PECVD를 이용한 Si$_3$N$_4$ 박막의 공정변수에 따른 특성분석과 응용 (Analyses of Si$_3$N$_4$ thin film as parameters of the processes using PECVD for MMIC applications)

  • 신재완;이복형;이성대;이일형;윤관기;전병철;양성환;이호준;이진구
    • 대한전자공학회:학술대회논문집
    • /
    • 대한전자공학회 1999년도 하계종합학술대회 논문집
    • /
    • pp.926-929
    • /
    • 1999
  • In this paper, we have studied the role of sources gases, SiH$_4$, NH$_3$ and $N_2$, to produce Si-N and Si-H bond in PECVD. The correlations of a deposition rate, a refractive index and a permitivity were investigated with the NH$_3$ flow rate of 6, 9 and 12 sccm, and SiH$_4$ flow rate of 20, 30 and 40 sccm, and substrate temperature of 150, 250 and 35$0^{\circ}C$. But the $N_2$ flow rate and chamber pressure were fixed at 55 sccm and 700mTorr. And then MIM capacitors were fabricated and tested for MMIC applications.

  • PDF

Effects of Debinding Atmosphere on Properties of Sintered Reaction-bonded Si3N4 Prepared by Tape Casting Method

  • Park, Ji-Sook;Lee, Sung-Min;Han, Yoon-Soo;Hwang, Hae-Jin;Ryu, Sung-Soo
    • 한국세라믹학회지
    • /
    • 제53권6호
    • /
    • pp.622-627
    • /
    • 2016
  • The effects of the debinding atmosphere on the properties of sintered reaction-bonded $Si_3N_4$ (SRBSN) ceramics prepared by tape casting method were investigated. Si green tape was produced from Si slurry of Si powder, using 11.5 wt% polyvinyl butyral as the organic binder and 35 wt% dioctyl phthalate as the plasticizer. The debinding process was conducted in air and $N_2$ atmospheres at $400^{\circ}C$ for 4 h. The nitridation process of the debinded Si specimens was performed at $1450^{\circ}C$, followed by sintering at $1850^{\circ}C$ and 20 MPa. The results revealed that the debinding atmosphere had a significant effect on $Si_3N_4$ densification and thermal conductivity. Owing to the higher sintered density and larger grain size, the thermal conductivity of $Si_3N_4$ specimens debinded in air was higher than that of the samples debinded in $N_2$. Thus, debinding in air could be suitable for the manufacture of high-performance SRBSN substrates by tape casting.

하이브리드 코팅시스템에 의해 제조된 Mo-Si-N 박막의 미세구조 및 기계적 특성연구 (Microstructure and Mechanical Properties of Mo-Si-N Coatings Deposited by a Hybrid Coating System)

  • 허수정;윤지환;강명창;김광호
    • 한국표면공학회지
    • /
    • 제39권3호
    • /
    • pp.110-114
    • /
    • 2006
  • In this work, comparative studies on microstructure and mechanical properties between $Mo_2N$ and Mo-Si-N coatings were conducted. Ternary Mo-Si-N coatings were deposited on AISI D2 steel substrates by a hybrid method, where AIP technique was combined with a magnetron sputtering technique. Instrumental analyses of XRD, HRTEM, and XPS revealed that the Mo-Si-N coatings must be a composite consisting of fine $Mo_2N$ crystallites and amorphous $Si_3N_4$. The hardness value of Mo-Si-N coatings significantly increased from 22 GPa of $Mo_2N$ coatings to about 37 GPa with Si content of 10 at.% due to the refinement of $Mo_2N$ crystallites and the composite microstructure characteristics. The average friction coefficient of the Mo-Si-N coatings gradually decreased from 0.65 to 0.4 with increasing Si content up to 15 at.%. The effects of Si content on microstructure and mechanical properties of Mo-N coatings were systematically investigated.

전기로를 이용한 Si || SiO2/Si3N4 || Si 이종기판쌍의 직접접합 (Direct Bonding of Si || SiO2/Si3N4 || Si Wafer Pairs With a Furnace)

  • 이상현;이상돈;서태윤;송오성
    • 한국재료학회지
    • /
    • 제12권2호
    • /
    • pp.117-120
    • /
    • 2002
  • We investigated the possibility of direct bonding of the Si ∥SiO$_2$/Si$_3$N$_4$∥Si wafers for Oxide-Nitride-Oxide(ONO) gate oxide applications. 10cm-diameter 2000$\AA$-thick thermal oxide/Si(100) and 500$\AA$-Si$_3$N$_4$LPCVD/Si (100) wafers were prepared, and wet cleaned to activate the surface as hydrophilic and hydrophobic states, respectively. Cleaned wafers were premated wish facing the mirror planes by a specially designed aligner in class-100 clean room immediately. Premated wafer pairs were annealed by an electric furnace at the temperatures of 400, 600, 800, 1000, and 120$0^{\circ}C$ for 2hours, respectively. Direct bonded wafer pairs were characterized the bond area with a infrared(IR) analyzer, and measured the bonding interface energy by a razor blade crack opening method. We confirmed that the bond interface energy became 2,344mJ/$\m^2$ when annealing temperature reached 100$0^{\circ}C$, which were comparable with the interface energy of homeogenous wafer pairs of Si/Si.

Co/Ni 복합 실리사이드 제조 온도에 따른 측벽 스페이서 물질 반응 안정성 연구 (Reaction Stability of Co/Ni Composite Silicide on Side-wall Spacer with Silicidation Temperatures)

  • 송오성;김상엽;정영순
    • 한국표면공학회지
    • /
    • 제38권3호
    • /
    • pp.89-94
    • /
    • 2005
  • We investigate the reaction stability of cobalt and nickel with side-wall materials of $SiO_2\;and\;Si_3N_4$. We deposited 15nm-Co and 15nm-Ni on $SiO_2(200nm)/p-type$ Si(100) and $Si_3N_4(70 nm)/p-type$ Si(100). The samples were annealed at the temperatures of $700\~1100^{\circ}C$ for 40 seconds with a rapid thermal annealer. The sheet resistance, shape, and composition of the residual materials were investigated with a 4-points probe, a field emission scanning electron microscopy, and an AES depth profiling, respectively. Samples of annealed above $1000^{\circ}C$ showed the agglomeration of residual metals with maze shape and revealed extremely high sheet resistance. The Auger depth profiling showed that the $SiO_2$ substrates had no residual metallic scums after $H_2SO_4$ cleaning while $Si_3N_4$ substrates showed some metallic residuals. Therefore, the $SiO_2$ spacer may be appropriate than $Si_3N_4$ for newly proposed Co/Ni composite salicide process.