리콘 박막의 기계적 유연성 연구)

  • Lee, Mi-Kyoung;Lee, Eun-Kyung;Yang, Min;Chon, Min-Woo;Lee, Hyouk;Lim, Jae Sung;Choa, Sung-Hoon
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.20 no.3
    • /
    • pp.23-29
    • /
    • 2013
  • Development of flexible electronic devices has primarily focused on printing technology using organic materials. However, organic-based flexible electronics have several disadvantages, including low electrical performance and long-term reliability. Therefore, we fabricated nano- and micro-thick silicon film attached to the polymer substrate using transfer printing technology to investigate the feasibility of silicon-based flexible electronic devices with high performance and high flexibility. Flexibility of the fabricated samples was investigated using bending and stretching tests. The failure bending radius of the 200 nm-thick silicon film attached on a PI substrate was 4.5 mm, and the failure stretching strain was 1.8%. The failure bending radius of the micro-thick silicon film attached on a FPCB was 2 mm, and the failure strain was 3.5%, which showed superior flexibility compared with conventional silicon material. Improved flexibility was attributed to a buffering effect of the adhesive between the silicon film and the substrate. The superior flexibility of the thin silicon film demonstrates the possibility for flexible electronic devices with high performance.

Synthesis, Characterizations, and Applications of Metal-Ions Incorporated High Quality MCM-41 Catalysts (고품질 금속 이온 첨가 MCM-41 분자체 촉매의 제법, 특성화 및 응용 반응)

  • Lim, Steven S.;Haller, Gary L.
    • Korean Chemical Engineering Research
    • /
    • v.51 no.4
    • /
    • pp.443-454
    • /
    • 2013
  • Various metal ions (transition and base metals) incorporated MCM-41 catalysts can be synthesized using colloidal and soluble silica with non-sodium involved process. Transition metal ion-typically $V^{5+}$, $Co^{2+}$, and $Ni^{2+}$-incorporated MCM-41 catalysts were synthesized by isomorphous substitution of Si ions in the framework. Each incorporated metal ion created a single species in the silica framework, single-site solid catalyst, showing a substantial stability in reduction and catalytic activity. Radius of pore curvature effect was investigated with Co-MCM-41 by temperature programmed reduction (TPR). The size of metallic Co clusters, sub-nanometer, could be controlled by a proper reduction treatment of Co-MCM-41 having different pore size and the initial pH adjustment of the Co-MCM-41 synthesis solution. These small metallic clusters showed a high stability under a harsh reaction condition without serious migration, resulting from a direct anchoring of small metallic clusters to the partially or unreduced metal ions on the surface. After a complete reduction, partial occlusion of the metallic cluster surface by amorphous silica stabilized the particles against aggregations. As a probe reaction of particle size sensitivity, carbon single wall nanotubes (SWNT) were synthesized using Co-MCM-41. A metallic cluster stability test was performed by CO methanation using Co- and Ni-MCM-41. Methanol and methane partial oxidations were carried out with V-MCM-41, and the radius of pore curvature effect on the catalytic activity was investigated.

Improved design of a directional coupler by a novel concept (방향성 결합기의 성능 및 허용오차 개선을 위한 신제안)

  • 최철현;박순룡;오범환
    • Korean Journal of Optics and Photonics
    • /
    • v.11 no.6
    • /
    • pp.405-410
    • /
    • 2000
  • We propose a novel design concept to improve extinction ratio by minimizing $Cv_e-Cv_o$ . Improvements of loss and fabrication error limit are also obtained by this hybrid design of the lateral shift and curved waveguide to control transfer coefficients, $Cv_e and Cv_o$ . The concept of lateral shift merges two transfer coefficients, and additional curved waveguide controls mode profile asymmetrically to help this minimizing effect of $Cv_e-Cv_o$ with no serious decrease in transfer efficiency. For a given InP based waveguide structure, the mode propagation analysis with an effective index approximation provided a calculational improvement of extinction ratio to -39 dB and fabrication error limit to $57.19\mu\textrm{m}$, with a structure design of $300\mu\textrm{m}$ waveguide curvature and $0.1\mu\textrm{m}$lateral shift. shift.

  • PDF

Optimum Shape Synthesis of Cam And Follower in Cam-Valve System to Minimize Contact Force (캠-밸브 기구에서 접촉력 최소화를 위한 캠과 종동자 형상 최적 합성)

  • 김성훈;전혁수;박윤식
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.14 no.3
    • /
    • pp.534-546
    • /
    • 1990
  • In this work, an optimum shape synthesis for rolling contact components was done to minimize contact forces considering dynamic characteristics of the system. Even this method was applied to an OHC type cam follower system, it can be expanded to general rolling contact shape design problems which are strictly forced to follow predetermined motion. First, the follower optimum angular motion was derived to minimize the valve peak acceleration while satisfying all the constraints of valve motion. Then the cam and follower contact shape were synthesized to give the proposed follower motion. Theoretically, two components shape to generate a predetermined motion can not be uniquely determined. So the cam shape was syntehsized with parametric synthesis method to minimize the peak contact force between cam and follower when the follower shape is assumed as a circle or an ellipse.

Numerical Analysis on the Stress Behaviours Due to Geometry Effects of the Membrane Corrugation (멤브레인의 주름 형상이 응력거동에 미치는 영향에 관한 수치적 해석)

  • Kim Chung-Kyun;Lee Young-Suck;Cha Baeg-Soon;Kim Young-Gyu;Yoon In Soo;Hong Seong Ho
    • Journal of the Korean Institute of Gas
    • /
    • v.1 no.1
    • /
    • pp.21-26
    • /
    • 1997
  • This paper presents the numerical results of six corrugation models which compute the stress behaviours and stress levels of the membrane structure under the hydrostatic pressure of cryogenic liquids and thermal loadings using a non -linear finite element analysis program. A three-dimensional analysis of various corrugation geometries was performed on the maximum mean normal stress distributions along the upper surface of the membrane sheet. Comparisons of the FEM results for various geometry models of the corrugation are presented, which shows that the corrugated configuration of the ring knot model can be effectively performed for the combined forces such as the hydrostatic pressure and thermal loading in comparison with the Technigaz type corrugation which has small comer and apex curvatures. The FEM results show that the ring knot corrugation can be used for the deepest depth, 180m of the LNG storage tank in comparison with other corrugation models.

  • PDF

Effects of Boliing, Steaming, and Chemical Treatment on Solid Wood Bending of Quercus acutissima Carr. and Pinus densiflora S. et. Z. (자비(煮沸), 증자(蒸煮) 및 약제처리(藥劑處理)가 상수리나무와 소나무의 휨가공성(加工性)에 미치는 영향(影響))

  • So, Won-Tek
    • Journal of the Korean Wood Science and Technology
    • /
    • v.13 no.1
    • /
    • pp.19-62
    • /
    • 1985
  • This study was performed to investigate: (i) the bending processing properties of silk worm oak (Quercus acutissima Carr.) and Korean red pine (Pinus densiflora S. et Z.) by boiling and steaming treatments; (ii) the effects of interrelated factors - sapwood and heartwood, annual ring placement, softening temperature and time, moisture content. and wood defects on bending processing properties; (iii) the changing rates of bending radii after release from a tension strap, and (iv) the improving methods of bending process by treatment with chemicals. The size of specimens tested was $15{\times}15{\times}350mm$ for boiling and steaming treatments and $5{\times}10{\times}200mm$ for treatments with chemicals. The specimens were green for boiling treatments and dried to 15 percent for steaming treatments. The specimens for treatments with chemicals were soaked in saturated urea solution, 35 percent formaldehyde solution, 25 percent polyethylene glycol -400 solution, and 25 percent ammonium hydroxide solution for 5 days and immediately followed the bending process, respectively. The results obtained were as follows: 1. The internal temperature of silk worm oak and Korean red pine by boiling and steaming time was raised slowly to $30^{\circ}C$ but rapidly from $30^{\circ}C$ to $80-90^{\circ}C$ and then slowly from $80-90^{\circ}C$ to $100^{\circ}C$. 2. The softening time required to the final temperature was directly proportional to the thickness of specimen. The time required from $25^{\circ}C$ to $100^{\circ}C$ for 15mm-squared specimen was 9.6-11.2 minutes in silk worm oak and 7.6-8.1 minutes in Korean red pine. 3. The moisture content (M.C.) of specimen by steaming time was increased rapidly first 4 minutes in the both species, and moderately from 4 to 20 minutes and then slowly and constantly in silk worm oak, and moderately from 4 to 15 minutes and then slowly and constantly in Korean red pine. The M.C. of 15mm-squared specimen in 50 minutes of steaming was increased to 18.0 percent in the oak and 22.4 percent in the pine from the initial conditioned M.C. of 15 percent The rate of moisture adsorption measured was therefore faster in the pine than in the oak. 4. The mechanical properties of the both species were decreased significantly with the increase of boiling rime. The decrement by the boiling treatment for 60 minutes was measured to 36.6-45.0 percent in compressive strength, 12.5-17.5 percent in tensile strength, 31.6-40.9 percent in modulus of rupture, and 23.3-34.6 percent in modulus of elasticity. 5. The minimum bending radius (M.B.R.) of sapwood and heartwood was 60-80 mm and 90 mm in silk worm oak, and 260 - 300 mm and 280 - 300 mm in Korean red pine, respectively. Therefore, the both species showed better bending processing properties in sapwood than in heartwood. 6. The M.B.R. of edge-grained and flat-grained specimen in suk worm oak was 60-80 mm, but the M.B.R. in Korean red pine was 240-280 mm and 260-360 mm, respectively. Comparing the M.B.R. of edge-grained with flat-grained specimen, in the pine the edge-grained showed better bending processing property than the flat-grained. 7. The bending processing properties of the both species were improved by the rising of softening temperature from $40^{\circ}C$ to $100^{\circ}C$. The minimum softening temperature for bending was $90^{\circ}C$ in silk worm oak and $80^{\circ}C$ in Korean red pine, and the dependency of softening temperature for bending was therefore higher in the oak than in the pine. 8. The bending processing properties of the both species were improved by the increase of softening time as well as temperature, but even after the internal temperature of specimen reaching to the final temperature, somewhat prolonged softening was required to obtain the best plastic conditions. The minimum softening time for bending of 15 mm-squared silk worm oak and Korean red pine specimen was 15 and 10 minutes in the boiling treatment, and 30 and 20 minutes in the steaming treatment, respectively. 9. The optimum M.C. for bending of silk worm oak was 20 percent, and the M.C. above fiber saturation point rather degraded the bending processing property, whereas the optimum M.C. of Korean red pine needed to be above 30 percent. 10. The bending works in the optimum conditions obtained as seen in Table 24 showed that the M.B.R. of silk worm oak and Korean red pine was 80 mm and 240 mm in the boiling treatment, and 50 mm and 280 mm in the steaming treatment, respectively. Therefore, the bending processing property of the oak was better in the steaming than in the boiling treatment, but that of the pine better in the boiling than in the steaming treatment. 11. In the bending without a tension strap, the radio r/t of the minimum bending radius t to the thickness t of silk worm oak and Korean red pine specimen amounted to 16.0 and 21.3 in the boiling treatment, and 17.3 and 24.0 in the steaming treatment, respectively. But in the bending with a tension strap, the r/t of the oak and the pine specimen decreased to 5.3 and 16.0 in t he boiling treatment, and 3.3 and 18.7 in the steaming treatment, respectively. Therefore, the bending processing properties of the both species were significantly improved by the strap. 12. The effect of pin knot on the degradation of bending processing property was very severe in silk worm oak by side, e.g. 90 percent of the oak specimens with pin knot on the concave side were ruptured when bent to a 100 mm radius but only 10 percent of the other specimens with pin knot on the convex side were ruptured. 13. The changing rate in the bending radius of specimen bent to a 300 mm radius after 30 days of exposure to room temperature conditions was measured to 4.0-10.3 percent in the boiling treatment and 13,0-15.0 percent in the steaming treatment. Therefore, the degree of spring back after release was higher in the steaming than in the boiling treatment. And the changing rate of moisture-proofing treated specimen by expoxy resin coating was only -1.0.0 percent. 14. Formaldehyde, 35 percent solution, and 25 percent polyethylene glycol-400 solution found no effect on the plasticization of the both species, but saturated urea solution and 25 percent ammonium hydroxide solution found significant effect in comparison to non-treated specimen. But the effect of the treatment with chemicals alone was inferior to that of the steaming treatment, and the steaming treatment after the treatment with chemicals improved 10-24 percent over the bending processing property of steam-bent specimen. 15. Three plasticity coefficients - load-strain coefficient, strain coefficient, and energy coefficient - were evaluated to be appropriate for the index of bending processing property because the coefficients had highly significant correlation with the bending radius. The fitness of the coefficients as the index was good at load-strain coefficient, energy coefficient, and strain coefficient, in order.

  • PDF

A Numerical Analysis on the Diaphragm Structures for Improving Fatigue Performance in Orthotropic Steel Decks (강바닥판의 피로성능 향상을 위한 다이아프램 구조상세)

  • Shin, Jae Choul;An, Zu Og;Yoon, Tae Yang
    • Journal of Korean Society of Steel Construction
    • /
    • v.19 no.6
    • /
    • pp.559-573
    • /
    • 2007
  • Orthotropic steel decks are manufactured by welding thin plates therefore it is inevitable that there are abundant works of welding process. On connection of transverse rib web, crossing point of longitudinal rib, transverse rib and deck plate and cut-out parts of transverse rib are the significant position of stress concentration because of out of plane and oil-canning deformation caused by longitudinal rib distortion with shear force and distortion. At the current research, the crossing point where the orthotropic steel decks's effect of improving fatigue performance are high, not placing scallop and diaphragm which have same plane with transverse rib placed inside of longitudinal rib at the same time, the reduce effects of stress concentration at the cut-out section and the crossing are high. Especially the installation of the diaphragm causing great effects based on research results to stress concentration appearance reduce effects at the cut-out section, putting radius of curvature of the diaphragm's top and bottom as a target, as a result of carrying out the parametric analysis an optimal diaphragm form that has great effects in fatigue performance came to a conclusion. Also based on optimal diaphragm form, an advantage of the diaphragm optimal setting position for improvement of the fatigue performance came to a conclusion.

A Behavioral Analysis of Curved Steel Box Bridge Associated with Diaphragm's Shape and Spacing (다이아프램 형상 및 간격에 따른 곡선 강박스거더의 거동해석)

  • Kim, Yun-Tae;Kim, Sang-Chel
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.10 no.1
    • /
    • pp.205-215
    • /
    • 2006
  • In this study 3-D shell FEM model was applied to analyze the behavior of curved steel box girders stiffened by diaphragms. The reliability of the analytical method has been proved by comparing with the existing results. It was also found from this analysis that main factors affecting a distortional stress are length of a girder, curvature of the girder, and spacing of diaphragms. A modelled bridge with 30m of span length and 40m of radius was analyzed to find an optimum spacing of diaphragm, and as a result of applying different spacings, 5m was found to be most appropriate to control the stress ratio regulated by specifications. In the effect of diaphragm shape, the rhamen-typed diaphragm is found to be more effective than the fully filled-up one in the range of opening ratio of 0.4 to 0.6. But, the fully filled-up diaphragm had more efficiency in terms of reducing the distortional stress than X-truss typed diaphragm.

Evaluation of Shape Parameter Effect on the J-R Curve of Curved CT Specimen Using Limit Load Method (한계하중법을 이용한 Curved CT 시험편의 파괴저항곡선에 미치는 형상변수 영향 평가)

  • Shin, In Hwan;Park, Chi Yong;Seok, Chang Sung;Koo, Jae Mean
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.38 no.7
    • /
    • pp.757-764
    • /
    • 2014
  • In this study, the effect of shape parameters on the J-R curves of curved CT specimens was evaluated using the limit load method. Fracture toughness tests considering the shape factors L/W and $R_m/t$ of the specimens were also performed. Thereafter, the J-R curves of the curved CT specimens were compared using the J-integral equation proposed in the ASTM (American Society for Testing and Materials) and limit load solution. The J-R curves of the curved CT specimens were also compared with those of the CWP (curved wide plate), which is regarded to be similar to real pipe and standard specimens. Finally, the effectiveness of the J-R curve of each curved CT specimen was evaluated. The results of this study can be used for assessing the applicability of curved CT specimens in the accurate evaluation of the fracture toughness of real pipes.