The Characteristics of (Ba,Sr)$TiO_3$ Thin Films Etched With The high Density $BCl_3/Cl_2$/Ar Plasma ($BCl_3/Cl_2$/Ar 고밀도 플라즈마에서 (Ba,Sr)$TiO_3$ 박막의 식각 특성에 관한 연구)

  • Kim, Seung-Bum;Kim, Chang-Il
    • Proceedings of the KIEE Conference
    • /
    • 1999.11d
    • /
    • pp.863-866
    • /
    • 1999
  • (Ba,Sr)$TiO_3$ thin films have attracted groat interest as new dielectric materials of capacitors for ultra-large-scale integrated dynamic random access memories (ULSI-DRAMs) such as 1 Gbit or 4 Gbit. In this study, inductively coupled $BCl_3/Cl_2$/Ar plasmas was used to etch (Ba,Sr)$TiO_3$ thin films. RF power/dc bias voltage = 600 W/-250 V and chamber pressure was 10 mTorr. The $Cl_2/(Cl_2+Ar)$ was fixed at 0.2, the (Ba,Sr)$TiO_3$ thin films were etched adding $BCl_3$. The highest (Ba,Sr)$TiO_3$ etch rate is 480$\AA/min$ at 10 % $BCl_3$ adding to $Cl_2$/Ar. The characteristics of the plasmas were estimated using optical emission spectroscopy (OES). The change of Cl, B radical density measured by OES as a function of $BCl_3$ percentage in $Cl_2$/Ar. The highest Cl radical density was shown at the addition of 10% $BCl_3$ to $Cl_2$/Ar. To study on the surface reaction of (Ba,Sr)$TiO_3$ thin films was investigated by XPS analysis. Ion enhancement etching is necessary to break Ba-O bond and to remove $BaCl_2$. There is a little chemical reaction between Sr and Cl, but Sr is removed by physical sputtering. There is a chemical reaction between Ti and Cl, and Tic14 is removed with ease. The cross-sectional of (Ba,Sr)$TiO_3$ thin film was investigated by scanning electron microscopy (SEM), the etch slope is about $65\;{\sim}\;70$.

  • PDF

유도결합 $Cl_2/CHF_3, Cl_2/CH_4, Cl_2/Ar $플라즈마를 이용한 InGaN 건식 식각 반응 기구 연구

  • 이도행;김현수;염근영;이재원;김태일
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 1999.07a
    • /
    • pp.249-249
    • /
    • 1999
  • GaN과 같은 III-nitride 반도체 관한 식각 기술의 연구는 blue-emitting laser diode(LD)를 위한 경면(mirror facet)의 형성뿐만아니라 새로운 display 용도의 light emitting diodes (LED), 고온에서 작동되는 광전소자 제조 등에도 그 중요성이 증대되고 있다. 최근에는 III-nitride 물질의 높은 식각속도와 미려하고 수직한 식각형상을 이루기 위하여 ECR(Electron Cyclotron Resonance)이나 ICP(Inductively Coupled Plasma)와 같은 고밀도 플라즈마 식각과 CAIBE(Chemically assisted ion beam etching)를 이용한 연구가 진행되고 있다. 현재 제조되어 지고 있는 LED 및 LD와 같은 광소자의 구조의 대부분은 p-GaN/AlGaN/InGaN(Q.W)/AlGaN/n-GaN 와 같은 여러 층의 형태로 이루어져 있다. 이중 InGaN는 광소자나 전자소자의 특성에 영향을 주는 가장 중요한 부분으로써 현재까지 보고된 식각연구는 undoped GaN에 대부분 집중되고 있고 이에 비해 소자 특성에 핵심을 이루는 InGaN의 식각특성에 관한 연구는 미흡한 상황이다. 본 연구에서는 고밀도 플라즈마원인 ICP 장비를 이용하여 InGaN를 식각하였고, 식각에는 Cl2/CH4, Cl2/Ar 플라즈마를 사용하였다. InGaN의 식각특성에 영향을 미치는 플라즈마의 특성을 관찰하기 위하여 quadrupole mass spectrometry(QMS)와 optical emission spectroscopy(PES)를 사용하였다. 기판 온도는 5$0^{\circ}C$, 공정 압력은 5,Torr에서 30mTorr로 변화시켰고 inductive power는 200~800watt, bias voltage는 0~-200voltage로 변화시켰으며 식각마스크로는 SiO2를 patterning 하여 사용하였다. n-GaN, p-GaN 층 이외에 광소자 제조시 필수적인 InGaN 층을 100% Cl2로 식각한 경우에 InGaN의 식각속도가 GaN에 비해 매우 낮은 식각속도를 보였다. Cl2 gas에 소량의 CH4나 Ar gas를 첨가하는 경우와 공정압력을 감소시키는 경우 식각속도는 증가하였고, Cl2/10%Ar 플라즈마에서 공정 압력을 감소시키는 경우 식각속도는 증가하였고, Cl2/10%CHF3 와 Cl2/10%Ar 플라즈마에서 공정압력을 15mTorr로 감소시키는 경우 InGaN과 GaNrks의 선택적인 식각이 가능하였다. InGaN의 식각속도는 Cl2/Ar 플라즈마의 이온에 의한 Cl2/CHF3(CH4) 플라즈마에서의 CHx radical 형성에 의하여 증가하는 것으로 사료되어 진다.

  • PDF

Effects of $O_2$ Gas Addition to Etching of Platinum Thin Film by Inductively Coupled Plasmas (유도 결합 플라즈마를 이용한 백금 박막의 식각시 $O_2$ 가스 첨가 효과)

  • Kim, Nam-Hoon;Kim, Chang-Il;Kwon, Kwang-Ho;Chang, Eui-Goo
    • Proceedings of the KIEE Conference
    • /
    • 1998.11c
    • /
    • pp.770-772
    • /
    • 1998
  • The highest etch rate of Pt film was obtained at 10% $Cl_2$/90% Ar gas mixing ratio in our previous investigation. However, the problems such as the etch residues(fence) remained on the pattern sidewall, low selectivity to oxide as mask and low etch slope were presented. In this paper, the etching by additive $O_2$ gas to 10% $Cl_2$/90% Ar gas base was examined. As a result, the fence-free pattern and high etch slope was observed and the selectivity to oxide increased without decreasing of the etch rate. And the reasons for this phenomenon was investigated by XPS(x-ray photoelectron spectroscopy) surface analysis and plasma characteristic.

  • PDF

Etch characteristics of TiN thin film adding $Cl_2$ in $BCl_3$/Ar Plasma ($BCl_3$/Ar 플라즈마에서 $Cl_2$ 첨가에 따른 TiN 박막의 식각 특성)

  • Um, Doo-Seung;Kang, Chan-Min;Yang, Xue;Kim, Dong-Pyo;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.168-168
    • /
    • 2008
  • Dimension of a transistor has rapidly shrunk to increase the speed of device and to reduce the power consumption. However, it is accompanied with several problems like direct tunneling through the gate dioxide layer and low conductivity characteristic of poly-Si gate in nano-region. To cover these faults, study of new materials is urgently needed. Recently, high dielectric materials like $Al_2O_3$, $ZrO_2$, and $HfO_2$ are being studied for equivalent oxide thickness (EOT). However, poly-Si gate is not compatible with high-k materials for gate-insulator. Poly Si gate with high-k material has some problems such as gate depletion and dopant penetration problems. Therefore, new gate structure or materials that are compatible with high-k materials are also needed. TiN for metal/high-k gate stack is conductive enough to allow a good electrical connection and compatible with high-k materials. According to this trend, the study on dry etching of TiN for metal/high-k gate stack is needed. In this study, the investigations of the TiN etching characteristics were carried out using the inductively coupled $BCl_3$-based plasma system and adding $Cl_2$ gas. Dry etching of the TiN was studied by varying the etching parameters including $BCl_3$/Ar gas mixing ratio, RF power, DC-bias voltage to substrate, and $Cl_2$ gas addition. The plasmas were characterized by optical emission spectroscopy analysis. Scanning electron microscopy was used to investigate the etching profile.

  • PDF

Ridge Formation by Dry-Etching of Pd and AlGaN/GaN Superlattice for the Fabrication of GaN Blue Laser Diodes

  • Kim, Jae-Gwan;Lee, Dong-Min;Park, Min-Ju;Hwang, Seong-Ju;Lee, Seong-Nam;Gwak, Jun-Seop;Lee, Ji-Myeon
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2012.02a
    • /
    • pp.391-392
    • /
    • 2012
  • In these days, the desire for the precise and tiny displays in mobile application has been increased strongly. Currently, laser displays ranging from large-size laser TV to mobile projectors, are commercially available or due to appear on the market [1]. In order to achieve a mobile projectors, the semiconductor laser diodes should be used as a laser source due to their size and weight. In this presentation, the continuous etch characteristics of Pd and AlGaN/GaN superlattice for the fabrication of blue laser diodes were investigated by using inductively coupled $CHF_3$ and $Cl_2$ -based plasma. The GaN laser diode samples were grown on the sapphire (0001) substrate using a metal organic chemical vapor deposition system. A Si-doped GaN layer was grown on the substrate, followed by growth of LD structures, including the active layers of InGaN/GaN quantum well and barriers layer, as shown in other literature [2], and the palladium was used as a p-type ohmic contact metal. The etch rate of AlGaN/GaN superlattice (2.5/2.5 nm for 100 periods) and n-GaN by using $Cl_2$ (90%)/Ar (10%) and $Cl_2$ (50%)/$CHF_3$ (50%) plasma chemistry, respectively. While when the $Cl_2$/Ar plasma were used, the etch rate of AlGaN/GaN superlattice shows a similar etch rate as that of n-GaN, the $Cl_2/CHF_3$ plasma shows decreased etch rate, compared with that of $Cl_2$/Ar plasma, especially for AlGaN/GaN superlattice. Furthermore, it was also found that the Pd which is deposited on top of the superlattice couldn't be etched with $Cl_2$/Ar plasma. It was indicating that the etching step should be separated into 2 steps for the Pd etching and the superlattice etching, respectively. The etched surface of stacked Pd/superlattice as a result of 2-step etching process including Pd etching ($Cl_2/CHF_3$) and SLs ($Cl_2$/Ar) etching, respectively. EDX results shows that the etched surface is a GaN waveguide free from the Al, indicating the SLs were fully removed by etching. Furthermore, the optical and electrical properties will be also investigated in this presentation. In summary, Pd/AlGaN/GaN SLs were successfully etched exploiting noble 2-step etching processes.

  • PDF

The surface kinetic properties between $BCl_3/Cl_2$/Ar plasma and $Al_2O_3$ thin film

  • Yang, Xue;Kim, Dong-Pyo;Um, Doo-Seung;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.06a
    • /
    • pp.169-169
    • /
    • 2008
  • To keep pace with scaling trends of CMOS technologies, high-k metal oxides are to be introduced. Due to their high permittivity, high-k materials can achieve the required capacitance with stacks of higher physical thickness to reduce the leakage current through the scaled gate oxide, which make it become much more promising materials to instead of $SiO_2$. As further studying on high-k, an understanding of the relation between the etch characteristics of high-k dielectric materials and plasma properties is required for the low damaged removal process to match standard processing procedure. There are some reports on the dry etching of different high-k materials in ICP and ECR plasma with various plasma parameters, such as different gas combinations ($Cl_2$, $Cl_2/BCl_3$, $Cl_2$/Ar, $SF_6$/Ar, and $CH_4/H_2$/Ar etc). Understanding of the complex behavior of particles at surfaces requires detailed knowledge of both macroscopic and microscopic processes that take place; also certain processes depend critically on temperature and gas pressure. The choice of $BCl_3$ as the chemically active gas results from the fact that it is widely used for the etching o the materials covered by the native oxides due to the effective extraction of oxygen in the form of $BCl_xO_y$ compounds. In this study, the surface reactions and the etch rate of $Al_2O_3$ films in $BCl_3/Cl_2$/Ar plasma were investigated in an inductively coupled plasma(ICP) reactor in terms of the gas mixing ratio, RF power, DC bias and chamber pressure. The variations of relative volume densities for the particles were measured with optical emission spectroscopy (OES). The surface imagination was measured by AFM and SEM. The chemical states of film was investigated using X-ray photoelectron spectroscopy (XPS), which confirmed the existence of nonvolatile etch byproducts.

  • PDF

Plasma Etching Characteristics of Sapphire Substrate using $BCl_3$-based Inductively Coupled Plasma ($BCl_3$ 계열 유도결합 플라즈마를 이용한 사파이어 기판의 식각 특성)

  • Kim, Dong-Pyo;Woo, Jong-Chang;Um, Doo-Seng;Yang, Xue;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2008.11a
    • /
    • pp.363-363
    • /
    • 2008
  • The development of dry etching process for sapphire wafer with plasma has been key issues for the opto-electric devices. The challenges are increasing control and obtaining low plasma induced-damage because an unwanted scattering of radiation is caused by the spatial disorder of pattern and variation of surface roughness. The plasma-induced damages during plasma etching process can be classified as impurity contamination of residual etch products or bonding disruption in lattice due to charged particle bombardment. Therefor, fine pattern technology with low damaged etching process and high etch rate are urgently needed. Until now, there are a lot of reports on the etching of sapphire wafer with using $Cl_2$/Ar, $BCl_3$/Ar, HBr/Ar and so on [1]. However, the etch behavior of sapphire wafer have investigated with variation of only one parameter while other parameters are fixed. In this study, we investigated the effect of pressure and other parameters on the etch rate and the selectivity. We selected $BCl_3$ as an etch ant because $BCl_3$ plasmas are widely used in etching process of oxide materials. In plasma, the $BCl_3$ molecule can be dissociated into B radical, $B^+$ ion, Cl radical and $Cl^+$ ion. However, the $BCl_3$ molecule can be dissociated into B radical or $B^+$ ion easier than Cl radical or $Cl^+$ ion. First, we evaluated the etch behaviors of sapphire wafer in $BCl_3$/additive gases (Ar, $N_2,Cl_2$) gases. The behavior of etch rate of sapphire substrate was monitored as a function of additive gas ratio to $BCl_3$ based plasma, total flow rate, r.f. power, d.c. bias under different pressures of 5 mTorr, 10 mTorr, 20 mTorr and 30 mTorr. The etch rates of sapphire wafer, $SiO_2$ and PR were measured with using alpha step surface profiler. In order to understand the changes of radicals, volume density of Cl, B radical and BCl molecule were investigated with optical emission spectroscopy (OES). The chemical states of $Al_2O_3$ thin films were studied with energy dispersive X-ray (EDX) and depth profile anlysis of auger electron spectroscopy (AES). The enhancement of sapphire substrate can be explained by the reactive ion etching mechanism with the competition of the formation of volatile $AlCl_3$, $Al_2Cl_6$ or $BOCl_3$ and the sputter effect by energetic ions.

  • PDF

A Study on the etching mechanism of $CeO_2$ thin film by high density plasma (고밀도 플라즈마에 의한 $CeO_2$ 박막의 식각 메커니즘 연구)

  • Oh, Chang-Seok;Kim, Chang-Il
    • Journal of the Institute of Electronics Engineers of Korea SD
    • /
    • v.38 no.12
    • /
    • pp.8-13
    • /
    • 2001
  • Cerium oxide ($CeO_2$) thin film has been proposed as a buffer layer between the ferroelectric thin film and the Si substrate in Metal-Ferroelectric-Insulator-Silicon (MFIS) structures for ferroelectric random access memory (FRAM) applications. In this study, $CeO_2$ thin films were etched with $Cl_2$/Ar gas mixture in an inductively coupled plasma (ICP). Etch properties were measured for different gas mixing ratio of $Cl_2$($Cl_2$+Ar) while the other process conditions were fixed at RF power (600 W), dc bias voltage (-200 V), and chamber pressure (15 mTorr). The highest etch rate of $CeO_2$ thin film was 230 ${\AA}$/min and the selectivity of $CeO_2$ to $YMnO_3$ was 1.83 at $Cl_2$($Cl_2$+Ar gas mixing ratio of 0.2. The surface reaction of the etched $CeO_2$ thin films was investigated using x-ray photoelectron spectroscopy (XPS) analysis. There is a Ce-Cl bonding by chemical reaction between Ce and Cl. The results of secondary ion mass spectrometer (SIMS) analysis were compared with the results of XPS analysis and the Ce-Cl bonding was monitored at 176.15 (a.m.u). These results confirm that Ce atoms of $CeO_2$ thin films react with chlorine and a compound such as CeCl remains on the surface of etched $CeO_2$ thin films. These products can be removed by Ar ion bombardment.

  • PDF

Deposition Of $TiB_2$ Films by High Density Plasma Assisted Chemical Vapor Deposition (고밀도 플라즈마 화학 증착 장치를 이용한 $TiB_2$ 박막 제조)

  • Lee S. H.;Nam K. H.;Hong S. C.;Lee J. J.
    • Journal of the Korean institute of surface engineering
    • /
    • v.38 no.2
    • /
    • pp.60-64
    • /
    • 2005
  • The ICP-CVD (inductively coupled plasma chemical vapor deposition) process was applied to the deposition of $TiB_2$ films. For plasma generation, 13.56 MHz r.f. power was supplied to 2-turn Cu coil placed inside chamber. And the gas mixture of $TiCl_4,\;BCl_3,\;H_2$ and Ar was used for $TiB_2$ deposition. $TiB_2$ films with high hardness (<40 GPa) were obtained at extremely low deposition temperature $(250^{\circ}C)$, and the films hardness increased with ICP power and gas flow ratio of $TiCl_4/BCl_3$. The film structure was changed from (100) preferred orientation to random orientation with increasing RF power. It is supposed that the enhanced hardness of films was caused by a strong Ti-B chemical bonding of stoichiometric $TiB_2$ films and film densification induced by high density plasma.

Electrical Characterization of PZT and Electrodes after Dry Etching in Inductively Coupled plasma (유도결합 플라즈마를 이용한 PZT/전극의 식각 후 전기적 특성)

  • Kim, Kyung-Tae;Kang, Myoung-Gu;Park, Young;Song, Jun-Tae;Lee, Cheol-In;Jang, Eui-Goo;Kim, Chang-Il
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.07a
    • /
    • pp.275-278
    • /
    • 2001
  • Ferroelectric PZT thin films were fabricated on the RuO$_2$/Pt, Pt bottom electrode with a PZT(53/47) metal alkoxide solutions. All PZT thin films showed a uniform grain structure without the presence of rosette structure. The PZT thin films were etched as a function of Cl$_2$/Ar and additive CF$_4$ into Cl$_2$(80%)/Ar(20%). The etch rates of PZT thin films were 1970 ${\AA}$/min at 30 % additive CF$_4$ into Cl$_2$(80%)/Ar(20%). The remanent polarization and leakage current density in PZT thin film on the RuO$_2$/Pt were 64.2 ${\mu}$C/cm$^2$, 1.4${\times}$10$\^$-6/ respectively.