$(La_2O_3-B_2O_3-TiO_2)$ 세라믹 조성에서의 미세 조직 과 마이크로 유전체 특성 (Microstructure and Microwave Dielectric Properties of Glass $(La_2O_3-B_2O_3-TiO_2)$/Ceramic Composites)

  • Jung, Byung-Hae;Hwang, Seong-Jin;Han, Tae-Hee;Kim, Hyung-Sun
    • 한국재료학회:학술대회논문집
    • /
    • 한국재료학회 2003년도 추계학술발표강연 및 논문개요집
    • /
    • pp.138-138
    • /
    • 2003
  • Low temperature co-fired ceramic (LTCC) technology offers significant benefits over the other established packaging technologies for high density, high microwave frequency, and fast signal application. Most conventional electroceraramics do not meet the basic requirements in respect of sinterability for LTCC technology. Attention is, therefore, focused on the role of glasses because of the capability they supply with lower sintering temperatures. In this study, commercial ceramic (MBRT-90) in the system BaO-N $d_2$ $O_3$-Ti $O_2$ (BNT: 40 ~ 80 wt%) and L $a_2$ $O_3$- $B_2$ $O_3$-Ti $O_2$ glass (LBT;60 ~ 20 wt%) were prepared. These glass/ceramic composites were evaluated for sintering behavior, phase evaluation, densities, interface reaction, crystallinity, microstructure and microwave dielectric properties. It was found that the addition LBT glass frits significantly lowered the sintering temperature to below 90$0^{\circ}C$ and as temperature increased (750~90$0^{\circ}C$) densification developed dynamically which was meant to be as over 95% of relative density. It is supposed that in the microstructure, the grain size was increased accompanying with the formation of different phases such as LaB $O_3$ and Ti $O_2$ under the condition of increasing sintering temperature. The sintered bodies represented applicable dielectric properties, namely 20 ~ 40 for $\varepsilon_{{\gamma}}$, ~ 10000 GHz for Q* $f_{0}$ and 10~80 ppm/$^{\circ}C$ for $\tau$$_{f}$. The results suggest that the composite is one of feasible candidates for the microwave use in LTCC technology.y.e use in LTCC technology.y.

  • PDF

전신성 홍반성 루푸스 (Systemic lupus erythematosus)

  • 김광남
    • Clinical and Experimental Pediatrics
    • /
    • 제50권12호
    • /
    • pp.1180-1187
    • /
    • 2007
  • Systemic lupus erythematosus (SLE) is an episodic, multi-system, autoimmune disease characterized by widespread inflammation of blood vessels and connective tissues and by the presence of antinuclear antibodies (ANAs), especially antibodies to native (double-stranded) DNA (dsDNA). Its clinical manifestations are extremely variable, and its natural history is unpredictable. Untreated, SLE is often progressive and has a significant fatality rate. The most widely used criteria for the classification of SLE are those of the American College of Rheumatology (ACR), which were revised in 1982 and modified in 1997. The presence of four criteria have been diagnosed as a SLE. Rashes are common at onset and during active disease. The oral mucosa is the site of ulceration with SLE. Arthralgia and arthritis affect most children and these symptoms are short in duration and can be migratory. Lupus nephritis may be more frequent and of greater severity in children than in adults. The initial manifestation of nephritis is microscopic hematuria, followed by proteinuria. The most common neuropsychiatric symptoms are depression, psychosis(hallucination and paranoia) and headache. CNS disease is a major cause of morbidity and mortality. Pericarditis is the most common cardiac manifestation. Libman-Sacks endocarditis is less common in children. The most frequently described pleuropulmonary manifestations are pleural effusions, pleuritis, pneunonitis and pulmonary hemorrhage. During the active phase ESR, CRP, gamma globulin, ferritin and anti-dsDNA are elevated. Antibodies to dsDNA occur in children with active nephritis. Antibodies to the extractable nuclear antigens (Sm, Ro/SS-A, La/SS-B) are strongly associated with SLE. Specific treatment should be individualized and based on the severity of the disease. Sepsis has replaced renal failure as the most common cause of death.

MA법으로 제조된 Ni기 합금에서 Y2O3 첨가에 따른 인장강도변화와 시효처리 효과 (Variation of Tensile Strength by Addition of Y2O3 and Effect of Aging Treatment in Ni Base Alloy Fabricated by MA Method)

  • 김일호;이원식;고세현;장진만;권숙인
    • 한국분말재료학회지
    • /
    • 제15권1호
    • /
    • pp.23-30
    • /
    • 2008
  • Ni-20Cr-20Fe-5Nb alloy with or without $Y_2O_3$ was manufactured by mechanical alloying process and consolidated by spark plasma sintering (SPS). The grain size of the alloy with $Y_2O_3$ was smaller than that of alloy without $Y_2O_3$ which results from the effect of $Y_2O_3$ suppressing grain growth. The tensile strength at room temperature was increased by the addition of $Y_2O_3$ but decreased abruptly at temperature above $600^{\circ}C$. It seems to result from the change of deformation mechanism due to fine grain size, that is, grain boundary sliding is predominant at above $600^{\circ}C$ while internal dislocation movement is predominant at below $600^{\circ}C$. After conventional heat treatment process of solution treatment and aging, a small amount of ${\delta}(Ni_3Nb)$ phase was formed in Ni-20Cr-20Fe-5Nb alloy while a large amount of ${\gamma}"(Ni_3Nb)$ was formed in Inconel 718 in the previous report. This is due to exhaustion of Nb content by the formation of NbC during consolidation.

흡착튜브 - 열탈착 정량분석 기법에 기반한 과일시료로부터 자연적 휘발성유기화합물의 배출특성 연구 (Biogenic Volatile Organic Compounds (BVOC) Emissions from Fruit Samples Based on Sorbent Tube Sampling and Thermal Desorption (ST-TD) Analysis)

  • 안정현;김기현
    • 한국대기환경학회지
    • /
    • 제29권6호
    • /
    • pp.757-772
    • /
    • 2013
  • In this study, a combination of sorbent tube (ST)-thermal desorption (TD)-gas chromatography (GC)-mass spectrometry (MS) was used for quantitative analysis of liquid phase standards of 10 BVOC ((1) (+)-${\alpha}$-pinene, (2) (+)-${\beta}$-pinene, (3) ${\alpha}$-phellandrene, (4) (+)-3-carene, (5) ${\alpha}$-terpinene, (6) p-cymene, (7) (R)-(+)-limonene, (8) ${\gamma}$- terpinene, (9) myrcene, and (10) camphene). The results of BVOC calibration yielded comparatively stable pattern with response factor (RF) of 23,560~50,363 and coefficient of determination ($R^2$) of 0.9911~0.9973. The method detection limit (MDL) of BVOC was estimated at 0.03~0.06 ng with the reproducibility of 1.30~5.13% (in terms of relative standard error (RSE)). Emissions of BVOC were measured from four types of fruit samples ((1) tangerine (TO), (2) tangerine peel (TX), (3) strawberry (SO), and (4) sepals of strawberry (SX)). The sum of BVOC flux (${\sum}flux$ (BVOC) in ng/hr/g) for each sample was seen on the descending order of (1) TX=291,614, (2) TO=2,190, (3) SO=1,414, and (4) SX=2,093. If the results are compared between the individual components, the highest flux was seen from (R)-(+)-limonene (265,395 ng/hr/g) from TX sample.

TonEBP suppresses adipocyte differentiation via modulation of early signaling in 3T3-L1 cells

  • Kim, Soo Jin;Kim, Taehee;Choi, Han Na;Cho, Eun Jung;Park, Jin Bong;Jeon, Byeong Hwa;Lee, Sang Do
    • The Korean Journal of Physiology and Pharmacology
    • /
    • 제20권6호
    • /
    • pp.649-655
    • /
    • 2016
  • TonEBP belongs to the Rel family of transcription factors and plays important roles in inflammation as well as kidney homeostasis. Recent studies suggest that TonEBP expression is also involved in differentiation of several cell types such as myocytes, chondrocytes, and osteocytes. In this study, we investigated the roles of TonEBP during adipocyte differentiation in 3T3-L1 cells. TonEBP mRNA and protein expression was dramatically reduced during adipocyte differentiation. Sustained expression of TonEBP using an adenovirus suppressed the formation of lipid droplets as well as the expression of FABP4, a marker of differentiated adipocytes. TonEBP also inhibited the expression of $PPAR{\gamma}$, a known master regulator of adipocytes. RNAi-mediated knock down of TonEBP promoted adipocyte differentiation. However, overexpression of TonEBP did not affect adipogenesis after the initiation of differentiation. Furthermore, TonEBP expression suppressed mitotic clonal expansion and insulin signaling, which are required early for adipocyte differentiation of 3T3-L1 cells. These results suggest that TonEBP may be an important regulatory factor in the early phase of adipocyte differentiation.

니켈기 초내열합금 분말의 고용화 열처리 후 냉각속도에 따른 크리프특성 분석 (Analyses of Creep Properties of Ni-base Superalloy Powders as Cooling Rate after Solid Solution Heat Treatment)

  • 전찬;이영선;배병범;김홍규;홍성석;김동훈;윤존도;윤은유
    • 한국분말재료학회지
    • /
    • 제23권3호
    • /
    • pp.247-253
    • /
    • 2016
  • In this study, solid solution heat treatment of consolidated nickel-based superalloy powders is carried out by hot isotactic pressing. The effects of the cooling rate of salt quenching, and air cooling on the microstructures and the mechanical properties of the specimens are analyzed. The specimen that is air cooled shows the formation of serrated grain boundaries due to their obstruction by the carbide particles. Moreover, the specimen that is salt quenched shows higher strength than the one that is air cooled due to the presence of fine and close-packed tertiary gamma prime phase. The tensile elongation at high temperatures improves due to the presence of grain boundary serrations in the specimen that is air cooled. On the contrary, the specimen that is salt quenched and consists of unserrated grain boundaries shows better creep properties than the air cooled specimen with the serrated grain boundaries, due to the negative creep phenomenon.

Ca-Ma-Zn 합금계에서 비정질 형성능 및 특성 평가 (Glass Forming Ability and Characteristic Evaluation in Ca-Mg-Zn Alloy System)

  • 박은수;김원태;김도향
    • 한국주조공학회지
    • /
    • 제26권2호
    • /
    • pp.77-84
    • /
    • 2006
  • The effect of alloy composition on the glass forming ability (GFA) of the Ca-rich Ca-Mg-Zn alloys has been investigated in $Ca_{65}Mg_{5+x}Zn_{30-x}$ and $Ca_{55+x}Mg_{15}Zn_{30-x}$ (x=0, 5, 10, 15, 20) alloys. In a wide composition range of 15-25% Zn and 10-20% Mg bulk metallic glass (BMG) samples with the diameter larger than 6 mm are fabricated by conventional copper mold casting method in air atmosphere. Among the alloys investigated, the $Ca_{65}Mg_{15}Zn_{20}$ alloy exhibits the highest GFA enabling to form BMG sample with the diameter of at least 15 mm. The crystalline phase formed during solidification of $Ca_{65}Mg_{15}Zn_{20}$ ($D_{max}=15\;mm$) could be identified as a mixture of $Ca_3Zn$ and $CaMg_2$ cause by the redistribution of the constituent elements on long-range scale. The compressive fracture strength and fracture elongation of the $Ca_{65}Mg_{15}Zn_{20}$ BMG are 602 MPa and 2.08% respectively. The ${\sigma}$ parameter which has been recently proposed for evaluating GFA exhibits better correlation with GFA of Ca-Mg-Zn alloys than other parameters suggested so far such as ${\Delta}T_x$, $T_{rg}$, K, ${\gamma}$, and ${\Delta}T^*$ parameters.

Fe-0.7%C-2.3%Si강의 미세조직과 기계적 성질에 미치는 잔류 오스테나이트 변태 거동 (Transformation Behavior of Retained Austenite on Microstructure and Mechanical Properties in Fe-0.7wt%C-2.3wt%Si Steel)

  • 손제영;권도영;김지훈;김원배;김학진;예병준
    • 한국주조공학회지
    • /
    • 제32권3호
    • /
    • pp.138-143
    • /
    • 2012
  • This steel has been synthesized integrating concepts from Austempering Ductile Cast Iron (ADI) technology. While ADI has excellent mechanical and physical properties, the Young's modules of ADI is approximately 20% lower than steel. In addition, the presence of graphite nodules in ADI can be sites of crack initiation, where fracture takes place at graphite matrix interface. Because of this limitations of ADI, there has been a growing interest in austempered steels as structural materials in resent years. In this investigation, a new steel with microstructure composed of ferrite and austenite and with simultaneous high tensile strength (1,150 MPa) and high ductility (33%) was developed. The goal of this investigation is to obtain a better understanding of deformation and transformation behaviour in high carbon retained austenite(${\gamma}_{HC}$) and over-saturated ferrite(${\alpha}$) during the plastic deformation. A detailed study of the microstructure of this steel was carried out by means of X-ray diffraction (XRD) and electron back scattering diffraction (EBSD) technic. In this way it was shown that BCC phase (BCC) took up the larger part of the nominal strain whereas the a part of retained austenite responded to the mechanincal load by partial martensite transformation, and misorientation change in the retained austenite after plastic strain could be attributed to the large elongation.

Acetaminophen으로 유도한 쥐의 간 독성에 대한 미나리(Oenanthe javanica) 추출액의 간 보호 작용 (Protective Effect of Oenanthe javanica Extract on Acetaminophen-induced Hepatotoxicity in Rats)

  • 박종철;김종연;이윤주;이지선;김보금;이승호;남두현
    • 약학회지
    • /
    • 제52권4호
    • /
    • pp.316-321
    • /
    • 2008
  • The hepatoprotection by the methanol extract of Oenanthe javanica DC (water dropwort) (OJME) was investigated in Sprague Dawley rats with inducing liver damage by acetaminophen. After OJME administration for 1 week, the increase of hepatic lipid peroxide level by acetaminophen-induced hepatotoxicity was significantly reduced. In case of phase I microsomal enzyme systems including cytochrome P-450, aminopyrine N-demethylase and aniline hydroxylase, any significant differences between in control and in OJME-pretreated group was observed after acetaminophen treatment. However, the pretreatment of OJME maintained the hepatic glutathione level and the activity of liver cytosolic glutathione S-transferase, which was significantly decreased by the acetaminophen intoxication. Among the glutathione-generating system, glutathione reductase was more responsible for its biosynthesis rather than ${\gamma}-glutamylcystein$ synthetase. OJME itself showed the strong inhibition activity on DPPH radical generation. In conclusion, OJME administration maintains the liver glutathione pool and hepatic glutathione S-transferase activity, in addition with its high anti-oxidative capability, to show hepatoprotective effect from acetaminophen intoxication.

교류임피던스법에 의한 Nimonic 80A 초내열합금 시효열처리재의 부식거동 고찰 (The Corrosion Behavior Study by AC Impedance Method for the Aging Heat Treated Nimonic 80A Superalloy)

  • 백신영
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제23권6호
    • /
    • pp.761-769
    • /
    • 1999
  • In this paper the effect of aging heat treatment to the Corrosion behavior for the Nimonic 80A superalloy was studied by AC Impedance methods. Tested solution was 3.5% with tempera-ture $25^{\circ}C$ Electro-chemical corrosion test were carried out for the Nimonic 80A super-alloy which solution heat treated at $1080^{\circ}C$ for 8 hours followed by aging heat treated at $650^{\circ}C,\;700^{\circ}C,\;750^{\circ}C\;800^{\circ}C$ and $850^{\circ}C$ with 16hours under vacuum environment. The obtained results were as follows; 1. Base metal and solution-treated materials were exhibited similar corrosion tendency as Ran-dle equivalent cell. The value of passive film resistance was 579 ohms for the base metal and 124,770 ohms for the solutionized metal such a difference was arose by the ${{\gamma}_^'}$ precipitate on the metal surface during heat treatment. 2. The measure value of $R_p$ for heat-treated at $650^{\circ}C,\;700^{\circ}C,\;800^{\circ}C$and $850^{\circ}C$ were 97,943, 93, 111, 26,961, 15,798 and 11,780ohm respectively. Which indicated that the passive film resistance Rp was reduced as aging temperature increased due to the growth of grain size and sensitization at the grain boundary. 3. The similar tendency was exhibited for corrosion behavior of the electro-chemical corrosion polarization method and AC impedance method and confirmed that AC impedance method was useful tool for corrosion research.

  • PDF