• Title/Summary/Keyword: $LiTaO_3$single crystal

Search Result 36, Processing Time 0.028 seconds

Raman Spectroscopy of the Solid Solution Limit in $Li_{1-X}Al_{2X}Ta_{1-X}O_3$ System (Raman 분광법을 이용한 $Li_{1-X}Al_{2X}Ta_{1-X}O_3$ 고용한계 분석)

  • Kim, Chong-Don;Hong, Kug-Sun;Joo, Gi-Tae
    • Analytical Science and Technology
    • /
    • v.5 no.1
    • /
    • pp.115-120
    • /
    • 1992
  • The upper limit of solid solution of $Al_2O_3$ in $LiTaO_3$ was investigated using X-ray diffraction and Raman spectroscopy. By substituting cations in $LiTaO_3$ with $Al^{3+}$, the melting temperature was lowed and the ferroelectric properties can be improved. It is easier at lower temperature to fabricate the single crystal used for SAW filters and IR sensors. From the measured lattice constants and Raman band broadening, the solubility limit was X=0.25mol in $Li_{1-X}Al_{2X}Ta{1-X}O_3$, above which $Al_2O_3$ was obsered as a second phase. The Raman band of sintered $LiTaO_3$ was compared with that of the single crystal to see the effect of grain size on the band broadening.

  • PDF

$LiTaO_3$ single crystals growth for SAW device application (표면탄성파 소자 응용을 위한 $LiTaO_3$ 단결정 성장)

  • Chung, D.S.;Roh, Y.R.;Park, B.H.;Kim, Y.S.
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.4 no.2
    • /
    • pp.134-138
    • /
    • 1994
  • $LiTaO_3 (LT)$ single crystals (Y, X-axis) were grown from the congruent composition, 48.65 mole %, $Li_2O$ for SAW (Surface Acoustic Wave) applications. Basic SAW filters were fabricated on the RIST prepared LT wafers (Y-cut) using phtolithography. SAW filter performance was evaluated. The results were compared of the SAW characteristics between RIST prepared LT wafer (Y-cut) and commercial Yamaju wafer (Y-cut). The SAW filter prepared on the RIST grown LT wafer was shown better SAW performances than that of Yamaju wafer.

  • PDF

Electron Paramagnetic Resonance Study of impurity Fe3+ ion in LiTaO3 single crystal (Fe3+ 불순물이 첨가된 LiTaO3 단결정에서의 전자 상자성 공명 연구)

  • Min, S.G.;Yeon, T.H.;Lee, S.H.;Lee, M.K.;Shin, H.K.;Yu, Y.M.;Kim, T.H.;Yu, S.C.
    • Journal of the Korean Magnetics Society
    • /
    • v.13 no.4
    • /
    • pp.171-175
    • /
    • 2003
  • Electron paramagnetic resonance (EPR) of Fe$^{3+}$ in LiTaO$_3$ single crystal, grown by Czochralski method, has been studied by employing an X-band spectrometer. Resonance spectra of Fe$^{3+}$ ion on the crystallographic principal axes were obtained with 9.447 ㎓ at room temperature. The spectroscopic splitting parameter g and zero-field splitting (ZFS) parameter D (= 3 B$_{2}$sup 0/) are calculated with effective spin Hamiltonian. Fe$^{3+}$ center in stoichometric single crystal turns out to be different with that in congruent single crystal reported previously. From the analysis of temperature dependence of resonance fields for Fe$^{3+}$ ion, there is no any phase transition at the temperature range (from -160 $^{\circ}C$ to 20 $^{\circ}C$).

Crystal Growth of $LiTaO_3$ and the Effect pf Crucible Type and Atmosphere ($LiTaO_3$ 단결정 성장과 용기 및 분위기의 영향)

  • 박승익;채승욱;김정돈;주기태;정수진
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.1
    • /
    • pp.39-46
    • /
    • 1994
  • LiTaO3 single crystals were growth without cracking using Pt-Rh crucible and Ir crucible. The starting composition to get the melt of congruent melting composition, which has been dependent upon the experimental procedure, was taken after fixing the total growing process by the result of preliminary experiments. The Rh contamination from the Pt-Rh crucible was to be neglected if the crystal had been grown under inert atmosphere, which resulted in the crystal color being slightly yellow. This color was decolored after 24 hour's annealing at 1200℃ under air atmosphere. The optimum conditions for the crystal growing and the diameter control were so dependent upon the crucible material in spite of using the crucible of the same size. The liquid-solid interface of LiTaO3 crystal of 1" diameter has been flat if the rotation speed was 45rpm.

  • PDF

Development of Piezoelectric Transformer Using The Single Crystal of LiTaO3 (LiTaO3 단결정을 사용한 압전변압기의 개발)

  • Hwang, Sung-Phil;Kim, Moo-Joon;Ha, Kang-Lyeol;Kang, Gab-Joong
    • Journal of Sensor Science and Technology
    • /
    • v.11 no.3
    • /
    • pp.132-137
    • /
    • 2002
  • The single crystal of $LiTaO_3$ ($x-112^{\circ}$ y) has very stable thermal characteristics in a piezoelectric transformer. In this paper, a piezoelectric transformer made of the crystal is newly designed and its operating characteristics are analyzed. The length of the transformer is determined as twice as its width for Lame'-mode because the single crystal of $LiTaO_3$ has low electro-acoustic efficiency. The electric and vibrational characteristics of the transformer is simulated by the PSpice program, and its results are compared to experimental ones. As the results, the ratio of output voltage to input shows large than 10 at 290.83[kHz], which is the frequency coupled the 2nd harmonic for length and the fundamental for width of the Lame'-mode transformer.

Structure and Properties of $LiTaO_3$ Type Solid Solutions in $Li_2O-Al_2O_3-Ta_2O_5$ Ternary System ($Li_2O-Al_2O_3-Ta_2O_5$ 삼성분계에 있어 $LiTaO_3$ 고용체의 구조 및 특성에 관한 연구)

  • 김정돈;흥국선;주기태
    • Journal of the Korean Ceramic Society
    • /
    • v.33 no.4
    • /
    • pp.405-410
    • /
    • 1996
  • The partial substitution of LiTaO3 with Al2O3 caused the variation of dielectric properties and a lower melting temperature yielding an easier growth of single crystal. The lattice constants and Raman band broadening were measured for the LiTaO3 solid solution in which the cations of Li+ and Ta5+ were partially substituted by Al3+ cation. The LiTaO3 type limit phases were obtained. ; Li1.15Al0.45Ta0.7O3 for cationic excess Li1.15Al0.45Ta0.7O3 for stoichiometry Li0.85Al0.05TaO3 for cationic deficit. The second phase was formed beyond the solubility limit. The limit phase (Li0.85Al0.05TaO3) in the region of cationic deficit showed the lowest Cuire temperature of 61$0^{\circ}C$ and melting point of 152$0^{\circ}C$ compared to the solid solutions in other regions (TMp=1$650^{\circ}C$, Tc=69$0^{\circ}C$ for LiTaO3)

  • PDF

Thermal Effects on Stoichiometric LiTaO3 Single Crystal (정비조성 LiTaO3 단결정에 대한 열처리 효과)

  • Yeom, T.H.;Lee, S.H.
    • Journal of the Korean Magnetics Society
    • /
    • v.15 no.3
    • /
    • pp.177-180
    • /
    • 2005
  • Ferroelectric $LiTaO_3$ single crystals, grown by the Czochralski method, were thermally treated at temperature $1000^{\circ}C\;and\;1100^{\circ}C$. Electron paramagnetic resonance (EPR) study of stoichiometric $LiTaO_3$ and thermally treated $LiTaO_3$ crystals has been investigated by employing an X-band spectrometer. From the $Fe^{3+}$ EPR spectra, it turned out that there is no change of site location and local site symmetry around $Fe^{3+}$ impurity ion between stoichiometric and thermally treated $LiTaO_3$ single crystals. We confirmed that the ionic state of $Fe^{3+}$ ion changed after thermal treatment. The EPR parameters of $Fe^{3+}$ ion in $LiTaO_3$ single crystals are determined with effective spin Hamiltonian.

Electron Magnetic Resonance Study of Paramagnetic Impurities in LiTaO3 and LiMbO3 Single Crystals (LiTaO3 및 LiMbO3 단결정 내의 상자성 불순물에 관한 전자 자기공명 연구)

  • Yeom, Tae-Ho
    • Journal of the Korean Magnetics Society
    • /
    • v.13 no.5
    • /
    • pp.204-210
    • /
    • 2003
  • Electron magnetic resonance (EMR) of paramagnetic Cr$^{3+}$, Mn$^{2+}$, and Fe$^{3+}$ impurity ions in ferroelectric LiNbO$_3$ and LiTaO$_3$ single crystals has been studied. The actual sites location of paramagnetic impurity ions in the crystals was suggested from the experimental results and zero field splitting parameters calculated by superposition model. It turns out that Cr$^{3+}$ ions in LiNbO$_3$ crystal have two resonance centers and enter both the Li$^{+}$ and Nb$^{5+}$ ions. Mn$^{2+}$ and Fe$^{3+}$ impurity ions in LiNbO$_3$ substitute for Nb$^{5+}$ ions. However, both Cr$^{3+}$ and Fe$^{3+}$ ions in LiTaO$_3$ crystal reside at Li$^{+}$ ions.$ +/ ions.+/ ions.