• Title/Summary/Keyword: $Bi_{2212}$

Search Result 198, Processing Time 0.026 seconds

Phase Stability Region of Bi System Superconducting Thin films Fabricated by Ion Beam Sputtering Method with Crucible (도가니를 이용해서 IBS법으로 제작한 Bi계 초전도 박막의 상안정 영역)

  • Yang, Sung-Ho;Kim, Jong-Seo;Park, Yong-Pil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.07b
    • /
    • pp.1204-1207
    • /
    • 2003
  • BiSrCaCuO superconducting thin films have been fabricated by co-deposition using IBS(ion Beam Sputtering) method. Despite setting the composition of thin film Bi2212 or Bi2223, in both cases, Bi2201, Bi2212 and Bi2223 phase were appeared. It was confirmed the obtained field of stabilizing phase was represented in the diagonal direction of the right below end in the Arrhenius plot of temperature of the substrate and $PO_3$, and it was distributed in the rezone.

  • PDF

Effect of External Reinforcement on Stress/Strain Characteristics of Critical Current in Ag Alloy Sheathed Bi-2212 Superconducting Tapes. (Bi-2212 초전도 테이프에서 임계전류의 응력/변형률 특성에 미치는 외부강화의 영향)

  • ;;K. Katagiri
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 2001.02a
    • /
    • pp.17-20
    • /
    • 2001
  • Stress/strain dependencies of the critical current I$_{c}$ in AgMgNi sheathed multifilamentary Bi(2212) superconducting tapes were evaluated at 77K. The external reinforcement was accomplished by soldering Ag-Mg tapes to single side or both sides of the sample. With the external reinforcement, the strength of tapes increased but I$_{c}$ decreased. The I$_{c}$ degradation characteristic according to the external reinforcement was improved markedly in terms of the stress although it appeared less remarkable on the basis of the strain. Effects of external reinforcement were discussed in a viewpoint of monitoring sensitivity of cracking in superconducting filaments by considering n-value representing the transport behavior of the current, which is closely associated with the location of them relative to the voltage-monitoring region in the tape. tape.

  • PDF

Characteristics of BSCCO Superconductor Tube Using Partial Melting Process (부분용융법을 이용한 BSCCO 초전도 튜브 특성)

  • 박용민;장건익
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 2001.02a
    • /
    • pp.25-28
    • /
    • 2001
  • Bi-2212 HTS tube was fabricated by centrifugal forming process(CFP). As a variation of melt casting process(MCP) or centrifugal casting technique, the centrifugal forming process is a flexible method for manufacturing Bi-2212 bulk tubes and has been optimized to achieve smooth surface and uniform thickness. At this process, the slurry was prepared in the mixing ratio of 10:1 between Bi-2212 powder and binder and initially charged into the rotating mold under the speed of 300~450 rpm Heat-treatment was performed at the temperature ranges of 860 ~ $890^{\circ}C$ in air for partial melting. The HTS tube fabricated by centrifugal forming process at $890^{\circ}C$ under the rotating speed of 450 rpm was highly densified and the plate-like grains with more than 20$\mu$m were well oriented along the rotating axis. The measured Tc and Jc at 10K were around 85K and 3,000A/cm2 respectively.

  • PDF

Effect of Processing Factors on Critical Current Density in Bi2212/Ag Wires

  • Kim, Sang-Cheol;Ha, Dong-Woo;Oh, Sang-Soo;Han, Il-Yong;Ha, Hong-Soo;Sohn, Ho-Sang
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1243-1244
    • /
    • 2006
  • Five kinds of double stacked 385 (55 x7) filamentary Bi2212/Ag round wires and 55 filamentary tapes with different Ag ratios (silver area/superconductor area) have been fabricated via PIT method, and the effects of Ag ratio and processing factors on critical current density were studied. The effects of the maximum temperature and average filament diameter on critical current density were also studied. The wire of 0.74 mm diameter having Ag ratio 3.7 showed critical current density of $2,218\;A/mm^2$ at 4.2 K, 0 T.

  • PDF

R-T characteristic of Bi2212 Epitaxial thin films by growth in MgO(100) substrate (MgO(100)기판에 성장시킨 Bi2212 에피택셜 박막의 R-T특성)

  • Yang, Seung-Ho;Lim, Jung-Kwan;Park, Yong-Pil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2006.06a
    • /
    • pp.537-538
    • /
    • 2006
  • BSCCO thin films have been fabricated by epitaxy growth at an ultra-low growth rate. The growth rates of the films was set in the region from 0.17 to 0.27 nm/min. MgO(100) was used as a substrate. In order to appreciate stable existing region of Bi 2212 phase with temperature and ozone pressure, the substrate temperature was varied between 650 and $720^{\circ}C$ and the highly condensed ozone gas pressure ($PO_3$) in vacuum chamber was varied between $2.0{\times}10^{-6}$ and $2.3{\times}10^{-5}\;Torr$.

  • PDF

Superconducting Properties of the Mg-Bi(Pb)SrCaCuO (110 K Phase) Composite System focusing on the Microstructure (Mg가 혼합된 Bi(Pb)SrCaCuO(110 K 상) 고온초전도체의 미세구조에 따른 초전도 특성 변화에 대한 연구)

  • 이정화;최봉수;이민수
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.6
    • /
    • pp.530-538
    • /
    • 2003
  • Samples with the nominal composition, B $i_{1.84}$P $b_{0.34}$S $r_{1.91}$C $a_{2.03}$C $u_{3.06}$ $O_{10+}$$\delta$/ (110 K phase) high $T_{C}$ superconductors containing MgO as an additive were fabricated by a solid-state reaction method. Samples with 5~50 wt% MgO were sintered at 820~86$0^{\circ}C$ for 24 h. The structural characteristics, critical temperature and grain size of the samples with different MgO contents were analyzed by XRD and SEM. As the MgO content increased, the intensity of MgO peaks and ratio of Bi-2212 phase in superconductors were intensified and the proportion of the phase transition from Bi-2223 to Bi-2212 was increased.d.creased.d.

Study on fabrication process of long length of Bi-2223/Ag MTS wires for high critical current (Bi-2223/Ag HTS 장선재의 Ic 특성 향상 공정 연구)

  • 하동우;양주생;황선역;이동훈;최정규;하홍수;오상수;권영길
    • Proceedings of the Korea Institute of Applied Superconductivity and Cryogenics Conference
    • /
    • 2003.02a
    • /
    • pp.105-108
    • /
    • 2003
  • Long length of Bi-2223 superconducting wires were fabricated by stacking, drawing process with different precursor owders and different heat-treatment histories. The precursor powders were 2 kinds of Pb content. And a part of the tapes were experienced pre-annealing process which caused tetragonal structure of Bi-2212 phase to orthorhombic structure of it was during drawing process. We confirmed the transformation of Bi-2212 phase from tetragonal structure to orthorhombic structure and reduction of second phases. We designed and made a continuous Ic measurement system for Bi-2223/Ag HTS tape. We could achieve best Ic of 65 A at the Bi-2223/Ag tape using low Pb content of precursor powder and experienced pre-annealing process.

  • PDF

Analysis of Sticking Coefficient in BSCCO Thin Film (BSCCO 박막의 부착계수 해석)

  • Chun, Min-Woo;Park, Yong-Pil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2002.11a
    • /
    • pp.252-255
    • /
    • 2002
  • BSCCO thin films are fabricated by an ion beam sputtering method, and sticking coefficients of the respective elements are evaluated. The sticking coefficient of Bi element in BSCCO film formation was observed to show a unique temperature dependence; it was almost a constant value of 0.49 below about $730^{\circ}C$ and decreased linearly over about $730^{\circ}C$. In contrast, Sr and Ca, displayed no such remarkable temperature dependence. This behavior of the sticking coefficient was explained consistently on the basis of the evaporation and sublimation processes of $Bi_{2}O_{3}$. It was concluded that Bi(2212) thin film constructs from the partial melted Bi(2201) phase with the aid of the liquid phase of $Bi_{2}O_{3}$.

  • PDF

Bi-sticking Coefficient of Bi-superconducting Thin Film Prepared by IBS Method

  • Lee, Hee-Kab;Lee, Joon-Ung;Park, Yong-Pil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.11a
    • /
    • pp.213-216
    • /
    • 1999
  • BSCCO thin films are fabricated via a co-deposition process by an ion beam sputtering with an ultra-low growth rate, and sticking coefficients of the respective elements are evaluated. The sticking coefficient of Bi element exhibits a characteristics temperature dependence : almost a constant value of 0.49 below 730$^{\circ}C$ and decreases linearly with temperature over 730$^{\circ}C$. This temperature dependence can be elucidated from the evaporation and sublimation rates of bismuth oxide, Bi$_2$O$_3$ from the film surface. It is considered that the liquid phase of the bismuth oxide plays an important role in the Bi(2212) phase formation in the co-deposition process.

  • PDF