• 제목/요약/키워드: $Zn^{2+}$ complex

검색결과 336건 처리시간 0.03초

다공성 SiO2/ITO 나노박막의 전기적 특성 (Electrical Properties of Porous SiO2/ITO Nano Films)

  • 신용욱;김상우
    • 한국재료학회지
    • /
    • 제12권1호
    • /
    • pp.94-99
    • /
    • 2002
  • The electrical properties of porous $SiO_2/ITO$ nano thin film were studied by complex impedance and conductive mechanisms were analyzed. According to the results of complex impedance, the activation energy of $SiO_2/ITO$ and $Zn-SiO_2/ITO$ were 0.309 eV, 0.077 eV in below $450^{\circ}C$ and 0.147 eV in over $450^{\circ}C$, respectively. In case of $SiO_2/ ITO$, slightly direct tunneling occurred at room temperature. The contribution for conduction was very tiny because of high barrier of silica. However, the conductivity abruptly increased in over $300^{\circ}C$ by Thermally assisted tunneling. In case of $Zn-SiO_2/ITO$, high conductivity in 1.26 ${\Omega}^{ -1}{cdot}cm^{-1}$ at room temperature appeared by space charge conduction or Frenkel-poole emission that Zn ions play a role as localized electron states.

산화아연 나노로드 전극을 이용한 전기화학발광 셀의 제작 및 발광특성 고찰 (Fabrication of ZnO Nanorod-based Electrochemical Luminescence Cells and Fundamental Luminescence Properties)

  • 오형석;성열문
    • 전기학회논문지
    • /
    • 제63권1호
    • /
    • pp.76-79
    • /
    • 2014
  • We report Zinc oxide (ZnO) nanorods synthesis and electrochemical luminescence (ECL) cell fabrication. The ECL cell was fabricated using the electrode of ZnO nanorods and Ru(II) complex ($Ru(bpy)_3{^{2+}}$) as a luminescence materials. The fabricated ECL cell is composed of F-doped $SnO_2$ (FTO) glass/ Ru(II)/ZnO nanorods/FTO glass. The highest intensity of the emitting light was obtained at the wavelength of ~620 nm which corresponds to dark-orange color. At a bias voltage of 3V, the measured ECL efficiencies were 5 $cd/m^2$ for cell without ZnO nanorod, 145 $cd/m^2$ for ZnO nanorods-$5{\mu}m$, 208 $cd/m^2$ for ZnO nanorods-$8{\mu}m$ and 275 $cd/m^2$ for ZnO nanorods-$10{\mu}m$, respectively. At a bias voltage of 3.5V, the use of ZnO nanorods increases ECL intensities by about 3 times compared to the typical ECL cell without the use of ZnO nanorods.

TRPHs - 중금속 복합오염토양의 동시 처리를 위한 과황산 산화 - 구연산 세척 혼성공정 개발 (A Continuous Process of Persulfate Oxidation and Citric acid Washing for the Treatment of Complex-Contaminated Soil Containing Total Recoverable Petroleum Hydrocarbons and Heavy Metals)

  • 윤나경;최지연;신원식
    • 한국환경과학회지
    • /
    • 제27권1호
    • /
    • pp.1-10
    • /
    • 2018
  • A continuous process of persulfate oxidation and citric acid washing was investigated for ex-situ remediation of complex contaminated soil containing total recoverable petroleum hydrocarbons (TRPHs) and heavy metals (Cu, Pb, and Zn). The batch experiment results showed that TRPHs could be degraded by $Fe^{2+}$ activated persulfate oxidation and that heavy metals could be removed by washing with citric acid. For efficient remediation of the complex contaminated soil, two-stage and three-stage processes were evaluated. Removal efficiency of the two-stage process (persulfate oxidation - citric acid washing) was 83% for TRPHs and 49%, 53%, 24% for Cu, Zn, and Pb, respectively. To improve the removal efficiency, a three-stage process was also tested; case A) water washing - persulfate oxidation - citirc acid washing and case B) persulfate oxidation - citric acid washing (1) - citric acid washing (2). In case A, 63% of TRPHs, 73% of Cu, 60% of Zn, and 55% of Pb were removed, while the removal efficiencies of TRPHs, Cu, Pb, and Zn were 24%, 68%, 62%, and 59% in case B, respectively. The results indicated that case A was better than case B. The three-stage process was more effective than the two-stage process for the remediation of complex-contaminated soil in therms of overall removal efficiency.

속 이온과 CFP 상호작용: 흡수 형광 분광법에 의한 금속 이온과 CFP의 착물 형성 (Interaction of CFP with Metal ions: Complex Formation of CFP with Metal ion by Absorption and Fluorescence Spectrophotometery)

  • Siddiqi, K.S.;Mohd, Ayaz;Khan, Aftab Aslam Parwaz;Bano, Shaista
    • 대한화학회지
    • /
    • 제53권2호
    • /
    • pp.152-158
    • /
    • 2009
  • 산성 용액에서 $Ca^{2+},\;Mg^{2+},\;Mn^{2+},\;Fe^{3+},\;Co^{2+},\;Ni^{2+},\;Cu^{2+}$$Zn^{2+}$와 Cefpodoxime proxetil (CFP)의 상 호작용을 분광학적으로 조사한 결과 1:1 착물이 형성됨을 알 수 있다. 순수한 약품의 흡수스펙트럼은 270과 345 nm에서 두 개의 현저한 봉오리를 보였다. 여러 pH에서 스펙트럼은 두 개의 isosbestic 점(305 과 330 nm)을 나타내었다. 이는 용액상에서 약품의 쯔비터 이온이 존재함을 의미한다. 다른 농도의 금 속이온에서 CFP의 형광방출 스펙트럼은 chelating enhancement fluorescence(CHEF)효과에 의해 형광강 도가 증가함을 알 수 있었다. 착체의 화학량론은 Job’'s 와 Benesi-Hildebrand 방법에 의해 결정되었다. 착 체의 안정도는 다음 순서와 같다. $Ca^{2+}\;<\;Mg^{2+}\;<\;Co^{2+}\;<\;Ni^{2+}\;<\;Zn^{2+}\;<\;Mn^{2+}\;<\;Cu^{2+}\;<\;Fe^{3+}$.

Energy Band Structure and Photocatalytic Property of Fe-doped Zn2TiO4 Material

  • Jang, Jum-Suk;Borse, Pramod H.;Lee, Jae-Sung;Lim, Kwon-Taek;Jung, Ok-Sang;Jeong, Euh-Duck;Bae, Jong-Seong;Won, Mi-Sook;Kim, Hyun-Gyu
    • Bulletin of the Korean Chemical Society
    • /
    • 제30권12호
    • /
    • pp.3021-3024
    • /
    • 2009
  • $Zn_2Ti_{1-x}Fe_xO_4\;(0\;{\leq}\;x\;{\leq}\;0.7)$ photocatalysts were synthesized by polymerized complex (PC) method and investigated for its physico-chemical as well as optical properties. $Zn_2Ti_{1-x}Fe_xO_4$ can absorb not only UV light but also visible light region due to doping of Fe in the Ti site of $Zn_2TiO_4$ lattice because of the band transition from Fe 3d to the Fe 3d + Ti3d hybrid orbital. The photocatalytic activity of Fe doped $Zn_2TiO_4$ samples for hydrogen production under UV light irradiation decreased with an increase in Fe concentration in $Zn_2TiO_4$. Consequently, there exists an optimized concentration of iron for improved photocatalytic activity under visible light (${\lambda}{\leq}$420 nm)

Zinc Porphyrin-Cored Dendrimers; Axial Coordination of Pyridine and Photoinduced Electron Transfer to Methyl Viologen

  • Park, Ji-Eun;Choi, Dae-Ock;Shin, Eun-Ju
    • Bulletin of the Korean Chemical Society
    • /
    • 제32권12호
    • /
    • pp.4247-4252
    • /
    • 2011
  • The porphyrin-incorporated arylether dendrimers ZnP-D1 and ZnP-D4 were investigated to discover the influence of dendritic environments for the axial ligation of pyridine and photoinduced electron transfer by methyl viologen. Absorption and fluorescence spectra of ZnP, ZnP-D1, and ZnP-D4 were measured in dichloromethane with the addition of pyridine or methyl viologen dichloride. Axial ligation of pyridine was confirmed by red-shifted absorption spectrum. The complex formation constants $K_f$ (Table 1) for axial coordination of pyridine on ZnP, ZnP-D1, and ZnP-D4 were estimated to be $4.4{\times}10^3\;M^{-1}$, $3.3{\times}10^3\;M^{-1}$, and $1.7{\times}10^3\;M^{-1}$, respectively. The photoinduced electron transfer to methyl viologen dichloride was confirmed by fluorescence quenching. Stern-Volmer constants Ksv for ZnP, ZnP-D1, and ZnP-D4 were calculated to be $2.6{\times}10^3$, $2.5{\times}10^3$, and $2.1{\times}10^3$, respectively. ZnP-D4 surrounded by 4 aryl ether dendrons shows the smallest $K_f$ and Ksv values, with comparison to ZnP and ZnP-D1.

복합형 등방성 Ferrite-Rubber Composite의 전자파 흡수특성에 관한 연구 (A Study on Electromagnetic Wave Absorbing Properties of Complex Isotropic Ferrite-Rubber Composite)

  • 김동일;박연준;김하근;사공건
    • 한국정보통신학회논문지
    • /
    • 제3권1호
    • /
    • pp.35-42
    • /
    • 1999
  • This paper describes the characteristics of the complex isotropic ferrite-rubber composite for a super wideband electromagnetic absorber in RP-A-PF type, which can be used for an anechoic chamber, wall material to prevent TV ghost, etc. The $Ni_x-A_{0.1}-ZN_{(1-x0.1)}$. $Fe{_2}O_4$ ferrite powder has been fabricated. Using this, then, [$Ni_x-A_{0.1}-ZN_{(1-x0.1)}$. $Fe{_2}O_4$]-Rubber composite for RF-layer in the RF-A-PF type absorber has been fabricated and it's characteristics has been analyzed. As a result, it has been shown that the [$Ni_x-A_{0.1}-ZN_{(1-x0.1)}$. $Fe{_2}O_4$].Rubber composite has excellent electromagnetic wave absorbing properties.

  • PDF

NiCuZn 페라이트의 제조 조건에 따른 전자파흡수 특성에 관한 연구 (A Study on the Electromagnetic Wave Absorption Properties by the Preparing Condition of NiCuZn Ferrite)

  • 이영구;박찬규;이문수
    • 한국전자파학회:학술대회논문집
    • /
    • 한국전자파학회 2001년도 종합학술발표회 논문집 Vol.11 No.1
    • /
    • pp.304-309
    • /
    • 2001
  • With the development of electromagnetic communication technology and increased use of electromagnetic wave, the countermeasure of EMI(Electromagnetic Interference) becomes more important socially, and interest for the electromagnetic wave absorber has also increased. In this paper, we have studied characteristics of frequency dependency on complex permittivity and complex permeability according to the changes of composition rate and sintering temperature of NiCuZn ferrite also known as electromagnetic wave absorber and further looked into effect of electromagnetic wave absorption properties. From the measurement where the composition of Fe$_2$O$_3$ and ZnO of NiCuZn ferrite was fixed at 49 and 34 mol% respectively while composition of NiO and CuO has been varied at each test, we found out that initial permeability and permittivity were high and the absorbing ability of electromagnetic wave recorded best with loss tangent(${\mu}$r"/${\mu}$r′) displays more than 1 within the frequency band of 2MHz~9.5MHz when the composition ratio of NiO was ranged around 8.5~9.5 mol% and the sintering temperature was 1,080$^{\circ}C$.

  • PDF

A Study on photoluminescience of ZnSe/GaAs epilayer

  • Park, Changsun;Kwangjoon Hong
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2003년도 춘계학술발표강연 및 논문개요집
    • /
    • pp.84-84
    • /
    • 2003
  • The ZnSe epilayers were grown on the GaAs substrate by hot wall epitaxy. After the ZnSe epilayers treated in the vacuum-, Zn-, and Se-atmosphere, respectively, the defects of the epilayer were investigated by means of the low-temperature photoluminescence measurement. The dominant peaks at 2.7988 eV and 2.7937 eV obtained from the PL spectrum of the as-grown ZnSe epilayer were found to be consistent with the upper and the lower polariton peak of the exciton, I$_2$ (D$^{\circ}$, X), bounded to the neutral donor associated with the Se-vacancy. This donor-impurity binding energy was calculated to be 25.3meV The exciton peak, lid, at 2.7812 eV was confirmed to be bound to the neutral acceptor corresponded with the Zn-vacancy. The I$_1$$\^$d/ peak was dominantly observed in the ZnSe/GaAs:Se epilayer treated in the Se-atmosphere. This Se-atmosphere treatment may convert the ZnSe/GaAs:Se epilayer into the p-type. The SA peak was found to be related to a complex donor like a (V$\sub$se/ - V$\sub$zn/) - V$\sub$zn-/

  • PDF

Properties of photoluminescience for ZnSe/GaAs epilayer grown by hot wall epitaxy

  • Hong, Kwangjoon;Baek, Seungnam
    • 한국결정성장학회지
    • /
    • 제13권3호
    • /
    • pp.105-110
    • /
    • 2003
  • The ZnSe epilayers were grown on the GaAs substrate by hot wall epitaxy. After the ZnSe epilayers treated in the vacuum-, Zn-, and Se-atmosphere, respectively, the defects of the epilayer were investigated by means of the low-temperature photoluminescence measurement. The dominant peaks at 2.7988 eV and 2.7937 eV obtained from the PL spectrum of the as-grown ZnSe epilayer were found to be consistent with the upper and the lower polariton peak of the exciton, $I_{2}$ ($D^{\circ}$, X), bounded to the neutral donor associated with the Se-vacancy. This donor-impurity binding energy was calculated to be 25.3 meV, The exciton peak, $I_{1}^{d}$ at 2.7812 eV was confirmed to be bound to the neutral acceptor corresponded with the Zn-vacancy. The $I_{1}^{d}$ peak was dominantly observed in the ZnSe/GaAs : Se epilayer treated in the Se-atmosphere. This Se-atmosphere treatment may convert the ZnSe/GaAs : Se epilayer into the p-type. The SA peak was found to be related to a complex donor like a $(V_{se}-V_{zn})-V_{zn}$.