The Electrical Characteristics of Pentacene Thin-Film for the active layer of Organic TFT deposited at the Various Evaporation conditions and the Annealing Temperatures (증착조건 및 열처리 온도에 따른 유기 TFT의 활성층용 펜타센 박막의 전기적 특성 연구)

  • 구본원;정민경;김도현;송정근
    • Proceedings of the IEEK Conference
    • /
    • 2000.06b
    • /
    • pp.80-83
    • /
    • 2000
  • In this work we deposited Pentacene thin film by OMBD at the various substrate temperatures, deposition rate and the various annealing temperatures for the fabrication of organic TFT and investigated the electrical and film surface characteristics such as sheet resistance, contact resistance and conductance Film thickness were measured by $\alpha$-step and the sheet resistance, contact resistance and conductance were extracted from the relation between the distance of the contacts and the resistance. During the film deposition the substrate temperature was held at 3$0^{\circ}C$, 4$0^{\circ}C$, 5$0^{\circ}C$, 6$0^{\circ}C$, 8$0^{\circ}C$ and 10$0^{\circ}C$, respectively. After the film deposition, Au contact was deposited by thermal evaporation. For the effect of annealing, the thin film was annealed in the nitrogen environment at 10$0^{\circ}C$ and 14$0^{\circ}C$ for 10 seconds, respectively. Film surface characteristics at the vatious substrate temperatures were measured by AFM. The crystallization of thin film was improved as the substrate temperatures were increased and the maximum gram size was 4${\mu}{\textrm}{m}$. The conductivity of thin film was found to be 7.40 $\times$10$^{-7}$ ~ 7.78$\times$10$^{-6}$ S/cm and the minimum contact resistance was 2.5324 ㏁.

  • PDF

A Study on the Fabrications and the Principal features of Solar Cell (CdS 태양전지의 제작과 그 특성에 관하여)

  • Kim, Myeong-Gi;Hong, Chang-Hui;Choe, Bu-Gwi
    • Journal of the Korean Institute of Telematics and Electronics
    • /
    • v.15 no.3
    • /
    • pp.18-23
    • /
    • 1978
  • In order to improve the efficiency of Cu2-xS-CdS PN junction type solar cell, a method of reducing the series resiatance is considered. In the fabrication of the thin film of Cu2-xS, what has the largest value of conductivity is fabricated at 250 $^{\circ}C$. The thin film of CdS which has beer fabricated at the temperature 250-30$0^{\circ}C$ of the substrate and 800-85$0^{\circ}C$ of evaporating material has the largest value of conductivity and also fairly good photoelectric characteristics. Therefore, the evaporated thin aim type CdS solar cell has been fabricated at the temperature 25$0^{\circ}C$ of the substrate and 800-85$0^{\circ}C$ of the evaporating material, and its efficiency is measured to he 6%.

  • PDF

YBa$_2$Cu$_3$O$_{7-x}$films fabricated on IBAD templates by MOCVD process (MOCVD 공정으로 IBAD 템플릿 위에 제조된 YBa$_2$Cu$_3$O$_{7-x}$ 박막)

  • Jun Byung-Hyuk;Choi Jun-Kyu;Kim Ho-Jin;Kim Chan-Joong
    • Progress in Superconductivity and Cryogenics
    • /
    • v.6 no.3
    • /
    • pp.21-26
    • /
    • 2004
  • Deposition condition of YBa$_2$Cu$_3$$O_{7-x}$ (YBCO) films on moving IBAD templates (CeO$_2$/IBAD-YSZ/SS) was studied in a hot-wall type metal organic chemical vapor deposition (MOCVD) process using single liquid source. The reel velocity was 40 cm/hr and the source mole ratios of Y(tmhd)$_3$:Ba(tmhd)$_2$:Cu(tmhd)$_2$ were 1:2.3:3.1 and 1:2.1:2,9, Two different types of IBAD templates with thin CeO$_2$ and thick CeO$_2$ layers were used, The YBCO films were successfully deposited at the deposition temperatures of 780~89$0^{\circ}C$ ; the a-axis growth was observed together with the c-axis growth up to 83$0^{\circ}C$. while the c-axis growth became dominant above 83$0^{\circ}C$. The top surface of the c-axis film was fairly dense and included a small amount of the a-axis growth, although the peaks of the a-axis grains were not observed in XRD pattern, The YBCO film deposited on IBAD template with thin CeO$_2$ layer showed low critical current of 2.5 A/cm-width. while the YBCO film deposited on IBAD template with thick CeO$_2$ layer showed higher critical current of 50 A/cm-width. This result indicates that thick CeO$_2$ layer is thermally more stable than thin CeO$_2$ layer at the high deposition temperature of the MOCVD process.s.

Electrical properties of the Al doped ZnO thin films fabricated by RF magnetron sputtering system with working pressure and oxygen contents (RF magnetron sputtering법으로 제조한 Al doped ZnO 박막의 산소함량과 압력변화에 따른 전기적 특성 변화)

  • Kim, Jong-Wook;Kim, Hong-Bae
    • Journal of the Semiconductor & Display Technology
    • /
    • v.9 no.4
    • /
    • pp.77-81
    • /
    • 2010
  • The AZO thin films were deposited on the corning 1737 glass plate by the RF magnetron sputtering and effects of working pressure and oxygen contents on the electrical properties were investigated. XRD spectra showed a preferred orientation along the c-axis and a minimum FWHM for the 70mTorr. From the surface analysis (AFM), the number of crystal grain of AZO thin film increased as working pressure increased. The film deposited with 70mTorr of working pressure showed n-type semiconductor characteristic having suitable resistivity $-1.59{\times}10^{-2}{\Omega}cm$, carrier concentration $-10.1{\times}10^{19}cm^{-3}$, and mobility $-4.35cm^2V^{-1}s^{-1}$ while other films by 7 mTorr, 20 mTorr of working pressure closed to metallic films. The films including the oxygen represent stoichiometric composition similar to the oxide. The transmittance of the film was over 85% in the visible light range regardless of the changes in working pressure and oxygen contents.

Study on Low Temperature Formation of Ferroelectric $Sr_{0.9}4$Bi_{2.1}$$Ta_2$$O_9$ Thin Films by Sol-Gel Process and Rapid Thermal Annealing (솔-젤법 및 급속열처리에 의한 $Sr_{0.9}4$Bi_{2.1}$$Ta_2$$O_9$ 박막의 저온형성에 관한 연구)

  • 장현호;송석표;김병호
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.13 no.4
    • /
    • pp.312-317
    • /
    • 2000
  • Ferroelectric S $r_{0.9}$/B $i_{2.1}$/T $a_{2}$/ $O_{9}$ solutions were synthesized using sol-gel process in which strontinum ethoxide bismuth ethoxide trantalum ethoxide were used a s startring materials. SBT thin films were coated on Pt/Ti/ $SiO_2$/Si substrates by spin-coating. rapid thermal annealing (RTA) was used to promote crystallization. Thin films were annealed at $700^{\circ}C$ for 1 hr in an oxygen atmosphere. This temperature is about 10$0^{\circ}C$ lower than the usual annealing temperature for SBT thin films. Pt top-electrode was deposited by sputtering and thin films were post-annealed at $700^{\circ}C$ for 30 min. to enhance electrical properties. As the RTA temperature increased the higher 2 $P_{r}$ values were obtained. At RTA temperature being 78$0^{\circ}C$ remanent polarization of S $r_{0.9}$/B $i_{2.1}$/T $a_{2}$/ $O_{9}$ thin film was 7.73 $\mu$C/cm $_2$ and the leakage current density was 1.14$\times$10$^{-7}$ A/c $m^2$ at 3 V. As RTA temperature increased the breakdown voltage was decreased. It is considered that the low-field breadown is caused by the rough surface of SBT films and forming bismuth metal in SBT thin films.films.lms.

  • PDF

A Study on the Ferromagnetic Resonance of FeNb Thin Films (FeNb 박막의 강자성 공명 연구)

  • Lim, Woo-Young;Baek, Jong-Sung;Lee, Soo-Hyung
    • Journal of the Korean Magnetics Society
    • /
    • v.14 no.4
    • /
    • pp.120-126
    • /
    • 2004
  • In order to understand the temperature dependence of magnetic properties of $F_{84}Nb_{16}$(wt.%) thin films, ferromagnetic resonance experiments have been carried out. The ferromagnetic resonance spectra for all temperatures consist of several volume modes and one (or two) surface modes. It is suggested that both surface of the film have a perpendicular hard axis to the film plane (negative surface magnetic anisotropy). Saturation magnetization coincides with the Block's T$\^$2/3/ and spectroscopic splitting factor is almost constant in the temperature range from 113 K to 293 K. The surface magnetic anisotropy constant K$\_$s2/ of the film-substrate interface increased with decreasing temperature in the temperature range from 233 K to 293 K. The surface magnetic anisotropy constant K$\_$s1/ of the air-substrate interface decreased from -0.322 erg/$\textrm{cm}^2$ to -0.394 erg/$\textrm{cm}^2$ as the temperature decreased to 253 K and was almost constant below 233 K.233 K.

Microwave measurement of Ba$^{0.7}Sr^{0.3}TiO^{3}$ thin film capacitors (Ba$^{0.7}Sr^{0.3}TiO^{3}$ 박막 커패시퍼의 마이코로파 측정)

  • 장병택;차선용;이승훈;곽동화;이희철;유병곤;백종태;유형준
    • Journal of the Korean Institute of Telematics and Electronics A
    • /
    • v.33A no.2
    • /
    • pp.114-121
    • /
    • 1996
  • Thin film Ba$^{0.7}Sr^{0.3}TiO^{3}$ (BST) capacitors were fabricated on SiO$_{2}$/Si substrates by RF magnetron sputtering method and characterized at microwave frequencies ranging from 40 MHz to 1GHz to examine the dielectric dispersion of the capacitors. The BST thin films were electrode material of BST thin films capacitor which is known as one of the best electrode materials for BST films. 50$\AA$-thick titanium (Ti) layers were introduced to increase adhesion between bottom Pt and SiO$_{2}$. The leakage current density of the capacitors was about 1.7${\times}10^{7}A/cm^{2}$ at 1.5V and the dielectric constant was about 140 at 1MHz. Microwave measurement patterns having a coplanar waveguide type were fabricated and their S parameters were measured using network analyzer. After de-embedding parasitic components in microwave measurement patterns nearly frequency-invariant dielectric constant of about 120 was extracted in the measurement range of 40 MHz to 1 GHz.

  • PDF

Electronic and Optical Properties of amorphous and crystalline Tantalum Oxide Thin Films on Si (100)

  • Kim, K.R.;Tahir, D.;Seul, Son-Lee;Choi, E.H.;Oh, S.K.;Kang, H.J.;Yang, D.S.;Heo, S.;Park, J.C.;Chung, J.G.;Lee, J.C.
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2010.02a
    • /
    • pp.382-382
    • /
    • 2010
  • $TaO_2$ thin films as gate dielectrics have been proposed to overcome the problems of tunneling current and degradation mobility in achieving a thin equivalent oxide thickness. An extremely thin $SiO_2$ layer is used in order to separate the carrier in MOSFETchannel from the dielectric field fluctuation caused by phonons in the dielectric which decreases the carrier mobility. The electronic and optical properties influenced the device performance to a great extent. The atomic structure of amorphous and crystalline Tantalum oxide ($TaO_2$) gate dielectrics thin film on Si (100) were grown by utilizing atomic layer deposition method was examined using Ta-K edge x-ray absorption spectroscopy. By using X-ray photoelectron spectroscopy and reflection electron energy loss spectroscopy (REELS) the electronic and optical properties was obtained. In this study, the band gap (3.400.1 eV) and the optical properties of $TaO_2$ thin films were obtained from the experimental inelastic scattering cross section of reflection electron energy loss spectroscopy (REELS) spectra. EXAFS spectra show that the ordered bonding of Ta-Ta for c-$TaO_2$ which is not for c-$TaO_2$ thin film. The optical properties' e.g., index refractive (n), extinction coefficient (k) and dielectric function ($\varepsilon$) were obtained from REELS spectra by using QUEELS-$\varepsilon$(k, $\omega$)-REELS software shows good agreement with other results. The energy-dependent behaviors of reflection, absorption or transparency in $TaO_2$ thin films also have been determined from the optical properties.

  • PDF

Preparation of p-type transparent semiconductor $SrCu_2O_2$ thin film by RF magnetron sputtering (RF 마그네트론 스퍼터링에 의한 p형 투명 반도체 $SrCu_2O_2$ 박막의 제조)

  • Kim, Sei-Ki;Seok, Hye-Won;Lee, Mi-Jae;Choi, Byung-Hyun;Jeong, Won-Hee
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.47-47
    • /
    • 2008
  • P-type transparent semiconductor $SrCu_2O_2$ thin films have been prepared by RF sputtering using low-alkali glass for LCD and quartz as substrates. Single phase of $SrCu_2O_2$ powder was obtained by heating a stoichiometric mixture of CuO and $SrCO_3$ at 1223K for 96h under N2 gas flow, and target was fabricated at 1243K for 24h. Room temperature conductivity of the sintered body was about 0.02S/cm, and the activation energy in the temperature range of $-50^{\circ}C$~RT and RT~$150^{\circ}C$ were 0.18eV, 0.07eV, respectively. Effects of deposition pressure and post-annealing temperature on the electrical and optical properties of the obtained thin film have been investigated.

  • PDF

Influence of Deposition Pressure on Structural and Optical Properties of SnS Thin Films Grown by RF Magnetron Sputtering (RF 마그네트론 스퍼터링법으로 성장 된 SnS 박막의 구조적 및 광학적 특성에 대한 증착 압력의 영향)

  • Son, Seung-Ik;Lee, Sang Woon;Son, Chang Sik;Hwang, Donghyun
    • Current Photovoltaic Research
    • /
    • v.8 no.1
    • /
    • pp.33-38
    • /
    • 2020
  • Single-phased SnS thin films have been prepared by RF magnetron sputtering at various deposition pressures. The effect of deposition pressure on the structural and optical properties of polycrystalline SnS thin films was studied using X-ray diffraction (XRD), field-emission scanning electron microscopy (FE-SEM), X-ray photoelectron spectroscopy (XPS) and ultraviolet-visible-near infrared (UV-Vis-NIR) spectrophotometer. The XRD analysis revealed the orthorhombic structure of the SnS thin films oriented along the (111) plane direction. As the deposition pressure was increased from 5 mTorr to 15 mTorr, the intensity of the peak on the (111) plane increased, and the intensity decreased under the condition of 20 mTorr. The binding energy difference at the Sn 3d5/2 and S 2p3/2 core levels was about 324.5 eV, indicating that the SnS thin film was prepared as a pure Sn-S phase. The optical properties of the SnS thin films indicate the presence of direct allowed transitions with corresponding energy band gap in the rang 1.47-1.57 eV.