A Study on Optimum Proportion of FA and BS for Ternary Cement (3성분계 시멘트에서 FA 및 BS의 최적혼합비율 도출에 관한 연구)

  • Han, Cheon-Goo;Park, Sung-Bae
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.4 no.2
    • /
    • pp.143-148
    • /
    • 2016
  • The aim of research is inducing the optimum proportion of fly ash(FA) and blast furnace slag(BS) for ternary cement. In this research, hence, the fundamental properties of mortar mixtures were evaluated depending on various proportion of FA and BS. The results of the experiment, within the scope of the study, obtained the following conclusions. Flow of the mixtures was increased with addition of binary supplementary cementitious material(SCM), and especially, portion of FA. The air content of the mixtures was increased with addition of binary SCMs, while it was decreased with increased FA content. In the case of unit mass, increased value was obtained due to the increased air content within 25 to 45% of binary SCM content, while it was increased within 65 to 100% of binary SCM up to only 20% of FA content and decreased more than 20% of FA because of the low density of FA. The setting time of the mixtures was delayed with addition of binary SCM and FA. In the case of compressive strength, at 91-day age, the highest value was obtained with 25 and 45% of binary SCM with the proportion of FA to BS of 40 to 60. Therefore, based on the compressive strength, it is considered that the binary SCM content of 25 and 45% with the proportion of FA to BS of 2 : 3 is the most favorable conditions in this research scope.

A Study on the Fundamental Properties of Ultra Rapid Hardening Mortar using Coal-Ash (잔골재 대체재로서 석탄회를 이용한 초속경 보수모르타르의 기초적 특성에 관한 연구)

  • Lee, Gun-Cheol;Oh, Dong-Uk;Kim, Young-Geun;Cho, Chung-Ki
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.1
    • /
    • pp.128-135
    • /
    • 2011
  • In this study, in order to develop ultra rapid hardening mortar(URHM) for tunnel repairs using bottom ash of low recycle ratio and Admixture as Eco concept, fundamental properties of URHM on temperature condition of construction field were performed. Test result, URHM of three types for fluidity and setting time were as in the following : B > C > A. Those for low temperatures were later than the standard condition. Compressive, bending and bond strength were similar with three types as follow. In compressive strength, initial strength of the low were smaller than the standard but the low in the long-term were similar with the standard. On the contrary to this, bending strength were similar in initial strength but the low in the long-term were smaller than the standard. The low in bond strength was average 35% less than the standard. Length changes was as in the following : A > C > B. the low is two times much as the standard but the case using blast furnace slag particles noticeably reduced length changes. Water absorption coefficient and water vapor resistance were as in the following : C > A > B. In case of URHM added bottom ash, water absorption coefficient and water vapor resistance were increased because bottom ash is porous material.

  • PDF

Repair Cost Analysis for Chloride Ingress on RC Wall Considering Log and Normal Distribution of Service Life (로그 및 정규분포 수명함수를 고려한 콘크리트 벽체의 염해 보수비용 산정)

  • Yoon, Yong-Sik;Kwon, Seung-Jun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.23 no.2
    • /
    • pp.10-19
    • /
    • 2019
  • Management plan with repairing is essential for RC structures exposed to chloride attack since durability problems occur with extended service life. Conventionally deterministic method is adopted for evaluation of service life and repair cost, however more reasonable repair cost can be obtained through continuous repair cost from probabilistic maintenance technique. Unlike the previous researches considering only normal distribution of life time, PLTFs (Probabilistic Life Time Function) which can be capable of handling log and normal distributions are attempted for initial and repair service life, and repair cost is evaluated for OPC and GGBFS concrete. PLTF with log distributions in initial service life is more effective to save repair cost since it is more dominant after average than normal distribution. Repair cost in GGBFS concrete decreases to 30% of OPC concrete due to longer initial service life and lower repairing event. The proposed PLTF from the work can handle not only normal distributions but also log distributions for initial and repair service life, so that it can provide more reasonable repair cost evaluation.

Characteristics of Mine Liner According to the Replacement Ratio of Nano-Silica and Silica-Fume (나노실리카 및 실리카흄 대체율에 따른 차수재의 특성)

  • Kang, Suk-Pyo;Lee, Hee-Ra;Kang, Hye-Ju;Nam, Seong-Young;Kim, Chun-Sik
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.7 no.1
    • /
    • pp.66-73
    • /
    • 2019
  • Approximately 80% of the mines are vacated or abandoned mines and are mostly left without suitable environmental treatment facilities. In the area around the abandoned mine site, problems such as drainage of acidic city drainage and leakage of leachate occur, and ground subsidence caused by this can cause a safety accident due to sink hole occurrence. In this study, flow, compressive strength, water uptake, pore and hydration characteristics were investigated to investigate the basic properties of liner and cover material based on the replacement ratio of nano silica and silica fume in the existing blast - furnace slag fine powder. As a result, as the substitution ratio of nano silica and silica fume increased, the flow and compressive strength of nano silica specimens increased and the absorption rate decreased. In the case of pore characteristics, the amount of pores decreased as the substitution ratio of nano silica and silica fume increased. Especially, the capillary porosity of 10-1,000 nm diameter decreased. Ray diffraction analysis and SEM measurement showed that the peak positions of the hydration products were almost the same when compared with the 5% alternative test samples of Plain and silica fume.

Chloride Threshold Value for Steel Corrosion considering Chemical Properties of Concrete (콘크리트의 화학적 특성을 고려한 철근 부식 임계 염소이온 농도)

  • Song, Ha-Won;Jung, Min-Sun;Ann, Ki Yong;Lee, Chang-Hong
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.29 no.1A
    • /
    • pp.75-84
    • /
    • 2009
  • The present study assesses the chloride threshold level for corrosion of steel in concrete by examining the properties of four different binders used for blended concrete in terms of chloride binding, buffering of cement matrix to a pH fall and the corrosion behaviour. As binders, ordinary Portland cement (OPC), 30% pulverised fuel ash (PFA), 60% ground granulated blast furnace slag (GGBS) and 10% silica fume (SF) were used in a concrete mix. Testing for chloride binding was carried out using the water extraction method, the buffering of cement matrix was assessed by measuring the resistance to an artificial acidification of nitric acid, and the corrosion rate of steel in mortar with chlorides in cast was measured at 28 days using an anodic polarisation technique. Results show that the chloride binding capacity was much affected by $C_{3}A$ content and physical adsorption, and its order was 60% GGBS>30% PFA>OPC>10% SF. The buffering of cement matrix to a pH fall was varied with binder type and given values of the pH. From the result of corrosion test, it was found that the chloride threshold ranged 1.03, 0.65, 0.45 and 0.98% by weight of cement for OPC, 30% PFA, 60% GGBS and 10% SF respectively, assuming that corrosion starts at the corrosion rate of $0.1-0.2{\mu}A/cm^{2}$. The mole ratio of [$Cl^{-}$]:[$H^{+}$], as a new presentation of the chloride threshold, indicated the value of 0.008-0.009, irrespective of binder, which would be indicative of the inhibitive characteristic of binder.

A Review on the Recycling of the Concrete Waste Generate from the Decommissioning of Nuclear Power Plants (원전 해체 콘크리트 폐기물의 재활용에 대한 고찰)

  • Jeon, Ji-Hun;Lee, Woo-Chun;Lee, Sang-Woo;Kim, Soon-Oh
    • Economic and Environmental Geology
    • /
    • v.54 no.2
    • /
    • pp.285-297
    • /
    • 2021
  • Globally, nuclear-decommissioning facilities have been increased in number, and thereby hundreds of thousands of wastes, such as concrete, soil, and metal, have been generated. For this reason, there have been numerous efforts and researches on the development of technology for volume reduction and recycling of solid radioactive wastes, and this study reviewed and examined thoroughly such previous studies. The waste concrete powder is rehydrated by other processes such as grinding and sintering, and the processes rendered aluminate (C3A), C4AF, C3S, and ��-C2S, which are the significant compounds controlling the hydration reaction of concrete and the compressive strength of the solidified matrix. The review of the previous studies confirmed that waste concretes could be used as recycling cement, but there remain problems with the decreasing strength of solidified matrix due to mingling with aggregates. There have been further efforts to improve the performance of recycling concrete via mixing with reactive agents using industrial by-products, such as blast furnace slag and fly ash. As a result, the compressive strength of the solidified matrix was proved to be enhanced. On the contrary, there have been few kinds of researches on manufacturing recycled concretes using soil wastes. Illite and zeolite in soil waste show the high adsorption capacity on radioactive nuclides, and they can be recycled as solidification agents. If the soil wastes are recycled as much as possible, the volume of wastes generated from the decommissioning of nuclear power plants (NPPs) is not only significantly reduced, but collateral benefits also are received because radioactive wastes are safely disposed of by solidification agents made from such soil wastes. Thus, it is required to study the production of non-sintered cement using clay minerals in soil wastes. This paper reviewed related domestic and foreign researches to consider the sustainable recycling of concrete waste from NPPs as recycling cement and utilizing clay minerals in soil waste to produce unsintered cement.

Evaluation of Chloride Diffusion Behavior and Analysis of Probabilistic Service Life in Long Term Aged GGBFS Concrete (장기 재령 GGBFS 콘크리트의 염화물 확산 거동 평가 및 확률론적 염해 내구수명 해석)

  • Yoon, Yong-Sik;Kim, Tae-Hoon;Kwon, Seung-Jun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.24 no.3
    • /
    • pp.47-56
    • /
    • 2020
  • In this study, three levels of W/B(Water to Binder) ratio (0.37, 0.42, 0.47) and substitution ratio of GGBFS (Ground Granulated Blast Furnace Slag) rate (0 %, 30 %, 50 %) were considered to perform RCPT (Rapid Chloride Diffusion Test) at the 1,095 aged day. Accelerated chloride diffusion coefficient and passed charge of each concrete mixture were assessed according to Tang's method and ASTM C 1202, and improving behaviors of durability performance with increasing aged days are analyzed based on the test results of previous aged days from the preceding study. As the age of concrete increases, the passed charge and diffusion coefficient have been significantly reduced, and especially the concrete specimens containing GGBFS showed a significantly more reduction than OPC(Ordinary Portland Cement) concrete specimen by latent hydraulic activity. In the case of OPC concrete's results of passed charge, at the 1,095 days, two of them were still in the "Moderate" class. So, if only OPC is used as the binder of concrete, the resistance performance for chloride attack is weak. In this study, the time-parameters (m) were derived based on the results of the accelerated chloride diffusion coefficient, and the deterministic and probabilistic analysis for service life were performed by assuming the design variable as a probability function. For probabilistic service life analysis, durability failure probabilities were calculated using Monte Carlo Simulation (MCS) to evaluate service life. The service life of probabilistic method were lower than that of deterministic method, since the target value of PDF (Probability of Durability Failure) was set very low at 10 %. If the target value of PDF suitable for the purpose of using structure can be set and proper variability can be considered for each design variable, it is believed that more economical durability design can be made.