Setting Time and Strength of Slip-form Method Applied Caisson in Low-temperature Period (슬립폼공법 적용된 동절기 케이슨의 온도에 따른 응결시간 및 압축강도)

  • Kim, Bong-Joo;Kim, Jae-Hun;Kim, Chan-Soo;Jo, Ho-Kyoo
    • Journal of the Korean Society of Hazard Mitigation
    • /
    • v.6 no.1 s.20
    • /
    • pp.1-7
    • /
    • 2006
  • In the harbor construction work, caisson is made by slip-form method and curing temperature of caisson concrete need heating in the low-temperature. To get the setting time and compression strength of slip-form method applied caisson at various curing temperature. The curing temperature is divided to the temperature of slip-form and the temperature of second curing curtain. In consideration of setting time, compression strength of concrete and form-removal time, the best temperature is $25^{\circ}C$ at 6 hours slip-form curing time.

Strength Properties of Concrete According to Types of High Early Strength Cement and Curing Method (조강형 시멘트의 종류 및 양생방법에 따른 콘크리트의 강도특성)

  • Chang, Chun-Ho;Lee, Wang-Sup;Jung, Yong-Wook;Chung, Youn-In
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.5 no.1
    • /
    • pp.76-84
    • /
    • 2017
  • This study selected a method which uses high early strength cement as a way to reduce the curing time and curing energy source of concrete secondary products and reviewed the improvement in the initial strength of concrete secondary products setting the target strength of the concrete capable of removing the form to 15MPa and the curing time to 6 hours. As a result of the test, the only specimen which achieved the form removal strength of 15 MPa only through atmospheric curing within the target curing time of 6hours was ACC-100, and the specimens of TRC-100 and TRC-50 satisfied the values of 6 hours and 15MPa through steam curing. However, we could see that it was difficult to secure workability in the case of the specimen of ACC-100 due to its high rapid setting property and a retarder such as anhydrous citric acid was required to be used to improve the workability. When we look into the pattern following changes in the water to binder ratio, while, in the case of stream curing, OPC-100, TRC-100, and TRC-50 were all found to satisfy achievement of the form removal strength within 6hours as the water to binder ratio decreased, in the case of atmospheric curing, TRC-100, and TRC-50 achieved 15MPa within 12hours.

A Study on the Thermal Crack Control of Foundation for Large Turbine (대형 터빈 기초 구조물의 온도균열 제어에 관한 연구)

  • Ha, Ju-Hyung;Cho, Yun-Gu;Lee, Kewn-Chu;Lim, Chang-Keun
    • Journal of the Korea Concrete Institute
    • /
    • v.26 no.3
    • /
    • pp.287-297
    • /
    • 2014
  • Heat of hydration of mass concrete is one of the most important factors that significantly affect structural quality and construction period. Therefore, appropriate methods to control heat of hydration are essential technologies for mass concrete construction. In this study, probability of thermal cracking was checked by thermal analysis prior to the construction of a turbine foundation in a domestic power plant. Subsequently, changes of concrete mix proportion and an effective curing method were proposed to control heat of hydration of mass concrete structures. Concrete manufactured by slag cement was proposed instead of concrete produced by ordinary Portland cement, and an automated curing method was proposed to improve the curing method using typical moist curing with blanket. The automated curing method maintains the temperature difference between center and surface of concrete below a setting value by temperature monitoring. Concrete with slag cement was used for actual construction. One of two identical turbine foundations was cured by an insulated curing method, and the other was cured by the automated curing method to compare the curing methods. And then, the effects of control of heat of hydration were evaluated based on temperature/strain monitoring and crack investigations.

Strength of Recycled Concrete with Furnace Slag Cement under Steam Curing Condition (순환골재 및 고로슬래그 시멘트를 사용한 증기양생 콘크리트의 강도 특성)

  • Lee Myung-Kue;Kim Kwang-Seo;Lee Keun-Ho;Jung Sang-Hwa
    • Journal of the Korea Concrete Institute
    • /
    • v.17 no.4 s.88
    • /
    • pp.613-620
    • /
    • 2005
  • There are some problems in utilizing recycled concrete aggregate go structural use because of the difficulties concerning about quality control and durability. It seems to be possible to utilize recycled concrete aggregate for making concrete products because quality control of concrete products is easier than ready-mixed concrete, but there are little studies about the properties of the steam-cured recycled aggregate concrete. In this study, various tests were performed such as compressive strength, flexural strength, splitting tensile strength, bonding strength and chloride ion penetration test to evaluate the effect of substitution of recycled concrete aggregate. The results of strength test showed that the concrete strength decreased with the increase of the substitution ratio of recycled concrete aggregate, but it was in the reasonable range and almost equal to that of normal concrete below the substitution ratio of $50\%$. On the other hand, strength test of furnace slag cement concrete shows that the strength of recycled concrete with furnace slag cement under curing condition lower than that of recycled concrete with ordinary portland cement under same condition. From the result of this study, it can be concluded that recycled concrete aggregate is able to be utilized for structural use but substitution ratio should be decided with care in each case. The result of this study could be used as the basic data for the structural use of recycled concrete aggregate.

Mechanical Properties and Autogenous Shrinkage of Ultra High Performance Concrete Using Expansive Admixture and Shrinkage Reducing Agent depending on Curing Conditions (팽창재 및 수축저감제를 사용한 초고성능 콘크리트의 양생조건별 역학 및 자기수축 특성)

  • Park, Chun-Jin;Han, Min-Cheol
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.16 no.11
    • /
    • pp.7910-7916
    • /
    • 2015
  • This paper examines the mechanical and autogenous shrinkage characteristics per curing condition of Ultra High Performance Concrete (UHPC) according to the change in the quantities of expansive admixture and shrinkage-reducing agent. In view of the mechanical properties according to the curing condition, all the UHPC specimens that experienced steam curing at $90^{\circ}C$ developed compressive strength higher than 190 MPa, and the specimens that experienced water curing at $20^{\circ}C$ developed compressive strength comparable to that developed at 91 days by the steam-cured specimens. The specimens steam-cured at $90^{\circ}C$ showed high tensile strength of 23.4 MPa whereas slight loss of the tensile strength was observed in those water-cured at 20. Besides, in view of the autogenous shrinkage according to the curing condition, no particular change could be found in the final shrinkage. The compressive strength developed by UHPC according to the use of expansive and shrinkage-reducing agents reached values higher than 190 MPa in case of steam curing at $90^{\circ}C$. Shrinkage reduced by about 45% when using both expansive and shrinkage-reducing agents without difference according to the curing condition.

Influence of Na/Al Ratio and Curing Temperature of Geopolymers on Efflorescence Reduction (Na/Al 비와 양생온도가 지오폴리머의 백화억제에 미치는 영향)

  • Kim, Byoungkwan;Heo, Ye-Eun;Chon, Chul-Min;Lee, Sujeong
    • Resources Recycling
    • /
    • v.27 no.6
    • /
    • pp.59-67
    • /
    • 2018
  • Efflorescence is a white deposit of powders in the surface of cement concrete which can also occur in geopolymers. Efflorescence occurs when sodium ions in alkali activator react with atmospheric carbon dioxide to form sodium carbonate components. In this study, we investigated whether the secondary efflorescence can be reduced by controlling the Na/Al mole ratio or by changing the curing temperature and heat curing time in fly ash-based geopolymers. The 28 days compressive strength in geopolymers having Na/Al ratio of 1.0 was higher than geopolymers having Na/Al ratio of 0.8. The strength increased with the increasing curing temperature and longer heat curing time. On the other hand, efflorescence was lower when the curing temperature was high and the heat curing time was longer in the geopolymers having Na/Al ratio of 1.0. The geopolymers having Na/Al ratio of 0.8 showed accelerated efflorescence occurrence than the geopolymers having Na/Al ratio of 1.0. In order to reduce the occurrence of the secondary efflorescence of fly ash-based geopolymers, it will be advantageous to maintain the Na/Al ratio at 1.0, increase the curing temperature, and lengthen the heating curing time.

Evaluation of Compressive Strength and Freeze-thaw Resistance Properties of Concrete using Superabsorbent Polymer (고 흡수성 폴리머를 혼입한 콘크리트의 압축 강도 및 동결융해 저항성 평가)

  • Kim, Il-Sun;Choi, So-Yeong;Yang, Eun-Ik
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.24 no.5
    • /
    • pp.86-94
    • /
    • 2020
  • When the Superabsorbent Polymer (SAP) is added into concrete, the slump decreases rapidly, deteriorating the workability, the internal curing effect can be obtained through the water absorption and discharge process, and the internal voids of the concrete are increased. In this study, the effects of internal curing and voids were evaluated by evaluating the compressive strength, freeze-thaw resistance, and chloride penetration resistance of SAP-adding concrete that secured workability using a water reducing agent. Also, the internal curing effect of SAP was evaluated by dividing the curing conditions of concrete into water curing and sealed curing. From the result, as the SAP adding ratio increased, the amount of water reducing agent increased, and as for the compressive strength, the SAP adding ratio of 1.5% showed the greatest compressive strength. In particular, in the case of sealed curing showed higher compressive strength than the water curing. It is considered that the compressive strength increased due to the reduction of the effective water-cement ratio and the internal curing effect. Adding 1.0~1.5% of SAP improved the freeze-thaw resistance similar to the case of adding the AE agent, and the addition of more than 1.0% of SAP improved the chloride penetration resistance. The optimal adding ratio of SAP is 1.5%, and the adding ratio of 2.0% or more adversely affects the compressive strength and freeze-thaw resistance.

Comparison of Correlation between Chloride Diffusion and Pores Characteristics in Concrete Cured under Extreme Condition (가혹 조건에서 양생된 콘크리트의 염화물 확산과 공극 특성의 상관관계 비교 )

  • So Yeong Choi;Seong Joon Yang;Il Sun Kim;Eun Ik Yang
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.27 no.4
    • /
    • pp.54-61
    • /
    • 2023
  • In this paper, the compressive strength, pore characteristics, and chloride diffusion coefficient were measured at 28 days of age in order to examine the influence of curing conditions for the chloride diffusion and pores in concrete cured under extreme condition. According to the test results, the compressive strength was improved as the relative humidity increased. Additionally, higher compressive strength was observed when the specimens were cured at 35℃. However, the compressive strength of specimens cured at 45℃ was decreased. Meanwhile, the chloride diffusion coefficient decreased with an increase in curing temperature and relative humidity, indicating a difference compared to the trend observed for compressive strength. On the other hand, the excellent correlation showed between compressive strength and chloride diffusion coefficient, porosity and chloride diffusion coefficient when the concrete cured under water. However, when the concrete cured under extreme condition, this correlation was significantly reduced compared to the water curing case. In contrast, it has been determined that there is no significant correlation between the average pore size and chloride diffusion coefficient, regardless of the curing conditions.

Modified Sulfur Distribution and Compressive Strength Characteristics of Modified Sulfur Mortar Based on the Mixing Method and Curing Condition (비빔방법과 양생조건에 따른 개질유황 모르타르의 개질유황 분포도 및 압축강도 특성)

  • Jung, Byeong-Yeol;Lee, Sang-Soo;Song, Ha-Young
    • Journal of the Korea Institute of Building Construction
    • /
    • v.14 no.1
    • /
    • pp.61-67
    • /
    • 2014
  • As industry advances, the production of industrial sulfur is increasing every year. Therefore, this study intended to investigate the modified sulfur distribution and compressive strength characteristics of modified sulfur mortar based on the mixing method and curing conditions by adding modified sulfur with a melting point of approximately $65^{\circ}C$ in order to provide basic data for the application of the modified sulfur to the mortar or concrete. The results of the experiment showed that the mixture of fine aggregate and cement with water, followed by the addition of modified sulfur, would be most advantageous in terms of fluidity and strength. The results of EDS analysis also showed that the distribution of sulfur was the best. In terms of the curing conditions, the highest compressive strength was achieved through water curing and air dry curing at $20^{\circ}C$. However, it was found that the long-term strength was adversely affected by curing at over $40^{\circ}C$.

Study on the Crack Control Effect of Moist Curing Equipment in Side Wall of Building (습윤양생 장치를 이용한 아파트 측벽 균열제어에 관한 연구)

  • Kim, Dae-Geon;Lee, Dong-Woon
    • Journal of the Korea Institute of Building Construction
    • /
    • v.17 no.2
    • /
    • pp.127-134
    • /
    • 2017
  • In this study, moist curing equipment was used in the exist gang-form system. By achieving sufficient spray curing, the quality of the concrete was improved and the cracking occurred in building's side wall was decreased. The following results could be made as the conclusion. For the compressive strength, all zones showed the similar results. Comparing with the zone without using moist curing equipment, the zone used moist curing equipment showed higher rebound hardness results. For the cracking, the zone utilized moist curing equipment showed the cracking averaged as 6.6 m and the zone without using moist curing equipment showed the cracking averaged as 10.3m. The effectof reducing cracking by utilizing moist curing equipment is about 36 %. Using moist curing equipment is considered as a good solution to reduce the cracking in the structure. Considering all the factors analysed, using moist curing equipment improved the quality of the concrete and decreased the cracking. When this equipment was used in the construction site, it is expected that the construction periodcan be shrunk and the ratio of defect caused by drying shrinkage can be decreased. In this research conditions, The 0.3mm sized moist curing equipment provided the most desirable results on concrete quality and preventing cracking.